전기화학적 수소 주입에 의한 Ti-6Al-4V 합금의 미세조직과 수소 취성에 미치는 어닐링 처리의 영향 (Effect of Annealing Treatment on Microstructure and Hydrogen Embrittlement of Ti-6Al-4V Alloys Subject to Electrochemical Hydrogen Charging)

  • 고석우;이지민;권용남;황병철
    • 소성∙가공
    • /
    • 제29권4호
    • /
    • pp.211-217
    • /
    • 2020
  • This paper presents a study on the hydrogen embrittlement of Ti-6Al-4V alloys with different microstructures depending on annealing treatment. They were electrochemically charged with hydrogen and subjected to tensile tests to investigate hydrogen embrittlement behavior. Tensile test results showed that the elongation of Ti-6Al-4V alloy specimens was remarkably decreased with increasing the volume fraction of β phase after hydrogen charging. This is because the β phase with a relatively low diffusivity tends to easily form a hydride at grain boundaries during electrochemical hydrogen charging. After hydrogen charging of the Ti-6Al-4V alloy specimen, it found that silver particles were decorated mostly at the grain boundary, and coarser silver particles were usually formed in the specimen annealed at 950 ℃. Therefore, the specimen having higher β phase fraction shows a poor hydrogen embrittlement resistance because the β phase promotes the formation of coarse hydride during electrochemical hydrogen charging, which leads to a large decrease in ductility.

소형펀치 시험법을 이용한 INCONEL Alloy 617의 수소취화거동 평가 (Evaluation of Hydrogen Embrittlement Behavior in INCONEL Alloy 617 by Small Punch Test)

  • 서현욱;마영화;윤기봉
    • 한국수소및신에너지학회논문집
    • /
    • 제21권4호
    • /
    • pp.340-345
    • /
    • 2010
  • For the conversion into hydrogen society, not only studying facilities of hydrogen production, storage, transportation and charging system but also developing technique of ensuring safety are essentially needed. Hence, for the first step of that, evaluated the hydrogen embrittlement of Inconel alloy 617, Ni-based super heat-resisting alloy, by small punch test. Prepared the various specimens through changing electrochemical charging time and measured the toughness degradation of the specimens by small-punch test. The analysis of hydrogen embrittlement behavior were carried out by investigating the fractured surface of specimens. This study has significance on revealing mechanism of hydrogen embrittlement behavior and the factor affecting hydrogen embrittlement in the future study.

극저온용 오스테나이트계 Fe-30Mn-0.2C(-1.5Al) 고망간강의 수소 취화 특성 (Hydrogen Embrittlement Properties of Austenitic Fe-30Mn-0.2C(-1.5Al) High-Manganese Steels for Cryogenic Applications)

  • 이상인;이지민;황병철
    • 열처리공학회지
    • /
    • 제31권6호
    • /
    • pp.283-289
    • /
    • 2018
  • This present study deals with the hydrogen embrittlement properties of austenitic Fe-30Mn-0.2C(-1.5Al) high-manganese steels for cryogenic applications. They were electrochemically charged with hydrogen and then subjected to tensile tests for evaluating hydrogen embrittlement behavior. Tensile test results showed that after hydrogen charging the tensile strength and elongation of the Al-free steel were more remarkably decreased with increasing current density when compared to the Al-added steel. After hydrogen charging of the Al-added steel, it was found that the measured hydrogen content was small and silver particles were relatively less decorated. Therefore, the Al-added steel has a superior hydrogen embrittlement resistance to the Al-free steel because the addition of Al suppresses the injection of hydrogen during electrochemical hydrogen charging.

