6mm$^{t}$ 조선용 Primer코팅강판의 $CO_2$레이저 용접성 (III) - X-선 투과영상시스템에 의한 결함형성거동의 리얼타임관찰 - (The Weldability of 6mm$^{t}$ Primer-coated Steel for Shipbuilding Using $CO_2$ Laser (III) - Real-time X-ray Imaging Observation of Defect Formation of Laser Welding -)

  • 김종도;박현준;이종봉;김영식
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.103-105
    • /
    • 2004
  • 키홀 용접현상에 관한 연구는, 키홀 현상이 용융금속내부에서 아주 빠른 속도로 과도적으로 이루어지기 때문에 그 계측과 해석이 곤란하여 수 많은 가정이나 가설 하에서 용입형상과 키홀의 거동에 관한 해석이 국한된 영역에서 이루어지고 있는 것이 현실이다. (중략)

  • PDF

펄스 Nd:YAG 레이저에 의한 브라운관 부품의 용접시 빔의 출력특성과 광학변수 (Characteristics of Output Energy and Optical Parameters in Welding of Braun Tubes by Pulsed Nd:YAG Laser)

  • 김종도;하승협
    • 한국레이저가공학회지
    • /
    • 제8권1호
    • /
    • pp.27-37
    • /
    • 2005
  • During laser spot welding of the braun tube electron gun, phenomena such as serious spattering and oxidative reaction, etc. were occurred. The spatter occurred from weld pool affects the braun tube, namely it blocks up a very small hole on the shadow mask and causes short circuit between two poles of the electron gun. We guessed that high power density and oxidative reaction are main sources of these problems. So, we studied to prevent and to reduce spatter occurring in spot welding of the braun tube electron gun using pulsed Nd:YAG laser. The characteristics of laser output power was estimated, and the loss of laser energy by optical parameter and spatter was measured by powermeter. The effects of welding parameters, laser defocused distance and incident angle, were investigated on the shape and penetration depth of the laser welded bead in flare and flange joints. From these results, the laser peak power was a major factor to control penetration depth and to occur spatter. It was found that the losses of laser energy by optic parameter and sticked spatter affect seriously laser weldability of thin sheets.

  • PDF

스테인레스 박강판의 레이저 점 용접 시 음향방출 실시간 모니터링 (Acoustic Emission Monitoring during Laser Spot Welding of Stainless Steel Sheets)

  • 이성환;최정욱;최장은
    • 한국정밀공학회지
    • /
    • 제22권4호
    • /
    • pp.60-67
    • /
    • 2005
  • Compared with conventional welding, laser spot welding offers a unique combination of high speed, precision and low heat distortion. This combination of advantages is attractive for manufacturing industries including automotive and electronics companies. In this paper, a real time monitoring scheme fur a pulsed Nd:YAG laser spot welding was suggested. Acoustic emission (AE) signals were collected during welding and analyzed for given process conditions such as laser power and pulse duration. A back propagation artificial neural network, with AE frequency content inputs, was used to predict the weldability of stainless steel sheets.

리튬이온전지의 전해액 주입구 볼에 대한 Nd:YAG 레이저 용접성 (The Weldability of Aluminum Ball in Electrolyte Injection Hole by Nd:YAG Laser)

  • 김종도;유승조;김장수
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제30권6호
    • /
    • pp.740-745
    • /
    • 2006
  • This study suggested the occurrence source of weld-defects and its solution methods in a welding of Electrolyte injection hole by pulsed Nd:YAG laser. In experiment, the ramp down was used in order that solidification crack was removed. Furthermore. shrinkage stress and heat input were reduced by changing of weld trajectory and defocused distance. As a results of a experiment, a sound weld bead shape and crack-free weld bead can be obtained. In conclusion this show that the welding stability is greatly affected by modulation of laser pulse shape for the same laser energy and welding parameters.

고출력 레이저에 의한 이종금속 용접특성 (Welding characteristics of Dissimilar Metal by High Power Laser)

  • 신호준;유영태;임기건;안동규
    • 한국공작기계학회:학술대회논문집
    • /
    • 한국공작기계학회 2004년도 추계학술대회 논문집
    • /
    • pp.250-256
    • /
    • 2004
  • For many years and primarily for economical reasons, Dissimilar Metal Welds have been used as transition joints in a variety of equipment and applications. But Dissimilar Metal Welds have several fabrication and metallurgical drawbacks that can often lead to in-service failures. In this paper, the laser weldability of STS304 stainless steel and SM45C at dissimilar metal welds using a continuous wave Nd:YAG laser are experimentally investigated. An experimental study was conducted to determine effects of welding parameters, on eliminating or reducing the extent welding zone formation at dissimilar metal welds and to optimize those parameters that have the most influence parameters such as focus length, power, beam speed, shielding gas, and wave length of laser were tested.