Mechanical and Magnetic Properties Variation of YBCO Superconductors with Resin and Ag Impregnation (Resin, Ag를 첨가한 YBCO 초전도체의 기계, 자기적 특성 변화)

  • Lee, N.I.;Jang, G.E.;Kim, C.J.;Jung, S.Y.;Han, Y.H.;Sung, T.H.
    • Progress in Superconductivity
    • /
    • v.8 no.1
    • /
    • pp.119-121
    • /
    • 2006
  • We studied the mechanical and magnetic properties of Y-Ba-Cu-O superconductor with and without resin and Ag impregnation. Bulk YBCO superconductor was manufactured with the top-seeded melt-growth method. Typical sample of 40mm X 20mm X 3mm was made and then 8 holes with 0.5mm diameter were drilled arbitrally. Epoxy resin and $AgNO_3$ were systematically added into the holes to compare the mechanical and magnetic properties of YBCO superconductor before and after reinforcement of resin and Ag. Based on the result of 3 point bending, bending strength increased with increasing amounts of resin and carbon nano-tube. However, it was found that the levitation force decreased after making hole, compared with virgin sample without hole.

  • PDF

Effect of Ethylene Inhibitors on In Vitro Shoot Multiplication and their Impact on Ethylene Production in Cucumber (Cucumis sativus L.)

  • Vasudevan A.;Selvaraj N.;Ganapathi A.;Anbazhagan V. Ramesh;Choi, C.W.
    • Journal of Plant Biotechnology
    • /
    • v.33 no.4
    • /
    • pp.249-255
    • /
    • 2006
  • Effects of ethylene inhibitors like silver nitrate $(AgNO_3)$, cobalt chloride $(CoCl_2)$ and Salicylic acid (SA) on multiple shoot induction and their impact on ethylene production using embryonal cotyledon cultures of Cucumis sativus L. were examined. The optimum concentration of $AgNO_3\;(40{\mu}M),\;CoCl_2\;(20{\mu}M)\;and\;SA\;(20{\mu}M)$, separately, induced maximum number of shoots on Murashige and Skoog's (MS) medium supplemented optimally with $4.44{\mu}M$ BA and $0.25{\mu}M$ NAA. Among the three ethylene inhibitors tested, $AgNO_3$ produced maximum number of shoots when compared to $CoCl_2$ and SA Ethylene production was monitored in all the treatments with $AgNO_3/CoCl_2/SA$ and it was observed that the treatment with $AgNO_3$ alone showed increase in ethylene production when compared to $CoCl_2$ and SA Even though ethylene concentration was the highest in $AgNO_3$ treated explants, maximum number of shoots was obtained.

RF Sputtering 방법으로 증착시킨 ZnO:Ag 박막의 광학적 특성 연구

  • An, Byeong-Gon;Gang, Hyeon-Cheol
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.424-424
    • /
    • 2012
  • 나노 구조의 반도성 산화물은 독특한 구조적 특성으로 전기적, 광학적 특성을 향상 시킬 수 있다. 현재 연구되고 있는 나노 구조의 반도성 산화물 중 Zinc oxide (ZnO)는 3.37 eV의 bandgap를 갖는 wurtzite 구조체로서 상온에서 60 meV의 exciton binding energy 등 우수한 특성으로 인하여 최근 많이 연구되고 있다. 특히 단파장 light emitting diode 재료로써 기대를 모으고 있는데, 이를 실현하기 위한 가장 큰 문제점이 바로 안정적인 p-type ZnO 박막의 제조이다. 지금까지 알려진 바에 따르면 P를 doping한 후 급속 열처리한 경우 p-type의 전기전도도를 갖는 ZnO 박막을 제조할 수 있다고 보고되어 있으나 vacancy 농도에 따른 불안정적인 요소가 해결해야 할 문제로 남아 있다. 최근 Ag를 doping 시킨 ZnO 박막의 p-type 반도체로서 가능성에 대한 보고가 제기되고 있다. 합성 방법과 조건에 따라서 수 nm에서 수십 또는 수백 nm 크기의 구형 입자나, 리본, 와이어, 로드 그리고 꽃모영 등 다양한 형상을 갖는 나노 구조체를 합성 할 수 있다. 본 연구에서는 ZnO:Ag 박막을 radio-frequency sputtering 방법으로 증착하여 그 물성을 분석하였다. 보통의 sputtering 증착법에서 사용되는 sintering된 타겟과 달리 본 실험은 분말 타겟을 이용하여 박막을 증착하였다. 타겟은 95 wt% ZnO와 5 wt% Ag를 서로 혼합하여 제조하였다. 본 발표에서는 박막의 증착압력 및 증착 온도의 변화에 따른 ZnO:Ag 박막의 구조적, 광학적 특성에 대하여 논의 할 것이다.

