• Title/Summary/Keyword: compacting test

Search Result 131, Processing Time 0.019 seconds

A Study on Basic Properties of Super Early Strength Self Compacting Concretes( I ) (속경성 자기충전 콘크리트의 기초특성 연구( I ))

  • 엄태선;임채용;유재상;이종열;이근호;한재명
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.05a
    • /
    • pp.79-84
    • /
    • 2002
  • We carried out the feasibility study of super early self compacting concrete having the characteristics of 1 day demoulding without steam curing, high flowable concrete with self compacting, high strength and high durability etc. Here, We test and selected by several methods using high early cement with and without admixtures for the condition of super early strength self compacting concrete's manufacture (SSCC). we sucessed to meet at the goal of SSCC with 20-35N/mm$^2$ at 1 day, without steam curing and with slump flow about 60-65cm. We continue to search the effectual conditions of SSCC's manufacture by changing mix designs, several of admixture (superplasticizer, stabilising agent), slag, fly ash, high early cement and apply the products for practical use.

  • PDF

Behaviour of self compacting repair mortars based on natural pozzolana in hot climate

  • Benyahia, A.;Ghrici, M.
    • Advances in concrete construction
    • /
    • v.6 no.3
    • /
    • pp.285-296
    • /
    • 2018
  • In the present paper, the results of an experimental study of the bond between repair materials and mortar substrate subjected to hot climate is presented. Half-prisms of size $40{\times}40{\times}80mm$, serving as a substrate mortar samples (SUBM) were manufactured in the laboratory and then stored at an ambient temperature for 6 months. Five self compacting mortar mixes (SCMs) incorporating 0%, 10%, 20%, 30%, and 40% of natural pozzolana as white cement replacement were used as repair materials. Repaired composite samples (SCMs/SUBM) were cured at hot climate for different lengths of time (28 and 56-days). During the first week of curing, the composite samples were watered twice a day. The test carried out to assess the bond between SCMs and SUBM was based on three-point bending (3 PB) test. The obtained results have proved that it was feasible to produce compatible repair materals in this curing environment by using up to 30% natural pozzolana as white cement replacement.

A study on the rheological properties of superfluidity self compacting concrete utilizing tailings from the tungsten mine (광산광미를 활용한 초유동 자기충전 콘크리트의 유변학적 특성 연구)

  • Choi, Yun-Wang;Kim, Yong-Jic;Choi, Wook;Lee, Kwang-Myong
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.05b
    • /
    • pp.89-92
    • /
    • 2006
  • This study has focused on the possibility for recycling of tailings from the Sangdong tungsten mine as powder of superfluidity self-compacting concrete. The experimental tests for slump-flow, time required to reach 500mm of slump flow(sec), time required to flow through V-funnel(sec) and filling height of U-box test(mm) were carried out in accordance with the specified by the Japanese Society of Civil Engineering(JSCE). The result of this study, in case of superfluidity self-compacting concrete mixed with tailings, slump-flow was decreased with increasing mixing ratio. But time required to reach 500mm of slump flow(sec), time required to flow through V-funnel(sec) and filling height of U-box test(mm) were satisfied a prescribed range.

  • PDF

Optimum Mix Proportion and Characteristics of the Combined Self Compacting Concrete according to Cement Types (시멘트 종류에 따른 병용계 자기충전 콘크리트의 최적배합비와 특성)

  • Kwon, Yeong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.21 no.1
    • /
    • pp.55-64
    • /
    • 2009
  • This study is aimed to derive the optimum mix proportion of the combined self compacting concrete according to cement types (blast-furnace slag cement and belite cement) and to propose the basic data to field construction work after evaluating the quality properties. Specially, lime stone powder (LSP) as binder and viscosity agent are used in the combined self compacting concrete because slurry wall of an underground LNG storage tank should be kept stability of quality during concrete working. Replacement ratio of LSP is determined by confined water ratio test and main design factors including fine aggregate ratio ($S_r$), coarse aggregate ratio ($G_v$) and water-cement ratio (W/C) are selected. Also, quality properties including setting time, bleeding content, shortening depth and hydration heat on the optimum mix proportion of the combined self compacting concrete according to cement type are compared and analyzed. As test results, the optimum mix proportion of the combined self compacting concrete according to cement type is as followings. 1) Slag cement type-replacement ratio of LSP 13.5%, $S_r$ 47% and W/C 41%. 2) Belite cement type-replacement ratio of LSP 42.7%, Sr 43% and W/C 51%. But optimum coarse aggregate ratio is 53% regardless of cement types. Also, as test results regarding setting time, bleeding content, shortening depth and hydration heat of the combined self compacting concrete by cement type, belite cement type is most stable in the quality properties and is to apply the actual construction work.

