Six-year clinical performance of lithium disilicate glass-ceramic CAD-CAM versus metal-ceramic crowns

  • Ahmed Aziz;Omar El-Mowafy
    • The Journal of Advanced Prosthodontics
    • /
    • 제15권1호
    • /
    • pp.44-54
    • /
    • 2023
  • PURPOSE. To assess the clinical performance of monolithic CAD-CAM lithium disilicate glass-ceramic (LDGC) crowns and metal-ceramic (MC) crowns provided by predoctoral students. This study also assessed the effects of patient and provider-related factors on their clinical performance as well as patient preference for these types of crowns. MATERIALS AND METHODS. Twenty-five patients who received 50 crowns (25 LDGC CAD-CAM and 25 MC) provided by predoctoral students were retrospectively examined. LDGC CAD-CAM crowns were milled in-house using the CEREC Bluecam system and cemented with either RelyX Unicem or Calibra Esthetic resin cements. MC crowns were cemented with RelyX Unicem cement. Clinical assessment of the crowns and the supporting periodontal structures were performed following the modified California Dental Association (CDA) criteria. Patients' preference was recorded using a visual analog scale (VAS). The results were statistically analyzed using log-rank test, Pearson Chi-squared test and Kaplan-Meier survival analysis. RESULTS. Twelve complications were observed in the MC crown group (9-esthetic, 2-technical and 1-biological). In comparison, 2 complications in the LDGC CAD-CAM crown group were observed (1-technical and 1-esthetic). The 6-year cumulative survival rates for MC crowns and LDGC CAD-CAM were 90.8% and 96%, respectively, whereas the success rates were 83.4% and 96%, respectively. Overall, patients preferred the esthetic outcomes of LDGC CAD-CAM crowns over MC crowns. CONCLUSION. The high survival and success rates, low number of complications, and the high level of patients' acceptance of monolithic LDGC CAD-CAM crowns lend them well as predictable and viable alternatives to the "gold standard" MC crowns.

The effects of cement thickness and cement shade on the final color of lithium disilicate crowns

  • Yigit Yamali;Merve Bankoglu Gungor;Secil Karakoca Nemli;Bilge Turhan Bal
    • The Journal of Advanced Prosthodontics
    • /
    • 제15권2호
    • /
    • pp.93-100
    • /
    • 2023
  • PURPOSE. The aim of this study is to evaluate the effect of resin cement color, cement thickness, and thermocycling on the final color of monolithic lithium disilicate crowns. MATERIALS AND METHODS. A total of ninety prepared central incisors of typodont teeth were restored with lithium disilicate crowns which have different cement thicknesses (40 ㎛, 80 ㎛, and 120 ㎛) and cement shades (clear, yellow, and white). Color parameters of restorations were measured with a spectrophotometer in three different steps 1) before cementing 2) after cementing and 3) after thermocycling with 10000 cycles. Color differences (ΔE00) were calculated with the CIEDE2000 formula and evaluated according to perceptibility (0.8) and acceptability (1.8) thresholds. The ΔE00 data were analyzed by using two-way ANOVA before and after thermocycling (α = .05). RESULTS. There was no interaction between the cement shade and the cement thickness factors. After cementation, the mean ΔE00 was under the perceptibility threshold in the group of 40 ㎛ cement thickness and clear cement while it was between the perceptibility and acceptability thresholds (0.8 < ΔE00 < 1.8) for all other groups. After thermocycling, the ΔE00 values were between the perceptibility and acceptability thresholds for all experimental groups. Although there were no significant differences among the groups, thermocycling increased the color difference values. CONCLUSION. The cementation of restorations with clear, yellow, and white resin cements resulted in color differences with uncemented restorations except for the group cemented with clear cement in 40 ㎛ cement thickness. All study groups revealed perceptible color change after thermocycling.

Doujet GF 골 시멘트를 사용한 인공 슬관절치환술의 임상적, 방사선적 고찰 (Clinical and radiologic study of total knee replacement arthroplasty using Doujet GF bone cement (liquid-powder bone cement containing gentamicin))

