Many researchers have studied the eutectic solidification of CV Graphite Cast Iron qualitatively. However quantative studies have not been done. The type of eutectic solidification of CV Graphite Cast Iron treated with CG Alloy (Fe-Si-Mg-5Ti-Ca-Ce) was studied quantitatively through M.D.E. value (Mushy Degree of Eutectic Solidification) = $t_2/t_1)$, where $t_1$ is the difference of the eutectic solidification starting time between surface and center part of the casting sample, and $t_2$ is the time of eutectic solidification of the center part. Following results were obtained. (1) The M.D.E. value of CV graphite cast iron lies between that of spheroidal graphite and that of flake graphite cast iron but is closer to that of Flake graphite cast iron. (2) The M.D.E. value of CV graphite cast iron depends upon CV ratio. (3) The time required for eutectic solidification increases as graphite form is changed from Flake, CV. to spheroidal graphite. (4) The M.D.E. value increases as cooling rate increases.
The effect of bronze sintered friction materials on frictional and mechanical properties is studied with the content(8~18 wt,%) and shapes (flake and irregular) of graphite that is used as solid lubricants to meet diverse characteristics such as low coefficient of friction, low wear rate and high bending strength. The content and shapes of graphite are optimized by statistical experiments. Friction test was carried out measure friction coefficient, temperature dependence and wear rate. As a result of experiments, the density, hardness and bending strength with a shape of flake graphite are lower and decrease rapidly than that of Irregular, as the content of graphite increases up to 18 wt% Aftei friction test, coefficient of friction is 0.3~0 4 and wear rate is $0.32{\sim}2.98{\times}10^{-7}cm^3/kg{\cdot}m$. When the content of graphite increases, coefficient of friction increases In a shape of flake graphite and decreases in a shape of irregular graphite.
CV graphite cast iron has been studied and generally known to have properties close to the average values of those between flake and spheroidal graphite cast iron. However, the thermal diffusivity of CV graphite cast iron is much larger than that of the average value of those between flake and spheroidal graphite cast iron. In this study, an easy production method of CV graphite cast iron with small additions of a Al-Cu which is known as the element of the graphitization was investigated. The effects of hold time and of Al-Cu additions after the treatments with spheroidizer (Fe-Si-Mg alloy) were also investigated. Increasing the additions of a Al-Cu alloy, the holding time to form a CV graphite cast iron was decreasing. Tensile strength and thermal diffusivity (flash method) were measured in order to find the changes of the mechanical properties and the physical properties. Spheroidal, CV, and flake graphite cast iron have tensile strengths 46.44, 38.29, and $27.29\;kg/mm^2$ and thermal diffusivities $3.95{\times}10^{-6,}$$8.41{\times}10^{-6}$, $8.81{\times}10^{-6}m^2/sec$, respectively at room temperature.
This study aims to establish the fundamental basis for the design of materials used in high-speed trains, by using a lab-scale dynamometer to evaluate the characteristic behavior of metallic sintered friction materials in relation to the shape of graphite. The test results clearly demonstrate that when flake graphite and granular graphite are added equivalently, the average coefficient of friction is much lower, and it is less influenced by speed variation; moreover, friction wear is observed to be insignificantly low. Adding flake graphite increases the coefficient of friction, which leads to higher friction wear. In addition, the roughness of the disc surface was equivalent regardless of the shape of the graphite.
It is well known that the graphite flakes become spherulite, when a suitable amount of nodulizing element, such as cerium or magnesium, is added to the cast iron. The change of graphite from flake to nodular shape improves not only the tensile strength but the ductility as well. However, the mechanism of spheroidization of graphite in cast iron has not yet been clearly understood, and various theories proposed by a number of investigators were such that it may be due to the special nucleation effect, prevention of flake formation by the adsorption of magnesium vapour on the graphite surface or file surface free energy difference between plain graphite and magnesium-adsorbed graphite. Regardless of the speculations of spheroidizing mechanism of the graphite in the cast iron, the final phenomenon comes to the conclusion that it may be due to the lack of wettability between graphite and iron matrix. In order to collaborate this fact through an experimental method, the authors have constructed a vacuum arc furnace for the wettability measurement as its first step. Our study and experiments were then directed to the comparison of the wettability between iron and graphite on the two cases (namely, the one where magnesium was preliminarily coated on the graphite surface and the other not coated), by means of contact angle measurements. The result was such that a significant difference of the contact angles has been shown between the above two cases. indicating the spheroidization of graphite which might have resulted from the lack of wettability between magnesium-adsorbed graphite and iron matrix.
