• Title/Summary/Keyword: electrode thickness

Search Result 847, Processing Time 0.028 seconds

ANSYS Simulation of VHF Ceramic Resonator Using Thickness-longitudinal vibration mode (두께 진동모드를 이용한 고주파 세라믹 Resonator의 ANSYS Simulation)

  • 홍재일;윤현상;민석규;윤광희;류주현;김종선;박창엽
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2000.11a
    • /
    • pp.259-262
    • /
    • 2000
  • In this study, 3.1$\times$3.7$\times$0.365 $\textrm{mm}^2$ model of thickness-longitudinal vibration mode VHF ceramic resonator with (Pb,Ca)(Co,W,Ti)O$_3$ ceramics was simulated by ANSYS according to the electrode size. With the variations of electrode size of the model, fundamental and the third overtone dynamic ratio was investigated. At the ratio of electrode to model thickness(1/t) 2.5, third overtone dynamic ratio was largely increased. That model is suitable for 20 MHz resonator.

  • PDF

Optimization of Process Parameters for Dry Film Thickness to Achieve Superior Water-based Coating in Automotive Industries

  • Prasad, Pranay Kant;Singh, Abhinav Kr;Singh, Sandeep;Prasad, Shailesh Kumar;Pati, Sudhanshu Shekher
    • Corrosion Science and Technology
    • /
    • v.21 no.2
    • /
    • pp.121-129
    • /
    • 2022
  • A study on water-based epoxy coated on mild steel using the electroplating method was conducted to optimize the process parameters for dry film thickness to achieve superior paint quality at optimal cost in an automotive plant. The regression model was used to adjust various parameters such as electrode voltage, bath temperature, processing time, non-volatile matter, and surface area to optimize the dry film thickness. The average dry film thickness computed using the model was in the range of 15 - 35 ㎛. The error in the computed dry film thickness with reference to the experimentally measured dry film thickness value was - 0.5809%, which was well within the acceptable limits of all paint shop standards. Our study showed that the dry film thickness on mild steel was more sensitive to electrode voltage and bath temperature than processing time. Further, the presence of non-volatile matter was found to have the maximum impact on dry film thickness.

Study on optimal elctrode's thickness at passive OLED on power consumption

  • Kim, Sang-Gil;Park, Sung-Joon;Kim, Jeong-Hoon;Song, Keun-Joo;Kim, Hee-Je
    • Proceedings of the KIEE Conference
    • /
    • 2004.07c
    • /
    • pp.1945-1947
    • /
    • 2004
  • "CRT" which had dominated the market of display until 2000 is not appropriate for information indicating media due to several limitations. Thus, TFT-LCD, PDP, OLED, etc are growing in display industry instead of CRT because they meet demands of information indicating media. OLED display which responses within 1ms fits any picture manifestation medias because it uses self radiance OLED for picture clement that has no obstacles in showing the angle of vision. OLED's characteristic of action is very sensitive to thickness of electrode so that this has been an important issue. This study tried to find the most suitable thickness of electrode using ITO, Mo, and AL. Using the results of IVL measurements, analyzed equality of electrode board. As a result, found the thickness of electrode that has high electrical efficiency and optimized it.

  • PDF

A Study of Interface Layer on CdZnTe Radiation Sensor for Potable Isotope Identifier (이동형 핵종 분석 장치용 CZT 반도체 검출기의 완충전극에 대한 연구)

  • Cho, Yun Ho;Park, Se-Hwan;Kim, Yong Kyun;Ha, Jang Ho
    • Journal of Radiation Industry
    • /
    • v.5 no.1
    • /
    • pp.95-99
    • /
    • 2011
  • The electrical and mechanical properties of electrode for radiation detection are very important. In general, Au electrode and CZT crystal are combined to form ohmic contacts, and the best energy resolution is shown at the Au electrode. The metal contacts are fabricated by electroless deposition method, sputtering deposition method and thermal evaporation method. The electrode fabrication is easy with use of the thermal evaporation method, while an adhesive strength is weak. Thus interface materials such as Ag, Al and Ni were investigated to overcome defects generated by the this method. The thickness of the interface material between the Au electrode and the CZT crystal was 100 Angstroms, the Au electrode with thickness of 400 Angstroms was deposited. The Al+Au electrode is shown that the results of current-voltage and radiation response are similar to results of Au electrode.

