일반 현미경용 유리에 증착시킨 Indium-Tin Oxide 박막의 제작 및 특성 (Fabrication and characterization of Indium-Tin Oxide thin film on the commercial glass substrate)

  • 김여중;조길호
    • 한국진공학회지
    • /
    • 제9권1호
    • /
    • pp.30-35
    • /
    • 2000
  • Indium-Tin Oxide (ITO) thin films were deposited on the commercial glass substrate by rf-magnetron sputtering. The ITO films with the thickness of 2,000~2,400 $\AA$ were prepared by changing the oxygen partial pressures of 2, 3, and 5%, as well as by changing the substrate temperature of $300^{\circ}C$ and $500^{\circ}C$. spectrophotometer, XRD, SEM, AFM, 4-point probe and Hall effect system were employed to characterize the ITO films. The optimum deposition conditions were the substrate temperature of $500^{\circ}C$ and oxygen partial pressure of 2-3%. At theses conditions, the ITO film showed the transmittance of 91%, the resistivity of $5.4\times10^{-3}\Omega$cm, the carrier concentration of $1.0\times10^{19}\textrm{cm}^{-3}$, and the carrier mobility of 150$\textrm{cm}^2$/Vsec. In XRD spectra, the (222) and (400) $In_2O_3$ planes were dominant under the optimum deposition conditions When the substrate was cleaned only by the method of ultrasonic cleaning without both pre-annealing and chemical treatment of the substrate, the ITO film exhibited the transmittance of 86%, the carrier concentration of $5.4\times10^{19}\textrm{cm}^{-3}$ and the mobility of 24$\textrm{cm}^2$/Vsec.

  • PDF

마그네트론 스퍼터링법을 이용한 Indium-Tin Oxide 박막의 제작과 그 특성에 관한 연구 (A Study on the Fabrication and Characteristics of ITO Thin Film Deposited by Magnetron Sputtering Method)

  • 조길호;김여중;김성종;문경만;이명훈
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제24권6호
    • /
    • pp.61-69
    • /
    • 2000
  • Indium-Tin Oxide (ITO) films were prepared on the commercial glass substrate by the Magnetron Sputtering method. The target was a 90wt.% $In_2O_3$-10wt.% $SnO_2$with 99.99% purity. The ITO films deposited by changing the partial pressure of oxygen gas ($O_2$/(Ar+$O_2$)) of 2, 3 and 5% as well as by changing the substrate temperature of $300^{\circ}C$ or $500^{\circ}C$. The influence of substrate pre-annealing and pre-cleaning on the quality of ITO film were examined, in which the substrate temperature was $500^{\circ}C$ and oxygen partial pressure was 3%. The characteristics of films were examined by the 4-point probe, Hall effect measurement system, SEM, AFM, Spectrophotometer, and X-ray diffraction. The optimum ITO films have been obtained when the substrate temperature is $500^{\circ}C$ and oxygen partial pressure is 3%. At optimum condition, the film showed transmittance of 81%, sheet resistivity of $226\Omegatextrm{cm}^2$, resistivity($\rho$) of $5.4\times10^{-3}\Omega$cm, carrier concentration of $1.0\times10^{19}cm^{-3}$, and carrier mobility of $150textrm{cm}^2$Vsec. From XRD spectrum, c(222) plane was dominant in the case of substrate temperature at $300^{\circ}C$, without regarding to oxygen partial pressure. However, in the case of substrate temperature at $500^{\circ}C$, c(400) plane was grown together with c(222) plane, only for oxygen partial pressure of 2 and 3%. In both case of chemical and ultrasonic cleaning without pre-annealing the substrate, it showed much almost same sheet resistivity, resistivity($\rho$), transmittance, carrier concentration, and carrier mobility. In case of $500^{\circ}C$/60min pre-annealing before ITO film deposited, both transimittance and carrier mobility are better than no pre-annealing, because pre-annealing is supposed to remove alkari ions diffusion from substrate. ITO film deposited on the Corning 0080 sybstrate showed a little bit better sheet resistivity, resistivity($\rho$), transimittance, carrier concentration than the film deposited on commercial glass. But no differences between Corning substrate and pre-annealed commercial glass substrate are found.

