폐유리를 활용한 콘크리트의 물리.역학적 특성에 관한 실험적 연구 (An experimental Study on the Physical.Mechanical Properties of Concrete Utilizing Waste Glass Aggregate)

  • 김정환;조광연;조청휘;이봉춘;박승범
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.251-256
    • /
    • 2001
  • Recently, as industrialization is rapidly growing and the standard of life is rising, the quantities of waste glasses have been hastily increased and most of them are not recycled but abandoned. It cause some problems such as the waste of natural resources and environmental Pollution. Therefore, this study was conducted basic experimental research to analyze the possibilities of recycling of waste glasses(crushed waste glasses outbreaking from our county such as brown, green, colorlessness) as fine aggregates for concrete. Test results of fresh concrete, slump and compacting factors decrease because grain shape is angular and air content increase due to involving small size particles so much in waste glasses. Also compressive, tensile and flexural strengths decrease with increase of the content of waste glasses. In conclusion, the content of waste glasses below 30% is reasonable

  • PDF

폐대리석 분말을 혼입한 고유동 콘크리트의 특성 (A Study on Properties of High Fluidity Concrete adding Waste Marble Powder)

  • 정의창;이용무;김영수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2014년도 춘계 학술논문 발표대회
    • /
    • pp.262-263
    • /
    • 2014
  • The purpose of this study was to investigate properties of high fluidity concrete adding waste marble powder. A change in the replacement ratios of waste marble powder was measured compressive strength and slump flow, O-Lot and U-Box. Waste marble powder has replaced binder of high fluidity concrete at certain contents of 0~20%. As a results, Slump flow, O-Lot and U-box adding waste marble powder up to 10% have increased by adding waste marble powder. As the concrete with a replacement ratio of waste marble powder up to 10% was found to have a compressive strength superior to that of plain.

  • PDF

폐활성탄을 사용한 다공성 콘크리트의 물리.역학적 성질 (Physical and Mechanical Properties of Porous Concrete Using Waste Activated Carbon)

  • 윤준노;성찬용;김영익
    • 한국농공학회논문집
    • /
    • 제51권4호
    • /
    • pp.21-27
    • /
    • 2009
  • This study was performed to evaluate the physical and mechanical properties of porous concrete using waste activated carbon. Material used were ordinary portland cement, recycled coarse aggregate, waste activated carbon and superplasticizer. The replacement ratios of waste activated carbon were 0,1,2,3,4,5,6,7,8,9, and 10 %. The void ratio was decreased and ultrasonic pulse velocity was increased with increasing the waste activated carbon powder, respectively. The compressive strength and flexural strength of porous concrete using waste activated carbon powder were in the range of 8.21${\sim1}$6.58 MPa and 1.69${\sim1}$3.68 MPa, respectively. The pH degree of porous concrete in 1day and 77days were shown in 12.50${\sim1}$12.63 and 10.21${\sim1}$10.70, respectively. Accordingly, waste activated carbon can be used for porous concrete material.

Experimental and numerical studies on flexural behavior of high strength concrete beams containing waste glass

  • Haido, James H.;Zainalabdeen, Marwa A.;Tayeh, Bassam A.
    • Advances in concrete construction
    • /
    • 제11권3호
    • /
    • pp.239-253
    • /
    • 2021
  • The behavior of concrete containing waste glass as a replacement of cement or aggregate was studied previously in the most of researches, but the present investigation focuses on the recycling of waste glass powder as a substitute for silica fume in high strength concrete (HSC). This endeavor deals with the efficiency of using waste glass powder, as an alternative for silica fume, in the flexural capacity of HSC beam. Thirteen members with dimensions of 0.3 m width, 0.15 m depth and 0.9 m span length were utilized in this work. A comparison study was performed considering HSC members and hybrid beams fabricated by HSC and conventional normal concrete (CC). In addition to the experiments on the influence of glass powder on flexural behavior, numerical analysis was implemented using nonlinear finite element approach to simulate the structural performance of the beams. Same constitutive relationships were selected to model the behavior of HSC with waste glass powder or silica fume to show the matching between the modeling outputs for beams made with these powders. The results showed that the loading capacity and ductility index of the HSC beams with waste glass powder demonstrated enhancing ultimate load and ductility compared with those of HSC specimens with silica fume. The study deduced that the recycled waste glass powder is a good alternative to the pozzolanic powder of silica fume.

재생굵은골재를 사용한 콘크리트의 유동특성에 관한 실험적 연구 (The Experience Study on the Floating Properties of Concrete with Recycled Coarse Aggregate)

  • 백철우;김호수;최성우;반성수;류득현
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.94-97
    • /
    • 2003
  • Recently, owing to the deterioration of reconstruction and the construction, much of the construction waste is discharged in our construction field, and the amount of construction waste are rapidly increased. These waste are raised to financial and environmental problems, so the method of reusing waste concretes has been studied and carried out many direction. Especially being want of resources, if waste concrete could be recycled as aggregate for concrete, it will contribute to solve the exhaustion of natural aggregate, in terms of saving resources and protecting environment. This study is that the floating properties of concrete with recycled coarse aggregate were investigated for the substitution of recycled coarse aggregate. The result of this study, in case of water reducing, the property of harden concrete for the substitution ratio of recycled coarse aggregate was increased. The Quality of recycled coarse aggregate concrete was improved by water reducing.

