  • Although porcelain fused to metal crowns made from non-precious metal have good mechanical properties, they also have disadvantages such as the poor biological acceptability and the low corrosional resistance. Titanium is used as the alternative metal for porcelain fused to metal crowns, in spite of difficulties in casting. For that reason non-precious alloy including titanium which is easy to cast is currently used. This study evaluated the bond strength between non-precious alloy including titanium and Ni-Cr alloy. $Tilite^{(R)}V$ as non-precious alloy including titanium, $Rexilium^{(R)}V$ as Ni-Cr alloy and $Omega900^{(R)}$ and $Vintage(Regular)^{(R)}$ as porcelain powders were used. The results were as follows. 1. In comparison with the kind of alloy, the bond strength of $Tilite^{(R)}V$ was lower than that of $Rexilium^{(R)}V$. There was no significant difference between two groups. 2. In comparison with the kind of porcelain powder, the bond strength of $Omega900^{(R)}$ was higher than that of $Vintage(Regular)^{(R)}$ in $Tilite^{(R)}V$. There was significant difference between two groups(p < 0.05).

표면 변화에 따른 주조용 티타늄 합금과 도재와의 결합강도 변화에 관한 연구 (A Study of Porcelain Bond Strength to Cast Ti Alloy with respect to Change of Surface Characteristic)

  • 정인성;최성민
    • 대한치과기공학회지
    • /
    • 제30권1호
    • /
    • pp.65-71
    • /
    • 2008
  • The use of titanium in the field of dentistry has increased, due to their excellent biocompatibility, appropriate mechanical properties, corrosion-resistance and low price. However, many difficulties with the use of titanium for metal-ceramic crowns remain to be solved. The objective of this study was to evaluate the influence of surface modifications on the bonding characteristics of specific titanium porcelain bonded to cast titanium. The surfaces of Titanium were prepared with 4 test groups, i) sandblasted with particles of different size, ii) sandblasted after treated oxidization and oxidized after sandblast. We observed the bond strength and node aspect of titanium and ceramic, and respect to the methods of modifying surface of titanium by the test of mean roughness of surface, Scanning Electron Microscope, and 3-point flexural bend test. The results show that, 1. The specimens, which treated oxidization after process of sandblast with particles of 50um size, were the better for the bond strength in comparison with other specimen. 2. The specimen with process of sandblasting after oxidization treatment were the better for stability of the bond strength. 3. The wettability of titanium surface affect the bond strength.

  • PDF

교합력의 방향에 따른 소형견 치과보철물의 압축파절강도 비교 (Comparison of compressive fracture strength of small dog dental prosthesis along the direction of bite force)

  • 박유진;최성민
    • 대한치과기공학회지
    • /
    • 제42권2호
    • /
    • pp.129-137
    • /
    • 2020
  • Purpose: The aim of this study is to observe the compressive fracture strength of the crown according to the direction of the occlusal force of the mandibular canine and carnassial of the small dog. Methods: The abutment models of mandibular canine and carnassial were prepared, specimens of zirconia, PMMA and Ni-Cr alloy were produced. The experimental jig was fabricated with Co-Cr alloy and buried in acrylic resin after make tilt to specified angle. The specimen was attached to a jig and loaded using a universal testing machine until the specimen fractured. Results: The compressive fracture strengths of CXZ and CXP specimens were found to be 999.21 ± 31.15 N on average and 731.42 ± 59.13 N on average. And CZZ and CZP specimens were 730.48 ± 70.14 N on average and 377.65 ± 11.87 N on average. CXN and CZN specimens were not fractured. In addition, MZZ and MZP specimens were 746.46 ± 50.75 N and 258.64 ± 31.86 N on average. The MZN specimens were not fractured. Conclusion: Zirconia has compressive fracture strength that can be applied to small dog's canine and Carnassial prosthetics, while PMMA has inadequate strength to small dog's carnassial prosthesis.

도재소부용 Ni-Cr-Mo계 치과용 합금의 미세조직 및 기계적성질 (Microstructure and Mechanical Properties of Ni-Cr-Mo Based Dental Cast Iron for Porcelain-Fused-to-Metal Firing)

  • 최답천
    • 한국주조공학회지
    • /
    • 제27권3호
    • /
    • pp.120-125
    • /
    • 2007
  • The microstructure, mechanical properties and melting range of Ni-Cr-Mo based alloys were investigated to develop Be-free Ni-Cr-Mo base dental alloys for Porcelain-Fused-to-Metal Firing(PFM). All as-cast alloys showed dendritic structure. Rockwell hardness of 20Cr7Mo was increased with addition of Si and Ti. On the contrary, it was decreased with addition of Co. The duplex alloying elemental addition such as 3Co + xTi, 2Si + xCo and 2Si + xTi to 20Cr7Mo resulted in much increase of hardness. Rockwell hardness and compressive strength for 20Cr3CoSiTi or 17Cr6CoSiTi alloy that add Si-Ti had similar values compared to the commercial alloys. Melting range for 20Cr3CoSiTi and 17Cr6CoSiTi alloy that add Si-Ti showed similar or lower than commercial alloys. In conclusion, 20Cr3CoSiTi and 17Cr6CoSiTi alloys can be applied for commercial use.

