Wear behavior of SM55C steel by rolling contact (구름접촉에 의한 SM55C의 마멸 거동)

  • Park, Beom-Su;Chae, Young-Hun;Kim, Seock-Sam
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2002.05a
    • /
    • pp.240-247
    • /
    • 2002
  • The rolling wear behavior of SM55C is investigated under lubrication. This is a comparative tribological behavior of heat treatment effect for SM55C. Rolling wear test method is used for Ball-on-disk type. Specimens can be classified into two main groups: as-annealing and non-annealing. As result of wear behavior, flanking initial time of non-annealing specimen keep at retard but it have not under high normal load. One of the notable features of annealing specimen is steady flanking initial time for a normal load in this experiment. Failure mechanism of SM55C is due to the fatigue wear such like flanking, pitting etc.. Flanking leads to abruptly fracture of worn surface. Fracture mechanism has a connection with normal load and polishing direction of specimens.

  • PDF