• Title/Summary/Keyword: fire resistant materials

Search Result 83, Processing Time 0.035 seconds

Studies on the disease resistance of tobacco varieties to Black shank, Black root rot Wild fire, Brown spot, CMV-Y and Blue mold -Disease resistance of Korean native varieties- (담배중요병해저항성에 관한 연구 특히 한국재래종에 대하여)

  • Il Hou
    • KOREAN JOURNAL OF CROP SCIENCE
    • /
    • v.4 no.1
    • /
    • pp.103-108
    • /
    • 1968
  • Resistance to various diseases of Korean native varieties were investigated in field. The results obtained are summarized as follows: 1) The varieties Ubangtchio and Osib-eubthio were moderately resistant to black shank, but Suantchio, Usultchio and Gwangtchio were slightly resistant. Dixie Bright 101, $H_2$ and Bright Yellow 4 were more resistant to black shank than any of the Korean native varieties. 2) Mokgitchio, Ubangtchio and Osib-eubtchio were moderately resistant to black root rot, but Useultchio Suantchio and Hoetchio were susceptible than Others. 3) Muktchio, Hoetchio and Ubangtchio were slightly resistant to wild fire. 4) Osib-ebthio was highly resistant to brown spot, but Ubangtchio, Hyangtchio and Mokgitchio were moderately resistant and Useultchio was susceptible to brown spot, but it was resistant than Bright ellow 4 or Bernhart 1000-1. 5) Hyangtchio was slightly resistant to CMV-Y. According to these results, except Virus disease, Ubangtchio was resistant to all of the above mentioned diseases. Osib-eubtchio, Hoetchio, Hyangtchio and Suantchio showed proferable disease resistant and these might be well utilized as breeding materials.

  • PDF

An Experimental Study on the Development of Dry Wall System using Wood-wool Board (목모보드를 이용한 건식벽체시스템 개발에 대한 실험적 연구)

  • Kim, Dae-Hoi;Park, Soo-Young;Choi, Dong-Ho
    • Fire Science and Engineering
    • /
    • v.22 no.3
    • /
    • pp.208-215
    • /
    • 2008
  • Existent wood wool cement boards are low-quality cement boards made out of wood chip wastes. Recently, however, they are produced by making wood chips into fibrous forms to have good looks and excellent performances in sound absorption and thermal insulation. Though they have been broadly used in the advanced countries, they were rather expensive products with limited use in Korea having no domestic manufacturers of them. Since 2005, however, it has been possible for the boards to be used in various fields due to their lowered prices and stable supplies by the arrival of domestic manufacturers. For the purpose of encouraging broad use of the boards, this research aims to explore their practical applications by way of assessing the flame retardant and fire resistant performances when they are applied to dry-wall system.

Study on the Determination of Fire Protection Thickness based on Section Factor (강재의 단면형상에 따른 내화피복두께 산정 연구)

  • 정청운;지남용;권인규
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2003.05a
    • /
    • pp.139-142
    • /
    • 2003
  • Traditionally, the thickness of fire protection materials of structural elements such as beam and column have been decided by fire test using the predominant steel section of $H-300{\times}300{\times}10{\times}15$ for column and $H-400{\times}200{\times}8{\times}13$ for beam in Korea. But this way of determination of fire protection thickness yields very unduly results. Because the temperature-increment rate of structural steel elements depends mainly on magnitude of their cross-areas. In general, the thicker size of cross-areas for structural elements, the lower temperature shows up. It had already proved that the fire protection thickness only depends on the size of cross-areas and the fire protection method for three-fide or four-side exposed conditions in European countries, the United State of America and so on. To demonstrate there would be differences among various cross-areas for structural elements, we conducted several fire tests with full-scale specimens of beams and columns. For the determination of critical temperature for steel section when the fire resistant performance is needed to be decided, we conducted with a loaded fire test for beam and column, respectively. The small column in 1.0 meter length and beam in 1.5 meter length were used in order to deprive the rational fire protection thickness of structural elements such as beam and column, respectively. After test, we could obtain there were significant temperature lass between higher cross-areas and lower cross-areas. The critical temperature of steel as a criterion is used 538$^{\circ}C$ for column and 593$^{\circ}C$ for beam which is from ASTM E 119 because we don't make provisions as critical temperature by elements. We could consider that the best way of determination of fire protection thickness is using the following multi-regression equation which was deprived from several fire tests using the concept of section factor, FR(column) = 0.17 +5191.49t A/Hp + 40.77t, FR(beam) = 0.25 +6899.31t A/Hp + 32.60t(where, FR means fire resistant time, t means thickness, A means cross-area and Hp means heated parameter).

