• Title/Summary/Keyword: klason lignin

Search Result 23, Processing Time 0.022 seconds

Chemical Composition and Alkaline Pulping of a Stem of Red Pepper (Capsium annuum L.) (고추 줄기의 화학 조성분 및 알칼리 펄프화)

  • Kim, Chul Hyun;Kim, Young Yook;Park, Soung Bae;Eom, Tae Jin
    • Journal of the Korean Wood Science and Technology
    • /
    • v.32 no.2
    • /
    • pp.26-32
    • /
    • 2004
  • Chemical compositions and chemical structure of lignin and alkali cooking condition and fiber length of red pepper were investigated and compared to those of woods. The chemical compositions of red pepper were higher component of extraction than that of wood. The contents of carbon and hydrogen of Klason lignin in red pepper were similar to that of pine and birch wood. On the other hand, the contents of oxygen and nitrogen of Klason lignin in the red pepper were higher than that of wood. The result of nitrobenzene oxidation shows that Klason lignin of red pepper was similar to lignin of softwood. The best alkali cooking condition of red pepper was 0.2%-anthraquinone, active alkali of 20% and liquor ratio of 1:7. The fiber length of red pepper was about 0.47 mm. Therefore, the red pepper fiber will be able to use special purpose of short fiber.

Lignin Degradation of Pine Wood by Unidentified Decay Fungi and Observation by Scanning Electron Microscope (미동정 부후균에 의한 소나무재의 Lignin 분해와 주사전자현미경(SEM)을 이용한 관찰)

  • Park, Heon;Min, Kyeong-Heui
    • Journal of the Korean Wood Science and Technology
    • /
    • v.31 no.4
    • /
    • pp.71-80
    • /
    • 2003
  • The lignin degrading fungi were isolated from decayed woods and fruiting bodies gathered in forest area. Lignin degradation ability was investigated by Klason lignin of microbial treated pine wood. Among selected fungi, CJ-6 had 49.48% Klason lignin loss which was greater than 40.58% shown by Trametes versicolor that it is known as a typical lignin degrading fungus. Also, the biodegradation process and morphological features of degraded pine wood by selected fungi were observed with the scanning electron microscope. At the stage of 20 days incubation, mycelia invasion was observed without any failure of wood structure. At 60 days, wood decay was gone in some degree and one part of tracheid and ray wall was destroyed. At 100 days, tracheid wall was severely destroyed, and distinction between ray cell was difficult as cell wall was decayed much.

Screening and Evaluating of Wood-Rotting Fungi for Lignin Degradation and Ligninolytic Enzyme Production(I) - Screening of High Active Lignin-Degrading Fungi - (리그닌분해(分解)와 리그닌분해효소(分解酵素) 생산(生産)을 위한 목재부후균(木材腐朽菌)의 선발(選拔)과 평가(評價)(I) - 고활성(高活性) 리그닌분해균(分解菌)의 선발(選拔) -)

  • Jung, Hyun-Chae;Park, Seur-Kee;Kim, Byeong-Soo;Park, Chong-Yawl
    • Journal of the Korean Wood Science and Technology
    • /
    • v.23 no.4
    • /
    • pp.108-116
    • /
    • 1995
  • This experiment was conducted to screen a superior wood-rotting fungi for lignin degradation and ligninolytic enzyme production by evaluation of red colored zone width on potato-dextrose agar medium and oak woodmeal medium complimented guaiacol. Relationship between the red colored zone width on GU-WA medium and klason lignin loss on woodmeal medium showed the positive correlation. Thus, the potential ligninolytic activity of wood rotting fungi which are not elucidated yet may be estimated to some extent by the evaluation of the red colored zone width on GU-WA medium. Of the isolates screened from fruit bodies and decayed woods. LKY-12, LKY-7 and C. versicolor-13 isolates having preferential lignin degradation and laccase activity were selected. These isolates exhibited characteristics of superior wood-rotting fungi as Klason lignin loss ranged from 30% to 35% and ligninolytic enzyme activity of these isolates on glucose-peptone broth was higher than that of other isolates. And then, these isolates were considered to be able to use in biological pulping and bleaching and ligninolytic enzyme production.

