• 제목/요약/키워드: electrolytic material

검색결과 137건 처리시간 0.026초

플라즈마 전해 산화 코팅에 있어서 인산염 전해액과 모재 성분 변화가 Al 산화피막 물성에 미치는 영향 I. PEO층의 물성 (Effect of Na2P2O7 Electrolyte and Al Alloy Composition on Physical and Crystallographical Properties of PEO Coating Layer : I. Physical Properties of PEO Layer)

  • 김배연;김정곤;이득용;전민석;김용남;김성엽;김광엽
    • 한국세라믹학회지
    • /
    • 제49권3호
    • /
    • pp.241-246
    • /
    • 2012
  • Physical properties of plasma electrolytic oxidized layers of 8 different kinds of Al alloys, A-1100, A-2024, A-5052, A-6061, A-6063, A-7075, ACD-7B and ACD-12 were investigated. The electrolyte for plasma electrolytic oxidation was mixture of distilled water, $Na_2P_2O_7$, KOH and some metal salts. Growth rate of oxide layer was slower in $Na_2P_2O_7$ electrolyte system than in $Na_2SiO_3$ system, and Ra50 surface roughness of oxidized layer was below $1.2{\mu}m$. Surface hardness in $Na_2P_2O_7$ electrolyte system is higher than in $Na_2SiO_3$ system, and roughness was lower in $Na_2P_2O_7$ electrolyte system than in $Na_2SiO_3$ system.

PEO 처리조건에 따른 마그네슘 합금 AZ31과 AZ91의 산화표면피막특성에 대한 연구. I. 전압과 시간의 영향 (Effect of PEO Process Conditions on Oxidized Surface Properties of Mg alloy, AZ31 and AZ91. I. Applied Voltage and Time)

  • 함재호;전민석;김용남;신민철;김광엽;김배연
    • 한국전기전자재료학회논문지
    • /
    • 제29권4호
    • /
    • pp.218-224
    • /
    • 2016
  • The surface of Mg alloy, AZ31 and AZ91, were treated by PEO (plasma electrolytic oxidation) in Na-P system electrolyte, with different applied voltage and time. Thickness, roughness and X-ray crystallographic analysis revealed several results. The more applied time and voltage of PEO treated, the thicker oxidized surface coating layer were covered. And surface roughness increased with the thickness of oxidized layer. It was thought that when oxide layer grew, resistivity and breakdown voltage increased with the thickness of layer, and then, the energy of micro plasma need to be higher then before. So, it made craters and pores of surface become greater, which were responsible for the coarse surface.

전해구리막의 표면 조건과 어닐링 과정을 통한 그래핀 성장 최적화 (Optimizing Graphene Growth on the Electrolytic Copper Foils by Controlling Surface Condition and Annealing Procedure)

  • 이우진;고하은;구태림;이재성;이준우;홍순기;김상호
    • 한국표면공학회지
    • /
    • 제56권3호
    • /
    • pp.192-200
    • /
    • 2023
  • Graphene, a two-dimensional material, has shown great potential in a variety of applications including microelectronics, optoelectronics, and graphene-based batteries due to its excellent electronic conductivity. However, the production of large-area, high-quality graphene remains a challenge. In this study, we investigated graphene growth on electrolytic copper foil using thermochemical vapor deposition (TCVD) to achieve a similar level of quality to the cold-rolled copper substrate at a lower cost. The combined effects of pre-annealing time, graphenized temperature, and partial pressure of hydrogen on graphene coverage and domain size were analyzed and correlated with the roughness and crystallographic texture of the copper substrate. Our results show that controlling the crystallographic texture of copper substrates through annealing is an effective way to improve graphene growth properties, which will potentially lead to more efficient and cost-effective graphene production. At a hydrogen partial pressure that is disadvantageous in graphene growth, electrolytic copper had an average size of 8.039 ㎛2, whereas rolled copper had a size of 19.092 ㎛2, which was a large difference of 42.1% compared to rolled copper. However, at the proper hydrogen partial pressure, electrolytic copper had an average size of 30.279 ㎛2 and rolled copper had a size of 32.378 ㎛2, showing a much smaller difference of 93.5% than before. This observation suggests this potentially leads the way for more efficient and cost-effective graphene production.