Effect of Temperature on the Deterioration of Graphite-Based Negative Electrodes during the Prolonged Cycling of Li-ion Batteries

  • Yang, Jin Hyeok;Hwang, Seong Ju;Chun, Seung Kyu;Kim, Ki Jae
    • Journal of Electrochemical Science and Technology
    • /
    • v.13 no.2
    • /
    • pp.208-212
    • /
    • 2022
  • In this paper, we report the effects of temperature on the deterioration of graphite-based negative electrodes during the longterm cycling of lithium-ion batteries (LIBs). After cycling 75 Ah pouch-type LIB full cells at temperatures of 45℃ (45-Cell) and 25℃ (25-Cell) until their end of life, we expected to observe changes in the negative electrode according to the temperature. The thickness of the negative electrode of the cell was greater after cycling; that of the electrode of 45-Cell (144 ㎛) was greater than that of the electrode of 25-Cell (109 ㎛). Cross-sectional scanning electron microscopy analysis confirmed that by-products caused this increase in the thickness of the negative electrode. The by-products that formed on the surface of the negative electrode during cycling increased the surface resistance and decreased the electrical conductivity. Voltage profiles showed that the negative electrode of 25-Cell exhibited an 84.7% retention of the initial capacity, whereas that of 45-Cell showed only a 70.3% retention. The results of this study are expected to be relevant to future analyses of the deterioration characteristics of the negative electrode and battery deterioration mechanisms, and are also expected to provide basic data for advanced battery design.

Analysis on Variation of Primary Elements of Stainless Steel Interacting with Alkali Solution (알칼리 전해액의 상호작용에 의한 Stainless Steel 주성분의 변화 분석)

  • Byun, Chang-Sub;Lim, Soo-Gon;Kim, Su-Kon;Choi, Ho-Sang;Shin, Hoon-Kyu
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.26 no.7
    • /
    • pp.522-527
    • /
    • 2013
  • In this paper, We studied the change of surface and variation of elements on both electrodes of hydrogen generator of alkaline electrolysis in use of FE-SEM and SIMS. We used the stainless steel 316(600 ${\mu}m$) as electrode in condition of 25%KOH, $60^{\circ}C$ Temperature. The results show that the intensity of elements (C, Si, P, S, Ti, Cr, Mn, Fe, Ni, Mo) of Positive Electrode are decreased as much as about $10^1{\sim}10^3 $than the original electrode. Thickness of Positive Electrode is decreased about 40 ${\mu}m$ after chemical reaction. The negative electrode, however, shows a slight variation in the intensity of elements (C, Si, P, Fe, Ni, Mn, Mo) but Change of thickness and surface' shape of electrode show nothing after chemical reaction. The change in thickness and variation of Stainless Steel 316 cause the lifetime of electrode to be shorted. We also observed hydrogen, oxygen, potassium in both electrodes. Especially, The potassium is increased in proportional with depth of positive electrode. this means the concentration of alkali solutions is changed. and so we have to supply alkaline solution to generator in order to produce same quantity of hydrogen gas continuously. we hope that this study gives a foundation to develop the electrode for hydrogen generator of alkaline electrolysis.

Morphology and Electrical Properties of Back Electrode for Solar Cell Depending on the Mo : Na/Mo Bilayer Thickness (Mo : Na/Mo 이중층 구조 두께에 따른 태양전지 후면전극의 조직 및 전기적 특성)

  • Shin, Younhak;Kim, Myunghan
    • Korean Journal of Materials Research
    • /
    • v.23 no.9
    • /
    • pp.495-500
    • /
    • 2013
  • Mo-based thin films are frequently used as back electrode materials because of their low resistivity and high crystallinity in CIGS chalcopyrite solar cells. Mo:Na/Mo bilayer thin films with $1{\mu}m$ thickness were deposited on soda lime glass by varying the thickness of each layer using dc-magnetron sputtering. The effects of the Mo:Na layer on morphology and electrical property in terms of resistivity were systematically investigated. The resistivity increased from $159{\mu}{\Omega}cm$ to $944{\mu}{\Omega}cm$; this seemed to be caused by increased surface defects and low crystallinity as the thickness of Mo:Na layer increased from 100 nm to 500 nm. The surface morphologies of the Mo thin films changed from a somewhat coarse fibrous structures to irregular and fine celled structures with increased surface cracks along the cell boundaries as the thickness of Mo:Na layer increased. Na contents varied drastically from 0.03 % to 0.52 % according to the variation of Mo:Na layer thickness. The change in Na content may be ascribed to changes in surface morphology and crystallinity of the thin films.