  • PDF

Anatomical, Chemical, and Topochemical Characteristics of Transgemic Poplar Down-regulated with O-methyltransferase

  • Wi, Seung Gon;Lee, Kwang Ho;Park, Byung Dae;Park, Young Goo;Kim, Yoon Soo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.32 no.3
    • /
    • pp.15-24
    • /
    • 2004
  • The present work was undertaken to investigate the anatomical and chemical characteristics of transgenic poplar down-regulated with antisense OMT gene. Also the distribution of lignin in transgenic poplar trees was investigated at cellular level. No visible abnormal phenotype was observed in the fibers and vessel elements of transgenic poplar. Any marked differences in the staining intensities of Wiesner and Mäule color reaction were not identified in the transgenic poplar. TEM micrographs did not show any staining intensities in the cell walls stained with KMnO4. Interestingly, the UV spectroscopy of semi-thin sections exhibited a distinct decrease of lignin absorption at 280 nm in the vessel walls, indicating transgenic poplar wood with lower amount of guaiacyl lignin in vessel elements. Chemical composition of antisense OMT poplar was almost identical to that of wild-type poplar. Klason lignin content of transgenic poplar did not show any significant difference from that of the controls. The solid state NMR spectra revealed the transgenic poplar with only slightly more syringyl lignin than the control. The present work showed that antisense OMT gene constructed in the poplar was not enough to reduce the overall content of Klason lignin, and suggested that the expression of transformation was confined to vessel walls.

Effect of Delignification Treatment after Autohydrolysis on Yields of Cellulosic Substrates, Lignin Contents, and Enzymatic Hydrolysis (목분(木粉)의 Autohydrolysis후(後) 탈리그닌처리(處理)가 섬유소기질(纖維素基質)의 수율(收率), 리그닌함량(含量)과 효소가수분해(酵素加水分解)에 미치는 영향(影響))

  • Park, Jong-Moon;Ahn, Won-Yung;Shin, Dong-So
    • Journal of the Korean Wood Science and Technology
    • /
    • v.12 no.4
    • /
    • pp.19-30
    • /
    • 1984
  • This experiment was carried out to investigate the effects of autohydrolysis and extraction conditions on the separation of the chemical substances, the extractability of lignin by dioxane, and the yield of reducing sugars from cellulosic substrates by using a commercial cellulase derived from Trichoderma viride. Air-dried wood meals through 0.42mm (40 mesh) screen and retained on 0.25 mm (60 mesh) of Populus alba-glandulosa and Pinus koraiensis were autohydrolyzed with water at $180^{\circ}C$ for 30 and/or 60 minutes in a 6 liter stainless-steel digester with or without 2% 2-naphthol. The hydrothermally-treated wood meals were extracted the lignin with 100%, 90%, 75% and 50% dioxane solutions at $70^{\circ}C$ for 4 hours, respectively. The results obtained were as follows; 1) After autohydrolysis of Populus alba-glandulosa, the yield of wood meals decreased with lengthening the auto hydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. In case of Pinus koraiensis, the yield was not affected by 2%, 2-naphthol addition at the autohydrolysis in the digester. 2) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the yield of wood meals decreased with lengthening the autohydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. Extraction of 50% dioxane solution was the best solvent for the yield among the solutions of 100%, 90%. 75% and 50% dioxane. In case of Pinus koraiensis, the yield was not affected by 2% 2-naphthol addition and the solution of 90% dioxane was the poorest solvent for the yield. 3) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the Klason lignin content in cellulosic substrates for enzymatic hydrolysis decreased with lengthening the autohydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. Klason lignin content was the lowest after extraction by 90% or 75% dioxane solution. The content was also affected by interaction of the three factors-autohydrolysis time, 2% 2-naphthol addition and concentration of dioxane. In case of Pinus koraiensis, the Klason lignin content increased with 2% 2-naphthol addition but was not affected by the concentration of dioxane solution. 4) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the extractable Klason lignin content by extraction increased with lengthening the auto hydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. The extractable lignin content was the highest after extraction by 90% or 75% dioxane solution. In case of Pinus koraiensis, the extractable lignin content increased with 2% 2-naphthol addition. Extractions by 100%, 90% and 50% dioxane solutions were more effective for the extraction of Klason lignin than by 75% dioxane solution. 5) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the yield of reducing sugars increased with lengthening the autohydrolysis time from 30 minutes to 60 minutes but was not affected by 2% 2-naphthol addition and the concentration of dioxane. The yield of reducing sugars after enzymatic hydrolysis was slightly higher by extractions with 90%, 75% and 50% dioxane solutions than with 100% dioxane. In case of Pinus koraiensis, the yield of reducing sugars was not affected by 2% 2-naphthol addition but affected by the concentration of dioxane. The yield of reducing sugars was the highest in cellulosic substrates extracted by 100% dioxane solution.

