숯을 이용한 견직물의 염색 (Dyeing of Silk Fabrics Using Charcoals)

  • 조원주;이정숙
    • 한국의류학회지
    • /
    • 제29권2호
    • /
    • pp.279-285
    • /
    • 2005
  • In order to activate the characteristics of charcoals in fiber systems, this study was carried out to experiment with the particle size from two micrometers to ten micrometers of charcoal powders on silk fabrics. The results obtained were as follows; The silk fabrics were dyed with gray color by charcoals effectively. The K/S value, that is indicative of the dye affinity, became higher as the increase of dyeing temperature, dyeing time, and dyeing concentration. Te dyeing effects were the highest with 50%(o.w.f.) of charcoals at $100^{\circ}C$ for 120 minutes in this experiments, It was observed the surfaces of silk fibers were mainly adcorbed with charcoal powders of the particle size from two micrometers to four micrometers by scanning electron microscope. Dyed silk fabrics showed comparatively low fastness to the fade of launding, the stain of the treatment of perspirations, and the strain of water fastness test, but good fastness to the stran of laundering, te drycleaning, the fade of treatment of perspirations, and the fade of water fastness test. In connection with the functional properties of dyed fabrics, the deodorizations were drastically improved, and the far-infrared emissions improved highly, and also the antibacterials were comparatively good.

복합 천연염색한 면직물의 밀도 및 강도 변화 (The Change of Density and Tensile Strength on Cotton with Complexed Natural Dyeing)

  • 박영미
    • 한국염색가공학회지
    • /
    • 제35권4호
    • /
    • pp.189-195
    • /
    • 2023
  • In this study, as one of the eco-friendly dyeing methods, indigo, Phellodendron amurense and Caeasapinia sappan were complexed dyed on cotton fabric. For complexed dyeing, the cotton that was pre-dyed 5 times with indigo was dyed 1 ~ 2 times repeatedly with Phellodendron amurense and Caeasapinia sappan. Then the color, tensile strength, density, and color fastness of complexed dyed sample were analyzed and the following analysis results could be obtained. As a result of color difference measurement, the L* value was 22.7 in the sample in which the cotton was dyed 5 times and then the Phellodendron amurense was dyed 1 time, and the K/S value was 15 or higher in all samples. As a result of measuring the strength, cotton fabrics tended to have a slight decrease in tensile strength when complexed dyeing. As a result of measuring the density, the density decreased by 15 ~ 20% in all samples at the warp and increased by 20 ~ 30% in the weft due to the complexed dyeing of cotton fabric. Moreover, the fastness to washing and drycleaning showed good results of 2 ~ 3 or higher, and the light fastness was 4 or higher.

직물의 피노에 관한 연구 -착용에 의한 역학적 성질과 태의 변화- (A Study on the Fatigue Phenomena of Woven Fabrics -On the Changes of Mechanical Properties and Handle of Woven Fabrics Caused by the Wearing-)

  • 서영숙
    • 한국의류학회지
    • /
    • 제10권1호
    • /
    • pp.47-57
    • /
    • 1986
  • The purpose of this study is to investigate fatigue phenomema of woven fabric. In order to obtain the basic data which is available for predicting the fabric fatigue phenomena, the change of mechanical properties of woven fabrics caused by the wearing and the changes of mechanical properties of woven fabrics which were subjected to repeated tensile-shearing deformation using fabric testing machine has been investigated and compared. The fatigue of woven fabrics was examined with the value of basic mechanical properties of specimens measured by the KES-F fabric testing system and their hand value and wearing ability. The results were as follows. 1) The fatigue phenomena of woven fabrics by the wearing for 800 hours are different on the position of the body: On the portion of hip, the change of surface property was the greatest, bending hysterisis was greatly increased, thickness weight, stiffness, fullness shearing hysterisis were more increased than original fabric and T.H.V. was decreased. On the portion of knee, decreasing of tensile resilience and increasing of bending, shearing hysterisis were observed greater than any other part, and increasing of stiffness, crispness was more than original fabric. On the bottom area, the changes of mechanical property was comparatively small, H.V. and T.H.V. showed near the value of the original fabric. 2) By drycleaning most of mechanical properties showed the tendency to recover the value of the original fabric, but bending hysterisis and thickess were increased, tensile and com-pression resilience were decreased more than original fabric in all parts. 3) The fatigue phenomena caused by fabric fatigue testing machine were as follows. The decreasing of hystersis in the repeated deformation such as bending, shearing was appeared at the $10^2$ deformation, but with the increasing cycle, the tendency was slightly regained. Handle value was also appeared the lowest value at the $10^2$ deformation.

