• 제목/요약/키워드: gold recovery

검색결과 69건 처리시간 0.027초

Gold Recovery Using Inherently Conducting Polymer Coated Textiles

  • Tsekouras, George;Ralph, Stephen F.;Price, William E.;Wallace, Gordon G.
    • Fibers and Polymers
    • /
    • 제5권1호
    • /
    • pp.1-5
    • /
    • 2004
  • The ability of inherently conducting polymer (ICP) coated textiles to recover gold metal from aqueous solutions containing $[AuCl_4]^-$ was investigated. Nylon-lycra, nylon, acrylic, polyester and cotton were coated with a layer of polypyrrole (PPy) doped with 1,5-naphthalenedisulfonic acid (NDSA), 2-anthraquinonesulfonic acid (AQSA) or p-toluenesulfonic acid (pTS). Textiles coated with polyaniline (PAn) doped with chloride were also used. The highest gold capacity was displayed by PPy/NDSA/nylon-lycra, which exhibited a capacity of 115 mgAu/g coated textile, or 9700 mgAu/g polymer. Varying the underlying textile substrate or the ICP coating had a major effect on the gold capacity of the composites. Several ICP coated textiles recovered more than 90 % of the gold initially present in solutions containing 10 ppm $[AuCl_4]^-$ and 0.1 M HCl in less than 1 min. Both PPy/NDSA/nylon-lycra and PAn/Cl/nylon-lycra recovered approximately 60 % of the gold and none of the iron present in a solution containing 1 ppm $[AuCl_4]^-$, 1000 ppm $Fe^{3+}$ and 0.1 M HCl. The spontaneous and sustained recovery of gold metal from aqueous solutions containing $[AuCl_4]^-$ using ICP coated textiles has good prospects as a potential future technology.

시안을 이용한 PCB 금 박리용액으로부터 사이클론 전해조에서의 금 회수거동에 미치는 차아염소산나트륨과 금 도금첨가제의 영향 (Effect of NaOCl and Gold Plating Additive on the Gold Recovery in Cyclone Electrolytic Cell from Solution for Stripping Gold of PCB by Cyanide)

  • 조현지;유경근;배무기;손정수;양동효;김수경
    • 자원리싸이클링
    • /
    • 제26권4호
    • /
    • pp.88-94
    • /
    • 2017
  • 시안을 이용한 PCB 금 박리용액으로부터 사이클론 형태의 전해조를 적용하여 금 회수 연구를 수행하였다. 이때 첨가제로서 전해생성 된 차아염소산나트륨(NaOCl)과 금 도금 첨가제(KG-120)를 사용하였고 이들의 농도와 반응시간에 따른 금의 전해회수 거동을 조사하였다. 전해생성 NaOCl은 침출액 내의 시안과 알칼리 염소화 반응을 촉진함으로써 $NaOCl(g)/CN^-(g)$ 비율 1.0 이상에서 약 99% 이상 시안을 제거할 수 있었다. 금 전해회수 시 전해생성 NaOCl을 첨가할 경우 $NaOCl(g)/CN^-(g)$ 비율이 0.5~2.5일 때 480분 내에 금은 98% 회수되었으며 비율이 3.0이상에서는 오히려 금의 회수율이 현저히 감소하는 것을 알 수 있었다. KG-120 용액의 경우, 1.5~4.5%(v/v)까지의 농도범위에서 480분 내에 금이 99% 회수되었으며, 특히 KG-120의 농도가 3.5 및 4.5%(v/v) 일 경우 240분 내에 금이 96% 이상 회수되어 반응 초기 회수속도가 상대적으로 더 빨랐다. 이로부터 경제성과 효율성을 감안한 최적의 KG-120의 농도는 3.5%(v/v)로 판단된다.

