• Title/Summary/Keyword: friction Welding

검색결과 569건 처리시간 0.023초

Zr-기 벌크 금속 유리의 마찰 접합 공정 개발 (Development of Friction Welding Process of Zr-based Bulk Metallic Glasses)

  • 신형섭;정영진;김기현
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 추계학술대회
    • /
    • pp.337-341
    • /
    • 2004
  • Bulk metallic glasses(BMG) with good mechanical properties have problems that engineering application fields have been limited because of limitation of the alloy size. In order to solving this problem, the friction welding of BMG has been tried using the superplastic-like deformation behavior under the supercooled liquid region. The apparatus for friction welding test was designed and constructed using pneumatic cylinder and gripper based on a conventional lathe. Friction welding have been tried to combination of same BMG alloy and crystalline alloys. The results of welding test were evaluated by X-ray diffraction, measurement of hardness and mechanical properties test. In order to obtain the optimized welding test conditions the temperature of friction interface was measured using Infrared thermal imager.

  • PDF

열간 금형재의 마찰용접 최적화와 AE평가 (Friction Welding Optimization of Hot Die Punch Materials and Its AE Evaluation)

  • 오세규;공유식;박일동;유인종
    • 동력기계공학회지
    • /
    • 제4권4호
    • /
    • pp.54-58
    • /
    • 2000
  • The complete joining method for dissimilar hot die punch materials and its real-time evaluation method are not available at present. Brazing method has been used for joining them, but it is known that the welded joint by the brazing has the lower bonding efficiency and reliability than the diffusion welding. The friction welding with a diffusion mechanism in bonding was applied in this study. So, this work was carried out to determine the optimal friction welding conditions and to analyze mechanical properties of friction welded joints of hot die punch materials (STD61 for the blade part of hot die punch) to alloy steel (SCM440 for the shank part of hot die punch) such as plunger. In addition, acoustic emission test was carried out during friction welding to evaluate the weld quality.

  • PDF

스프링강(SUP9A)-SM25C의 이종재 마찰용접 피로특성에 관한 연구 (A Study on Fatigue Characteristics of Dissimilar Spring Steel(SUP9A)-SM25C by Friction Welding)

  • 정석주;이기중
    • 한국안전학회지
    • /
    • 제16권3호
    • /
    • pp.19-25
    • /
    • 2001
  • The friction-welding SM25C is a substitute for the suing steel that is utilized in the machinery, airplane, and automobile, ok. This substitution would provide reduction of material and weight of welding parts. From the result we found that the strength of the friction welded joint was 529-617MPa and the toughness 1.2 times higher than that of the base metal. The optimal condition of friction welding was found as follows : n=2000rpm, $P_1$=68㎫, $P_2$=137MPa, $t_2$=2sec, $t_1$=2-4sec, Considering the strength, the hardness, and the reduction of area in the friction welding, the fiction welding using SUP9A and SM25C was found to cause no problem in on-the-job application.

  • PDF

EVALUATION OF FRICTION WELDABILITY OF TYPE 5052 ALALLOY/LOW CARBON STEEL JOINT.

  • Kim, Kyung-Kyun;Lee, Won-Bae;Yeon, Yun-Mo;Kim, Dae-Up;Jung, Seung-Boo
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2002년도 Proceedings of the International Welding/Joining Conference-Korea
    • /
    • pp.528-533
    • /
    • 2002
  • The mechanical and metallurgical properties of friction welded joints type 5052 Al alloy/A36 steel have been studied in this paper. The joint strength increased with increasing upset pressure and friction time till it reached the critical value. The joint strength was fixed at low strength compare to that of base metal in the case of increasing friction time. Microstructure of 5052 Al alloy was greatly deformed near the weld interface. The very fine and equaxied grain structure was observed at the near interface. The elongated grain was formed outside dynamic recrystallizatoin region at the peripheral part, while the A36 steel' side was not deformed. The hardness of the near interface was slightly softer than that of 5052 Al alloy base metal. The maximum softening width was about 8mm from the interface. In the present work, the friction welding condition, t$_1$=0.5sec, P$_2$=137.5MPa, showed a maximum joint strength (202MPa) when friction pressure, upset time and rotation speed were fixed at 75MPa, 5sec, 2000rev/min and these were the optimum friction welding condition of 5052Al/A36 steel joints.

