• Title/Summary/Keyword: chromium ($Cr^{3+}$

Search Result 461, Processing Time 0.024 seconds

EFFECTS OF CHROMIUM PICOLINATE ON GROWTH PERFORMANCE, CARCASS COMPOSITION AND SERUM TRAITS OF BROILERS FED DIETARY DIFFERENT LEVELS OF CRUDE PROTEIN

  • Kim, S.W.;Han, I.K.;Choi, Y.J.;Kim, Y.H.;Shin, I.S.;Chae, B.J.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • v.8 no.5
    • /
    • pp.463-470
    • /
    • 1995
  • An experiment was conducted to evaluate the effects of chromium picolinate on growth performance, nutrient utilizability, carcass composition, serum traits and in vitro protein synthesis of 3 day old Arbor Acres broiler chickens when dietary crude protein levels were varying in diets. Six replicates of eight chicks each (average initial weitht = 59.4 g) were randomly assigned to three levels (low, medium, high) of dietary crude protein at two levels of chromium (0, 200 ppb Cr/kg diet) as chromium picolinate. Six chicks/treatment were randomly chosen for analyses of carcass composition, six additional chicks/treatment were randomly chosen for analyses of serum components, and a chick/treatment was chosen for in vitro culture of liver tissue. Chromium picolinate did not affect feed intake, protein and fat utilizability, regradless of dietary crude protein level. But feed/gain ratio were more improved in groups fed the low protein diets added with chromium picolinate compared with groups fed the medium and high protein diets with chromium picolinate. Carcass fat tended to decrease whereas carcass protein tended to increase when added with chromium picolinate. Broilers fed diets with chromium picolinate exhibited lower serum triglyceride and nonesterified fatty acid concentrations than those fed without chromium picolinate (p < 0.05). Both secreted and retained proteins in cultured acinar cell were higher in groups fed diets with chromium picolinate than those fed diets without chromium picolinate (p < 0.05). It could be suggested that chromium picolinate was effective in improving weight gain and nutrient utilizability when dietary crude protein was low (p < 0.05), and also effective in manipulating carcass fat when dietary crude protein level was high (p < 0.05).

Creep Rupture Due to Molybdenum Rich $M_6C$ Carbide in 1.0Cr-1.0Mo-0.25V Steel Weldment (1.0Cr-1.0Mo-0.25V강 용접부의 $M_6C$ 탄화물에 의한 크립 파단)

  • O, Yeong-Geun;Kim, Byeong-Cheol;Gang, Gye-Myeong;Min, Tae-Guk
    • Korean Journal of Materials Research
    • /
    • v.6 no.12
    • /
    • pp.1257-1262
    • /
    • 1996
  • 1.0Cr-1.0Mo-0.25V강 용접부의 크립 파단 시험시 파단 발생 원인에 관한 연구가 시행되었다. 파괴는 Intercritical Heat Affected Zone에서 발생하였으며 파단면에서 구상의조대한 M6C탄화물이 발견되었다. 모재는 molybdenum 주성분의 M2C, vanadium 주성분의 M4C3 및 chromium 주성분의 M23C6와 M7C3 탄화물이 존재하였다. 모의 실험 결과 준안정 상태인 M2C 탄화물은 85$0^{\circ}C$, 10oh에서 안정한 M6C탄화물로 변태하였다. M6C 탄화물은 주변의 molybdenum 농도를 떨어뜨려 강도의 저하를 가져오며 크립 기공의 발생 원인을 제공하였다.

  • PDF

Determination of Thermal Conductivity and Numerical Analysis of Al-Cr-N-O Composites Layer Formed by Hydro-thermal Process (수열합성된 Al-Cr-N-O계 도포층의 열전도 측정과 수학적 해석)

  • Kim, Ma-Ro;Yang, So-Eun;Lee, Jong-Jae;Kim, Byeong-Du;Choe, Yong
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2014.11a
    • /
    • pp.215-215
    • /
    • 2014
  • Composites layer of Al-Cr-Ni-O system was prepared on a steel plate by hydro-thermal process at $700^{\circ}C$ for 12 hours, which phase identification and thermal conductivity were determined. The composites layer consisted of aluminum nitride, alumina, chromium carbide and aluminium, which density was $3.7kg/m^3$. The thermal conductivity of the coating layer determined by thermal data acquisition system was about 98.0 W/m/ which depended on the AlN content. Numerical modelling of the heat transfer behavior of the coating layer was well agreement with the empirical data.

