• Title/Summary/Keyword: corona charging

Search Result 65, Processing Time 0.023 seconds

Numerical Study of Particle Collection and Entrainment in Electrostatic Precipitator (집진기내 입자 포집과 비산 문제에 대한 수치적 연구)

  • Kim, Ju-Hyeon;Kweon, Soon-Cheol;Kwon, Ki-Hwan;Lee, Sang-Hwan;Lee, Ju-Hee
    • The KSFM Journal of Fluid Machinery
    • /
    • v.15 no.1
    • /
    • pp.27-35
    • /
    • 2012
  • A numerical simulation for particle collection efficiency in a wire-plate electrostatic precipitator (ESP) has been performed. Method of characteristics and finite differencing method (MOC-FDM) were employed to obtain electric field and space charge density, and lattice boltzmann method (LBM) was used to predict the Electrohydrodynamic (EHD) flow according to the ion convection. Large eddy simulation (LES) was considered for turbulent flow and particle simulation was performed by discrete element method (DEM) which considered field charging, electric force, drag force and wall-collision. One way coupling from FDM to LBM was used with small and low density particle assumption. When the charged particle collided with the collecting plate, particle-wall collision was calculated for re-entertainment effect and the effect of gravity force was considered.

UV Aging on EPDM rubber for use in polymer Insulators (폴리머 애자용 EPDM 고무의 자외선 열화특성)

  • Youn, Bok-Hee;Lee, Sang-Yong;An, Jong-Sik;Huh, Chang-Su
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05c
    • /
    • pp.62-65
    • /
    • 2001
  • The effects of accelerated UV radiation on EPDM used for a polymeric insulator were investigated by contact angle, surface voltage decay after corona charging, SEM-EDX, ATR-FTIR and XPS. EPDM occurs as loss of hydrophobicity by UV treatment, which followed by surface cracking and chalking. The surface voltage decay on UV-treated EPDM show that the shorter decay time corresponded to the treated samples with a longer UV exposure time. The surface oxygen and aluminum content were found to increase and carbon decrease, as is observed in EDX analysis. The ATR-FTIR and XPS indicated that C-C and C-H groups decreased and the highly oxidized carbon bonds such as C-O, C=O and O-C=O increase with time. Also, the effects of surface charges on hydrophobicity based on our results is discussed.

  • PDF

A Study on Influence Factors on Drop Formation in Electrohydrodynamic Atomization (전기수력학적 미립화에서 액적 형성에 영향을 미치는 인자에 관한 실험적 연구)

  • Sung, K.A.;Lee, C.S.
    • Journal of ILASS-Korea
    • /
    • v.8 no.2
    • /
    • pp.24-30
    • /
    • 2003
  • An experimental study was performed to investigate the influence factors of drop formation in electrohydrodynamic atomization. The mode of electrohydrodynamic atomization depended on the various factors such as the flow rate of the liquid, the inner diameter of the nozzle, the distance between the nozzle tip and the ground electrode, the shape of the ground electrode. and the applied high voltage. This work was performed to investigate the experimental analysis for the flow pattern visualization of droplets, and the relationship between voltage application and the behavior of liquid atomization. Uniform drops of different sizes can be obtained at the inception of the spindle mode by charging the flow rate and the electric field. The drop size also decreased when the flow rate was raised for the spindle mode. The whipping motion occurred beyond 7kV and before the corona started to take effect.

  • PDF

Analysis of the Surface Degradation in UV-irradiated High-Temperature Vulcanized Silicone Rubber (자외선 조사된 HTV 실리콘 고무의 표면열화 분석)

  • 연복희;이태호;허창수;이종한
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.5
    • /
    • pp.411-419
    • /
    • 2000
  • In this paper we have investigated the surface degradation by ultraviolet-irradiation in high-temperature vulcanized silicone rubber. Through the measurement of surface potential decay by corona-charging and of contact angle it is found that the change of surface electrostatic properties and the decrease of contact angle under UV-radiation. For the changes in micro-morphological and chemical structure of the UV-treated silicone rubber we utilized several analytical techniques such as SEM, ATR-FTIR,XPS. From this study it is shown that the chemical reactions(scissoring of side chain(S-$CH_3$) cross-linking and branching) occur on the surface of silicone rubber during the UV-irradiation. Also we obtained the results of the loss of low molecular weight chain by cross-linking and oxidation reaction.