  • PDF

Usage potential of recycled aggregates in mortar and concrete

  • Yaragal, Subhash C.;Muhammad, Roshan A.K.
    • Advances in concrete construction
    • /
    • 제5권3호
    • /
    • pp.201-219
    • /
    • 2017
  • With the rapid growth in construction sector, it becomes all the more important to assess the amount of Construction and Demolition (C&D) waste being generated and analyze the practices needed to handle and use this waste before final disposal. This serves waste management and disposal issues, paving way to waste utilization in construction industry from the sustainability point of view. C&D waste constitutes a major bulk of total solid waste produced in the world. In this work, an attempt is made to study the performance of concrete using water soaked Recycled Coarse Aggregates (RCA) in replacement levels of 0%, 25%, 50%, 75% and 100% to Natural Coarse Aggregates (NCA). Experiments were designed and conducted to study the performance of RCA based concrete. Further suitable performance enhancement techniques to RCA based concrete were attempted, to achieve compressive strength at least equal to or more than that for no RCA based concrete (control concrete). Performance enhancement study is reported here for 50% and 100% RCA based concretes. All four techniques attempted have given favorable results encouraging use of RCA based concretes with full replacement levels, to adopt RCA based concrete in structural applications, without any kind of concern to the stake holder. Further attempts have also been made to use Recycled Fine Aggregates (RFA) with appropriate modifications to serve as fine aggregates in mortar and concrete. Using RFA blended with river sand fractions as well as RFA with Iron Ore Tailings (IOT) fractions, have given good results to serve as fine aggregates to the extent of 100% replacement levels in mortars and concretes.

Effect of marble waste fines on rheological and hardened properties of sand concrete

  • Djebien, R.;Belachia, M.;Hebhoub, H.
    • Structural Engineering and Mechanics
    • /
    • 제53권6호
    • /
    • pp.1241-1251
    • /
    • 2015
  • Faced with the growing needs of material resources and requirements of environmental protection for achieving sustainable development, it has become necessary to study and investigate all possibilities of exploring crushed and dune sand, reusing industrial wastes and by-product, and also applying new technologies including sand concrete which can replace the conventional concretes in certain structures to surmount the deficit on construction materials, conserve natural resources, lessen the burden of pollutants to protect the environment and reduce the consumption of energy sources. This experimental study is a part of development and valorization of local materials project in Skikda region (East of Algeria). It aims at studying the effects of partial replacement of sand with marble waste as fines on several fresh and hardened properties of sand concrete in order to reuse these wastes in the concrete manufacturing, resolve the environmental problems caused by them and find another source of construction materials. To achieve these objectives, an experimental program has been carried out; it was consisted to incorporate different percentages of marble waste fines (2, 4, 6, 8, 10 and 12%) in the formulations of sand concrete and study the development of several mechanical and rheological properties. We are also trying to find the optimal percentage of marble waste fine replaced in sand concrete that makes the strength of the concrete maximum. Obtained results showed that marble waste fines improve the properties of sand concrete and can be used as an additive material in sand concrete formulation.

Safety Analysis of Concrete Treatment Workers in Decommissioning of Nuclear Power Plant

  • Hwang, Young Hwan;Kim, Si Young;Lee, Mi-Hyun;Hong, Sang Beom;Kim, Cheon-Woo
    • 방사성폐기물학회지
    • /
    • 제20권3호
    • /
    • pp.349-356
    • /
    • 2022
  • Nuclear power plant decommissioning generates significant concrete waste, which is slightly contaminated, and expected to be classified as clearance concrete waste. Clearance concrete waste is generally crushed into rubble at the site or a satellite treatment facility for practical disposal purposes. During the process, workers are exposed to radiation from the nuclides in concrete waste. The treatment processes consist of concrete cutting/crushing, transportation, and loading/unloading. Workers' radiation exposure during the process was systematically studied. A shielding package comprising a cylindrical and hexahedron structure was considered to reduce workers' radiation exposure, and improved the treatment process's efficiency. The shielding package's effect on workers' radiation exposure during the cutting and crushing process was also studied. The calculated annual radiation exposure of concrete treatment workers was below 1 mSv, which is the annual radiation exposure limit for members of the public. It was also found that workers involved in cutting and crushing were exposed the most.

폐콘크리트 미분말을 활용한 콘크리트의 감수제 함유량에 따른 강도특성(PNS계 혼화제) (Strength Characteristics of Concrete Using Superplasticizer content of Waste Concrete Powder)

  • 박신우;정의인;김봉주
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.103-104
    • /
    • 2015
  • This study is an experiment about what affects the compressive strength by using a reducing agent (PNS based admixtures) to play cement using the cement paste based Waste Concrete Powder of waste concrete, which accounts for more than 60% of construction waste around the latest domestic and international It was. Securing the replacement of cement with Waste Concrete Powder and, by varying the admixture was to compensate for the low absorption of liquidity and obtain a fine powder. And the experiment was conducted with a constant water cement ratio and aggregate usage for the purpose of lowering the water cement ratio promoting strength development. When substituted with the experimental results of 0.3% based on 3 ~ 28 days as strength 36Mpa exhibited the highest strength.

  • PDF

폐콘크리트 슬러지를 혼합 사용한 시멘트 모르터의 기초 특성 (Fundamental Properties of Cement Mortar with Waste Concrete Sludge)

  • 이명진;이하나;유재성;김진만
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.160-161
    • /
    • 2015
  • This research reviewed the characteristics of waste concrete sludge occurred from recycled aggregate producing process and the physical and mechanical properties of the mortar incorporated the pulverized the waste concrete sludge. From the results of the experiment, as the replacement ratio of waste concrete sludge powder was increased, the dosage of superplasticizer to satisfy the target flow of 200 ± 10 was increased, and the compressive and flexural strengths were decreased. On the other hand, when the sludge powder replacement ratio was 25 %, outstanding performance of general characteristics of mortar was obtained while it was lower than Plain mixture, thus, further detail study on various replacement ratios of waste concrete sludge powder is needed.