수분사 Fe 분말의 산화물 및 이의 수소가스 환원거동 (Hydrogen Reduction Behavior of Oxide Scale in Water-atomized Iron Powder)

  • 신해민;백경호
    • 한국분말재료학회지
    • /
    • 제21권6호
    • /
    • pp.422-428
    • /
    • 2014
  • In this study, the reduction kinetics and behaviors of oxides in the water-atomized iron powder have been evaluated as a function of temperature ranging $850-1000^{\circ}C$ in hydrogen environment, and compared to the reduction behaviors of individual iron oxides including $Fe_2O_3$, $Fe_3O_4$ and FeO. The water-atomized iron powder contained a significant amount of iron oxides, mainly $Fe_3O_4$ and FeO, which were formed as a partially-continuous surface layer and an inner inclusion. During hydrogen reduction, a significant weight loss in the iron powder occurred in the initial stage of 10 min by the reduction of surface oxides, and then further reduction underwent slowly with increasing time. A higher temperature in the hydrogen reduction promoted a high purity of iron powder, but no significant change in the reduction occurred above $950^{\circ}C$. Sequence reduction process by an alternating environment of hydrogen and inert gases effectively removed the oxide scale in the iron powder, which lowered reduction temperature and/or shortened reduction time.

Enhance degradation of insecticide chlorpyrifos by iron salts and potassium persulfate during zerovalent iron treatment in aqueous solution

  • Rahman, M. Mokhlesur;Hwang, Jung-In;Kwak, Se-Yeon;Kim, Jang-Eok
    • Journal of Applied Biological Chemistry
    • /
    • 제61권4호
    • /
    • pp.383-389
    • /
    • 2018
  • Degradation of the insecticide O,O-diethyl O-3,5,6-trichloro-2-pyridyl phosphorothioate (chlorpyrifos) in aqueous solution was investigated using iron salts and potassium persulfate during ZVI treatment through a series of batch experiments. The degradation rate of chlorpyrifos increased with increases in the concentrations of iron salts and potassium persulfate in the aqueous system. Ferric chloride was found to be the most effective iron salt for the ZVI-mediated degradation of chlorpyrifos in aqueous solution. Further, the iron salts tested could be arranged in the following order in terms of their effectiveness: $FeCl_3$> $Fe_2(SO_4)_3$> $Fe(NO_3)_3$. The persulfate-ZVI system could significantly degrade chlorpyrifos present in the aqueous medium. This revealed that chlorpyrifos degradation by treatment with $Fe^0$ was promoted on adding ferric chloride and potassium persulfate. The kinetics of the degradation of chlorpyrifos by persulfate-amended $Fe^0$ was higher than that for iron-salt-amended $Fe^0$. This suggests that using a sequential $Fe^0$ reduction-ferric chloride or $Fe^0$ reduction-persulfate process may be an effective strategy to enhance the removal of chlorpyrifos in contaminated water.

개질 영가철을 이용한 산성 및 염기성 염료의 탈색 특성 (Decolorization Characteristics of Acid and Basic Dyes Using Modified Zero-valent Iron)

  • 최정학;김영훈
    • 한국환경과학회지
    • /
    • 제25권12호
    • /
    • pp.1717-1726
    • /
    • 2016
  • In this study, the reductive decolorization of three acid and basic dyes using modified zero-valent iron (i.e., acid-washed iron (Aw/Fe) and palladium coated iron (Pd/Fe)) at various pH conditions (pH 3~5) was experimentally investigated and the decolorization characteristics were evaluated by analyzing the absorbance spectra and reaction kinetics. In the case of acid dyes such as methyl orange and eriochrome black T, color removal efficiencies increased as initial pH of the dye solution decreased. However, the color removal of methylene blue, a basic dye, was not affected much by the initial pH and more than 70% of color was removed within 10 min. During the decolorization reaction, the absorbance of methyl orange (${\lambda}_{max}=464nm$) and eriochrome black T (${\lambda}_{max}=528nm$) decreased in the visible range but increased in the UV range. The absorbance of methylene blue (${\lambda}_{max}=664nm$) also decreased gradually in the visible range. Pseudo-zero order, pseudo-first order, and pseudo-second order kinetic models were used to analyze the reaction kinetics. The pseudo-second order kinetic model was found to be the best with good correlation. The decolorization reaction rate constants ($k_2$) of methylene blue were relatively higher than those of methyl orange and eriochrome black T. The reaction rate constants of methyl orange and eriochrome black T increased with a decrease in the initial pH.

금속 철을 이용한 TNT의 환원시의 동역학 산정 (Kinetics of 2,4,6-Trinitrotoluene reduction by zero valent iron)

  • 배범한
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 1999년도 정기총회 및 춘계 공동 학술발표회
    • /
    • pp.62-63
    • /
    • 1999
  • Reduction 2,4,6-Trinitrotoluene by zero valent iron was studied in a batch reactor under anoxic conditions. Results showed that the removal of TNT was a pseudo-first order and the rate was dependent on the available metal surface area. Final product, presumably triaminotoluene, accumulated in the solution as well as on the metal surface. However, little amounts of aminodinitrotoluenes were detected. Therefore, it is postulated that the reduction of nitro group occurs simultaneously in all three position.