  • PDF

The Effect of Chemical Composition of Sintering Atmosphere on the Structure and Mechanical Properties of PM Manganese Steels with Chromium and Molybdenum Additions

  • Sulowski, Maciej;Cias, Andrzej;Stoytchev, Marin;Andreev, Tchavdar
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.561-562
    • /
    • 2006
  • The effect of chemical composition of the sintering atmosphere on density, microstructure and mechanical properties of Fe-3%Mn-(Cr)-(Mo)-0.3%C steels is described. Pre-alloyed Astaloy CrM and CrL, ferromanganese and graphite were used as the starting powders. Following pressing in a rigid die, compacts were sintered at 1120 and $1250^{\circ}C$ in atmospheres having different $H_2/N_2$ ratio and furnace cooled to room temperature. It has been found that the atmosphere composition has negligible effect on the as-sintered properties of the investigated materials.

  • PDF

Contents of Cr and Co in Some Fisheries Caught in the West Coast (서해안지역 어패류의 크롬(Cr)과 코발트(Co) 함량)

  • Kim, Ae-Jung;Kim, Sun Yeou;Lee, Won-Chu
    • Analytical Science and Technology
    • /
    • v.11 no.1
    • /
    • pp.29-35
    • /
    • 1998
  • This study was performed to assess the levels of the Cr and Co in fisheries caught from the some areas of west coast in Korea. The samples were 26 kinds of fishes, 19 kindly of Mollusca and 3 kinds of Crustacea. They were ashed with 5 ml $HNO_3$ and then wet-decomposed with 10 ml of a mixture of $HNO_3:H_2SO_4:HClO_4$ (10:1:4). After ashing of samples, the amounts of Cr and Co in the samples were determined by ICP-AES analysis. The moisture content of molluscans was significantly higher than that of crustaceans (p<0.05), but there was no significant difference among fisheries in the Cr content. And the Co content of crustaceans was significantly higher than that of fishes and molluscans (p<0.001). There was no significance between contents of Cr and Co in fisheries. The Cr content of Arkshell was 422.00 ppm, which was the most amount compared with those of the other samples. And the Co in Myong-Ge was 3.78 ppm, which was the most amount. Areliscus honaleus (Cr:2.76 ppm, Co:0.97 ppm), Solen (Cr:6.56 ppm, Co:1.59 ppm) and dried barley shrimp (Cr:1.06 ppm, Co:0.90 ppm) contained great amount of Cr and Co.

  • PDF

Study on the extraction mechanism and the optimization of extraction method for Chromium using anion exchangers (음이온 교환체를 이용한 크롬의 추출메카니즘 및 추출방법 최적화에 관한 연구)

  • Kim, S.W.;Kim, D.M.;Kim, Y.S.;Lim, H.B.
    • Analytical Science and Technology
    • /
    • v.7 no.3
    • /
    • pp.387-393
    • /
    • 1994
  • Quantitative analytical conditions for chromium using solvent extraction followed by atomic absorption spectrometry was studied. Trioctylamine(TOA) in tertiary amine or Trioctylmethylammoniumchloride(TOMAC) in quaternary ammonium salt, both containing octyl group was used as an anion exchangers. Absorbance were measured for the different kinds of acid added and as changing the concentration of acid by graphite furnace atomic absorption spectrometer. The maximum absorbance was obtained at the concentrations of HCl, 0.1M to 0.3M for TOA and 0.03M to 0.1M for TOMAC. Mole ratios over 1:1 of TOA or TOMAC dissolved in MIBK solution to chromium in sample shows optimum extraction efficiency while HCl was added to the MIBK. As a result of scrutinizing the extraction process, the methods employed in this experiment turned out to be better extraction efficiency for chromium, compared to similar extraction methods.