Effect of Electrode Design on Electrochemical Performance of Highly Loaded LiCoO2 Positive Electrode in Lithium-ion Batteries (리튬이온 이차전지용 고로딩 LiCoO2 양극의 전극설계에 따른 전기화학적 성능연구)

  • Kim, Haebeen;Ryu, Ji Heon
    • Journal of the Korean Electrochemical Society
    • /
    • v.23 no.2
    • /
    • pp.47-55
    • /
    • 2020
  • Highly loaded LiCoO2 positive electrodes are prepared to construct high-energy density lithium-ion batteries, their electrochemical performances are evaluated. For the standard electrode, a loading of about 2.2 mAh/㎠ is used, and for a high-loading electrode, an electrode is manufactured with a loading level of about 4.4 mAh/㎠. The content of carbon black as electronic conducting additive, and the porosity of the electrode are configured differently to compare the effects of electron conduction and ionic conduction in the highly loaded LiCoO2 electrode. It is expected that the electrochemical performance is improved as the amount of the carbon black increases, but the specific capacity of the LiCoO2 electrode containing 7.5 weight% carbon black is rather reduced. When the conductive material is excessively provided, an increase of electrode thickness by the low content of the LiCoO2 active material in the same loading level of the electrode is predicted as a cause of polarization growth. When the electrode porosity increases, the path of ionic transport can be extended, but the electron conduction within the electrode is disadvantageous because the contact between the active material and the carbon black particles decreases. As the electrode porosity is lowered through the sufficient calendaring of the electrode, the electrochemical performance is improved because of the better contact between particles in the electrode and the reduced electrode thickness. In the electrode design for the high-loading, it is very important to construct the path of electron conduction as well as the ion transfer and to reduce the electrode thickness.

Electro-optic Characteristics of External Electrode Fluorescent Lamps Depending on the Glass Thickness

  • Yu, Mi-Yeon;Ko, Jae-Hyeon;Kim, Young-Youb;Kim, Kyung-Ran
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2009.10a
    • /
    • pp.703-706
    • /
    • 2009
  • The external electrode fluorescent lamp(EEFL) has recently been applied to backlight of LCD TV as a new light source. The dependence of the electro-optic characteristics of the EEFL used in direct-lit backlights on the glass thickness was examined in detail, and the ultraviolet(UV)-light efficiency was estimated. It was found that the lamp efficiency became larger as the glass thickness decreased if other conditions were the same.

  • PDF

Characterization of $V_2O_5$ thin films as a counter electrode for complementary electrochromic devices (상보형 전기변색소자용 $V_2O_5$박막의 대향전극 특성)

  • 조봉희;김영호
    • Electrical & Electronic Materials
    • /
    • v.9 no.7
    • /
    • pp.690-695
    • /
    • 1996
  • We have systematically investigated the characterization of V$_{2}$O$_{5}$ thin films as a counter electrode for lithium based complementary electrochromic devices. The V$_{2}$O$_{5}$ thin films were prepared by thermal vacuum evaporation with varing the substrate temperature and film thickness. In electrochromic devices for smart windows, the WO$_{3}$ thin films with 400-800 nm thickness require to be capable of reversibly injection 10-15 mC/cm$^{2}$ of lithium, which is readily accomplished charge-balanced switching in a V$_{2}$O$_{5}$ thin films with 100-150nm thick. The V$_{2}$O$_{5}$ thin films produces considerably small changes in optical modulation properties in the visible and near infrared region(500-1100 nm) compared to the amorphous WO$_{3}$ thin films on 10-15 mC/cm$^{2}$ of lithium injection and the V$_{2}$O$_{5}$ thin films can therefore act as a counter electrode to WO$_{3}$ in a lithium based complementary clectrochromic devices. After 10$^{5}$ coloration/bleaching switching time, the degradation does not occurs and the devices exhibit a stable optical modulation in V$_{2}$O$_{5}$ thin films. It has shown that the injected lithium ion amounts in crystalline V$_{2}$O$_{5}$ thin films with the same thickness is large by 3-5 mC/cm$^{2}$ of lithium compared to the amorphous thin films in the same driving conditions. Therefore, to optimize the device performance, it is necessary to choose an appropriate film thickness and crystallinity of V$_{2}$O$_{5}$ for amorphous WO$_{3}$ film thickness as a working electrode.

  • PDF