  • PDF

The Enzymatic Hydrolysis of Exploded Woody Biomass(I) -Effects of Lignin Contents and Cellulose Crystallinity on the Enzymatic Hydrolysis- (폭쇄처리(爆碎處理)된 목질계(木質系) Biomass의 산소가수분해(酸素加水分解)(I) -리그닌의 함량(含量)과 섬유소(纖維素)의 결정화도(結晶化度)가 산소가수분해(酸素加水分解)에 미치는 영향)

  • Park, Young-Ki;Oh, Jung-Soo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.21 no.3
    • /
    • pp.53-60
    • /
    • 1993
  • Substrates used were hardwood-Suwon poplar-(Populus alba${\times}$glandulosa L.) and softwood-pitch pine-(Pinus rigida M.). And these substrates were steam exploded then treated with sodium chlorite at 75$^{\circ}C$ with occasional stirring in order to obtain samples which had different lignin contents and crystallinity. And then this resulting samples incubated with a commercial cellulase derived from Trichoderma ressei. The contents of Klason lignin were decreased as the increasing of the ratio of sodium chlorite in the two species. The effect of hardwood was more effective than that of softwood in the same ratio of sodium chlorite. The minimum contents of Klason lignin were 0.8% and 5.1% respectively. And the crystallinities of cellulose were increased very little as increasing of the ratio of sodium clorite. The hydrolysis extent of the two species were increased as the increasing of delignification. Especially, the hydrolysis extent of hardwood was more higher than that of softwood. The maximum hydrolysis extent were 89.8% and 71.1%, respectively.

  • PDF

Impact of Residual Extractives and Hexenuronic Acid on Lignin Determination of Kraft pulps

  • Shin Soo Jeong;Schroeder Leland R;Lai Yuan Zong
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.36 no.5 s.108
    • /
    • pp.62-68
    • /
    • 2004
  • The amount of non-lignin components in unbleached and oxygen-delignified kraft pulps and their impact on lignin determinations was investigated. The lignin analyses investigated were kappa number and Klason lignin in conjunction with acid-soluble lignin. The species investigated were loblolly pine, and aspen. The non-lignin components that impacted on lignin determination were residual extractives and hexenuronic acid in unbleached and oxygen-delignified kraft pulps. In the hardwoods, significant amounts of extractives remained after kraft pulping and oxygen delignification. These residual extractives in the hardwood pulps had an impact on the lignin determination, more so on the acid lignin method than kappa number. Hexenuronic acid only impacts on kappa number determination both softwood and hardwood pulps, not on acid lignin. Hexeneuronic acid contributed as lignin content more in aspen than pine pulps, and more in oxygen-delignified than unbleached kraft pulps. Impact of hexenuronic acid on should be corrected both softwood and hardwood pulps for accurate kappa number.