  • PDF

An experimental study of the strength and internal structure of solder joint of fixed partial denture (가공의치(架工義齒) 납착부(蠟着部)의 강도(强度)와 내부구조(內部構造)에 관(關)한 실험적(實驗的) 연구(硏究))

  • Park, Sang-Nam;Kay, Kee-Sung
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.23 no.1
    • /
    • pp.39-59
    • /
    • 1985
  • The purpose of this study was to investigate how gap distances of 0.13mm, 0.15mm, 0.20mm, and 0.30mm affects solder joint strength from gold alloys and nickel-chromium base alloys and to examine the composition of solder gold, the solder joint of gold alloys and nickel-chromium base alloys. The tensile test specimens were prepared in the split stainless steel mold with a half dumbbell shape 2.5mm in diameter and l2mm in length. 6 pairs of specimens of each gap distance group of gold alloys and nickel-chromium base alloys were made and 48 pairs of all specimens were soldered with solder gold of 666 fineness. All soldered specimens were machined to a uniform diameter and then a tensile load was applied at a cross-head speed of 0.10mm/min using Instron Universal Testing Machine, Model 1115. The fractured specimens at solder gold of solder joint fracture with each gap distance of 0.13mm, 0.15mm, 0.20mm, and 0.30mm were examined under the Scanning Electron Microscope, JSM-35c and the composition of solder gold, the solder joint of gold alloys and nickel-chromium base alloys was analyzed by Electron Probe Micro Analyzer. The results of this study were obtained as follows: 1. In case of soldering of gold alloys, the tensile strength between gold alloys showed $37.33{\pm}2.52kg/mm^2$ at 0.13, $39.14{\pm}3.35kg/mm^2$ at 0.15mm, $43.76{\pm}2.97kg/mm^2$ at 0.20mm, and $49.18{\pm}4.60kg/mm^2$ at 0.30mm. There was statistically significant difference at each gap distance, and so the greater increase of gap distance showed the greater tensile strength. 2. In case of soldering of nickel-chromium base alloys, the tensile strength between nickel-chromium base alloys showed $34.84{\pm}4.26kg/mm^2$ at 0.13mm, $37.25{\pm}2.49kg/mm^2$ at 0.15mm, $42.91{\pm}4.32kg/mm^2$ at 0.20mm, and $46.93{\pm}4.21kg/mm^2$ at 0.30mm. There was not statistically significant difference only between 0.13mm and 0.15mm and bet ween 0.20 mm and 0.30mm, but generally the greater increase of gap distance showed the greater tensile strength. 3. The greater increase of gap distance shoed less porosities in solder gold at solder joint fracture. 4. In solder gold Au, Cu, Ag, Zn, and Sn were composed and Au and Cu were mostly distributed uniformly. 5. In solder joints of solder gold and gold alloys Au, Cu, Ag, Zn, and Sn were composed in solder gold and Au, Cu, Ag, Pt, and Pd were composed in gold alloys. Au and Cu of solder gold and gold alloys were mostly distributed uniformly and the diffusion of other elements except Pt and Pd around the solder joint was not almost found. In solder joints of solder gold and nickel-chromium base alloys Au, Cu, Ag, Zn, and Sn were composed in solder gold and Ni, Cr, and Al were composed in nickel-chromium base alloys. Au and Cu of solder gold and Ni and Cr of nickel-chromium base alloys were mostly distributed uniformly and the diffusion of other elements except Cr around the solder joint was not almost found.

  • PDF

High-Temperature Oxidation of Ti Containing Stainless Steel in O2-N2 Atmosphere

  • Onishi, Hidenori;Saeki, Isao;Furuichi, Ryusaburo;Okayama, Toru;Hanamatsu, Kenko;Shibayama, Tamaki;Takahashi, Heishichiro;Kikkawa, Shinichi
    • Corrosion Science and Technology
    • /
    • v.3 no.4
    • /
    • pp.140-147
    • /
    • 2004
  • High temperature oxidation of Fe-19Cr and Fe-19Cr-0.2Ti alloys is studied at 1173-1373 K in 16.5 kPa $O_2$ - balances $N_2$ atmosphere aimed at clarifying the effect of titanium addition. Oxidation rate of Fe-19Cr alloy was accelerated with titanium. For both alloys chromium rich $(Fe,\;Cr)_2O_3$ was formed as a major oxidation product. On Fe-19Cr-0.2Ti alloy, a thin layer composed of spinel type oxide and titanium oxide was also formed and an internal oxidation of titanium was observed. Titanium was concentrated at the oxide surface and internal oxidation zone but a small amount of titanium was also found in the intermediate corundum type $(Fe,\;Cr)_2O_3$ layer. Crystals of corundum type $(Fe,\;Cr)_2O_3$ formed on Fe-19Cr alloy are coarse but that formed on Fe-19Cr -0.2Ti alloys were fine and columnar. Reason for the difference in oxidation kinetics and crystal structure will be discussed relating to the distribution of aliovalent titanium in corundum type $(Fe,\;Cr)_2O_3$ oxide layer.

