Influence of ground pumice powder on the bond behavior of reinforcement and mechanical properties of self-compacting mortars

  • Benli, Ahmet;Karatas, Mehmet;Sastim, M. Veysel
    • Computers and Concrete
    • /
    • v.20 no.3
    • /
    • pp.283-290
    • /
    • 2017
  • The aim of this study is to investigate the effect of the bond strength of self-compacting mortars (SCMS) produced from ground pumice powder (GPP) as a mineral additive. In this scope, six series of mortars including control mix were prepared that consist of 7%, 12%, 17%, 22% and 27% of ground pumice powder by weight of cement. A total of 54 specimens of $40{\times}40{\times}160mm$ were produced and cured at the age of 3, 28 and 90-day for compressive and tensile strength tests and 18 specimens of $150{\times}150{\times}150mm$ mortar were prepared and cured at 28 days for bond strength tests. Flexural tensile strength and compressive strength of $40{\times}40{\times}160mm$ specimens were measured at the curing age of 7, 28 and 90-day. Mini V-funnel flow time and mini slump flow diameter tests were also conducted to obtain rheological properties. As a result of the study, it was observed that the SCMs containing 12% of GPP has the highest bond strength as compared to control and GPP mortars. Compressive strength slightly increased up to 12% of GPP.

Mechanical properties of SFRHSC with metakaolin and ground pumice: Experimental and predictive study

  • Saridemir, Mustafa;Severcan, Metin Hakan;Celikten, Serhat
    • Steel and Composite Structures
    • /
    • v.23 no.5
    • /
    • pp.543-555
    • /
    • 2017
  • The mechanical properties of steel fiber reinforced high strength concrete (SFRHSC) made with binary and ternary blends of metakaolin (MK) and ground pumice (GP) are investigated in this study. The investigated properties are ultrasonic pulse velocity ($U_{pv}$), compressive strength ($f_c$), flexural strength ($f_f$) and splitting tensile strength ($f_{st}$) of SFRHSC. A total of 16 steel fiber reinforced concrete mixtures were produced by a total binder content of $500kg/m^3$ for determining the effects of MK and GP on the mechanical properties. The design $f_c$ was acquired from 70 to 100 MPa by using a low water-binder ratio of 0.2. The test results exhibit that high strength concrete can be obtained by replacing the cement with MK and GP. Besides, correlations between these results are executed for comprehending the relationship between mechanical properties of SFRHSC and the strong correlations are observed between these properties. Moreover, two models in the gene expression programming (GEP) for predicting the $f_c$ of SFRHSC made with binary and ternary blends of MK and GP have been developed. The results obtained from these models are compared with the experimental results. These comparisons proved that the results of equations obtained from these models seem to agree with the experimental results.

Interpretation of volcanic eruption types from granulometry and component analyses of the Maljandeung tuff, Ulleung Island, Korea (울릉도 말잔등응회암의 입도와 구성원 분석으로부터 화산분화 유형 해석)

  • Hwang, Sang Koo;Lee, So-Jin;Han, Kee Hwan
    • Journal of the Geological Society of Korea
    • /
    • v.54 no.5
    • /
    • pp.513-527
    • /
    • 2018
  • We have carried out granulometry and component analysis on pyroclastic deposits of the Maljandeung Tuff, Ulleung Island, to interpret the eruption types and prime dynamic mechanisms. It is divided into three members in the extracaldera area, each of which comprises the lithofacies of coarse tuffs and lapillistones in the lower part, and pumice deposits in upper one. The lithofacies present quantitative evidences in the granularity and component distribution patterns. As compared to the pumice deposits, the coarse tuffs and lapillistones exhibit a relative increase in both the lithic/juvenile and the crystal/juvenile ratios, and a preferential fragmentation of the juvenile fraction. The abundance of lithics and crystals in the tuffs and lapillistones can be attributed to preferential fragmentation of the aquifer-hosting rocks due to explosive evaporation of ground water, and indirect enrichment in lithics and crystals due to removal of juvenile fines from eruptive cloud. The above data exhibit that early phreatopmagmatic phase was followed by purely magmatic fragmentation phases. The coarse tuffs and lapillistones suggest phreatoplinian eruption derived from explosive interaction of magma with ground water near the conduit, while pumice deposits indicate magmatic eruption by magmatic explosion from juvenile gas pressure. In early stage, phreatoplinian eruption occurred from explosive magma/water interaction in connecting confining water with drawdown of the magma column in the conduit; Later it shifted to plinian eruption by explosive expansion of only magmatic volatiles in intercepting water influx due to higher magmatic gas pressure than confining water pressure with rising of the magma column in the conduit.