Method for estimating workability of self-compacting concrete using mixing process images

  • Li, Shuyang;An, Xuehui
    • Computers and Concrete
    • /
    • v.13 no.6
    • /
    • pp.781-798
    • /
    • 2014
  • Estimating the workability of self-compacting concrete (SCC) is very important both in laboratories and on construction site. A method using visual information during the mixing process was proposed in this paper to estimate the workability of SCC. First, fourteen specimens of concrete were produced by a single-shaft mixer. A digital camera was used to record all the mixing processes. Second, employing the digital image processing, the visual information from mixing process images was extracted. The concrete pushed by the rotating blades forms two boundaries in the images. The shape of the upper boundary and the vertical distance between the upper and lower boundaries were used as two visual features. Thirdly, slump flow test and V-funnel test were carried out to estimate the workability of each SCC. Finally, the vertical distance between the upper and lower boundaries andthe shape of the upper boundary were used as indicators to estimate the workability of SCC. The vertical distance between the upper and lower boundaries was related to the slump flow, the shape of the upper boundary was related to the V-funnel flow time. Based on these relationships, the workability of SCC could be estimated using the mixing process images. This estimating method was verified by three more experiments. The experimental results indicate that the proposed method could be used to automatically estimate SCC workability.

Optimal Mixture Proportion for High Performance Concrete Incorporating Ground Granulated Blast furnace Slag

  • Choi Jae-Jin;Kim Eun-Kyum;Yoo Jung-Hoon
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.3 s.87
    • /
    • pp.473-480
    • /
    • 2005
  • In this study, a mix design for self compacting concrete was based on Okamura's method and concrete incorporated just a ground granulated blast furnace slag. Replacement ratio of slag is in the range of $20-80\%$ of cement matrix by volume. For the optimal self compactability in mixture incorporating ground granulated blast furnace slag, the paste and mortar tests were first completed. Then the slump flow, elapsed time of 500mm slump flow, V funnel time and filling height by U type box were conducted in concrete. The volume of coarse aggregate in self compacting concrete was in the range of $50-60\%$ to the solid volume percentage of coarse aggregate. Finally, the compressive and splitting tensile strengths were determined in the hardened self compacting concrete incorporating ground granulated blast furnace slag. From the test results, it is desirable for self compacting concrete that the replacement of ground granulated blast furnace slag is in the range of $40-60\%$ of cement matrix by volume and the volume of coarse aggregate to the solid volume percentage of coarse aggregate with a limit of $55\%$.

The self-compacting property of concrete as to specific gravity and mixing proportion of lightweight coarse aggregate (경량 굵은골재 비중 및 혼합률에 따른 콘크리트의 자기충전성)

  • Choi, Yun-Wang;Kim, Yong-Jic;Choi, Wook;Lee, Sang-Ho;Cho, Sun-Kyu
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.11a
    • /
    • pp.747-750
    • /
    • 2004
  • Lightweight concrete is known for its advantage of reducing the self-weight of the structures, reducing the areas of sectional members as well as making the construction convenient. Thus the construction cost can be saved when applied. to . structures such as long-span bridge and high rise buildings. However, the lightweight concrete requires specific design mix method that is quite different from the typical concrete, since using the typical mix method would give rise the material segregation as well as lower the strength by the reduced weight of the aggregate. In order to avoid such problems, it is recommended to apply the design mix method of high performance self-compacting concrete for the lightweight concrete. Therefore, this study introduces a production of self-compacting concrete, PF-modified and improved version of Nan-Su's design mix method of self-compacting concrete. Through a series of test mixes conducted during the study, the quality of the concrete at its fresh condition has been evaluated per the 2nd class rating standards of self-compacting concrete published by JSCE, especially focused in its fluidity, segregation resistance ability, and filling ability.