The effect of the microstructure of gray cast iron on friction properties was investigated by using a pad-on-disk type friction tester. Cast iron samples used in this investigation were obtained from "step block" castings, which were designed to produce microstructure with different graphite flake morphologies from different cooling rate and solidification rate. Results of this work showed that the gray cast iron disks with long graphite flakes showed less fading. The rotors containing smaller amounts of ferrite showed higher friction coefficient and better fade resistance than others.an others.
Two different types of graphite, such as flake graphite (FG) and spherical graphite (SG), were used as anode materials for a lithium-ion secondary battery in order to investigate their electrochemical performance. The FG particles were prepared by pulverizing natural graphite with a planetary mill. The SG particles were treated by immersing them in acid solutions or mixing them with various carbon additives. With a longer milling time, the particle size of the FG decreased. Since smaller particles allow more exposure of the edge planes toward the electrolyte, it could be possible for the FG anodes with longer milling time to deliver high reversible capacity; however, their initial efficiency was found to have decreased. The initial efficiency of SG anodes with acid treatments was about 90%, showing an over 20% higher value than that of FG anodes. With acid treatment, the discharge rate capability and the initial efficiency improved slightly. The electrochemical properties of the SG anodes improved slightly with carbon additives such as acetylene black (AB), Super P, Ketjen black, and carbon nanotubes. Furthermore, the cyclability was much improved due to the effect of the conductive bridge made by carbon additives such as AB and Super P.
The effects of Mn content and cooling rate on the eutectic reaction of flake graphite cast irons were studied by a combined analysis of macro/micro-structure and cooling curve data. The correlation between the eutectic reaction parameter and macro/microstructure was systematically investigated. Two sets of chemical compositions with different Mn contents were designed to cast. Three types of molds for cylindrical specimens with different diameters were prepared to analyze the cooling rate effect. The difference between undercooling temperature and cementite eutectic temperature (${\Delta}T_1=T_U-T_{E,C}$), which is decreased by increasing the Mn content or increasing the cooling rate, is considered to be a suitable eutectic reaction parameter for predicting graphite morphology. According to the criterion, A-type graphite is mainly suggested to form for ${\Delta}T_1$ over $20^{\circ}C$, and D-type graphite is mainly suggested to form for ${\Delta}T_1$ below $0^{\circ}C$. Eutectic reaction time (${\Delta}T$), which is increased by increasing the Mn content and decreased by increasing the cooling rate, is regarded as a suitable eutectic reaction parameter for predicting eutectic cell size. Eutectic cell size is found to decrease in proportion to the decrease of ${\Delta}T$.
The effects of rare earth element (R.E.) and cooling rate on the eutectic reaction of flake graphite cast irons were studied by combined analysis of macro/micro-structure and cooling curve data. The correlation between eutectic reaction parameter and macro/micro-structure was systematically investigated. Two sets of chemical compositions with the different addition of R.E. were designed to cast. Three types of molds for cylindrical specimens with the different diameters were prepared to analyze cooling rate effect. The difference between undercooling temperature and cementite eutectic temperature (${\Delta}T_1=T_{U}-T_{E,C}$), which is increased by adding R.E. and decreased by increasing cooling rate, is considered to be a suitable eutectic reaction parameter for predicting graphite morphology. According to the criterion, A-type graphite is mainly suggested to form for ${\Delta}T_1$ over $20^{\circ}C$. Eutectic reaction time (${\Delta}t$), which is decreased by adding R.E. or increasing cooling rate, is a suitable eutectic reaction parameter for predicting eutectic cell size. Eutectic cell size is found to decrease in a proportion to the decrease of ${\Delta}t$.
Influence of frictional and mechanical properties was studied with the content(8-18 wt.%) and shapes(flake of irregular) of graphite that was used as lubricant components of copper-based sintered materials. The density, hardness and bending strength of friction materials with the shape of flake graphite were lower and decreased rapidly than that of irregular, as the content of graphite increases up to 18 wt.%. In friction test, wear rate was about 2.0-$2.5{\times}10^{-7}\textrm{cm}^3$/kgf.m and coefficient of friction was 0.30-0.37, independent on graphite content and shape. As the temperature of friction materials increased, wear rate decreased rapidly because oxides such as $Cu_2O$ and $SnO_2$ in the surface of friction material were formed.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.