주입선의 설계가 임플란트 보철물의 적합도에 미치는 영향 (Effect of the Sprue Design on the Fitness of Implant Prosthesis)

  • 황성택;안재석;신상완
    • 대한치과기공학회지
    • /
    • 제30권2호
    • /
    • pp.57-63
    • /
    • 2008
  • Statement of problem: Conventional techniques for implant framework fabrication produce significant error that is inconsistent with passive-fit requirement for osseointegrated implants. One of the etiologic factors which cause the errors is a sprue which may deform the framework during solidification and contraction. Purpose: This study was aimed to evaluate objectively effect of the sprue design on the accuracy of fit of implant prosthesis. Materials and method: Three different designs were considered relative to effect of casting accuracy. The first design had straight sprues and a button of excess alloy at the non-casting end of the sprues. The second was runner bar design(with the button). The last was straight sprues design(without the button). Gold cylinder and laboratory analogue had been used to diminish variables affecting to casting accuracy. Gold alloy and pressure-vacuum casting machine had been used. Marginal gap had been measured by SEM. One-way ANOVA and Duncan test had been used for statistical analysis. Results: The first design showed $79.87{\pm}13.95{\mu}m$ marginal gap. The second and third were $40.17{\pm}15.8{\mu}m$ and $35.17{\pm}9.95{\mu}m$ respectively. Conclusion: Straight sprues without button and runner bar designs were more accurate than straight sprues with button design(P<.05).

  • PDF

심미도재관의 파절 강도 비교 연구 (A comparative study on the fracture strength of esthetic porcelain crowns)

  • 김은하;이명곤
    • 대한치과기공학회지
    • /
    • 제29권2호
    • /
    • pp.79-85
    • /
    • 2007
  • In this study, We tried to find out the fracture strength of zirconia coping all ceramic crown and collarless porcelain fused gold alloy crown as the compared group. Each of the collarless porcelain fused gold crown and zirconia all ceramic crown has been produced specimen 10 each. And after pasting them on the steel jig, it had load given at porcelain incisal edge by 130$^{\circ}$ and measured fracture strength by Universal Testing Machine and then We have results from that. 1. The average value of fracture strength suggested 950.49 N at collarless porcelain fused gold alloy crown, 656.81 N at zirconia coping all ceramic crown. 2. Fractured pattern showed that the whole of labial part was exposed in collarless porcelain fused gold crown, but porcelain of margin part did not show fracture in advance. In the practice, the concern that collarless might cause fracture strength to be weaken does not matter, we concluded zirconia all ceramic crown made fracture that only a part of labial porcelain was fractured. The combination of zirconia all ceramic crown and turned out to be excellent.

  • PDF

Electrochemical Behaviors of PEO-treated Ti-6Al-4V Alloy in Solution Containing Zn and Si Ions

  • Hwang, In-Jo;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.160-160
    • /
    • 2017
  • Commercially pure titanium (Cp-Ti) and Ti alloys (typically Ti-6Al-4V) display excellent corrosion resistance and biocompatibility. Although the chemical composition and topography are considered important, the mechanical properties of the material and the loading conditions in the host have, conventionally. Ti and its alloys are not bioactive. Therefore, they do not chemically bond to the bone, whereas they physically bond with bone tissue. The electrochemical deposition process provides an effective surface for biocompatibility because large surface area can be served to cell proliferation. Plasma electrolyte oxidation (PEO) enables control in the chemical composition, porous structure, and thickness of the TiO2 layer on Ti surface. Silicon (Si) in particular has been found to be essential for normal bone and cartilage growth and development. Zinc (Zn) plays very important roles in bone formation and immune system regulation, and is also the most abundant trace element in bone. The objective of this work was to study on electrochemical behaviors of PEO-treated Ti-6Al-4V Alloy in solution containing Zn and Si ions. The morphology, the chemical composition, and the microstructure analysis of the sample were examined using FE-SEM, EDS, and XRD. The potentiodynamic polarization and AC impedance tests for corrosion behaviors were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat. The promising results successfully demonstrated the immense potential of Si/Zn-TiO2 coatings in dental and biomaterials applications.

