• Title/Summary/Keyword: lithium recovery

Search Result 92, Processing Time 0.019 seconds

A Synthesis of LiCoO2 using the CoSO4 Recovered from Cathode Material Scrap and its Electrochemical Properties (폐 리튬 이차전지로부터 회수된 황산코발트 제조 및 이를 이용해 합성된 산화리튬코발트 양극활물질의 전기화학적 특성)

  • Kim, Mi-So;Ha, Jong-Keun;Park, Se-Bin;Ahn, Jou-Hyeon;Choi, Im-Sic;Cho, Kwon-Koo
    • Journal of the Korean Electrochemical Society
    • /
    • v.17 no.2
    • /
    • pp.111-118
    • /
    • 2014
  • The electrochemical properties using the cells assembled with the synthesized $LiCoO_2$(LCO) were evaluated in this study. The LCO was synthesized from high-purity cobalt sulfate($CoSO_4$) which is recovered from the cathode scrap in the wastes lithium ion secondary battery(LIB). The leaching process for dissolving the metallic elements from the LCO scrap was controlled by the quantities of the sulfuric acid and hydrogen peroxide. The metal precipitation to remove the impurities was controlled by the pH value using the caustic soda. And also, D2EHPA and $CYANEX^{(R)}272$ were used in the solvent extraction process in order to remove the impurities again. The high-purity $CoSO_4$ solution was recovered by the processes mentioned above. We made the 6 wt.% $CoSO_4$ solution mixed with distilled water. And the 6 wt.% $CoSO_4$ solution was mixed with oxalic acid by the stirring method and dried in oven. $LiCoO_2$ as a cathode material for LIB was formed by the calcination after the drying and synthesis with the $Li_2CO_3$ powder. We assembled the cells using the $LiCoO_2$ powders and evaluated the electrochemical properties. And then, we confirmed possibility of the recyclability about the cathode materials for LIBs.

Optimization of Characteristic Change due to Differences in the Electrode Mixing Method (전극 혼합 방식의 차이로 인한 특성 변화 최적화)

  • Jeong-Tae Kim;Carlos Tafara Mpupuni;Beom-Hui Lee;Sun-Yul Ryou
    • Journal of the Korean Electrochemical Society
    • /
    • v.26 no.1
    • /
    • pp.1-10
    • /
    • 2023
  • The cathode, which is one of the four major components of a lithium secondary battery, is an important component responsible for the energy density of the battery. The mixing process of active material, conductive material, and polymer binder is very essential in the commonly used wet manufacturing process of the cathode. However, in the case of mixing conditions of the cathode, since there is no systematic method, in most cases, differences in performance occur depending on the manufacturer. Therefore, LiMn2O4 (LMO) cathodes were prepared using a commonly used THINKY mixer and homogenizer to optimize the mixing method in the cathode slurry preparation step, and their characteristics were compared. Each mixing condition was performed at 2000 RPM and 7 min, and to determine only the difference in the mixing method during the manufacture of the cathode other experiment conditions (mixing time, material input order, etc.) were kept constant. Among the manufactured THINKY mixer LMO (TLMO) and homogenizer LMO (HLMO), HLMO has more uniform particle dispersion than TLMO, and thus shows higher adhesive strength. Also, the result of the electrochemical evaluation reveals that HLMO cathode showed improved performance with a more stable life cycle compared to TLMO. The initial discharge capacity retention rate of HLMO at 69 cycles was 88%, which is about 4.4 times higher than that of TLMO, and in the case of rate capability, HLMO exhibited a better capacity retention even at high C-rates of 10, 15, and 20 C and the capacity recovery at 1 C was higher than that of TLMO. It's postulated that the use of a homogenizer improves the characteristics of the slurry containing the active material, the conductive material, and the polymer binder creating an electrically conductive network formed by uniformly dispersing the conductive material suppressing its strong electrostatic properties thus avoiding aggregation. As a result, surface contact between the active material and the conductive material increases, electrons move more smoothly, changes in lattice volume during charging and discharging are more reversible and contact resistance between the active material and the conductive material is suppressed.