  • PDF

저일조 조건에서 몇 가지 친환경농자재가 고추와 토마토의 유묘 생육에 미치는 영향 (Effects of Some Environment-friendly Farming Materials on Growth of Pepper and Tomato Seedlings under Low Solar Radiation Conditions)

  • 엄영철;서태철;장윤아;이상규;이준구;최장선;오상석
    • 생물환경조절학회지
    • /
    • 제20권4호
    • /
    • pp.269-276
    • /
    • 2011
  • 저일조 조건에서 고추와 토마토 유묘의 생육에 미치는 몇 가지 친환경농자재의 이용효과를 검토하고자 하였다. 친환경농자재는 미생물제재, 효소제, 아미노산제 3종을 이용하였고 30% 차광조건에서 토마토와 고추를 육묘하였으며, 육묘용 상토 종류에 따른 차이를 보기위해 일반 원예용(유비)상토와 무비상토를 비교하였다. 토마토와 고추 모두 무비상토에서는 효소제와 아미노산제 처리에 의해 묘의 생육이 양호하였으나, 미생물제재 처리는 대조구와 차이가 없었다. 유비상토에서는 친환경농자재 처리에 의한 생장촉진효과가 나타나지 않았다. 차광처리에 의하여 묘의 건물중은 감소하고, 엽면적은 다소 증가하는 경향을 보였으나, 친환경농자재의 처리에 의한 생육촉진효과는 없었다. 정식 후 토마토 1화방의 개화소요일수 및 착과절위를 조사한 결과, 무비상토의 경우 효소제 및 아미노산제 처리구에서 개화소요일수가 3~4일 적었으나, 착과절위는 차이가 없었다. 다만 차광조건에서 착과절위가 낮아지는 경향을 보였다. 유비상토의 경우는 친환경농자재 처리나 차광 유무에 따른 개화소요일수나 착과절위의 차이가 없었다. 고추는 무비상토에서 차광에 관계없이 효소제 및 아미노산제 처리구에서 건물중이 증가하였으나 미생물제재 처리구에서는 효과가 없었다. 유비상토는 친환경 농자재의 처리효과가 없었다. 따라서 시판되고 있는 효소제와 아미노산제는 무비상토에서 생육촉진효과가 있었으나, 미생물제재 처리는 처리효과가 없었고, 양분이 함유된 상토에서는 친환경농자재의 처리효과가 없었다. 또 차광에 의한 저일조 조건에서 친환경농자재의 혼용 처리에 의한 토마토와 고추 유묘의 생육촉진효과는 없었다.

Float 공법을 고려한 Plasma Display Panel용 기판유리 용융체의 특성 (Melt Properties of Plasma Display Panel Substrate Glasses Based on Float Process)

  • 김기동;정우만;정현수;권성구;최세영
    • 한국세라믹학회지
    • /
    • 제43권7호
    • /
    • pp.433-438
    • /
    • 2006
  • In order to examine the working condition of melts in tin bath of float process it was investigated Sn diffusion behavior and solidification rate of melts for alkali-alkaline earth-silica PDP substrate glasses such as commercial CaO rich CS-77 glass, commercial $Al_2O_3$ rich PD-200 glass and self developed $SiO_2$ rich T-series (T-2, T-4, T-6) glasses. In the case of Sn depth and concentration created in glass surface by ion exchange between Sn and alkali, T-series showed lower value than CS-77, especially T-2 is more excellent than PD-200. The solidification rate of melts expressed by cooling time between $log{\eta}=4\;and\;7.6dPa{\cdot}s$ was low for T-series comparing with CS-77 and PD-200. Therefore, it was concluded that T-series is desirable considering forming condition in the tin bath of the float process.