Diagnostic metallurgy of porphyry copper-gold deposits in the Pan-Pacific

  • Kim Joe Y.;Kim Sun S.;Shin Hyung J.;Kong Bong S.;Lee Keon K.
    • 한국지구물리탐사학회:학술대회논문집
    • /
    • 한국지구물리탐사학회 2003년도 Proceedings of the international symposium on the fusion technology
    • /
    • pp.581-589
    • /
    • 2003
  • The variable flotation response ores from different deposits results basically from mineralogical association and their differences. Development of new techniques for analyzing the metallurgical performance of flotation and other concentration processes is demanded even in the treatment of rather simple ores such as porphyry ores. Diagnostic metallurgical analysis can be used to quantify the most possible recovery processes. Several porphyry copper/gold ores around the world were used to examine the responses in flotation, gravity separation and cyanidation in order to define the linkage between the recovery processes for both copper and old values. Laboratory batch flotation, gravity separation and cyanidation tests were carried out on these samples. All results were used to correlate the relative recovery of copper and gold, and to predict the highest possible metal recovery in the system. The metallurgical predictions were made according to the flotation conditions used and gravity separation. The results of various concentration processes on each porphyry ore samples are presented and discussed. All seven samples have shown significantly different gold/copper metallurgy. The grade/recovery relationships of gold and copper in the laboratory batch tests for the best results and the plants are given in the Figures below. The results of laboratory tests show that the copper recoveries converged to about $90\%$, but the gold recoveries were spread over $55-80\%$, except the K S ore. Series of standard cyanidation tests on the flotation concentrate samples and gravity separation using Knelson Separator on heads ores were carried out to cross-link the metallurgy and mineralogy of gold in the porphyry ores.

  • PDF

ELECTROLYTIC RECOVERY OF PRECIOUS METALS FROM DILUTED SOLUTIONS

  • Roland Kammel;Lieber, Hans-Wilhelm
    • 한국표면공학회지
    • /
    • 제14권4호
    • /
    • pp.209-214
    • /
    • 1981
  • Electrolytic recovery of gold and silver from diluted solutions has at first been applied nearly 100 years ago. Compared with other recovery techniques electrolytic treatment offers several advantages. But to achieve high space-time yields special constructions of electrolytic cells for improved mass transfer are necessary. Ex-tended cathode surface areas and vigorous agitation are important features. Gold and silver recovery by use of newly developed electrolytic cell constructions - rotating tubular bed reactor and impact rod reactor - has been described. Calculations based on industrial application during several years are confirming that electrolytic recovery of precious metalss from diluted solutions has been operated in a very economic way.

  • PDF

생체흡착, 탈착 및 회화를 이용한 시안 용액으로부터 금의 회수 (Gold Recovery from Cyanide Solution through Biosorption, Desorption and Incineration with Waste Biomass of Corynebacterium glutamicum as Biosorbent)

  • 배민아;곽인섭;원성욱;윤영상
    • 청정기술
    • /
    • 제16권2호
    • /
    • pp.117-123
    • /
    • 2010
  • 본 연구에서는 Au(I) 이온을 함유한 시안 용액으로부터 다른 형태의 금을 회수하기 위하여 생체흡착 후 탈착하는 방법과 생체흡착 후 회화하는 방법을 제안하였다. 생체흡착제로는 아미노산 발효 공정에서 발생하는 균체 폐기물(Corynebacterium glutamicum)을 사용하였다. 바이오매스의 흡착 특성을 알아 보기 위하여 pH edge 실험을 수행하였으며, 그 결과 흡착성능은 pH 2-3 부근에서 우수한 결과를 보였다. 또한, 등온흡착 실험 결과를 Langmuir 모델에 적용한 결과 Au(I)의 최대 흡착량은 pH 2.5에서 35.15 mg/g이었다. 흡착 속도론 실험을 통해 흡착 평형은 60분 이내의 짧은 시간 내에 이루어지는 것을 확인하였다. Au(I)을 회수하기 위하여 바이오매스에 흡착된 Au(I)을 탈이온수를 이용하여 탈착을 시켰으며, 탈착효율은 91%로 평가되었다. 이 결과는 바이오매스를 이용하여 흡착과 탈착을 통해 1가 금을 효과적으로 회수할 수 있음을 보여준다. 영가 형태로 회수하기 위하여, 금을 흡착하고 있는 생체흡착제를 회화하여 환원된 형태의 금을 성공적으로 회수하였으며, 회분 중 금의 순도는 85% 이상이었다. 따라서 본 연구에서 제시한 생체흡착 후 탈착(1가 형태) 공정과 생체흡착 후 회화(영가 형태) 공정은 회수하고자 하는 금의 산화수에 따라 선택하여 사용될 수 있을 것으로 기대된다.