  • PDF

A Study on the Effects of Fire-Resistant Coating Materials for Prevention of Concrete Spalling (콘크리트 폭렬 저감에 대한 내화 피복재의 영향에 관한 연구)

  • Jeong, Eui-Dam;Song, Myong-Shin;Kang, Hyun-Ju;Kang, Seung-Min
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.10 no.5
    • /
    • pp.9-15
    • /
    • 2010
  • Recently, the high-compressive strength concrete where the use is extending was weak in fire because of spalling that was occurring with rise of internal vapor pressure by high temperature. For preventing spalling of high-strength concrete in fire, Organic fibers have been using in concrete generally. By melting of organic fibers in concrete in fire, the internal moistures of concrete moves quickly to the outside, and so, preventing of spalling of high-strength concrete. But this method will be able to prevent the spalling of high-strength concrete, but makes the decrease of the concrete strength after fire. This study make a comparison between properties of preventing of spalling and remaining compressive strength of concrete using intumescence Alkali-Silicates fire-resistant material and that of concrete with organic fibers. Using organic fibers for preventing of spalling of concrete are P.P and Nylon fibers, and anti-fire intumescence material for protection of concrete surface is alkali-silicate materials. Fire resistance test executed as long as 3 hr under the flame temperature $1,200^{\circ}C$ over. In the case of concrete with P.P fibers, don't occurred the spalling, but the remaining compressive strength will not be able to measure, the concrete using intumescence Alkali-Silicates system fire-resistant material is not only preventing of the spalling but also the remaining compressive strength maintained until the maximum 96%.

An experimental study on the low temperature melting treatment of waste asbestos for using (폐석면의 활용을 위한 저온 용융처리에 대한 실험적 연구)

  • Song, Tae Hyeob;Kim, Young Hun;Park, Ji Sun;Lee, Sea Hyun
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.2
    • /
    • pp.83-90
    • /
    • 2010
  • As a reinforced fabric, asbestos has been utilized as a fire-resistant material as it has a superior flexural stiffness and heat resistance up to $1500^{\circ}C$. However, due to its harmfulness, its use has been prohibited recently and the even the installed asbestos materials are being repaired or supplemented if there is a concern about flying. Asbestos is mainly used for construction panels as a reinforced fabric and coating materials to ensure the fire-resistance of steel frames. Asbestos was used as fire-resistant materials for steel frames until 1991 and then prohibited as Act on Industrial Safety and Health limits the concentration of asbestos in the air. Classified as a designated waste according to Act on Waste Control, asbestos must be buried if there is no possibility of flying (panel-type materials) or cement-solidified and then buried if there is a possibility of flying (spray coating material) In general, it is required that a new waste landfill include a certain landfill facility for designated waste, but in reality there is an absolute storage of landfill facilities for designated waste as they only install facilities of the size required by the regulations. This could result in the 2nd environmental pollution as they cannot process asbestos wastes which will be generated in large volume in the future. This study explores a method that melts asbestos wastes at $700^{\circ}C$ rather than cement-solidifying the waste asbestos from construction sites, especially asbestos-containing spray coating. The study results showed that there was no change in the composition and shape even though asbestos wastes was melted at $1300^{\circ}C$, but there was a change for the specimen which was process in advance for low temperature melting and then melt at $900^{\circ}C$.

  • PDF

Analysis of Internal Structure in Alkali-Activated Fire Protection Materials Using Fly ash (플라이애시를 활용한 알칼리 활성화 내화성 마감재의 내부구조 분석)

  • Song, Hun;Chu, Yong-Sik;Lee, Jong-Kyu
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.4
    • /
    • pp.104-112
    • /
    • 2012
  • This study involves investigating the correlation between variation of internal structure and heating temperature of alkali-activated fire protection materials using fly ash. Dehydration and micro crack thermal expansion occur in cement hydrates of cementitious materials heated by fire. Internal structure difference due to both the dehydration of cement hydrates and pore solution causes and influences changes in the properties of materials. Also, this study is concerned with change in microstructure and dehydration of the alkali-activated fire protection materials at high temperatures. The testing methods of alkali-activated fire protection materials in high temperature properties are make use of TG-DSC and mercury intrusion porosimetry measurements. The study results show that the alkali-activated fire resistant finishing material composed of potassium hydroxide, sodium silicate and fly ash has the high temperature thermal stability. These thermal stability is caused by the ceramic binding capacity induced by alkali activation reaction.