  • PDF

일부 세탁소의 유기용제 관리실태 및 공기중 노출농도에 관한 조사 (A Survey on the Management of Chemical Substances and Airborne Concentration in Laundries Exposed to Organic Solvents)

  • 노영만;권기범;박승현;정지연
    • 한국산업보건학회지
    • /
    • 제11권1호
    • /
    • pp.70-77
    • /
    • 2001
  • This study was conducted to identify the current status of occupational safety and health by checklist and to evaluate the airborne exposure to chemicals and to provide the appropriate recommendation for safety and health of laundries. A total of 20 laundries located in tile Gyungi district area were surveyed from July 20 to September 15, 2000. The prevalence of laundries having a stove and gas range were found to be 25 % and 55 %, respectively. Smoking is not allowed in 60 % of the laundries. Only 10 % of dry-cleaners were isolated. Ventilation systems in laundries had not been annually inspected. Most of the workers didn't put on respirators, MSDS were not available, and storage bottles did not contain warning labels. The bulk samples of dry cleaning agent include many chemicals that are not controlled by the MOL in Korea. The detected airborne organic solvents in the laundries were benzene, toluene, p-xylene, m-xylene, o-xylene, perchloroethylene, and 2-butoxy ethanol. The airborne concentrations of organic solvents were much less than the occupational exposure limits proposed by the Ministry of Labor(MOL) in Korea. But the concentrations of benzene exceeded the TLV of ACGIH. This study showed that the current status of occupational safety and health was not appropriate for workers in laundries. It is recommended that laundry workers should be educated for the treatment and storage of hazardous organic solvents to improve the occupational safety and health of the working environment as well as MSDS usage. Also, extended research and survey for the organic solvents that are not controlled by the MOL has to be conducted.

  • PDF

드라이클리닝 시스템에서의 세척성과 재오염성 -계면활성제의 종류와 혼합이 미치는 영향- (Detergency and soil Redeposition in a Drycleaning System -The Effect of Surfactant Type and Their Mixture-)

  • 김주연;박정희
    • 한국의류학회지
    • /
    • 제23권7호
    • /
    • pp.1030-1039
    • /
    • 1999
  • The effect of surfactant mixture 9on detergency and soil redeposition in a dry-cleaning system was investigated employing Aerosol OT as an anionic surfactant and Span 80 as a nonionic surfactant. The effect of charge system on soil deposition was also investigated in order to determine the optimum condition at which soil redeposition is minimum,. Soil deposition instead of soil redeposition on cotton, polyester and wool fabrics was measured employing petroleum solvent and perchloroethylene as organic solvents. The results were as follows. 1. Surface tension or interfacial tension was not changed by the addition of any surfactant or surfactant mixtures. In petroleum solvent however interfacial tension between solrent and water decreased when surfactants were added and increased when surfactants were mixed,. 2. The maximum amount of water solubilization increased as the mole fraction of Aerosol OT increased and more water was solubilized in petroleum solvent than in perchloroethylene. 3. The detergency of cotton was greater and the soil deposition rate was lower in Span 80 solution than in Aerosol OT solution. The soil deposition on cotton fabric decreased when water was solubilized in Aersol OT solution 4. The detergency and soil deposition rate of polyester fabric did not change by the surfactant type of the addition of surfactant mixture and soil deposition rate increased bywater solubilization. 5. Soil deposition on wool fabric was very high when Arosol OT was employed in perchloroethylene and the soil deposition did not change greatly by water solubilization.