  • PDF

Growth and Optical Properties for $AgGaSe_2$ Single Crystal Thin Films by Hot Wall Epitaxy (Hot Wall Epitaxy (HWE)법에 의한$AgGaSe_2$ 단결정 박막 성장과 광학적 특성)

  • Hong, Kwang-Joon;Back, Seoung-Nam
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.124-127
    • /
    • 2003
  • The stochiometric $AgGaSe_2$ polycrystalline mixture of evaporating materials for the $AgGaSe_2$ single crystal thin film was prepared from horizontal furnance. To obtain the single crystal thin films, $AgGaSe_2$ mixed crystal and semi-insulating GaAs(100) wafer were used as source material and substrate for the Hot Wall Epitaxy (HWE) system, respectively. The source and substrate temperature were fixed at $630^{\circ}C$ and $420^{\circ}C$, respectively. The thickness of grown single crystal thin films is $2.1{\mu}m$. The single crystal thin films were investigated by photoluminescence and double crystal X-ray diffraction(DCXD) measurement. From the photoluminescence measurement of $AgGaSe_2$ single crystal thin film, we observed free excition ($E_x$) observable only in high quality crystal and neutral bound excition ($D^{\circ}$,X) having very strong peak intensity. And, the full width at half maximum and binding energy of neutral donor bound excition were 8 meV and 14.1 meV, respectively. By Haynes rule, an activation energy of impurity was 141 meV.

  • PDF

Silver (I)- Schiff-base complex intercalated layered double hydroxide with antimicrobial activity

  • Barnabas, Mary Jenisha;Parambadath, Surendran;Nagappan, Saravanan;Chung, Ildoo;Ha, Chang-Sik
    • Advances in nano research
    • /
    • v.10 no.4
    • /
    • pp.373-383
    • /
    • 2021
  • In this work, silver nitrate complexes of sulfanilamide-5-methyl-2-thiophene carboxaldehyde (SMTCA) ligand intercalated Zn/Al-layered double hydroxide [Ag-SMTCA-LDH] were synthesized for the potential application as an antimicrobial system. The SMTCA ligand was synthesized by reacting sulfanilamide and 5-methyl-2-thiophene carboxaldehyde in methanol and further complexation with silver nitrate metal ions [Ag-SMTCA]. The structural analyses of synthesized compounds confirmed an intercalation of Ag-SMTCA into Zn/Al-NO3-LDH by flake/restacking method. SMTCA, Ag-SMTCA and Ag-SMTCA-LDH were characterized by 1H nuclear magnetic resonance (1H NMR) spectroscopy, Fourier-transform infrared (FTIR), ultraviolet-visible (UV-Vis) spectrophotometer, scanning electron microscopy (SEM) and transmission electron microscopy (TEM), X-ray diffraction (XRD), and thermogravimetric analysis (TGA). It was found that Ag-SMTCA-LDH exhibited good antimicrobial activity against both gram-positive (Bacillus subtilis, [B. subtilis], Staphylococcus aures, [S. aureus]) and gram-negative (Escherichia coli, [E. coli], Pseudomonas aeruginosa [P. aeroginosa]) bacteria as well as excellent antioxidant activity.

Toxicity Assessment of Silver Ions Compared to Silver Nanoparticles in Aqueous Solutions and Soils Using Microtox Bioassay (Microtox 생물검정법을 이용한 은 이온과 은 나노입자의 수용액과 토양에서의 독성 비교 평가)

  • Wie, Min-A;Oh, Se-Jin;Kim, Sung-Chul;Kim, Rog-Young;Lee, Sang-Phil;Kim, Won-Il;Yang, Jae E.
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.45 no.6
    • /
    • pp.1114-1119
    • /
    • 2012
  • This study was conducted to assess the microbial toxicity of ionic silver solution ($Ag^+N$) and silver nanoparticle suspension ($Ag^0NP$) based on the Microtox bioassay. In this test, the light inhibition of luminescent bacteria was measured after 15 and 30 min exposure to aqueous solutions and soils spiked with a dilution series of $Ag^+N$ and $Ag^0NP$. The resulting dose-response curves were used to derive effective concentration (EC25, $EC_{50}$, EC75) and effective dose ($ED_{25}$, $ED_{50}$, $ED_{75}$) that caused a 25, 50 and 75% inhibition of luminescence. In aqueous solutions, $EC_{50}$ value of $Ag^+N$ after 15 min exposure was determined to be < $2mg\;L^{-1}$ and remarkably lower than $EC_{50}$ value of $Ag^0NP$ with $251mg\;L^{-1}$. This revealed that $Ag^+N$ was more toxic to luminescent bacteria than $Ag^0NP$. In soil extracts, however, $ED_{50}$ value of $Ag^+N$ with 196 mg kg-1 was higher than $ED_{50}$ value of $Ag^0NP$ with $104mg\;kg^{-1}$, indicating less toxicity of $Ag^+N$ in soils. The reduced toxicity of $Ag^+N$ in soils can be attributed to a partial adsorption of ionic $Ag^+$ on soil colloids and humic acid as well as a partial formation of insoluble AgCl with NaCl of Microtox diluent. This resulted in lower concentration of active Ag in soil extracts obtained after 1 hour shaking with $Ag^+N$ than that spiked with $Ag^0NP$. With longer exposure time, EC and ED values of both $Ag^+N$ and $Ag^0NP$ decreased, so their toxicity increased. The toxic characteristics of silver nanomaterials were different depending on existing form of Ag ($Ag^+$, $Ag^0$), reaction medium (aqueous solution, soil), and exposure time.