  • PDF

Supported Iron Nanoparticles on Activated Carbon, Polyethylene and Silica for Nitrate Reduction

  • Cho, Mi-Sun;Kim, E-Wha;Lee, Kyoung-Hee;Ahn, Sam-Young
    • 한국환경과학회지
    • /
    • 제17권7호
    • /
    • pp.711-717
    • /
    • 2008
  • The use of support materials on the nanoparticle synthesis and applications has advantages in many aspects; resisting the aggregation and gelation of nanoparticles, providing more active sites by dispersing over the supports, and facilitating a filtering process. In order to elucidate the influence of the supports on the nitrate reduction reactivity, the supported iron nanoparticles were prepared by borohydride reduction of an aqueous iron salt in the presence of supports such as activated carbon, silica and polyethylene. The reactivity for nitrate reduction decreased in the order of unsupported Fe(0) > activated carbon(AC) supported Fe(0) > polyethylene(PE) supported Fe(0) ${\ge}$ silica supported Fe(0). Rate constants decrease with increasing initial nitrate concentration implying that the reaction is limited by the surface reaction kinetics.

Sintering of Cobalt - (3-25 wt.%) Iron Materials

  • Romanski, Andrzej
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1126-1127
    • /
    • 2006
  • The kinetics of sintering of Co-Fe materials was studied. The main objective was to establish the effects of iron content and sintering parameters on the microstructure and phase composition of the as-sintered material. Specimens containing from 3 to 25 wt.% iron were sintered in a dilatometer for one hour at 900, 1000 and $1150^{\circ}C$ in either hydrogen or nitrogen atmosphere. The length of specimens during the heating, hold at temperature and cooling steps were monitored to establish the sample's shrinkage. Microstructural observations were carried out on polished and etched transverse sections which were also subjected to the X-ray phase analysis.

  • PDF

Comparison of Bioleaching Kinetics of Spent Catalyst by Adapted and Unadapted Iron & Sulfur Oxidizing Bacteria - Effect of Pulp Density; Particle Size; Temperature

  • Pradhan, Debabrata;Kim, Dong-Jin;Ahn, Jong-Gwan;Gahan, Chandra Sekhar;Chung, Hun-Saeng;Lee, Seoung-Won
    • 대한금속재료학회지
    • /
    • 제49권12호
    • /
    • pp.956-966
    • /
    • 2011
  • Bioleaching studies of metals from a spent catalyst were conducted using both adapted and unadapted bacterial cultures. The bacterium used in this experiment was Acidithiobacillus ferrooxidans. A comparison of the kinetics of leaching was made between the two cultures by varying the leaching parameters, including the pulp density, particle size and temperature. Both cultures showed similar effects with respect to the above parameters, but the leaching rates of all metals were higher with the adapted compared to the unadapted bacterial cultures. The leaching reactions were continued for 240 h in the case of the unadapted bacterial culture, but only for 40 h in the case of the adapted bacterial culture. The leaching reactions followed first order kinetics. In addition, the kinetics of leaching was concluded to be a diffusion control model; therefore, the product layers were impervious.

니켈로 코팅된 영가금속을 이용한 염소계 페놀화합물의 반응경로 및 반응율 평가 (Reductive Degradation Kinetics and Pathways of Chlorophenolic Organic Pollutants by Nickel-Coated Zero Valent Iron)

  • 신승철;김영훈;고석오
    • 대한환경공학회지
    • /
    • 제28권5호
    • /
    • pp.487-493
    • /
    • 2006
  • 본 연구에서는 지하수에 존재하는 다양한 클로로페놀류 화합물을 제거하기 위하여 니켈로 코팅된 영가철을 이용하여 적용 타당성을 검토하였다. 다섯가지 종류의 클로로페놀 화합물을 대상으로 처리효과를 평가하였으며 중간 생성물을 분석하였다. 실험결과를 이용하여 개질된 영가철에 의한 반응경로 및 반응율을 평가하기 위하여 수치해석적 방법을 적용하였다. 개질된 영가철에 의한 오염물의 제거는 반응계수를 기준으로 2-CP>4-CP>2,4-DCP>2,4,6-TCP>2,6-DCP의 순서를 나타내었다. 수치해석 결과 각 클로로페놀 화합물의 탈염소화 반응은 연속적 단계와 평행적 단계를 거쳐 최종 생성물인 페놀화합물에 도달되는 결과를 보여주었다.

Effect of Minerals surface characteristics On Reduction Dehalogenation of chlorination solvents in water-FeS/FeS$_2$ system

  • 김성국;허재은;박세환;장현숙;박상원;홍대일
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 2000년도 창립총회 및 춘계학술발표회
    • /
    • pp.108-111
    • /
    • 2000
  • FeS/FeS$_2$ minerals have been known to be potentially useful reductant to the removal of common organic contaminants in groundwater and soil. This research is aimed at improving our understanding of factors affecting the pathways and rates of reductive transformation of Hexachloroethane by catalytical iron minerals in natural system. Hexachloroethane is reduced by FeS/FeS$_2$ minerals under anaerobic condition to tetrachloroethylene and trichloroethylene with pentachloroethyl radical as the intermediate products. The kinetics of reductive transformations of the Hexachloroethane have been investigated in aqueous solution containing FeS, FeS$_2$. The proposed reduction mechanism for the adsorbed nitrobenzene involves the electron donor-acceptor complex as a precursor to electron transfer. The adsorbed Hexachloroethane undergo a series of electron transfer, proton transfer and dehydration to achieve complete reduction. It can be concluded that the reductive transformation reaction takes place at surface of iron-bearing minerals and is dependent on surface area and pH. Nitrobenzene reduction kinetics is affected by reductant type, surface area, pH, the surface site density, and the surface charge. FeS/FeS$_2$-mediated reductive dechlorination may be an important transformation pathway in natural systems.

  • PDF