• Title/Summary/Keyword: denture metal frameworks

Search Result 13, Processing Time 0.02 seconds

The Effects of Thermocycling on the Shear Bond Strength between Metal Denture Base and Relining Resin (Thermocycling이 첨상용 레진과 금속 의치상간의 전단결합강도에 미치는 영향)

  • Lee, Joon-seok
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.21 no.2
    • /
    • pp.95-103
    • /
    • 2005
  • Purpose: Recently, various metal primers have been developed, and these are known to increase the bond strength between metal and relining resin. In this study, the change in bond strength according to amount of thermocycling was evaluated. Materials and Methods: In this study, 216 specimens were fabricated. Tokuyama Rebase $II^{(R)}$(Tokuyama Corp., Japan) and $Kooliner^{(R)}$(GC America Inc., Japan) as relining material, and MR. $Bond^{(R)}$(Tokuyama Corp., Japan) and Alloy $Primer^{(R)}$(Kuraray Medical Inc., Japan) as a metal primers were used. Using Ni-Cr and various metal surface treatment methods, resin was bonded and the change in bond strength during thermocycling was measured. The data was analyzed by one-way ANOVA, t-test(p<.05 level of significance). Results: When comparing the groups with only sandblasting, rapid decrease in shear bond strength could be seen. In the groups using Tokuyama Rebase $II^{(R)}$, with the exception of the 1000 and 2000 cycle groups, each group showed statistically significant decrease in shear bond strength(p<0.05). In comparison according to relining materials, $Kooliner^{(R)}$ showed higher shear bond strength than Tokuyama Rebase $II^{(R)}$ in all groups. In groups using MR $bond^{(R)}$, $Kooliner^{(R)}$ had higher shear bond strength than Tokuyama Rebase $II^{(R)}$ but, there was no statistical significance(p<0.05). In the other groups, $Kooliner^{(R)}$ showed significantly higher shear bond strength(p<0.05). There was significant difference between groups with sandblasting and metal primer treatments(p<0.05). In comparison according to metal primer materials, Alloy $Primer^{(R)}$ showed the highest shear bond strength but there was no statistical significance(p>0.05). According to the number of thermocycling cycles, when using Tokuyama Rebase $II^{(R)}$, there were no significant differences between the 0, 1000 and 2000 cycle groups regardless of the type of metal primer. There were no differences between the 2000 and 3000 cycle groups. When using $Kooliner^{(R)}$, regardless of the type of metal primer, there were no significant differences between the 0, 1000, 2000 and 3000 cycle groups(p>0.05). Conclusion: The use of metal primers showed increase in bond strength, and the stability after to thermocycling has been authenticated. Thus, the use of metal primers in relining and rebasing of metal frameworks is essential. But when selecting the material various physical properties should be considered.

Fabrication of removable partial denture on scleroderma patient using 3-dimensional intraoral scanner (전신성 피부경화증 환자에서의 3차원 구강스캐너를 이용한 가철성 국소의치 제작 증례)

  • Kim, Ung-Gyu;Han, Jung-Suk;Yoon, Hyung-In;Yeo, In-Sung Luke
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.59 no.1
    • /
    • pp.116-125
    • /
    • 2021
  • A three-dimensional (3D) intraoral scanner, which is one of the major developments in digital dentistry, is widely used in fixed prosthodontics. The application of intraoral scanner is now increasing in removable prosthodontics. Sclerotic change induced by scleroderma causes the limitation of mouth opening and multiple loss of the teeth. Conventional prosthodontic procedures are challenging for patients with this disease. This study showed a case of digital approach to the removable prosthodontic treatment of a patient who had the scleroderma and the consequent microstomia. At the provisional stage, the optical impression of patient's oral structures was digitally obtained. Using a 3D printer, the provisional dentures were fabricated. After extraction of hopeless tooth, the definitive digital impression was taken and the metal frameworks were fabricated, based on the data acquired from the impression. The definitive removable partial dentures were completed and delivered to the patient, who was satisfied with the prostheses.

FLEXURE STRENGTH OF CAST-JOINED CONNECTOR WITH Ni-Cr-Be ALLOY (주조연결된 니켈-크롬-베릴리움 주조체의 굽힘강도에 관한 비교연구)

  • Jeong, Chang-Mo;Jeon, Young-Chan;Lim, Jang-Seop
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.36 no.6
    • /
    • pp.858-866
    • /
    • 1998
  • Soldering is the usual method used to correct an unstable fixed partial denture framework at patient's try-in; However, presoldering base metal alloys is technique-sensitve and results are unstable because it is difficult to maintain uniform heat distribution and to prevent oxidation of an alloy. A cast-joining technique has been developed by Weiss and Munyon for repair, correction and addition to base metal framework. This joining technique eliminates the problem with presoldering of non-precious frameworks. The object of this study was to 1) compare the relative flexure strength and the joining effectiveness of Ni-Cr-Be cast in two pieces and 'pre-soldered' versus in two pieces and 'cast-joined'. 2) determine the effect of increasing the number of retentive grooves on the face of the cast and 3) determine the effect of the relative matched position of groove patterns on flexure strength. The joining effectiveness can be expressed by the ratio of the mean flexure stress of soldered or cast-joined specimens to that of one-piece cast. Resin rods 3mm in diameter were used as pattern of specimens for one-piece casted, presoldered, and cast-joined groups. Cast-joined specimens had two different patterns of retentive grooves on the joined faces. Type A had cross-shaped grooves 1mm in depth. 0.6mm in width. Type B was the same except for the addition of one more retentive groove. In the experiment connecting cast-joined specimens, half of specimens with type A pattern had their patterns on the faces of paired casts matched with each other as mirror image. With the rest pairs, it was proceeded that one of paired casts turned 45 degrees so that the patterns crossed. Half of specimens with type B pattern also had the patterns matched as mirror image; However, here, one of paired casts turned 90 degrees with the other pairs. Retentive groove in this study lacked the intentional undercuts, in contrast with the suggestion of Weiss and Munyon. The specimens were subjected to four-point flexural loading in an Instron testing machine. The midspan flexural stress was calculated at the point of initial plastic strain as determined from a strip-chart recorder or at the point of failure if this occured at a lower stress level. Within the scope of this study, the following results were obtained. 1. The presoldered group showed flexural strength at least 2 times higher than the cast-joined groups. Its joining effectiveness was 82%. 2. In cast-joined groups, the flexural strength of joints with type B patterns exhibited 1.5 times that of joints with type A patterns. Joining effectivenesses were 38% for type B patterns, 25-26% for type A patterns. 3. The relative matched position of groove patterns did not have any significant effect on flexural strength of the cast-joined specimens with either type A patterns or type B patterns(p>.05).