  • PDF

A Study on the Refractory Performance Verification of the Thermal Insulators for AES Ducts and Piping (AES 계열 덕트·배관 단열재의 내화성능 검증에 관한 연구)

  • Kwang-Ho Ham;Jea-Chun Sa;Joo-Hwan Lee;Se-Hong Min
    • Journal of the Society of Disaster Information
    • /
    • v.20 no.2
    • /
    • pp.419-429
    • /
    • 2024
  • Purpose: To enhance the non-combustibility of fire protection piping insulation and improve the heat resistance of smoke extraction duct insulation, I plan to verify the suitability of AES insulation materials for these applications through performance testing. Method: The non-combustibility, heat resistance, and thermal insulation performance of AES insulation materials will be verified through various tests. Result: According to the 'Standards for Flame Retardancy and Fire Spread Prevention of Building Finishing Materials,' the results of non-combustibility and gas toxicity tests confirmed the non-combustible properties. The standard fire resistance tests verified the fire resistance performance. Additionally, the thermal insulation performance was confirmed through building insulation tests. Conclusion: As the performance tests on AES inorganic insulation materials have proven their noncombustibility, fire resistance, and thermal insulation performance, these materials are considered a viable alternative for improving fire spread prevention in buildings.

A Research for Identification Method of Sprayed Fire-Resistive Material by Thermal Analysis (열분석을 통한 내화 뿜칠재 일치성분석 연구)

  • Cho, Nam-Wook;Rie, Dong-Ho;Shin, Hyun-Jun
    • Fire Science and Engineering
    • /
    • v.25 no.1
    • /
    • pp.7-12
    • /
    • 2011
  • As recent buildings are getting more high-rise and larger, steel structures, not a reinforced concrete structure, for columns and beams among the main structural members in a building are being widely used. Steels used for the main members of a building are constructed with a fire-resistive structure by applying them with fire-resistive coatings. The introduction of a simple test method that can verify the performance of fire-resistive material constructed on a site without conducting a fire-resistant test(real scale fire test) is needed and this study derived a site analysis method possible to make a rapid and scientific analysis through the analysis of components (instrumental analysis) concerning tire-resistive materials. the possibility of application of it in analyzing congruence over site construction materials by recognizing it as a standard material after securing an inherent fingerprint area of tire-resistive materials of which performance was verified in the concrete through thermal analysis was proved through experiments. This research result can be minimize of casualties, who is harmed to building collapse according to structures fire.

Evaluation of Structural Stability of Fire Resistant Steel Produced by Thermo-Mechanical Control Process at High Temperature (TMCP 내화강재의 고온 내력 평가 연구)

  • Kwon, In-Kyu
    • Fire Science and Engineering
    • /
    • v.27 no.6
    • /
    • pp.21-25
    • /
    • 2013
  • Fire resistance steel, grading 490 MPa, had developed by using Thermo-mechanical control process (TMCP) and it has better performance at welding, seismic resistance than those of the ordinary structural steel, But the fire resistance performance is required to verify against the ordinary fire resistance, FR 490. Therefore this study was done to make database of mechanical properties at high temperature and to evaluate the structural stability at high temperature in terms of materials and structural member such as H-section from that of FR 490. The result of this study was that the structural stability of TMCP was lower than that of ordinary FR 490 at the range up about $700^{\circ}C$.

Development of Acceleration Duability test condition for Fireproof Spray-Application. (옥내용 뿜칠내화피복재의 촉진내구성 조건 설정 연구)

  • Kim, Dae-Hoi;Lee, Gun-Chol
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2014.05a
    • /
    • pp.170-171
    • /
    • 2014
  • The buildings constructed with steel structure is coated with certified fire resistive material to resist from fire. Coating materials lose their initial performances as time passes, so they need some maintenance. This study is covers standardization of the methods for assessing the durability of SFRM. In Korea, more than 90 percent of SFRM are used indoors. So This study is to decide proper test method through investigation and examination of effect factor to performance of fire-resistant structure and applicable test method.

  • PDF