Wettability Evaluation of Sn-0.3Ag-0.7Cu Solder Alloy with Different Flux Activity and Indium Addition (플럭스 활성도 및 In 첨가에 따른 Sn-0.3Ag-0.7Cu 솔더 조성의 젖음 특성 변화)

  • Yu, A-Mi;Kim, Jun-Ki;Kim, Mok-Soon;Hyun, Chang-Yong;Lee, Jong-Hyun
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.15 no.4
    • /
    • pp.51-57
    • /
    • 2008
  • In this paper, wetting and interfacial reaction properties for low Ag containing Sn-Ag-Cu Pb-free solder alloy, i.e., Sn-0.3Ag-0.7Cu were investigated and compared with those of Sn-1.0Ag-0.5Cu and Sn-3.0Ag-0.5Cu. Melting behavior and stress-strain curves of some Sn-xAg-xCu alloys were also measured using a differential scanning calorimeter(DSC) and a tensile test machine, respectively. In order to enhance insufficient wetting properties of Sn-0.3Ag-0.7Cu alloy, the improvement of wetting properties were analyzed by applying fluxes containing higher content of halide or indium adding of 0.2wt.% into the solder alloy. It was concluded that the small addition of indium is more effective for the improvement of wettability in low temperature range of $230{\sim}240^{\circ}C$ than applying flux containing higher content of halide.

  • PDF

The U-type Model on Ag Doping effect in Amorphous Chalcogenide thin films (비정질 칼코게나이드박막으로서의 Ag 도핑효과에 대한 U-형 모델)

  • 김민수;이현용;정홍배
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1995.05a
    • /
    • pp.50-53
    • /
    • 1995
  • In this paper we have obtained property by considering the change of optical energy gap as a function of photo-does for exposing photo on Ag/a-Se$\sub$75/Ge$\sub$25/ thin films. This U-type property was obsered for all photo-exposing except for blu-pass filtered Hg lamep. Expecially, very large band shift(~0.3[eV]) is obtained by exposing He-Ne laser (6328[${\AA}$]). It is impossible to explain this property for exposing He-Ne and semiconductor laser through DWP model, which was explained for photo-exposing above the energy gap. Therefore we suggest a new modified model of DWP model for Ag/a-Se$\sub$75/Ge$\sub$25/ bilayer thin films.

  • PDF

Morphology Control of Ag-doped ZnO Nanowires by Hot-walled pulse Laser Deposition

  • Kim, Gyeong-Won;Song, Yong-Won;Kim, Sang-Sik;Lee, Sang-Ryeol
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.04b
    • /
    • pp.25-26
    • /
    • 2009
  • We design and demonstrate the controlled morphologies of Ag-dpped ZnO nanowires (NWs) adopting self-contrived hot-walled pulsed laser deposition (HW-PLD). p-type Ag-doping is ensuired by low temperature photoluminescence (PL) spectrum to find the AoX peak at 3.349 eV. Morphology of grown NWs are controlled by changing the kinetic energy and flux of the ablated particles with adjusting the target - substrate (T-S) distance. The analysis on the resultant NWs is presented.

  • PDF

Luminacne Efficiency Improvement of OLED through Optical Interference Effect (광학적 간섭효과에 따른 OLED의 발광효율 개선)

  • Lim, J.S.;Lee, B.J.;Shin, P.K.;Kim, S.J.;Cheong, M.Y.;Lee, E.H.;Kim, D.H.;Jin, K.S.
    • Proceedings of the KIEE Conference
    • /
    • 2008.07a
    • /
    • pp.1275-1276
    • /
    • 2008
  • In this study, a micro-cavity organic light-emittingdevice (OLED) with semi-transparent-Ag/AgO hole injecting layer (HIL) was fabricated and their performance was investigated. For the fabrication of OLEDs N,N-diphenyl-N,N-(3-methyphenyl)-1,1-biphenyl-4-4-diamine (TPD), known as a hole transporting material and tris (8-hydroxyquinolinato)-aluminum ($Alq_3$) as both electron-transporting layer (ETL) and emission layer (EML) were deposited using thermal evaporation technique. And Al layer as cathode was then deposited using thermal evaporation technique. Effects of the semi-transparent-Ag/AgO layers on the resulting OLED performance were investigated.