The Fluidity of High Flowing Concrete According to the Component Ratio of Superplasticizer (고성능감수제 구성비율에 따른 고유동콘크리트의 유동특성)

  • Kim Moo-Han;Kim Yong-Ro;Kim Jae-Hwan;Ho Jang-Jong;Lee Tae-Hee
    • Journal of the Korea Concrete Institute
    • /
    • v.16 no.2 s.80
    • /
    • pp.147-154
    • /
    • 2004
  • It is the aim of this study to propose the fundamental data for the establishment of the application and qualify standard of the mixed type superplasticizer after investigating and comparing the fluidity of high flowing concrete according to the component ratio of superplasticizer such as naphthalene sulfonated and melamine sulfonated. The results of this study were shown as the followings; 1) The fluidity and adsorption ratio of cement-paste were improved according to the increasing of naphthalene sulfonated component ratio, and apparent viscosity of cement-paste was improved according to the Increasing of melamine sulfonated component ratio. 2) In case of using the granulated blast-furnace slag, the fluidity of cement-paste was considerably good and the adsorption ratio was decreased and in case of using fly-ash, the apparent viscosity and adsorption ratio of cement-paste were improved. 3) The dispersive capacity performance of concrete can be improved by means of the increasing of naphthalene sulfonated component ratio. Also the viscosity and early strength can be improved by means of the increasing of melamine sulfonated component ratio.

A field Application of Non-shrinkage High Strength Concrete Using CSA Expansive Additive (CSA 팽창재를 사용한 무수축 고강도 콘크리트 현장적용)

  • 조일호;양재성;김진희
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1999.10a
    • /
    • pp.77-80
    • /
    • 1999
  • Before the field applications, several basic laboratory test were the characteristics of workability and strength of the concrete containing CSA expansive additive. As a result, high strength concrete using CSA expansive additive show similar workability and compressive to that of plain concrete, the optimum replacement ratio of them to plain concrete were obtained for CSA expansive additive 10%. On the other hand, it can be concluded that the use of CSA component is effective to prevent shrinkage crack reducing concrete using superplasticizer and to achive volume stability of concrete structure.

  • PDF

The Properties of Multi-Component Blended High Fluidity Mortar (다성분계 고유동 모르타르의 특성)

  • Kim, Tae-Wan;Kang, Choonghyun;Bae, Ju-Ryong;Kim, In-Tae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.22 no.2
    • /
    • pp.124-132
    • /
    • 2018
  • This research presents the results of an investigation on the characteristic of multi-component blended high fluidity mortars. The binder was blended ordinary Portland cement(OPC), ground granulated blast furnace slag(GGBFS), calcium sulfoaluminate(CSA) and ultra rapid setting cement(URSC). The GGBFS was replaced by OPC from 30%(P7 series), 50%(P5 series) and 70%(P3 series), CSA and URSC was 10% or 20% mass. The superplasticizer of polycarboxylate type were used. A constant water-to-binder ratio(w/b)=0.35 was used for all mixtures. Test were conducted for mini slump, setting time, V-funnel, compressive strength and drying shrinkage. According to the experimental results, the contents of superplasticizer, V-funnel and compressive strength increases with an increase in CSA or URSC contents for all mixtures. Moreover, the setting time and drying shrinkage ratio decrease with and increase in CSA or URSC. CSA decreased dry shrinkage but URSC had less effect. However, the mixed binders of CSA and URSC had a large effect of reducing drying shrinkage by complementary effect. This is effective for improving the initial strength of URSC, and CSA is effective for the expansion and improvement of long-term strength.