• 제목/요약/키워드: dibutyl tin diacetate

검색결과 2건 처리시간 0.015초

반응 변수에 따른 $SnO_2$ 박막의 특성 (Properties of $SnO_2$ Thin Films Depending on Reaction Parameter)

  • 이정훈;장건익;김경원;손상희
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2006년도 하계학술대회 논문집 Vol.7
    • /
    • pp.356-357
    • /
    • 2006
  • Tin oxide thin films have been prepared on display glass from mixtures of dibutyl tin diacetate as a tin source, oxygen as an oxidant by Plasma Enhanced Chemical Vapor Deposition (PECVD) method. The relationships between the properties of tin oxide thin films and various reaction parameters such as the deposition temperature, deposition time and the oxygen gas flow rate were studied. As the deposition temperature increased, the texture plane of $SnO_2$ changed from (200) plane to denser (211) and (110) planes. Lower deposition temperature and thinner thickness of deposited film led to decreasing grain size, surface roughness and electrical resistivity of the formed thin films at $325{\sim}425^{\circ}C$. The properties of fabricated $SnO_2$ films are highly changed with variations of substrate temperature and deposition time.

  • PDF

투명전도성 Tin Oxide Film의 특성 (Characteristics of Transparent and Conducting Tin Oxide Film)

  • 지창섭;문탁진;최인훈;이덕열
    • 대한화학회지
    • /
    • 제31권1호
    • /
    • pp.102-109
    • /
    • 1987
  • 화학증착방법에 의해 dibutyl tin diacetate를 산소와 반응시켜 $SnO_2$박막을 slide glass에 증착시켜 각 조건에 형성된 $SnO_2$박막의 특성을 조사하였다. 본 연구에서 최적증착조건은 기판온도 420$^{\circ}C$, 증착시간 20분으로 나타났으며 증착속도는 증착시간이 증가함에 따라 증가하며 증착시간 25분이후에는 일정해졌으며 판저항의 값도 증착초기에는 감소하나 증착시간 20분이 지나면서 증가하였다. 증착온도 420$^{\circ}C$, 증착시간 20분에 형성된 박막은 두께 4000${\AA}$이며 가시광선 투과율이 90%이며 5800 ohms/${\square}$의 판저항을 가졌다. 그리고 산세척방법에 의해 표면처리한 기판과 반응기체중 수증기의 첨가는 더 좋은 특성의 투명전도성 $SnO_2$박막을 제조하는데 도움이됨을 알았다. 또한 증착막은 작은 구형의 입자들로 이루어져 있다는 것을 주사전자현미경으로 확인하였으며 X-선 회절 실험에 의해 rutile structure(tetragonal)를 갖는다는 것을 알 수 있었다.