ZnO가 PMN-PNN-PZT 세라믹스의 저온소결에 미치는 영향 (Effect of ZnO on Low Temperature Sintering of PMN-PNN-PZT Ceramics)

  • 이상호;류주현;홍재일;류성림
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.32-33
    • /
    • 2006
  • In this study, in order to develop multilayer ceramic actuator for ultrasonic nozzle and ultrasonic vibrator, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$. $Na_2CO_3$ and ZnO as sintering aids. And then, their piezoelectric and dielectric properties according to the amount of ZnO addition were investigated. The addition of ZnO improved density, dielectric constant, electromechanical coupling factor, mechanical quality factor and piezoelectric d constant of PMN-PNN-PZT ceramics due to the increase of sinterability and accepter doping effect. Electromechanical coupling factor and mechanical quality factor of PMN-PNN-PZT ceramics increased with ZnO amount up to 0.4wt% and then decreased. At the sintering temperature of $900^{\circ}C$ and 0.4wt% ZnO addition, density, dielectric constant, electromechanical coupling factor, mechanical quality factor and piezoelectric d constant showed the optimum value of 7.876g/$cm^2$, 1299, 0.612, 1151 and 369pC/N, respectively.

  • PDF

Piezoelectric and Dielectric Properties of Low Temperature Sintered Pb(Mn1/3Nb2/3)0.02(Ni1/3Nb2/30.12(ZrxTi1-x)0.86O3 System Ceramics

  • Yoo, Ju-Hyun;Lee, Sang-Ho
    • Transactions on Electrical and Electronic Materials
    • /
    • 제10권4호
    • /
    • pp.121-124
    • /
    • 2009
  • In this study, in order to develop compositions of ceramics suitable for piezoelectric actuator and ultrasonic vibrator applications using low temperature sintering, multilayer, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$ and $Na_2CO_3$ as sintering aids. Their structural, piezoelectric and dielectric characteristics were investigated according to the Zr/Ti ratio. As the Zr/Ti ratio increased, the electromechanical coupling factor $k_p$, and piezoelectric constant $d_{33}$ and the mechanical quality factor $Q_m$ all increased with Zr/Ti ratio and then decreased after the ratio exceeded 50/50. At the ratio of Zr/Ti =49/51 and sintering temperature of $900^{\circ}C$; the density, electromechanical coupling factor $k_p$, dielectric constant ${\varepsilon}_r$ piezoelectric $d_{33}$ constant and mechanical quality factor $Q_m$ all showed the optimum values of 7.900 $g/cm^3$, 0.576, 856, 312 pC/N, 1,326, respectively. These property values are very suitable for multilayer ceramics actuator applications.

압전 액츄에이터에 활용할 저온소결 압전 세라믹스에 관한 연구 (A Study on the Properties of the Low Temperature Sintered Piezoelectrics for Actuator Application)

  • 류성림;이상호;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제21권3호
    • /
    • pp.232-235
    • /
    • 2008
  • In this study, in order to develop the composition ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3$, $Na_2CO_3$, ZnO as sintering aids and their piezoelectric and dielectric properties were investigated according to the Bi substitution, Bi substitution induced grain growth and increase of sinterablity, And also, Bi substitution suppress secondary phase due to the liquid phase sintering effect. Bi substitution enhanced electromechanical coupling factor ($k_p$) and dielectric constant ($\varepsilon_r$), However, mechanical quality factor($Q_m$) was deteriorated, At the sintering temperature of 870 $^{\circ}C$ and Bi substitution of 1 mol%, density, electromechanical coupling factor ($k_p$), mechanical quality factor ($Q_m$), Dielectric constant ($\varepsilon_r$) and piezoelectric constant ($d_{33}$) of specimen showed the optimum values of 7,878 $g/cm^3$, 0,608, 835, 1603 and 397 pC/N, respectively for multilayer piezoelectric actuator application.