Plasma Display Panel용 기판 유리용융체의 내화물 침식 (Corrosion of Refractory in Glass Melts for Plasma Display Panel Substrate)

  • 김기동;정현수;김효광
    • 한국세라믹학회지
    • /
    • 제44권1호
    • /
    • pp.65-69
    • /
    • 2007
  • For self-developed alkali-alkaline earth-silicate and commercial glass melts for plasma display panel substrate, the corrosion behavior of fused casting refractory consisting of $Al_2O_3-ZrO_2-SiO_2$ was examined at the temperature corresponding to $10^2\;dPa{\cdot}s$ of melt viscosity by static finger methode. The corroded refractory specimens showed a typical concave shape due to interfacial convection of melts at their flux line. However, the corrosion thickness by commercial glass melts was $6\sim10$ times comparing to that by the self?developed melts. From the view point of the glass composition and the role of alkaline earth in glass network, it was discussed the effect of alkali/alkaline earth diffusion and temperature on the refractory corrosion.

해조류 톳 (Hizikia fusiforme)의 효소 가수분해 (Enzymatic Hydrolysis of Marine Algae Hizikia fusiforme)

  • 송부복;김성구;정귀택
    • KSBB Journal
    • /
    • 제26권4호
    • /
    • pp.347-351
    • /
    • 2011
  • In this study, we investigated the effect of reaction factors on enzymatic hydrolysis of Hizikia fusiforme, which is brown algae in marine biomass resource, using commercial enzymes. The composition of H. fusiforme is 38.9% of reducing sugar, 4.8% of moisture, 17.8% of ash, and 38.5% of others. In the condition of 1-5% substrate, the increase of substrate concentration enhanced the increase of reducing sugar formation; however, the hydrolysis yield did not increase after 24 h. After reaction of 75 h, conversion yield of reducing sugar were obtained to 16.45%, 17.99%, and 14.55% at 1, 2.5, and 5% substrate, respectively. As a result of effect of enzyme amount, the formation of reducing sugar did not show considerable change at 1% substrate. However, in the condition of 2.5% substrate, the great change of reducing sugar formation was observed by the increase of enzyme amount. The conversion yields of reducing sugar were obtained to 18.77% and 22.83% at 1% and 2.5% substrate with 30% enzyme, respectively. As a result of heat treatment of biomass, the high yield was obtained in 2.5% substrate and the yields were increased to 0.06-7.2% by the heat treatment. This result will provide the basic information for production process of biofuels and chemicals from marine biomass H. fusiforme.

강 표면의 다이아몬드/몰리브데늄/니켈 복합층의 생성 (Formation of Diamond/Mo/Ni Multi-Layer on Steel Substrate)

  • Lee, H.J.;J.I. Choe;Park, Y.
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2002년도 춘계학술발표회 초록집
    • /
    • pp.37-37
    • /
    • 2002
  • Diamoncl/Mo/Ni multi-layers on SKH-51 steel substrate was prepared to improve the abrasive wear resistance of a tool and die by a commercial chemical vapor deposition unit and electro-plating. The diamond after 7 hour deposition had cuba-octahedral structure with 2~5$\mu\textrm{m}$ grains. The existence of non-ferrous metals such as chromium, nickel and molybdenum between diamond and SKH-51 substrate results in forming higher quality of diamond layer by retarding carbon diffusion in the diamond layer during deposition, and also improving hardness and wear resistance. Surface cracks on the film was sometimes observed by the difference of by the thermal expansion coefficients between the steel substrate and the deposited layers during cooling.

