A Study on change in thermal properties and chemical structure of Zr-Ni delay system by aging (노화에 따른 Zr-Ni계 지연관의 열 특성 및 화학적 구조 변화에 관한 연구)

  • Park, Byung Chan;Chang, Il Ho;Kim, Sun Tae;Hwang, Taek Sung;Lee, Seungho
    • Analytical Science and Technology
    • /
    • v.22 no.4
    • /
    • pp.285-292
    • /
    • 2009
  • It has been observed that, after long term storage, some ammunitions are misfired by tamping (combustionstopping) due to aging of the chemicals loaded in the ammunitions. Used in ammunitions are percussion powder which provides the initial energy, igniter which ignites the percussion powder, and a delay system that delays the combustion for a period of time. The percussion powder is loaded first, followed by the igniter and then the delay system, and the ammunitions explode by the energy being transferred in the same order. Tamping occurs by combustion-stopping of the igniter or insufficient energy transfer from the igniter to the delay system or the combustion-stopping of the delay system, which are suspected to be caused by low purity of the components, inappropriate mixing ratio, size distribution of particulate components, type of the binder, blending method, hydrolysis by the humidity penetrated during the long term storage, and chemical changes of the components by high temperature. Goal of this study is to find the causes of the combustion-stopping of the igniter and the delay system of the ammunitions after long term storage. In this study, a method was developed for testing of the combustion-stopping, and the size distributions of the particulate components were analyzed with field-flow fractionation (FFF), and then the mechanism of chemical change during long term storage was investigated by thermal analysis (differential scanning calorimetry), XRD (X-ray diffractometry), and XPS (X-ray photoelectron spectroscopy). For the ignition system, M (metal)-O (oxygen) and M-OH peaks were observed at the oxygen's 1s position in the XPS spectrum. It was also found by XRD that $Fe_3O_4$ was produced. Thus it can be concluded that the combustion-stopping is caused by reduction in energy due to oxidation of the igniter.