PbO량에 따른 PMN-PNN-PZT 세라믹스의 유전 및 압전특성 (Piezoelectric and Dielectric Characteristics of PMN-PNN-PZT Ceramics According to the amount of PbO)

  • 김도형;김국진;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 추계학술대회 논문집 Vol.19
    • /
    • pp.219-220
    • /
    • 2006
  • In this study, m order to develop multilayer ceramics vibrator for ultrasonic nozzle, PMN-PNN-PZT ceramics were fabricated using $Li_2CO_3-Na_2CO_3$ as sintering aids and their piezoelectric and dielectric characteristics were investigated according to the aomunt of PbO. With increasing PbO contents. secondary phases were increased and phase structure were changed from tetragonal structure to rhombohedral structure and also electromechanical coupling factor were linearly decreased. At the composition ceramics with the sintering temperature of $870^{\circ}C$ and 1 mol% excess PbO, density, electromechanical coupling factor, dielectric constant, piezoelectric d constant and mechanical quality factor showed the optimum value of $7.879g/cm^2$, 0.55, 1149, 328pC/N, 1224, respectively for multilayer ceramics vibrator application for ultrasonic nozzle.

  • PDF

CeO2첨가에 따른 저온소결 PSN-PZT세라믹스의 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of Low Temperature Sintering PSN-PZT Ceramics with CeO2 Addition)

  • 류주현;정광현;정영호
    • 한국전기전자재료학회논문지
    • /
    • 제17권5호
    • /
    • pp.481-485
    • /
    • 2004
  • 0.91 (PSN-PZT) -0.05BF -0.04PNW+0.3wt%MnO$_2$+0.6wt%CuO+xwt%CeO$_2$ ceramics were fabricated with the variations of CeO$_2$addition at the sintering temperature of 95$0^{\circ}C$ and their microstructure, dielectric and piezoelectric characteristics were investigated. As the amount of CeO$_2$ addition increased, the grain size, density and electromechanical coupling factor(k$_{p}$) were increased and the mechanical quality factor(Q$_{m}$ ) was decreased. At the 0.3 wt% CeO$_2$, the density, grain size, electromechanical coupling factor(k$_{p}$), and pizoelectric constants(d$_{33}$, g$_{33}$) showed the maximum value of 7.87 g/㎤, 3.22 $\mu\textrm{m}$, 0.5, 289 pC/N, and 22.2 ㎷ㆍm/N, respectively. However, mechanical quality factor(Q$_{m}$ ) showed the minimum value of 807 at the 0.5 wt% CeO$_2$.$.EX>.EX>.

$BaTiO_3$ 치환에 따른 (Na,Li)$NbO_3$ 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Properties of (Na,Li)$NbO_3$ Ceramics According to the $BaTiO_3$ substitution)

  • 이상호;이갑수;류주현;류성림;송현선
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.272-273
    • /
    • 2007
  • In this study, in order to develop the composition ceramics of lead-free ultrasonic motor, (Na,Li)$NbO_3-BaTiO_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $BaTiO_3$, substitution. $BaTiO_3$ substitution enhanced density, dielectric constants$({\varepsilon}_r)$ and electromechanical coupling factor$(k_p)$. However, mechanical quality factor was deteriorated. At the $BaTiO_3$ substitution of 4mol%, density, electromechanical coupling factor$(k_p)$, dielectric constants$({\varepsilon}_r)$ and piezoelectric constant$(d_{33})$ of specimen showed the optimum value of $4.493g/cm^3$, 0.236, 175, 70pC/N, respectively.

  • PDF

SrTiO3 치환에 따른 (Na,K)NbO3계 세라믹스의 유전 및 압전특성 (Dielectric and Piezoelectric Properties of (Na,K)$NbO3 Ceramics as a Function of SrTiO3 Substitution)