  • PDF

저온 열처리 과정에서 일어나는 (0001) α-Al2O3 기판 표면의 형상 변화 (Surface Morphological Evolution of (0001) α-Al2O3 Substrate During Low Temperature Annealing)

  • 이근형
    • 한국전기전자재료학회논문지
    • /
    • 제23권11호
    • /
    • pp.859-863
    • /
    • 2010
  • Evolution of surface morphology of ${\alpha}-Al_2O_3$ substrate was investigated as a function of annealing temperature and time. Commercial (0001) ${\alpha}-Al_2O_3$ single crystal substrates were annealed in the range of $600-1000^{\circ}C$ in air. At $600^{\circ}C$, step-terrace structure started to be formed on the substrate. However, the surface roughness on the terrace was still considerable and a number of islands were observed on the step edges as well as the terraces. As the annealing temperature increased, the islands were absorbed into the step edges. Thus the terraces were smoother and the step edges were more straightened. Well-defined surface with a step height of 0.2 nm was formed above $900^{\circ}C$. On the other hand, when the substrate was annealed at a fixed temperature of $1000^{\circ}C$, the change of surface morphology was observed for the substrate annealed for 10 min. After the annealing for 30 min, the surface on which any islands could not survive was observed.

Effect of Different Substrates and Casing Materials on the Growth and Yield of Calocybe indica

  • Amin, Ruhul;Khair, Abul;Alam, Nuhu;Lee, Tae-Soo
    • Mycobiology
    • /
    • 제38권2호
    • /
    • pp.97-101
    • /
    • 2010
  • Calocybe indica, a tropical edible mushroom, is popular because it has good nutritive value and it can be cultivated commercially. The current investigation was undertaken to determine a suitable substrate and the appropriate thickness of casing materials for the cultivation of C. indica. Optimum mycelial growth was observed in coconut coir substrate. Primordia initiation with the different substrates and casing materials was observed between the 13th and 19th day. The maximum length of stalk was recorded from sugarcane leaf, while diameter of stalk and pileus, and thickness of pileus were found in rice straw substrate. The highest biological and economic yield, and biological efficiency were also obtained in the rice straw substrate. Cow dung and loamy soil, farm-yard manure, loamy soil and sand, and spent oyster mushroom substrates were used as casing materials to evaluate the yield and yield-contributing characteristics of C. indica. The results indicate that the number of effective fruiting bodies, the biological and economic yield, and the biological efficiency were statistically similar all of the casing materials used. The maximum biological efficiency was found in the cow dung and loamy soil casing material. The cow dung and loamy soil (3 cm thick) was the best casing material and the rice straw was the best substrate for the commercial cultivation of C. indica.

Assessment of Palm Press Fibre and Sawdust-Based Substrate Formulas for Efficient Carpophore Production of Lentinus squarrosulus (Mont.) Singer

  • Osibe, Dandy Ahamefula;Chiejina, Nneka Virginia
    • Mycobiology
    • /
    • 제43권4호
    • /
    • pp.467-474
    • /
    • 2015
  • Development of efficient substrate formulas to improve yield and shorten production time is one of the prerequisites for commercial cultivation of edible mushrooms. In this study, fifteen substrate formulas consisting of varying ratios of palm press fibre (PPF), mahogany sawdust (MS), Gmelina sawdust, wheat bran (WB), and fixed proportions of 1% calcium carbonate ($CaCO_3$) and 1% sucrose were assessed for efficient Lentinus squarrosulus production. Proximate compositions of mushrooms produced on the different substrate formulas were also analysed and compared. Substrate formulations containing 85% PPF, 13% WB, 1% $CaCO_3$, and 1% sucrose were found to produce the highest carpophore yield, biological efficiency and size (206.5 g/kg, 61.96%, and 7.26 g, respectively). Days to production (first harvest) tended to increase with an increase in the amount of WB in the substrate formulas, except for PPF based formulas. The addition of WB in amounts equivalent to 8~18% in substrate formulas containing 80~90% PPF resulted in a decrease in the time to first harvest by an average of 17.7 days compared to 80~90% MS with similar treatment. Nutritional content of mushrooms was affected by the different substrate formulas. Protein content was high for mushrooms produced on formulas containing PPF as the basal substrate. Thus, formulas comprising PPF, WB, $CaCO_3$, and sucrose at 85% : 13% : 1% : 1%) respectively could be explored as starter basal ingredients for efficient large scale production of L. squarrosulus.