A Study on the Bio-Based Polyurethane (바이오 폴리우레탄에 관한 연구)

  • Ko, Jong-Sung;Lee, Jin-Hui;Sung, Ki-Chun
    • Journal of the Korean Applied Science and Technology
    • /
    • v.29 no.3
    • /
    • pp.531-542
    • /
    • 2012
  • The thesis covers the trend of research on bio-based polyurethane which is made from polyols derived mainly from plant oils and isocyanates. Castor oil is a triglyceride of ricinoleic acid containing hydroxyl group. Hydroxylation is done on the unsaturated bonds of the oils by the reactions of epoxidation/ring opening, hydroformylation/hydrogenation, ozonolysis/hydrogenation, and thiol-ene reaction. Polyols from hyperbranch, primary alcohol, polysaccharide have been studied to control the reactivity of the polyol and morphology of the microdomains. Besides, researches cover biodegradable polylactic acid polyol for medical use, fatty acid dimer polyol for the prevention of hydrolysis, and polyol with ionic group for water-borne polyurethane. Bio-based polyurethanes are being used in flexible and rigid foams, coatings, sealants, and elastomers.

Synthesis and Properties of Hyperbranched Liquid Crystalline Polyesters by Direct Polycondensation (직접중축합법에 의한 하이퍼브랜치 액정 폴리에스터의 합성 및 성질)

  • Park, Jong-Ryul;Kim, Hye-Mi;Yoon, Doo-Soo;Sohn, Jeong Sun;Bang, Moon-Soo
    • Applied Chemistry for Engineering
    • /
    • v.28 no.2
    • /
    • pp.237-244
    • /
    • 2017
  • Hyperbranched liquid crystalline polymers with azomesogenic and cholesteryl groups in their terminal positions were designed and synthesized by direct polycondensation reaction. The chemical structures and thermal and mesomorphic properties of the synthesized polymers were investigated by FT-IR, $^1H-NMR$, differential scanning calorimetry (DSC), thermogravimetry analysis (TGA), and polarizing optical microscopy (POM). The inherent viscosities (${\eta}_{inh}$) of the polymers were measured to be between 0.30 and 0.50 dL/g in phenol/p-chlorophenol/1,1,2,2-tetrachloroethane (25/40/35 = w/w/w). The degree of branching (DB) in these polymers ranged from 0.37 to 0.75; they, as amorphous polymer, showed glass transition temperatures ranging from 80 to $120^{\circ}C$; the polymers readily dissolved in most of the organic solvents used in the experiments. Only hyperbranched polymers with a cholesteryl group as their mesogenic group showed liquid crystalline phases.