Relationship between Lignin Content and the Durability of Wood Pellets Fabricated Using Larix kaempferi C. Sawdust

  • Yang, In;Jeong, Hanseob;Lee, Jae Jung;Lee, Soo Min
    • Journal of the Korean Wood Science and Technology
    • /
    • v.47 no.1
    • /
    • pp.110-123
    • /
    • 2019
  • This work was conducted to examine the relationship between lignin content and the durability of larch (LAR) pellets. LAR sawdust was immersed in tap water (TW), sulfuric acid (AC) and sodium hydroxide (AK) solutions, and then the immersed sawdust was used for pellet fabrication. Klason lignin (KL) content of the immersed LAR, contents of soluble lignin (SL) and monomeric sugars liberated from the immersion of LAR, and durability of LAR pellets were measured. KL content decreased as the concentration of AC and AK solutions increased, but glucose content increased with increase in AC and AK concentration. Durability of wood pellets fabricated using non-immersed LAR sawdust was the highest, followed by those made using TW-, AK- and AC-immersed sawdust. LAR pellets became more durable as the concentration of KL and SL increased, but a significant positive correlation was found only between pellet durability and KL content. Through the fluorescent microscopic observation and SEM-EDX analysis, it was verified that lignin content of non-immersed LAR pellets was higher than that of AC- and AK-immersed LAR pellets. These results suggest that lignin might contribute to an increase in inter-particle bonding in wood pellets.

Comparative study of some analytical methods to quantify lignin concentration in tropical grasses

  • Velasquez, Alejandro V.;Martins, Cristian M.M.R.;Pacheco, Pedro;Fukushima, Romualdo S.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • v.32 no.11
    • /
    • pp.1686-1694
    • /
    • 2019
  • Objective: Lignin plays a relevant role in the inhibition of cell wall (CW) structural carbohydrate degradation. Thus, obtaining accurate estimates of the lignin content in tropical plants is important in order to properly characterize the mechanism of lignin action on CW degradation. Comparing conflicting results between the different methods available for commercial use will bring insight on the subject. This way, providing data to better understand the relationship between lignin concentration and implications with tropical forage degradation. Methods: Five grass species, Brachiaria brizantha cv $Marand{\acute{u}}$, Brachiaria brizantha cv $Xara{\acute{e}}s$(MG-5), Panicum maximum cv Mombaça, Pennisetum purpureum cv Cameroon, and Pennisetum purpureum cv Napier, were harvested at five maturity stages. Acid detergent lignin (ADL), Klason lignin (KL), acetyl bromide lignin (ABL), and permanganate lignin (PerL) were measured on all species. Lignin concentration was correlated with in vitro degradability. Results: Highly significant effects for maturity, lignin method and their interaction on lignin content were observed. The ADL, KL and ABL methods had similar negative correlations with degradability. The PerL method failed to reliably estimate the degradability of tropical grasses, possibly due to interference of other substances potentially soluble in the $KMnO_4$ solution. Conclusion: ADL and KL methods use strong acid ($H_2SO_4$) and require determination of ash and N content in the lignin residues, therefore, increasing time and cost of analysis. The ABL method has no need for such corrections and is a fast and a convenient method for determination of total lignin content in plants, thus, it may be a good option for routine laboratory analysis.

Chemical Characteristics of Cell Wall in Pinus thunbergii Parl. Grown with High Salinity (고염분 하에서 성장한 해송 세포벽의 화학 성상)

  • Kim, Kang-Jae;Eom, Tae-Jin
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.47 no.4
    • /
    • pp.144-150
    • /
    • 2015
  • Stems of Pinus thunbergii Parl. grown with high salinity were analyzed for chemical characteristics. Stem of 2 years was rich in soluble compounds and stem of 3 years reduced the amount of the soluble compound. But, the lignin content have not seen a large change. Also, Klason lignins of stem of 2 and 3 years has not changed in nitrogen and hydrogen content. In Klason process, it was significantly increased the carbon concentration due to the hydrolysis of the carbohydrate. In addition, the accumulation of xylan from Pinus thunbergii Parl. with salinity treatment were increased noticeably. Finally, functional group of Pinus thunbergii Parl. with salinity treatment were not changed.