• 제목/요약/키워드: in-situ reaction synthesis

검색결과 75건 처리시간 0.019초

기계적 합금화과정에서의 in situ 열분석에 의한 Ti-25.0~37.5at%Si 분말의 합성거동 (Synthesis Behavior of Ti-25.0~37.5at%Si Powders by In situ Thermal Analysis during Mechanical Alloying)

  • 변창섭;현창용;김동관
    • 한국재료학회지
    • /
    • 제14권5호
    • /
    • pp.305-309
    • /
    • 2004
  • Mechanical alloying (MA) of Ti-25.0~37.5at%Si powders was carried out in a high-energy ball mill, and in situ thermal analysis was also made during MA. In order to classify the synthesis behavior of the powders with respect to at%Si, the synthesis behavior during MA was investigated by in situ thermal analysis and X-ray diffraction (XRD). In situ thermal analysis curves and XRD patterns of Ti-25.0~26.1at%Si powders showed that there were no peaks during MA, indicating $Ti_{5}$ $Si_3$ was synthesised by a slow reaction of solid state diffusion. Those of Ti-27.1~37.5at%Si powders, however, showed that there were exothermic peaks during MA, indicating $_Ti{5}$ $Si_3$ and$ Ti_3$Si phase formation by a rapid exothermic reaction of self-propagating high-temperature synthesis (SHS). For Ti-27.1~37.5at%Si powders, the critical milling times for SHS decreased from 38.1 to 18.5 min and the temperature rise, ΔT (= peak temperature - onset temperature) increased form $19.5^{\circ}C$ to $26.7^{\circ}C$ as at%Si increased. The critical composition of Si for SHS reaction was found to be 27.1at% and the critical value of the negative heat of formation of Ti-27.1at%Si to be -1.32 kJ/g.

Ti기 (TiC+TiB) 하이브리드 복합재료 반응생성합성 및 정밀주조 (In-situ Synthesis and Investment Casting of Titanium Matrix (TiC+TiB) Hybrid Composites)

  • 성시영;박근창;이상화;김영직
    • 한국주조공학회지
    • /
    • 제24권3호
    • /
    • pp.159-164
    • /
    • 2004
  • The aim of the present work is to investigate the possibility of in-situ synthesis and net-shape forming of the titanium matrix (TiC+TiB) hybrid composites using a casting route. From the scanning electron microscopy, electron probe micro-analyzer, X-ray diffraction and thermodynamic calculations, the spherical TiC and needle like TiB reinforced hybrid titanium matrix composites could be obtained in-situ by the conventional melting and casting route between titanium and $B_4C$. No melt-mold reaction occurred between the titanium matrix (TiC+TiB) hybrid composites and the SKK mold, since the mold is consisted with interstitial and substitutional metal-mold reaction products. Not only the sound in-situ synthesis but also the economic net-shape forming of the titanium matrix (TiC+TiB) hybrid composites could be possible by the conventional casting route.

기계적 합금화과정에서의 in situ 열분석에 의한 Ti-50.0~66.7at%Si 분말의 합성거동 (Synthesis Behavior of Ti-50.0 ~ 66.7at%Si Powders by In situ Thermal Analysis during Mechanical Alloying)

  • 변창섭;이상호;이원희;현창용;김동관
    • 한국재료학회지
    • /
    • 제14권5호
    • /
    • pp.310-314
    • /
    • 2004
  • Mechanical alloying (MA) of Ti-50.0~66.7at%Si powders was carried out in a high-energy ball mill, and in situ thermal analysis was also made during MA. In order to classify the synthesis behavior of the powders with respect to at%Si, the synthesis behavior during MA was investigated by in situ thermal analysis and X-ray diffraction (XRD). In situ thermal analysis curves and XRD patterns of Ti-50.0~59.6at%Si powders showed that there were exothermic peaks during MA, indicating TiSi, $TiS_2$, and $Ti_{5}$ $Si_4$ phase formation by a rapid exothermic reaction of self-propagating high-temperature synthesis (SHS). Those of Ti-59.8~66.7 at%Si powders, however, showed that there were no peaks during MA, indicating any Ti silicide was not synthesised until MA 240 min. For Ti-50.0~59.6at%Si powders, the critical milling times for SHS increased from 34.5 min to 89.5 min and the temperature rise, $\Delta$T (=peak temperature-onset temperature) decreased form $26.2^{\circ}C$ to $17.1^{\circ}C$ as at%Si increased. The critical composition of Si for SHS reaction was found to be 59.6at% and the critical value of the negative heat of formation of Ti-59.6at%Si to be -1.48 kJ/g.

Ti-Al-C 합금의 고온 자전 합성 반응시 생성상에 관한 연구 (A Study on the Formation Phase of Self-propagating High-temperature Synthesis of Ti-Al-C alloys)

  • 문종태
    • 한국분말재료학회지
    • /
    • 제2권2호
    • /
    • pp.149-157
    • /
    • 1995
  • In this study, an attempt was made to fabricate TiAl as well as its in situ composite via combustion synthesis. The processing variable of the combustion synthesis which include aluminum content and the heating rate were found to affect the combustion temperature. The combustion temperature measured, however, was lower than the melting temperature of TiAl and the reaction product were found to include incomplet reaction products. Carbon was added in order to increase the combustion temperature as well as to form in situ reinforcements. The reaction products showed homogeneous microstructures with carbide phases formed within indicating that the addition of carbon increased the combustion temperature above the melting temperature of TiAl.

