The Surface Hardening Characteristics of Hot work Tool Steel by CW Nd:YAG Laser (CW Nd:YAG 레이저에 의한 열간금형 공구강의 표면경화특성)

  • Shin H.J.;Yoo Y.T.;Ahn D.G.;Shin B.H.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2006.05a
    • /
    • pp.219-220
    • /
    • 2006
  • Laser surface hardening technologies have been used to improve characteristics of wear and to enhance the fatigue resistance for mold parts. The objective of this research work is to investigate the influence of the process parameters, such as power of laser and defocused spot position, on the characteristics of laser surface hardening for the case of SKD61 steel. CW Nd:YAG laser is selected as the heat source. The optical lens with the elliptical profile is designed to obtain a wide surface hardening area with a uniform hardness. From the results of the experiments, it has been shown that the maximum hardness is approximatly 740 Hv when the power, focal position and the travel of laser are 1,095 W, +1mm and 0.3 m/min, respectively. In addition, the hardening width using the elliptical lens was three time larger than that using the defocusing of laser beam.

  • PDF

Characteristics Induction and Laser Surface hardening of SM45C Steel (SM45C강의 레이저표면경화와 고주파표면경화특성)

  • Na Gee-Dae;Shin Ho-Jun;Shin Byung-Heon;Yoo Young-Tae
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.23 no.7 s.184
    • /
    • pp.39-50
    • /
    • 2006
  • Laser heat treatment technologies have been used to improve characteristics of wear and to enhance the fatigue resistance for automotive parts. The bjective of this research work is to investigate the influence of the process parameters, such as power of laser and defocused spot position, on the characteristics of laser heat treatment for the case of SM45C medium carbon steel. CW Nd:YAG laser is selected as the heat source. The optical lens with the elliptical profile is designed to obtain a wide heat treatment area with a uniform hardness. From the results of the experiments, it has been shown that the maximum hardness is approximatly 780 Hv when the power and the travel of laser are 1,095 W and 0.6 m/min, respectively. In addition, the hardening width using the elliptical lens was three time larger than that using the defocusing of laser beam.

Microstructure and electrical properties of high power laser thermal annealing on inkjet printed Ag films

  • Yoon, Yo-Han;Yi, Seol-Min;Yim, Jung-Ryoul;Lee, Ji-Hoon;Joo, Young-Chang
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 2009.05a
    • /
    • pp.36.2-36.2
    • /
    • 2009
  • In this work, the high power CW Nd:YAG laser has been used for thermal treatment of inkjet printed Ag films-involving eliminating organic additives (dispersant, binder, and organic solvent) of Ag ink and annealing Ag nanoparticles. By optimizing laser parameters, such as laser power and defocusing value, the laser energy can totally be converted to heat energy, which is used to thermal treatment of inkjet printed Ag films. This results in controlling the microstructures and the resistivity of films. We investigated the thermal diffusion mechanisms during laser annealing and the resulting microstructures. The impact of high power laser annealing on microstructures and electrical characteristic of inkjet printed Ag films is compared to those of the films annealed by a conventional furnace annealing. Focused ion beam (FIB) channeling image shows that the laser annealed Ag films have large columnar grains and dense structure (void free), while furnace annealed films have tiny grains and exhibit void formation. Due to these microstructural characteristics of laser annealed films, it has better electrical property (low resistivity) compared to furnace annealed samples.

  • PDF

Manufacturing Process of Self-Luminous Glass Tube (SLGT) Utilizing Tritium Gas (I) (삼중수소 활용을 위한 자발광유리관 (SLGT) 제조기술)

  • Kim Kwangsin;Kim Kyeongsook;Chung Eun-Su;Son Soon Hwan;Nam Gi-Jung
    • Proceedings of the Korean Radioactive Waste Society Conference
    • /
    • 2005.11a
    • /
    • pp.87-95
    • /
    • 2005
  • Laser sealing/cutting technique, one of the 4 core technologies to manufacture self-luminous glass tubes (SLGTs) has been developed. Through the analysis of commercial products it is found that Pyrex Is used for SLGTs. A CO2 laser, which is commonly used for glass work was used for the study The factors affecting the sealing/cutting were laser intensity, duration. Irradiation method, and pressure inside the tube. The whole Process is composed of 2 stages. In the first stage. both ends of the tubes are sealed while tritium is insected in the tubes. And the tritium sealed tubes are cut in the desired size in the second stage. Defocused beam was used for seal ing and focused beam was used for cutting. After the sealing/cutting, the tubes were heat treated to prevent fracture due to the residual heat stress.

  • PDF

Collimation testing of a white light beam and measurement of chromatic aberration of a lens by using vernier Moire fringe patterns (버니어 무아레 무늬를 이용한 백색광의 시준 검사 및 렌즈의 색수차 측정)

  • 송종섭
    • Korean Journal of Optics and Photonics
    • /
    • v.11 no.4
    • /
    • pp.232-238
    • /
    • 2000
  • The new collimation testing technique of a white light beam using vernier Moire fringes of two line or circular gratings with different pitches is presented. We can visually measure the defocusing ($\Deltaf$), the divergence angle ($\theta$), and the longitudinal chromatic aberration $(L_{ch})$ of a collimating lens by using the technique. For example, we obtained $\Deltaf$= 21.9 mm and $\theta=0.0038^{\circ}$ for a testing lens with the focallengthf = 120.0 mm and F-number of F/2.4. The longitudinal chromatic aberration $L_{ch}$ of another testing lens withf = 65.0 mm, F/1.6, and the Abbe number V = 64.1 for the incident wavelengths of $\lambda_1=480 nm and \lambda_2=640 nm$ is easily measured by same technique. It is found that the measured value $L_{ch}=1.59mm(\pm0.01mm)$ is well agreed with $L_{ch}=1.58mm(\pm0.01mm)$ obtained by the autofocus method.