전해환원공정에서 $Y_2O_2$ 코팅층의 부식거동 (Corrosion Behavior of $Y_2O_3$ Coating in an Electrolytic Reduction Process)

  • 조수행;홍순석;강대승;정명수;박병흥;허진목;이한수
    • 방사성폐기물학회지
    • /
    • 제8권1호
    • /
    • pp.33-39
    • /
    • 2010
  • 산화물 사용 후 핵연료를 처리하는 전해환원공정에서는 LiCl 용융염계에서 산소가 생성되는 반응을 수반하게 되며, 생성된 산소로 인해 반응기의 구조재료를 상당히 부식시킬 수 있는, 화학적으로 심각한 반응환경을 조성한다. 따라서, 고온 용융염을 다루는 전해환원 공정장치를 위해서는 최적의 재료를 선택하는 것이 필수적이다. 본 연구에 서는 리튬용융염, $675^{\circ}C$, 216시간동안 산화분위기에서 코팅이 안 된 초합금과 코팅된 초합금 시편의 고온 부식연구를 수행하였다. IN713LC 초합금 시편에 aluminized NiCrAlY bond 코팅 후 $Y_2O_3$ top 코팅을 하였다. 코팅이 안 된 초합금은 부식층의 빠른 성장응력과 열적응력에 의한 부식층의 박리로 명확한 무게손실을 보인다. 탑 코팅의 화학적 및 열적 안정성으로 인해 고온 리튬용융염을 다루는 구조재료의 부식 저항성이 증가함을 확인할 수 있었다.

자성연마슬러리를 이용한 초미립 초경합금(WC-Co 18%)의 나노급 경면가공 특성 (Machining Properties to Nano-Level Mirror Surface Finishing for Fine Grained WC-Co 18% Alloy using Magnetic Polishing Slurry)

  • 곽태수
    • 한국세라믹학회지
    • /
    • 제46권1호
    • /
    • pp.102-107
    • /
    • 2009
  • This study has been focused on an effective surface finishing method combining ELID (ELectrolytic In-process Dressing) and MAP (Magnetic Assisted Polishing) for the nano-precision mirror grinding of glass-lens molding mould. ELID grinding is an excellent technique for mirror grinding of various advanced metallic or nonmetallic materials. A polishing process is also required for elimination of scratches present on ELID grinded surfaces. MAP has been used as polishing method due to its high polishing efficiency and superior surface quality. It also presents some techniques for achieving the nanometer roughness of the hard material such as WC-Co, which are extensively used in precision tooling material.

알루미늄 합금의 전해연마 가공특성에 관한 연구 (A Study on machining characteristics of the Electropolishing of Aluminum alloy)

  • 이은상;김창근
    • 한국공작기계학회논문집
    • /
    • 제12권2호
    • /
    • pp.17-22
    • /
    • 2003
  • Electropolishing is the electrolytic removal of metal in a highly ionic solution by means of an electrical potential and current. It is normally used to remove a very thin layer of material on the surface of a metal part or component. Electropolishing is able to enhance the material properties of a workpiece and to change its physical dimensions. Also, It is suitable for the polishing of both complex shapes and hardened materials, which are difficult to machine mechanically. therefore, the aim of the present study is to investigate the characteristic of Electropolishing A12024 in terms of current density, polishing time and electrode gap, etc.

FORMATION OF AMORPHOUS NICKEL-PHOSPHORUS ALLOY FILM

  • Yamashita, Tsugito;Komiyama, Toyohiko
    • 한국표면공학회지
    • /
    • 제29권6호
    • /
    • pp.720-723
    • /
    • 1996
  • The behavior of electrodeposition of amorphous nickel-phosphorus has been studied from the point of deposition mechanism, kinetic parameters, morphology and formation of alloy films. The electorode reaction and electrode kinetics of deposition of nickel were significantly influenced by the content of phosphorus. The cathodic deposition of nickel-phosphorus alloy might be governed by the diffusion process of phosphorous acid. The direction of growth layer of the nickel-phosphorus alloy was different with substrate material. The formation of nickel-phosphorus alloy films was affected considerably by the solution compositions, electrolytic conditions and properties of the material as an underlayer.