Recovery of Gold from Refractory Arsenic Gold Concentrate by a Process of Thiobacillus Ferrooxidans Oxidation - Cyanidation

  • Zhang, Chuanfu;Min, Xiaobo;Chai, Liyuan;Chen, Weiliang;Okido, Masazumi
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2001년도 The 6th International Symposium of East Asian Resources Recycling Technology
    • /
    • pp.159-164
    • /
    • 2001
  • A novel fluidized-bed reactor was designed and installed for bioleaching in a semi-continuous way, by which a process for bioleaching-cyanidation of Guangxi Jinya refractory gold arsenical concentrate was studied. An arsenic extraction rate reaches 82.5% after 4-day batch biooxidation of the concentrate under the optimized condition of pH 2.0, ftrric ion concentration 6.5g/L and pulp concentration 10%. And leaching rate of gold in the following gold cyanidation is over 90%. The parameters of three series fluid-bed reactors exhibit stability during the semi-continuous bioleaching of the concentrate. Arsenic in the concentrate can be got rid of 91% after 6-day leaching. Even after 4 days, 82% of arsenic extraction rate was still obtained. The recovery rates of gold are 92% and 87.5% respectively in cyaniding the above bioleached residues. The results will provide a base for further commercial production of gold development.

  • PDF

인쇄회로기판(印刷回路基板) 제조공정(製造工程)의 폐(廢) Back Board 및 금(金) 회수(回收) (Recovery of Waste Back Board and Gold from the Process of Printed Circuit Board)

  • 김유상
    • 자원리싸이클링
    • /
    • 제19권1호
    • /
    • pp.57-65
    • /
    • 2010
  • 최근, 인쇄회로기판 제조공정으로부터 유가자원을 회수하고자 하는 연구가 활발히 진행되고 있다. 인쇄회로기판의 드릴가공 받침대로 사용한 후 폐기되는 백보드 소재활용과 소형화, 고 신뢰성화에 따른 유가금속인 금 회수가 필수적이다. 특히 이동통신용 전자부품의 핵심소재로 사용되는 인쇄회로기판부품에는 최소 0.03 ${\mu}m$에서부터 최대 50 ${\mu}m$ 두께로 금이 도금되어 있다. 금, 원자재, 약품 값 폭등으로 생산현장의 유가자원 활용이 중요한 과제로 대두되면서 유가자원 활용을 위한 경쟁이 가속화되는 추세다. 본고에서는 인쇄회로기판 제조공정에서 발생하는 폐백보드 및 금의 회수에 대한 기술동향을 제공함으로써 유가자원 활용 산업발전에 기여하고자 하였다.

Dowex 21K XLT 수지를 이용한 산업폐수 내의 금-시안 착화합물의 선택적인 연속흡착 및 회수 (Selective Continuous Adsorption and Recovery for Gold-Cyanide Complex in Industrial Wastewater Using Dowex 21K XLT Resin)

  • 전충
    • 한국지반환경공학회 논문집
    • /
    • 제16권3호
    • /
    • pp.35-39
    • /
    • 2015
  • Dowex 21K XLT 수지를 이용하여 산업폐수 내에 존재하는 금과 납-시안 착화합물에 대한 연속흡착 및 회수 특성을 조사하였다. 충전층에 충진된 Dowex 21K XLT 수지는 0.5mL/min의 유입유속에서 금-시안 착화합물을 520 bed volume까지 95% 이상 연속적으로 제거할 수 있지만, 납-시안 착화합물은 전혀 제거할 수 없었다. Dowex 21K XLT 수지에 흡착된 금-시안 착화합물은 HCl과 Acetone을 7:3의 비율로 섞은 혼합액을 탈착제로 이용하였을 때, 8 bed volume 내에서 96% 탈착되어졌다. 또한 두 번 재사용된 Dowex 21K XLT 수지의 금-시안 착화합물에 대한 bed volume이 490을 유지하여 향후 금 이온을 포함하고 있는 산업폐수 처리공정에 충분히 적용될 수 있을 것으로 판단된다.