  • PDF

백굴채 추출물을 이용한 염색직물의 염색성 및 기능성 (The Dyeing Properties and The Functionality of Fabrics Dyed with Chelidonium Majus Extract)

  • 박영희
    • 한국의류산업학회지
    • /
    • 제10권2호
    • /
    • pp.242-248
    • /
    • 2008
  • This study was aimed to find whether the Chelidonium majus which grows naturally in Korean soil and has a various medical ingredient is valuable as a natural dyeing material and to examine the functionality of Chelidonium majus extract. As the test result of dyeing colorfastness, colorfastness to sunlight was 1st grade for all the dyed fabrics. The colorfastness to laundry for discoloration showed from 1st to 4th grade and that for discoloration showed from 4th to 5th grade through all the dyed fabrics. Colorfastness to perspiration, rubbing, and drycleaning showed from 4th to 5th grade through all the dyed fabrics. In the result of antibiosis test, the dyed cotton fabric showed the bacteria reduction rate of 99.0% for Staphylococcus aureus and Escherichia coli evenly when washed one, three, and five times, The dyed silk fabric, when washed one, three, and five times, showed the bacteria reduction rate of 99.0% for Staphylococcus aureus, but didn't showed the significant bacteria reduction. As the test result of sun protection test, in the case of the cotton fabric which was dyed but don't use mordant, after one-time washing, S.P.F.(Sun Protection Factor) showed 20.4, the interception rate of UV-A showed 94.3%, and that of UV-B showed 95.2%. After five-time washing, S.P.F. showed 14.3, the interception rate of UV-A showed 90.0%, and that of UV-B showed 93.2%. In the case of the silk fabric which was dyed but don't use mordant, after one time washing, S.P.F. showed 30.5, the interception rate of UV-A showed 95.9%, and that of UV-B showed 96.9%, after five-time washing, S.P.F. showed 31.0, the interception rate of UV-A showed 95.6%, and that of UV-B showed 96.7%.

자초 뿌리를 이용한 직물의 염색에 관한 연구 (The Fabrics Dyeing using Gromwell Roots)

  • 안경조;김정희;유혜자
    • 대한가정학회지
    • /
    • 제41권1호
    • /
    • pp.249-257
    • /
    • 2003
  • For the efficiency in extracting gromwell colorant, methanol, ethanol and aceton were used as solvents. Also, to compare the results when dyed in various conditions and on various fabrics, the ratio of water-dye mixture, pH, temperature, and varieties of fabrics -wool, silk, cotton, nylon, ramie- were selected. L, a, b, ΔE, munsell and K/S value of each sample was measured and compared for the practical use. Water-dye mixture of 5:5 ratio showed the optimum dyeability. Not to mention wool and silk, but also cotton showed a satisfying dying result at the acidity of pH4. As the temperature increased, the dyeability of all three fabrics improved greatly. Especially, wool showed the highest improvement in terms of dyeability as the temperature increased. K/S values for wool and nylon showed superior results to the others in the gromwell colorant. The resulting color turned out somewhat different depending on the solvents used and the sort of fabric that was tested on. When the gromwell colorant extracted with methanol or ethanol was applied, the color of fabrics came out as purple or purpleblue. When the colorant extracted with acetone was used, the color of fabrics came out to be redpurple. The colorfastness to light showed low glades regardless to whichever solvents were used. The grades of colorfastness to laundering were recorded low numerical values, and its record became even lower when the gromwell colorant extracted with aceton was applied. The staining grade of the colorfastness to laundering showed a good grade in the range of 4 to 5. All the dyed fabrics showed a excellent drycleaning fastness.