  • PDF

Surface Charcterization of plasma-treated silicone insulating materials (플라즈마 처리된 실리콘 절연재의 표면 특성화)

  • Song, J.Y.;Huh, C.S.;Youn, B.H.;Lee, T.H.;Yoo, H.C.;Seo, Y.J.;Lee, K.T.;Kim, N.R.;Lee, U.H.
    • Proceedings of the KIEE Conference
    • /
    • 2002.11a
    • /
    • pp.176-178
    • /
    • 2002
  • Surface states of silicone polymer treated by plasma were investigated by the analysis by x-ray photoelectron spectroscopy(XPS) and surface voltage decay after corona charging. Plasma treatment causes the silica -like oxidative layer, which was confirmed with XPS, and lowers surface resistivity with increasing the plasma treatment time. Using the decay time constant of surface voltage, the calculated surface resistivity was compared with the value directly measured by voltage-current method using three electrodes system. A good agreement between two methods was obtained. In addition, we estimated the thermal activation energy for surface conduction, Based on our results, we could understand the relationship between surface chemical states and surface electrical properties.

  • PDF

Nano Particle Charging Characteristics of Aerosol Charge Neutralizers (에어로졸 중화기의 나노 입자 하전 특성)

  • Ji, Jun-Ho;Bae, Swi-Nam;Hwang, Jung-Ho
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.27 no.10
    • /
    • pp.1489-1497
    • /
    • 2003
  • Aerosol charge neutralizers with various radioactive sources have been used to apply an equilibrium charge distribution to aerosols of unknown charge distribution. However, the performance of aerosol charge neutralizers is not well known, especially for highly charged particles. Measurements of highly charged particles are needed in air cleaning devices, e.g. electrostatic precipitator, bag filter with a pre-charger, and electrical cyclone. In this study, the particle charging characteristics of two different aerosol charge neutralizers were experimentally investigated for singly charged monodisperse particles and highly charged polydisperse particles. One has radioactive source of $^{85}$ Kr (beta source, 2 mCi) and the other has $^{210}$ Po (alpha source, 0,5 mCi). The air flow rate passing through each aerosol charge neutralizer was changed from 0.2 to 2.5 L/min. The results show that the charge distribution of singly charged monodisperse particles passing through the $^{85}$ Kr aerosol charge neutralizer is well agreed with the Boltzmann equilibrium charge distribution at an air flow rate of 0.3 L/min, However, it deviates from the equilibrium charge distribution when the air flow rates are 0.6, 1,0, and 1,5 L/min, On the other hands, the effect of air flow rate is insignificant for the $^{210}$ Po aerosol charge neutralizer. The non-equilibrium character in charge distribution of highly charged polydisperse particles passing through the $^{85}$ Kr aerosol charge neutralizer greatly depends on the air flow rate, however it is insensitive to the air flow rate for the $^{210}$ Po aerosol charge neutralizer.

Experiment on Collection Characteristics of Sub micron Particles in Two-Stage Parallel-Plate Electrostatic Precipitators (2단 평행판 전기집진기의 서브마이크론 입자 포집특성 실험)

  • Oh, M.D.;Yoo, K.H.
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.6 no.3
    • /
    • pp.237-246
    • /
    • 1994
  • Experimental data are reported for charging and collection of NaCl aerosols in the 0.03- to $0.2{\mu}m$-geometric-mean-diameter range in 2-stage parallel-plate electrostatic precipitators. The NaCl aerosols are generated with geometric standard deviation of about 1.74 and particle generation rate of about 10^9 particles/see by the constant output atomizer and injected into the air flow in the clean wind-tunnel. The 2-stage parallel-plate electrostatic precipitator installed in the test section of the wind-tunnel is operated with a positive corona discharge. The NaCl aerosols in the channel flow are sampled and transported to the aerosol particle number concentration measurement system by using the isoaxial sampling and transport system constructed based on the Okazaki and Willeke design. The aerosol particle number concentration measurement system measures the size distribution of submicrometer aerosols by an electrical mobility detection technique. It is confirmed from comparing the measured collection efficiencies in this study and the predicted ones by our previous theoretical analysis that the predicted collection efficiencies agree well with the experimental ones. It is also found from the comparison that below about $0.02{\mu}m$ all particles are not charged and the uncharged particles are not collected, and consequently 2-stage parallel-plate electrostatic precipitators are not suitable for that particle size range.