전기화학적 방법으로 수소장입시킨 자동차 강판재의 수소 영향 (The Effect of Hydrogen in Automobile High Strength Steel Sheets Charged with Hydrogen by Using Electrochemical Method)

  • 박재우;강계명
    • 한국표면공학회지
    • /
    • 제45권5호
    • /
    • pp.212-217
    • /
    • 2012
  • High strength steel sheets used for automobile outer-panels have been intensively studied for developing a lightweight automobile under a strong pressure of the requirements for enhancing the mileage and energy saving in production of automobile parts. It is known that high strength steels are susceptible to hydrogen embrittlement, The susceptibility to hydrogen embrittlement increases with increasing its strength. However, the effect of hydrogen on the fracture behavior of high strength steels, though investigated extensively, has not been fully understood. In this paper, hydrogen was charged with 590DP steels by electrochemical method and its content was measured by hydrogen determinator with the different charging conditions. It was shown that the SP energy and maximum load decreased with increasing charging time. The results of SEM-fractography investigation for the hydrogen contained samples showed that a small portion of dimples on cleavage-fractured surface were observed and the size of the dimples were decreased with increasing hydrogen charging time.

수소주입된 고강도 DP 박강판의 소형펀치시험결과 분석 (An Analysis of Small Punch Test Conducted with the High Strength Dual Phase Sheet Steels Charged with Hydrogen)

  • 최영철;박재우;강계명
    • 한국표면공학회지
    • /
    • 제46권5호
    • /
    • pp.229-233
    • /
    • 2013
  • The small punch(SP) tests that can be applied to high strength sheet steel in automobile were carried out to evaluate the behavior of hydrogen embrittlement of DP sheet steels. In order to charge hydrogen at DP sheet steels, DP sheet steels were treated by the electrochemical hydrogen charging method under the charging conditions of current densities of 100, 150 and 200 $mA/cm^2$ for charging times of 5, 10, 25 and 50 hrs. Respectively, After hydrogen charging with experimental conditions, SP tests were performed. From the SP results, the correlations between the variation of bulb diameters and bulb heights with the hydrogen charging conditions were analysed. It was shown that the variation of bulb diameters were not significant with the hydrogen embrittlement due to the amounts of hydrogen charging. On the other hand, the bulb heights were observed to decrease with increasing hydrogen contents. It was thought that these results of the variation of bulb shapes after SP tests would be estimated as the index of evaluation of hydrogen embrittlement.

Effect of Hydrogen Charging Time and Tensile Loading Speed on Tensile Properties of 304L Stainless Steels

  • Hwang, SeungKuk;Lee, Sangpill;Lee, Jinkyung;Bae, Dongsu;Lee, Moonhee;Nam, Seunghoon
    • 한국산업융합학회 논문집
    • /
    • 제22권1호
    • /
    • pp.11-20
    • /
    • 2019
  • This study dealt with the tensile strength characteristics of stainless steel 304L steel by hydrogen charging. Especially, the effect of hydrogen charging time on the tensile strength and ductility of 304L stainless steels was evaluated, in conjunction with the observation of their fracture surfaces. The tensile properties of hydrogen-charged 304L stainless steels were also investigated with the variation of tensile loading speeds. The hydrogen amount of 304L stainless steels obviously increased with the increase of hydrogen charging time. The tensile properties of 304L stainless steels were clearly affected by the short term charging of hydrogen. In particular, the elongation of 304L stainless steels decreased with increasing hydrogen charging time, due to the hydrogen embrittlement. It was also found that the tensile properties of hydrogen-charged 304L stainless steels were very sensitive to the crosshead speed for tensile loading.

미소경도 측정에 의한 590DP강 Subsurface Zone 내 수소취성 평가 (Hydrogen Embrittlement Evaluation of Subsurface Zone in 590DP Steel by Micro-Vickers Hardness Measurement)

  • 최종운;박재우;강계명
    • 한국재료학회지
    • /
    • 제21권11호
    • /
    • pp.581-586
    • /
    • 2011
  • This study describes a hydrogen embrittlement evaluation of the subsurface zone in 590DP steel by micro-Vickers hardness measurement. The 590DP steel was designed to use in high-strength thin steel sheets as automotive materials. The test specimens were fabricated to 5 series varying the chemical composition through the process of casting and rolling. Electrochemical hydrogen charging was conducted on each specimen with varying current densities and charging times. The relationship between the embrittlement and hydrogen charging conditions was established by investigating the metallography. The micro-Vickers hardness was measured to evaluate the hydrogen embrittlement of the subsurface zone in addition to the microscopic investigation. The micro-Vickers hardness increased with the charging time at the surface. However, the changing ratio and maximum variation of hardness with depth were nearly the same value for each test specimen under the current density of 150 mA/$cm^2$ and charging time of 50 hours. Consequently, it appears that hydrogen embrittlement in 590DP steel can be evaluated by micro-Vickers hardness measurement.