  • PDF

전기분해 이온수를 이용한 세정기술 개발 (Development of new cleaning technology using ionized water by electrolysis)

  • 변문기;백희원;조봉희;김영호
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1999년도 추계학술대회 논문집
    • /
    • pp.617-620
    • /
    • 1999
  • To reduce the consumption of chemicals and ultra pure water(UPW) in cleaning process used in device manufacturing, we proposed wet processes that use electrolytic ionized water(EIW), which is generated by electrolysis of a diluted electrolyte solution or UPW and systemically investicate the EIW\`s characteristics. EIW\`s pH values are increased in cathode chamber and decreased in anode chamber according to the electrolysis time and its varied ratio is reduced with time increasement. The variation of pH and ORP is increased accordin to the applied voltage until critical voltage. But more than that voltage, the variation is decreased because of ion\`s scattering effect. When electrolyte is added, the effects of electrolysis is increased because electrolyte acts as catalyst. But when the density of electrolyte is increased more than critical value, ion\`s flowage is obstructed and the effects of electrolysis is decreased.

  • PDF

지르코늄의 제조(製造)와 재활용기술(再活用技術) (Overview of Zirconium Production and Recycling Technology)

  • 박경태;김승현;홍순익;최미선;조남찬;유환준;이종현
    • 자원리싸이클링
    • /
    • 제21권5호
    • /
    • pp.18-30
    • /
    • 2012
  • Zr은 고온에서의 높은 치수안정성, 내식성은 물론 낮은 중성자 흡수단면적을 지녀 원자력산업용 소재 중 1차 방사능 차폐재인 핵연료 피복관으로 사용되며 현재까지 다른 소재로 대체 불가능하다. 하지만 Hf을 정제한 Zr sponge 제조기술은 미국, 프랑스, 러시아만 가지고 있어 원자력의존도가 높은 한국에서는 국가전략물자로 분류 철저히 관리되고 있다. 국내 유통되는 Zr의 대부분은 원자력산업에 사용되어 지며 유통구조는 정제된 Zr합금을 국외로부터 수입하여 tube로 가공 후 핵연료집합체로 제조되고, 그 외 소량이 합금첨가원소 및 폭약재 등 고부가가치 일반산업에 사용된다. 본 논문에서는 Zr 제조기술에 대한 현재산업현황 및 정련기술을 살펴보고, 최근 연구되고 있는 Electrolytic reduction process와 Molten oxide electrolysis와 같은 신 제련기술에 대한 소개 및 Zr recycling의 전반적인 기술소개도 포함하였다.

플렉서블 Li/MnO2 일차전지의 제조공정에 따른 전기적 특성 (Electrical Characteristics According to the Manufacturing Process of the Flexible Li/MnO2 Primary Cell)

  • 이미재;채유진;김진호;황종희;박상선
    • 한국재료학회지
    • /
    • 제22권12호
    • /
    • pp.717-721
    • /
    • 2012
  • Manganese dioxide ($MnO_2$) is one of the most important cathode materials used in both aqueous and non-aqueous batteries. The $MnO_2$ polymorph that is used for lithium primary batteries is synthesized either by electrolytic (EMD-$MnO_2$) or chemical methods (CMD-$MnO_2$). Commonly, electrolytic manganese dioxide (EMD) is used as a cathode mixture material for dry-cell batteries, such as a alkaline batteries, zinc-carbon batteries, rechargeable alkaline batteries, etc. The characteristics of lithium/manganese-dioxide primary cells fabricated with EMD-$MnO_2$ powders as cathode were compared as a function of the parameters of a manufacturing process. The flexible primary cells were prepared with EMD-$MnO_2$, active carbon, and poly vinylidene fluoride (PVDF) binder (10 wt.%) coated on an Al foil substrate. A cathode sheet with micro-porous showed a higher discharge capacity than a cathode sheet compacted by a press process. As the amount of EMD-$MnO_2$ increased, the electrical conductivity decreased and the electrical capacity increased. The cell subjected to heat-treatment at $200^{\circ}C$ for 1 hr showed a high discharge capacity. The flexible primary cell made using the optimum conditions showed a capacity and an average voltage of 220 mAh/g and 2.8 V, respectively, at $437.5{\mu}A$.