  • PDF

Steel - concrete bond potentials in self-compacting concrete mixes incorporating dolomite powder

  • Kamal, Mounir M.;Safan, Mohamed A.;Al-Gazzar, Mohamed A.
    • Advances in concrete construction
    • /
    • v.1 no.4
    • /
    • pp.273-288
    • /
    • 2013
  • The main objective of this research was to evaluate the potentials of self-compacting concrete (SCC) mixes to develop bond strength. The investigated mixes incorporated relatively high contents of dolomite powder replacing Portland cement. Either silica fume or fly ash was used along with the dolomite powder in some mixes. Seven mixes were proportioned and cast without vibration in long beams with 10 mm and 16 mm steel dowels fixed vertically along the flowing path. The beams were then broken into discrete test specimens. A push-put configuration was adopted for conducting the bond test. The variation of the ultimate bond strength along the flowing path for the different mixes was evaluated. The steel-concrete bond adequacy was evaluated based on normalized bond strength. The results showed that the bond strength was reduced due to Portland cement replacement with dolomite powder. The addition of either silica fume or fly ash positively hindered further degradation as the dolomite powder content increased. However, all SCC mixes containing up to 30% dolomite powder still yielded bond strengths that were adequate for design purpose. The test results demonstrated inconsistent normalized bond strength in the case of the larger diameter compared to the smaller one.

Fresh and hardened properties of rubberized concrete using fine rubber and silpozz

  • Padhi, S.;Panda, K.C.
    • Advances in concrete construction
    • /
    • v.4 no.1
    • /
    • pp.49-69
    • /
    • 2016
  • This work investigates the mechanical properties of conventional concrete (CC) and self compacting concrete (SCC) using fine rubber and silpozz were accompanied by a comparative study between conventional rubberized concrete (CRC) and self compacting rubberized concrete (SCRC). Fine rubber (FR) from scrap tires has replaced the fine aggregate (FA) and Silpozz has been used as a replacement of cement at the proportions of 5, 10 and 15%. Silpozz as a partial replacement of cement in addition of superplasticiser (SP) increases the strength of concrete. Fresh concrete properties such as slump test, compaction factor test for CRC, whereas for SCRC slump flow, $T_{500}$, V-funnel, L-box, U-box, J-ring tests were conducted along with the hardened properties tests like compressive, split tensile and flexural strength test at 7, 28 and 90 days of curing. The durability and microstructural behavior for both CRC and SCRC were investigated. FR used in the present study is 4.75 mm passing with fineness modulus 4.74.M30 grade concrete is used with a mix proportion of 1:1.44:2.91 and w/c ratio as 0.43. The results indicate that as FR quantity increases, workability of both CRC and SCRC decreases. The results also show that the replacement of natural fine aggregate (NFA) with FR particles decreases the compressive strength with the increase of flexural strength observed upto 5% replacement of FR. Also replacement of cement with silpozz resulted enhancement of strength in SCRC.

Optimum Mix Proportion of the High Strength and Self Compacting Concrete Used Above-Ground LNG Storage Tank (지상식 LNG 저장탱크용 고강도 자기충전 콘크리트의 최적배합에 관한 연구)

  • Kwon, Yeong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.1
    • /
    • pp.99-107
    • /
    • 2011
  • This study is to performed to find the optimum mix proportion of the high strength and self compacting concrete for the above-ground LNG storage tank construction and field application. If LNG storage tank wall thicknesscan be reduced, the construction cost and quality can be improved by using self-compacting high strength concrete with compressive strength 60~80 MPa. For this purpose, low heat cement (Type IV) and class F fly ash are used in concrete mix to control hydration heat, flowability, and viscosity. Mix design variables of unit water, fly ash replacement ratio, water-binder ratio, and fine aggregate ratio are selected and tested for material properties and manufacturing cost of the concrete. Also, fly ash replacement ratio is considered using confined water ratio test. The test results showed that the optimum mix proportion of the self-compacting high strength concrete characteristics are as follows. 1) In case of the concrete with specified compressive strength of 60 MPa, the optimum mix proportion is fly ash replacement ratio of 20% and water- binder ratio of 27~30%. 2) In case of the concrete with the strength of 80 MPa, the optimum mix proportion is fly ash replacement ratio of 10% and water-binder ratio 25%. But unit water and fine aggregate ratio are 165 $kg/m^3$ and $51{\pm}2%$, respectively, regardless of the traget concrete compressive strength range. Also, test results showed that concrete manufacturing cost of 60 MPa and 80 MPa concrete require additional costs of 14~22% and 33%, respectively, compared to the manufacturing cost of 40 MPa concrete. Therefore, application of the self-compacting high strength concrete has proven to be economical in the perspective of the material cost, quality control, and site management.