다상조직강의 조직 분율에 따른 수소주입의 영향 (The Influence of Hydrogen Charging with the Volume Fraction of Phases in Dual Phase Steels)

  • 김한상;강계명
    • 한국표면공학회지
    • /
    • 제45권6호
    • /
    • pp.284-288
    • /
    • 2012
  • A study on microstructure control of multi-phase steel have been implemented to higher strength with improved formability. However, it is well known that the high strength of steel are susceptible to hydrogen embrittlement. The mechanisms of hydrogen embrittlement is caused by complex interactions. In this paper, the test specimens were fabricated to 5 type of 590DP steels at different levels of volume faction. The hydrogen charging was conducted by electrochemical hydrogen-charge method with varying charging time. The relationship between hydrogen concentration and volume fraction of 590DP steel was established by SP test and SEM-fractography. It was shown that the hydrogen amounts charged in 590DP steels increased with increasing the volume faction of austenite. The maximum loads of the 590DP steels in SP test were sharply decreased with increasing hydrogen charging time. The results of SEM-fractography investigation showed typical brittle-fracture surfaces for hydrogen-charged 590DP steels.

소형펀치시험에 의한 TRIP강의 수소 지연파괴 거동 (Hydrogen Delayed Fracture of TRIP Steel by Small Punch Test)

  • 최종운;박재우;강계명
    • 한국표면공학회지
    • /
    • 제46권1호
    • /
    • pp.42-47
    • /
    • 2013
  • The strain-induced phase transformation from austenite to martensite is responsible for the high strength and ductility of TRIP steels. However high strength steels are susceptible to hydrogen embrittlement. This study aimed to evaluate the effects of hydrogen on the behavior of hydrogen delayed fracture in TRIP steel with hydrogen charging conditions. The electrochemical hydrogen charging was conducted at each specimen with varying current density and charging time. The relationship between hydrogen concentration and mechanical properties of TRIP steel was established by SP test and SEM fractography. The maximum loads and displacements of the TRIP steel in SP test decreased with increasing hydrogen charging time. The results of SEM fractography investigation revealed typical brittle mode of failure. Thus it was concluded that hydrogen delayed fracture in TRIP steel result from the diffusion of hydrogen through the ${\alpha}$' phase.

2종 전해질에서의 전기화학적 수소주입조건에 따른 680 MPa DP 박강판의 수소취성 (Hydrogen Embrittlement of 680 MPa DP sheet steel with Electrochemical Hydrogen charging conditions of Two Electrolytes)

  • 박재우;강계명
    • 한국표면공학회지
    • /
    • 제47권5호
    • /
    • pp.257-262
    • /
    • 2014
  • In this paper, the behavior of hydrogen embrittlement of 680MPa DP sheet steel according to hydrogen charging conditions in acid and alkali electrolytes atmosphere was investigated. At this time, 0.5 M $H_2SO_4$ and 0.5M NaOH was used for electrolytes atmosphere and the effect on embrittlemnet of 680MPa DP sheet steel according to current density and charging time was evaluated by the change of subsurface microhardness in DP specimens chared hydrogen. As a result of this experiment, the microhardness of the layer directly below the surface was increased more than the microhardness of the subsurface zone in both electrolytes cases, but the change of the subsurface microhardness in both electrolytes was more affected by the increase of charging time than the increase of current density. The microhardness of subsurface zone in 0.5 M $H_2SO_4$ acid electrolyte was increased more than the microhardness in 0.5M NaOH alkali electrolyte. It was supposed that acid atmosphere was more sensitive to hydrogen embrittlement than alkali atmosphere on electrolyte atmosphere of hydrogen charge.