  • 이상호;류주현;이의용;송현선;마석범;김성구
    • 한국전기전자재료학회논문지
    • /
    • 제22권6호
    • /
    • pp.484-488
    • /
    • 2009
  • In this study, in order to develop the lead-free piezoelectric ceramics with high piezoelectric and dielectric properties, $[(K_{0.5}Na_{0.5})_{0.95}Li_{0.05}(Nb_{0.96}Sb_{0.04})]O_3$ ceramics were fabricated using $Ag_2O$ as sintering aid and a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $SrTiO_3$ substitution. $SrTiO_3$ substitution enhanced density, dielectric constant(${\varepsilon}_r$) and electromechanical coupling factor($k_p$). However, mechanical quality factor was deteriorated. And also, Curie temperature ($T_c$), and phase transition temperature($T_p$) were rapidly decreased. At the 0.5 mol% $SrTiO_3$ substitution, density, electromechanical coupling factor($k_p$), dielectric constant(${\varepsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum value of $4.437\;g/cm^3$, 0.457, 1294, 265 pC/N, respectively.

K5.4Cu1.3Ta10O29 첨가에 따른 (Na,K)NbO3계 세라믹스의 압전특성 (Piezoelectric Properties of (Na,K)NbO3 Ceramics as a Function of K5.4Cu1.3Ta10O29 Addition)

  • 노정래;류주현;정영호
    • 한국전기전자재료학회논문지
    • /
    • 제23권5호
    • /
    • pp.379-382
    • /
    • 2010
  • In this study, in order to develop the lead-free piezoelectric ceramics with high piezoelectric and dielectric properties, $(K_{0.5}Na_{0.5})(Nb_{0.97}Sb_{0.03})O_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition. $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition enhanced density, electromechanical coupling factor($k_p$) piezoelectric constant $d_{33}$ and mechanical quality factor($Q_m$). At the 0.9 mol% $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition, density, electromechanical coupling factor($k_p$), dielectric constant(${\varepsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum values of 0.46, 471, and 148 pC/N, respectively.

$SrTiO_3$ 치환에 따른 (Na,K)$NbO_3$ 세라믹스의 압전 및 유전 특성 (Piezoelectric and Dielectric Properties of (Na,K)$NbO_3$ Ceramics as a Function of $SrTiO_3$ substitution)

  • 이상호;김도형;이일하;류주현
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2008년도 추계학술대회 논문집 Vol.21
    • /
    • pp.175-176
    • /
    • 2008
  • In this study, in order to develop the composition ceramics for lead-free ultrasonic motor, $[(K_{0.5}Na_{0.5})_{0.95}Li_{0.05}(Nb_{0.96}Sb_{0.04})]O_3$ ceramics were fabricated using $Ag_2O$ as sintering aid and a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $SrTiO_3$ substitution. $SrTiO_3$ substitution enhanced density, dielectric constant$(\varepsilon_r)$ and electromechanical coupling factor$(k_p)$. However, mechanical quality factor was deteriorated. At the 0.5mol% $SrTiO_3$ substitution, density, electromechanical coupling factor$(k_p)$, dielectric constant$(\varepsilon_r)$ and piezoelectric constant$(d_{33})$ of specimen showed the optimum value of 4.437g/$cm^3$, 0.457, 1294, 265pC/N, respectively.

  • PDF

BaTiO3 치환에 따른 NaNbO3-LiNbO3 세라믹스의 압전 및 유전특성 (Piezoelectric and Dielectric Properties of NaNbO3-LiNbO3 Ceramics according to the BaTiO3 Substitution)

  • 이상호;류주현;마석범;김성구
    • 한국전기전자재료학회논문지
    • /
    • 제22권3호
    • /
    • pp.205-209
    • /
    • 2009
  • In this study, in order to develop the composition ceramics for lead-free ultrasonic motor, (1-x-0.09)$NaNbO_{3-x}BaTiO_3-0,09LiNbO_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $BaTiO_3$ substitution. All the specimens showed orthorhombic phase structure without secondary phase, $BaTiO_3$ substitution enhanced density, dielectric constant(${\epsilon}_r$) and electromechanical coupling factor($k_p$), However, mechanical quality factor was deteriorated. Curie temperature of specimens was observed as about $380^{\circ}C$. At the $BaTiO_3$ substitution of 4 mol%, density, electromechanical coupling factor($k_p$), dielectric constant(${\epsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum value of $4.493g/cm^3$, 0.236, 175, 70 pC/N, respectively.