  • PDF

Reaction Synthesis and Mechanical Properties of $B_4C$-based Ceramic Composites

  • Han, Jae-Ho;Park, Sang-Whan;Kim, Young-Do
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1080-1081
    • /
    • 2006
  • In this investigation, $B_4C$ based ceramic composites were fabricated by in-situ reaction hot pressing using $B_4C$, TiC SiC powder as starting materials. The reaction synthesized composites by hot pressing at $1950^{\circ}C$ was found to posses very high relative density. The reaction synthesized $B_4C$ composites comprise $B_4C$, $TiB_2$, SiC and graphite by the reaction between TiC and $B_4C$. The newly formed $TiB_2$ and graphite was embedded both inside grain and at grain boundary $B_4C$. The mechanical properties of reaction synthesized $B_4C-TiB_2-SiC$-graphite composites were more enhanced compared to those of monolithic $B_4C$.

  • PDF

Hybrid Solar Cells with Polymer/Fullerene Bulk Heterojunction Layers Containing in-situ Synthesized CdS Nanocrystals

  • Kwak, Eunjoo;Woo, Sungho;Kim, Hwajeong;Kim, Youngkyoo
    • Current Photovoltaic Research
    • /
    • 제2권4호
    • /
    • pp.152-156
    • /
    • 2014
  • We report hybrid solar cells fabricated with polymer/fullerene bulk heterojunction layers that contain inorganic nanocrystals synthesized by in-situ reaction in the presence of polymer chains. The inorganic (cadmium sulfide) nanocrystal ($CdS_{NC}$) was generated by the reaction of cadmium acetate and sulfur by varying the reaction time up to 30 min. The synthesized $CdS_{NC}$ showed a rectangular flake shape, while the size of $CdS_{NC}$ reached ca. 150 nm when the reaction time was 10 min. The performance of hybrid solar cells with $CdS_{NC}$ synthesized for 10 min was better than that of a control device, whereas poor performances were measured for other hybrid solar cells with $CdS_{NC}$ synthesized for more than 10 min.

난류 용탕 In-Situ 합성법을 위한 스태틱 믹서의 형상에 따른 혼합 효과 (Mixing Effect by the Geometry of Static Mixer with Turbulent In-Situ Mixing Process)

  • 이대성;김효근;하만영;박용호;박익민
    • 대한기계학회논문집B
    • /
    • 제29권12호
    • /
    • pp.1307-1312
    • /
    • 2005
  • Turbulent in-situ mixing process is a new material process technology to get dispersed phase in nanometer size by controlling reaction of liquid/liquid, liquid/solid and liquid/gas, flow and solidification speed simultaneously. In this study mixing, the key technology to this synthesis method will be studied by computational fluid dynamics. For the simulation of mixing of liquid metal, static mixers will be investigated. Two inlets for different liquid metal meet and merge like 'Y' shape tube. The tube has various shapes such as straight and curved. Also, the radius of curve will be varied. The performance of mixer will be evaluated with quantitative analysis with coefficient of variance of mass fraction. Also, detailed plots of intersection will be presented to understand effect of mixer shape on mixing.

자전연소합성법 및 교반주조 공정으로 제조된 TiC/Mg 금속복합재료의 특성연구 (Characterization of TiC/Mg Composites Fabricated by in-situ Self-propagating High-temperature Synthesis followed by Stir Casting Process)

  • 이은경;조일국
    • Composites Research
    • /
    • 제33권5호
    • /
    • pp.256-261
    • /
    • 2020
  • 본 연구에서는 Al-Ti-C 반응계의 점화온도에 대해 고찰하고, 자전연소합성법 및 교반주조 공정을 통해 TiC/Mg 금속복합재료를 제조하여 미세조직 및 기계적 특성을 분석하였다. 0, 10, 20, 30 vol.% TiC 입자가 균일하게 분산된 Mg 복합재료를 제조하였고, 강화재의 양이 증가할수록 기지 대비 우수한 압축강도 및 내마모특성을 보였다. 이는 in-situ 자전연소합성법에 의해 결함이나 불순물 등의 오염이 적은 TiC/Mg 금속복합재료 제조로 기지에서 강화재로의 효과적인 하중 전달에 의한 것으로 판단된다.

기계적 압금화에 의한 $MoSi_2$-TiC 복합분말의 제조 (Fabrication of $MoSi_2$-TiC Composite Powders by Mechanical Alloying)

  • 윤종열
    • 한국분말재료학회지
    • /
    • 제6권2호
    • /
    • pp.178-185
    • /
    • 1999
  • MoSi$_2$-TiC composite powders were fabricated by in-situ reaction through mechanical alloying. Also the monolithic MoSi$_2$ as well as TiC were synthesiced by mechanical alloying for comparison. An abrupt increase of vial surface temperature was detected due to a sudden reaction between elemental powders during milling. The reaction time for synthesis of composite powders decreased with increasing the content of (Ti+C) powder. It was found that a significant decrease of Ti grain size was observed with increasing the milling time. And the synthesis reaction of MoSi$_2$-TiC composite powders were largely dependent on the reaction between Ti and C powders.

  • PDF