Formation of Multi-Component Boride Coatings Containing V and/or Cr and Evaluation of Their Properties (바나듐 및 크롬을 포함하는 다 성분 Boride 코팅의 생성 및 특성 평가)

  • Lee, Euiyeol;Yoon, Sanghyun;Kim, Jongha
    • Journal of Surface Science and Engineering
    • /
    • v.49 no.2
    • /
    • pp.211-217
    • /
    • 2016
  • Boride coating applied on steam turbine parts of power plants has provided good particle erosion resistance under temperature of $550^{\circ}C$, but it isn't able to protect the parts effectively any more in ultra super critical (USC) steam turbine which is being operated up to temperature of $650^{\circ}C$. To ensure stable durability for USC steam turbine parts, an alternative coating replacing boride coating should be developed. In this study, multi-component boride coatings containing elements such as chromium (Cr) and vanadium (V) were formed on base metal (B50A365B) using thermochemical treatment method called by pack cementation. The thermochemical treatments involve consecutive diffusion of boron(B) and Cr or/and V using pack powders containing diffusion element sources, activators and diluents. The top layer of Cr-boride coating is primarily consisted of $Cr_2B_3$ and $Cr_5B_3$, while that of V-boride coating is mostly consisted of $VB_2$ and $V_2B_3$. The (Cr,V)-boride coating is consisted of $Cr_2B_3$, $Cr_5B_3$ and $V_2B_3$ mostly. The top surfaces of 3 multi-component boride coatings show hardness of $3200-3400H_v$, which is much higher than that of boride, about $1600-2000H_v$. In 5 wt.% NaCl solution immersion tests, the multi-component boride coatings show much better corrosion resistance than boride coating.

Study on the Improvement of Strength for 12% Chromium Steel Rotor (12% Cr 로터강의 강도 개선에 관한 연구)

  • Jang, Yun-Seok;O, Se-Uk
    • Journal of Ocean Engineering and Technology
    • /
    • v.3 no.2
    • /
    • pp.125-137
    • /
    • 1989
  • To check technical improvement in the soundness and strength of 12% Cr steel rotor, a 25 tons of rotor with 65 tons of ingot was made in real size and was cut to pieces to take test samples, and the various mechanical tests such as impact, tensile, creep, and fatigue were carried out. The strengths are compared with those of 1% Cr-Mo-V rotor of same size. Microstructures of the samples are examined and reviewed. The results can be summarized as follows. 1) Fracture appearance transition temperatures are 80.deg. C at the center part and 60.deg. C near surface of 12% Cr rotor, and 8.deg. C near surface of 1% Cr-Mo-V rotor. 2) Comparative rapid softening occurs at higher temperatures above 600.deg. C for 12% Cr steel and 550.deg. C for 1% Cr-Mo-V steel in tension tests. 3) Fatigue crack propagation rate of 12% Cr steel is almost same as that of 1% Cr-Mo-V steel at the same corresponding surface part of the rotors. The crack growth rate of center part of 12% Cr rotor is faster than near surface part of the rotor, and the crack growth rate at the load condition of R=0.04 is slower than that of the load condition of R=0.5 for both 12% Cr steel and 1% Cr-Mo-V steel. 4) Crack growth rate of radial direction near surface of 12% Cr rotor is faster than that of transverse direction at the same part because of the difference in residual stresses. 5) Both creep and fatigue strengths of 12% Cr steel are superior to those of 1% Cr-Mo-V steel and the difference is thought the effect of climb and glide controlled creep by solid solution of alloying elements and dispersion of carbides.

  • PDF