  • PDF

Pd-Ag 및 Ni-Cr 합금의 금 전착이 전장 레진의 색채에 미치는 영향 (EFFECT OF GOLD ELECTRODEPOSIT OF PD-AG, NI-CR ALLOYS ON THE COLOR OF VENERRED RESIN)

  • 양홍서;박영준
    • 대한치과보철학회지
    • /
    • 제33권4호
    • /
    • pp.645-661
    • /
    • 1995
  • As the mechanical property of composite resin improved, composite resin has been widely used esthetic dentistry. In the field of esthetic dentistry, the color of prosthetic material is very important. The purpose of this study was to evaluate the color difference of specimens, by the types of alloys and gold electrodeposit. Experimental groups were as follows : Group Prec : Au-Pt alloy with no gold coating and no resin veneer. Group Semi : Pd-Ag alloy with no gold coating and no resin veneer. Group BAse : Ni-Cr alloy with no gold coating and no resin veneer. Group Gsem : Pd-Ag alloy with no gold coating and no resin veneer. Group Gbas : Ni-Cr alloy with no gold coating and no resin veneer. Group PreR : Resin veneer on the Pd-Ag alloy without gold coating. Group SemR : Resin veneer on the Pd-Ag alloy without gold coating. Group GbsR : Resin veneer on the Ni-Cr alloy with gold coating Group BasR : Resin veneer on the Ni-Cr alloy without gold coating. In this study, colors of metal surfaces and veneered resins were evaluated by the CIE $L^{*}a^{*}b$ system. The results obtained were as follows : 1. different alloy types and gold coating make the $L^{*}a^{*}b$ system. 2. The ${\Delta}E^*$ab value between groups semi and Base was less than 1.5 and there was no $a^*$ and $b^*$ value difference between groups Gsem and Gbas 3. The values of $L^*$ and $a^*$ ain groups GsemR and GbasR were so similar that the ${\Delta}E^*$ab value was as small as 0.58. 4. In resin specimens with gold coated semiprecious or base alloys showed yellower and redder deviation than the resin specimens with precious alloy. 5. The ${\Delta}E^*$ab values between goups PreR-GsemR and groups PreR-GbasR were as small as 2.68 and 2.22 respectively.

  • PDF

Bone-like Apatite Morphology on Si-Zn-Mn-hydroxyapatite Coating on Ti-6Al-4V Alloy by Plasma Electrolytic Oxidation

  • Park, Min-Gyu;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.158-158
    • /
    • 2017
  • Titanium and its alloys have been used in the field dental and orthopedic implants because of their excellent mechanical properties and biocompatibility. Despite these attractive properties, their passive films were somewhat bioinert in nature so that sufficient adhesion of bone cells to implant surface was delayed after surgical treatment. Recently, plasma electrolyte oxidation (PEO) of titanium metal has attracted a great deal of attention is a comparatively convenient and effective technique and good adhesion to substrates and it enhances wear and corrosion resistances and produces thick, hard, and strong oxide coatings. Silicon(Si), Zinc(Zn), and Manganese(Mn) have a beneficial effect on bone. Si in particular has been found to be essential for normal bone and cartilage growth and development. And, Zn has been shown to be responsible for variations in body weight, bone length and bone biomechanical properties. Also, Mn influences regulation of bone remodeling because its low content in body is connected with the rise of the concentration of calcium, phosphates and phosphatase out of cells. The objective of this work was research on bone-like apatite morphology on Si-Zn-Mn-hydroxyapatite coating on Ti-6Al-4V alloy by plasma electrolytic oxidation. Anodized alloys were prepared at 280V voltage in the solution containing Si, Zn, and Mn ions. The surface characteristics of PEO treated Ti-6Al-4V alloy were investigated using XRD, FE-SEM, and EDS.

  • PDF

Electrochemical characteristics of Ca, P, Sr, and Si Ions from PEO-treated Ti-6Al-4V Alloy Surface

  • Yu, Ji-Min;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.154-154
    • /
    • 2017
  • Ti-6Al-4V alloys are widely used as metal-lic biomaterials in dentistry and orthopedics due to its excellent biocompatibility and me-chanical properties. However, because of low biological activity, it is difficult to form bone growth directly on the surface of titanium implants. For this reason, surface treatment of plasma electrolytic oxidation(PEO) was used for dental implants. To enhance bioac-tivity on the surface, strontium(Sr) and sili-con(Si) ions can be added to PEO treated sur-face in the electrolyte containing these ions. The presence of Sr in the coating enhances osteoblast activity and differentiation, where-as it inhibits osteoclast production and prolif-eration. And Si has been found to be essen-tial for normal bone, cartilage growth, and development. In this study, electrochemical characteristics of Ca, P, Sr, and Si ions from PEO-treated Ti-6Al-4V alloy surface was re-searched using various experimental instruments. DC power is used and Ti-6Al-4V al-loy was subjected to a voltage of 280 V for 3 minutes in the electrolyte containing 5, 10, 20M% Sr ion and 5M% Si ion. The morphol-ogies of PEO-treated Ti-6Al-4V alloy by electrochemical anodization were examined by field-emission scanning electron micro-scopes (FE-SEM), energy dispersive x-ray spectroscopy (EDS), x-ray diffraction (XRD) and corrosion analysis using AC impedance and potentiodynamic polarization test in 0.9% NaCl solution at similar body tempera-ture using a potentiostat with a scan rate of 1.67mV/s and potential range from -1500mV to + 2000mV.