Two-Step Oxidation of Refractory Gold Concentrates with Different Microbial Communities

  • Wang, Guo-hua;Xie, Jian-ping;Li, Shou-peng;Guo, Yu-jie;Pan, Ying;Wu, Haiyan;Liu, Xin-xing
    • Journal of Microbiology and Biotechnology
    • /
    • 제26권11호
    • /
    • pp.1871-1880
    • /
    • 2016
  • Bio-oxidation is an effective technology for treatment of refractory gold concentrates. However, the unsatisfactory oxidation rate and long residence time, which cause a lower cyanide leaching rate and gold recovery, are key factors that restrict the application of traditional bio-oxidation technology. In this study, the oxidation rate of refractory gold concentrates and the adaption of microorganisms were analyzed to evaluate a newly developed two-step pretreatment process, which includes a high temperature chemical oxidation step and a subsequent bio-oxidation step. The oxidation rate and recovery rate of gold were improved significantly after the two-step process. The results showed that the highest oxidation rate of sulfide sulfur could reach to 99.01 % with an extreme thermophile microbial community when the pulp density was 5%. Accordingly, the recovery rate of gold was elevated to 92.51%. Meanwhile, the results revealed that moderate thermophiles performed better than acidophilic mesophiles and extreme thermophiles, whose oxidation rates declined drastically when the pulp density was increased to 10% and 15%. The oxidation rates of sulfide sulfur with moderate thermophiles were 93.94% and 65.73% when the pulp density was increased to 10% and 15%, respectively. All these results indicated that the two-step pretreatment increased the oxidation rate of refractory gold concentrates and is a potential technology to pretreat the refractory sample. Meanwhile, owing to the sensitivity of the microbial community under different pulp density levels, the optimization of microbial community in bio-oxidation is necessary in industry.

Extracting Gold from Pyrite Roster Cinder by Ultra-Fine-Grinding/Resin-in-Pulp

  • Guo, Bingkun;Wei, Junting
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2001년도 The 6th International Symposium of East Asian Resources Recycling Technology
    • /
    • pp.337-341
    • /
    • 2001
  • A new method to extract gold from pyrite roster cinder, which combines ultra-fine-grinding with resin-in-pulp, has been studied in this paper. Compared with traditional leaching technology, it can short leaching time, avoid complex filter process, lower sodium cyanide consumption and increase gold recovery by 35%. During leaching, aluminium oxide ball was used as stirred medium, hydrogen peroxide as leaching aid and sodium hexametaphosphate as grinding aid. With the high efficiency and chemistry effect of ultra-fine-grinding, the leaching process was developed and the gold leaching rate may reach 88%. With AM-2 Б resin as abosorber and sulfocarbamide (TU) as eluent, gold was recovered from cyanide pulp by resin-in-pulp. AM-2 Б resin has good adsorbability in cyanide solution(pH=10). It was easy to elude gold from the loaded resin with 0.1㏖/L cholhydric acid and 1㏖/L sulfocabamide. The effect of contact time, temperature and acidity etc. on the gold absorption had been examined with static methods. The results showed that the adsorption and desorption of gold could both reach over 98%. The effects of flow rate of solution on dynamic adsorption and elution of gold had been examined with dynamic methods. Breakthrough curve and elution curve had been drawn in this paper. A mild condition was determined through a number of experiments: leaching time 2 hours, liquid solid ratio 4:1, sodium cyanide 3kg/t, hydrogen peroxide 0.05%, sodium hexametaphosphate 0.05%; adsorption time 30 minutes, temperature 10-3$0^{\circ}C$, resin($m\ell$) solid(g) ratio 1:10, eluent resin ratio 10-20:1, velocity of eluent $1.5m\ell$/min. Under the mild condition, the gold recovery may reach 85%.

  • PDF