• Title/Summary/Keyword: irreversible flux loss

Search Result 3, Processing Time 0.02 seconds

High Coercive Nd-Fe-B Sintered Magnets for High Temperature Application

  • Kim, D.H.;Kim, A.S.;Lim, T.H.;Jang, T.S.
    • Journal of Magnetics
    • /
    • v.14 no.1
    • /
    • pp.27-30
    • /
    • 2009
  • Various sintered magnets containing $28{\sim}31\;wt%$ Nd and $0{\sim}7\;wt%$ Dy were evaluated for coercivity and irreversible flux loss as a preliminary study to develop highly-coercive, high-temperature magnets that can be applied for driving motors in a hybrid vehicle. The sintered magnets were prepared in sequence of strip casting, HD treatment, jet milling, magnetic field pressing, sintering and post-annealing. Increasing Dy content and adjusting post-annealing temperature monotonically increased coercivity of magnets from about 14 kOe to 30 kOe. A magnet containing 28 wt% Nd and 7 wt% Dy exhibits a $(BH)_{max}$+$_i{H_c}$ value of almost 64. This is very close to what the automobile industry considers as the minimum value (65) for a hybrid vehicle system. Moreover, irreversible flux loss of the magnet was about 3% at $200^{\circ}C$, which is well less than the allowable limit (5%) to a driving motor in hybrid vehicles.

A Study on the Iron Loss and Demagnetization Characteristics of an Inset-type Flux-Reversal Machine

  • Kim, Tae Heoung
    • Journal of Magnetics
    • /
    • v.18 no.3
    • /
    • pp.297-301
    • /
    • 2013
  • Flux-reversal machine (FRM) is cost effective and suitable for mass production due to its simple structure. However, there is a notable permanent magnet flux leakage which deteriorates the performance. To compensate this drawback with a design method, an Inset-Permanent-Magnet-Type FRM (ITFRM) has been proposed. The ITFRM has permanent magnets perpendicular to the stator teeth surface, and thus, is much more difficult to demagnetize. In this paper, we deal with the iron losses and irreversible permanent magnet demagnetization characteristics of the ITFRM according to various design variables and driving conditions. To analyze the characteristics, a two-dimensional finite-element method (2D-FEM) considering nonlinear analysis of permanent magnets is used. As a result, we propose the design variables that have the largest effects on the iron losses and irreversible magnet demagnetization.

Practical Calculation of Iron Loss for Cylindrical Linear Machine

  • Jeong, Sung-In
    • Journal of Electrical Engineering and Technology
    • /
    • v.13 no.5
    • /
    • pp.1901-1907
    • /
    • 2018
  • This paper is a study for accurate iron loss calculation of a cylindrical linear machine for free piston engine. This study presents that it is possible to accurately predict power loss in ferromagnetic laminations under magnetic flux by specially considering the dependence of hysteresis, classical, and excess loss components on the magnetic induction derivative. Significant iron loss in the armature core will not only compromise the machine efficiency, but may also result in excessive heating, which could lead to irreversible deterioration in the machine performance. Thus, correct prediction of power losses under a distorted flux waveform is therefore an important prerequisite to machine design, particularly when dealing with large apparatus where stringent efficiency standards are required. Finally, it will be discussed about the iron loss in various materials of cylindrical linear electric machine by geometric and electrical parameters. It will give elaborate information about the perfect design and design rules of cylindrical linear machine and in parallel tools for the calculation, simulation and design will be available.