THE INFLUENCE OF THE DEGREE OF SATURATION OF ACIDULATED BUFFER SOLUTIONS IN THE ROOT DENTIN DEMINERALIZATION (유기산 완충용액의 포화도가 상아질의 탈회에 미치는 영향)

  • Kang Hye-Sil;Lee Chan-Young
    • Restorative Dentistry and Endodontics
    • /
    • v.29 no.5
    • /
    • pp.454-461
    • /
    • 2004
  • The purpose of this study is to compare and to evaluate the effects of the degree of saturation on the progression of artificial root caries lesion. A total of 8 human premolars without any defects and cracks selected and the cementum were removed and the teeth were cleaned with ultrasonic device and pumice without fluoride. Each tooth was sectioned into 6 pieces and they were ground with #800 sandpaper until they had a thickness of 200pm. Specimens were applied with nail vanish except for the 2-3 mm window area after application of bonding agent. Under the constant pH, the specimens were divided into 6 groups (degree of saturation: 0.1415, 0.1503, 0.1597, 0.1676, 0.1771. 0.1977). Each group was immersed in acid buffer solution for 1. 2, 3, 5 days under controlled temperature ($25^{\circ}C$) and imbibed in water and examined using the polarizing microscope. The results were as follows 1. Although the degree of saturation of demineralization solution decreased, the depth of penetration in the dentin was constant. 2. Erosion was observed on the surface of all the teeth in the group I, II. In the group III, IV, V, surfaces were not changed. The teeth in the group VI showed the more mineralized surface but not the shape of the dentinal tubules distinctively. 3. In all groups, the lesion progressed rapidly at the first day of the experiment, but increased gradually as time elapsed.

A Study on the Traditional Costumes and Tattoo of the Maori (마오리族 傳統 服飾과 文身 考察)

  • 황춘섭;정현주
    • The Research Journal of the Costume Culture
    • /
    • v.3 no.2
    • /
    • pp.241-260
    • /
    • 1995
  • The Maori's traditional clothing materials, basic forms of dress, and the pattern and technique of tatoo were examined in the present study in order to deepen the appreciation of the cultural heritage of the Maori. The research method employed was the analysis of written materials. And a fild-trip was also made for the study. The study was limitted to the traditional culture of body adornment of the Maori including the clothing which is preserved and practicing by them at the present day, and the origin and the process of the historical development of those are not included in the scope of the present study. Followings are the results of the study: (1) By far the most widely used fiber for Maori clothing is abtained from what is commonly called New Zealand Flax. The fiber of kiekie(Freycinetia baueriana) and cabbage trees(Cordyline spp.) may also be used. The strong, long-lasting fiber of toi(cordyline indivisa) is used for a prestige warrior's cloak. Flat strips of ti kauka(Cordyline australi) are also used as thatch on rain cloaks. (2) Regardless of technique used, Maori weaving is always worked horizontally from left to right. Traditionally the work was suspended between two upright turuturu or weaving sticks. As the work progressed a second pair of uprights was used to keep the work off the ground. These uprights were moved forward as required. Because the weaver sat on the ground, the working edge was kept at a height that was comfortable to reach. No weaving tools are used, the wefts(aho) being manipulated by the fingers. The two main Maori weaving techniques are whatu aho patahi(single-pair twining) and whatu aho rua(double-pair twining). (3) The Maori wore two basic garments - a waist met and a cloak. The cloth of commoners were of plain manufacture, while those of people of rank were superior, sometimes being decorated with feather or dyed tags and decorated borders. Children ran more-or-less naked until puberty, being dressed only for special events. Some working dress consisted of nothing more than belts with leaves thrust under them. Chiefs and commoners usually went barefoot, using rough sandals on journeys over rough country (4) The adornment of men and women of rank was an important matter of tribal concern as it was in chiefly persons that prestige of the group was centred, The durable items of Maori persons adornment were either worn or carried. Ornaments of various kinds were draped about the neck or suspended from pierced earlobes. Combs decorated the head. Personal decorations not only enhanced the appearance of men and women, but many had protective magical function. The most evident personal ornament was the hei-tiki made of jade or other material. Maori weapons were treasured by their owners. They served on bottle and were also personal regalia. A man of rank was not fully dressed without a weapon in hand. Also weapons were essential to effective oratory. (5) No man or woman of rank went without some tattoo adornment except in extremely rare instances when a person was too sacred to have any blood shed. The untattooed were marked as beeing commoners of no social standing. This indelible mark of rank was begun, with appropriate rite and ritual, at puberty. And tattoo marked the person as being of a marriageable age. Maori tattoo was unlike most traditional tattoo in that its main line were 'engraved' on the face with deep cuts made by miniature bone chisels. The fill-in areas were not tattooed with cuts but with the multiple pricks of small bone 'combs' that only lightly penetrated the skin surface. The instrument of tattoo consisted of small pots of pumice or wood into which was placed a wetted black pigment made from burnt kauri gum, burnt vegetable caterpillars or other sooty materials. A bird bone chisel or comb set at right angles on a short wooden handle was dipped into the gigment, that a rod or stick was used to tap head of this miniature adze, causing penetration of the skin surface. Black pigment lodged under the skin took on a bluish tinge. A full made facial tattoo consisted of major spirals with smaller spirals on each side of the nose and sweeping curved lines radiating out from between the brows over the forehead and from the nose to the chin. The major patterns were cut deep, while the secondary koru patterns were lightly pricked into the skin.

  • PDF