  • PDF

Design and Performance Evaluation of a Faraday Cage and an Aerosol Charger (패러데이 케이지와 에어로졸 하전기의 설계 및 성능평가)

  • Ji, Jun-Ho;Bae, Kwi-Nam;Hwang, Jung-Ho
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.28 no.3
    • /
    • pp.315-323
    • /
    • 2004
  • An electrical cascade impactor is a multi-stage impaction device to separate airborne particles into aerodynamic size classes using particle charging and electrical detection techniques. A Faraday cage and an aerosol charger, which are basic components of the electrical cascade impactor, were designed and evaluated in this study. The low-level current response of the Faraday cage was investigated with changing particle size and air flow rate by using sodium chloride (NaCl) particles. The response of the prototype Faraday cage was very similar to that of a commercial aerosol electrometer (TSI model 3068) within ${\pm}$5% for singly-charged particles. The response linearity of the prototype Faraday cage could be extended up to flow rate of 30 L/min. For the performance evaluation of the aerosol charger the monodisperse liquid dioctyl sebacate (DOS) particles, with diameters of 0.1∼0.8$\mu\textrm{m}$, were generated using spraying from an atomizer followed by evaporation-condensation process. Typical performance parameters of the aerosol charger such as P$.$n, wall loss, and elementary charges per particle were evaluated. The performance of the prototype aerosol charger was found to be close to that of the aerosol charger used in an electrical low pressure impactor (ELPI, Dekati).

Analysis of Surface Degradation on Accelerated UV-treated Polymeric Housing Materials for Outdoor Insulator (자외선 가속열화에 따른 옥외용 폴리머 절연재료의 표면열화 분석)

  • Yeon, Bok-Hui;Lee, Sang-Yong;Heo, Chang-Su;Sim, Dae-Seop;Jo, Han-Gu
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.10
    • /
    • pp.479-488
    • /
    • 2001
  • The effects of accelerated Ultraviolet (UV) radiation on High temperature vulcanized (HTV), Room temperature vulcanized (RTV) silicone rubber and two types of ethylene propylene diene terpolymer (EPDM) used for composite insulator were inverstigated by hydrophobicity class (HC), surface voltage decay after corona charging, SEM-EDS, FTIR and XPS. The contact angle in two kinds of silicone rubber was scarcely change, but EPDM occurred to the loss of hydrophobicity followed by surface cracking and chalking. The surface voltage decay on UV-treated silicone rubber and EPDM showed a different decay trend with UV treatment. EDS and XPS analysis indicated that the oxygen content increased with UV treatment time in all samples. For silicone rubber, the oxidized groups of inorganic silica-like structure increased with UV treatment time. The oxidized carbon of C=0, O=C-O in EPDM increased. These oxidized surface for each material had different electrostatic characteristics, so deposited charges were expected to have different impacts on their surface hydrophobicity. The degradation mechanism based on our results was discussed.

  • PDF

Fabrication of the Superconducting Flux Flow Transistor Using the ICP Etching Method (ICP 장치를 이용한 초전도 자속 흐름 트랜지스터의 링크 제작)

  • Gang, Hyeong-Gon;Im, Yeon-Ho;Im, Seong-Hun;Choe, Hyo-Sang;Han, Yun-Bong;Han, Byeong-Seong
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.10
    • /
    • pp.494-499
    • /
    • 2001
  • The effects of accelerated Ultraviolet (UV) radiation on High temperature vulcanized (HTV), Room temperature vulcanized (RTV) silicone rubber and two types of ethylene propylene diene terpolymer (EPDM) used for composite insulator were investigated by hydrophobicity class (HC), surface voltage decay after corona charging, SEM-ES, FTIR and XPS. The contact angle in two kinds of silicone rubber was scarcely change, but EPDM occurred to the loss of hydrophobicity followed by surface cracking and chalking. The surface voltage decay on UV-treated silicone rubber and EPDM showed a different decay trend with UV treatment. EDS and XPS analysis indicated that the oxygen content increased with UV treatment time in all samples. For silicone rubber, the oxidized groups of inorganic silica-like structure increased with UV treatment time. The oxidized carbon of C=O, O=C-O in EPDM increased. These oxidized surface for each material had different electrostatic characteristics, so deposited charges were expected to have different impacts on their surface hydrophobicity. The degradation mechanism based on our results was discussed.

  • PDF