  • PDF

AE에 의한 소형 밸브스풀 마찰용접 품질의 실시간 평가 (Real-Time Evaluation of Friction Weld Quality of Small-Type Hydraulic Valve Spool by Acoustic Emission)

  • 오세규;오정환;전태언;김경균;오명석
    • Journal of Welding and Joining
    • /
    • 제12권2호
    • /
    • pp.97-107
    • /
    • 1994
  • Both in-process quality control and high reliability of the weld is one of the major concerns in applying friction welding to the economical and qualified mass-production. No reliable nondestructive monitoring method is available at present to determine the real-time evaluation of automatic production quality control for friction welding of special hydraulic valve spool of 16mm in diameter. This paper, so that, presents the experimental examinations and statistical quantitative analysis of the correlation between the initial cumulative counts of acoustic emission(AE) occurring during plastic deformation periods of the welding and the tensile strength and other properties of the welded joints of $\phi16$ valve spool as well as the various welding variables, as a new approach which attempts finally to develop real-time quality monitoring system for friction welding.

  • PDF

Grain Refinement and Phase Transformation of Friction Welded Carbon Steel and Copper Joints

  • Lee, W.B.;Lee, C.Y.;Yeon, Y.M.;Kim, K.K.;Jung, S.B
    • International Journal of Korean Welding Society
    • /
    • 제3권2호
    • /
    • pp.46-52
    • /
    • 2003
  • The refinement of microstructure and phase transformation near the interface of pure copper/carbon steel dissimilar metals joints with various friction welding parameters have been studied in this paper. The microstructure of copper and carbon steel joints were changed to be a finer grain compared to those of the base metals due to the frictional heat and plastic deformation. The microstructure of copper side experienced wide range of deformed region from the weld interface and divided into very fine equaxied grains and elongated grains. Especially, the microstructures near the interface on carbon steel were transformed from ferrite and pearlite dual structure to fine ferrite, grain boundary pearlite and martensite due to the welding thermal cycle and rapid cooling rate after welding. These microstructures were varied with each friction welding parameters. The recrystallization on copper side is reason for softening in copper side and martensite transformation could explain the remarkable hardening region in carbon steel side.

  • PDF

마찰용접을 이용한 대형선박 터보챠저용 이종 로타샤프트 개발 (Development of Large Rotor Shaft for Marine Turbo Charger Using Friction Welding with Dissimilar Materials)

  • 문광일;전종원;정호승;조종래;최성규
    • 한국정밀공학회지
    • /
    • 제33권4호
    • /
    • pp.257-264
    • /
    • 2016
  • Solid state joining techniques are increasingly applied in a wide range of industrial applications. Friction welding is a solid state welding technique that is used to join similar or dissimilar materials. In this study, friction welding was applied to rotor shaft composed of a disk and a shaft. The disk and shaft were manufactured by hot forging and rolling, respectively. The aim of the study was to predict the structural characteristics during hot forging and friction welding process for rotor shaft of turbo charger. The structural characteristics were determined by heat input and heat affected zone (HAZ) during a short cycle time. Thus, transient FE analysis for hot forging and friction welding was based on heat transfer. The results were used to predict structural characteristics during hot forging and friction welding processes. The prototype of rotor shaft was manufactured by the result-based process parameters.

이종재 막찰용접 이음부에서의 초음파 반사계수와 용접조건과의 관계 (The Relationship between Welding Conditions and Ultrasonic Reflection Coefficients of Dissimilar Metals Friction Welded Joints)

  • 오세규;김동조;한상덕
    • 한국해양공학회지
    • /
    • 제1권1호
    • /
    • pp.138-143
    • /
    • 1987
  • Friction welding has emerged as a reliable process for high-production commercial applications with significant economic and technical advantages. But nondestructive test in friction weld was not clearly developed. Therefore the experimental verification is necessary in order to understand the characteristcs of the pulse echo effects according to various change in welding conditions. This paper presents an attempt to determine the relationship between the varios welding conditions and the coefficients of reflection using the ultrasonic pulse echo method in dissibilar metals friction weld. The new approach of calculating the coefficients of reflection based on measured amplitudes of the echoes is applied in this paper. These coefficients provides a single quantitative measurement which involves both acoustic energy reflected at the welded interface as well as transmitted across the interface. As a result, it was known that the quantitave relationship between welding conditions and the coefficients of reflection using the ultrasonic pulse echo exists in dissimilar metals friction weld.

  • PDF