  • 최성욱;윤성민;노조셉;손인석
    • Journal of Medicine and Life Science
    • /
    • 제20권2호
    • /
    • pp.60-66
    • /
    • 2023
  • Gentamicin-loaded bone cement used in total joint arthroplasty is indispensable, as it provides stability by directly binding the surfaces of implants and bones. Depending on multiple factors, including the material of the bone cement used, common complications, such as aseptic loosening, osteolysis, and infection can occur postoperatively. In clinical practice, Doujet bone cement is easy to handle (pre-packed all-in-one system), and has shown low failure rates and non-inferior results compared with similar available products. We conducted a retrospective comparative study to analyze the clinical and radiological results of each bone cement group to establish the safety and usefulness of Doujet bone cement. From July 2020 to July 2022, we enrolled 198 patients in this study after an average follow-up period of 37 months (range, 6-48 months). In 99 patents, Doujet® bone cement (Injecta, Gunpo, Korea) was used for total knee arthroplasty (TKA), while Refobacin® bone cement (Biomet, Warsaw, IN, USA) was used in 99 patients. The average range of motion (ROM) of the knee increased by 2.4° (from 127.0° preoperatively to 129.4° postoperatively) in the Doujet group, and by 0.1° (from 128.7° to 128.8°) in the Refobacin group (P=0.701). The Western Ontario and McMaster Universities (WOMAC) osteoarthritis index scores decreased from 44.1 to 7.8 in the Doujet group, and from 44.2 to 6.3 in the Refobacin group (P=0.162). Complications, such as osteolysis or post-operative wound infection, did not occur in more than two cases in both groups. The WOMAC and ROM of the knee in both groups had no clinical differences. Both Doujet and Refobacin similarly showed low complication rates after TKA.

Effect of the type of resin cement on the fracture resistance of chairside CAD-CAM materials after aging

  • Laura Vitoria Rizzatto;Daniel Meneghetti;Marielle Di Domenico;Julia Cadorin Facenda;Katia Raquel Weber;Pedro Henrique Corazza;Marcia Borba
    • The Journal of Advanced Prosthodontics
    • /
    • 제15권3호
    • /
    • pp.136-144
    • /
    • 2023
  • PURPOSE. The study objective was to evaluate the influence of the type of resin cement on the flexural strength and load to fracture of two chairside CADCAM materials after aging. MATERIALS AND METHODS. A polymer-infiltrated ceramic network (PICN) and a nanoceramic resin (RNC) were used to produce the specimens. Two types of dual-cure resin cements, a self-adhesive and a universal, were investigated. Bilayer specimens were produced (n = 10) and aged for 6 months in a humid environment before the biaxial flexural strength test (σf). Bonded specimens were subjected to a mechanical aging protocol (50 N, 2 Hz, 37℃ water, 500,000 cycles) before the compressive load test (Lf). σf and Lf data were analyzed using two-way ANOVA and Tukey tests (α = .05). Chi-square test was used to analyze the relationship between failure mode and experimental group (α = .05). RESULTS. The type of resin cement and the interaction between factors had no effect on the σf and Lf of the specimens, while the type of restorative material was significant. RNC had higher σf and Lf than PICN. There was a significant association among the type of cracks identified for specimens tested in Lf and the restorative material. CONCLUSION. The type of resin cement had no effect on the flexural strength and load to fracture of the two investigated CAD-CAM chairside materials after aging.

Comparative analysis of bond strength to root dentin and compression of bioceramic cements used in regenerative endodontic procedures

  • Maykely Naara Morais Rodrigues;Kely Firmino Bruno;Ana Helena Goncalves de Alencar;Julyana Dumas Santos Silva;Patricia Correia de Siqueira;Daniel de Almeida Decurcio;Carlos Estrela
    • Restorative Dentistry and Endodontics
    • /
    • 제46권4호
    • /
    • pp.59.1-59.14
    • /
    • 2021
  • Objectives: This study compared the Biodentine, MTA Repair HP, and Bio-C Repair bioceramics in terms of bond strength to dentin, failure mode, and compression. Materials and Methods: Fifty-four slices obtained from the cervical third of 18 single-rooted human mandibular premolars were randomly distributed (n = 18). After insertion of the bioceramic materials, the push-out test was performed. The failure mode was analyzed using stereomicroscopy. Another set of cylindrically-shaped bioceramic samples (n = 10) was prepared for compressive strength testing. The normality of data distribution was analyzed using the Shapiro-Wilk test. The Kruskal-Wallis and Friedman tests were used for the push-out test data, while compressive strength was analyzed with analysis of variance and the Tukey test, considering a significance level of 0.05. Results: Biodentine presented a higher median bond strength value (14.79 MPa) than MTA Repair HP (8.84 MPa) and Bio-C Repair (3.48 MPa), with a significant difference only between Biodentine and Bio-C Repair. In the Biodentine group, the most frequent failure mode was mixed (61%), while in the MTA Repair HP and Bio-C Repair groups, it was adhesive (94% and 72%, respectively). Biodentine showed greater resistance to compression (29.59 ± 8.47 MPa) than MTA Repair HP (18.68 ± 7.40 MPa) and Bio-C Repair (19.96 ± 3.96 MPa) (p < 0.05). Conclusions: Biodentine showed greater compressive strength than MTA Repair HP and Bio-C Repair, and greater bond strength than Bio-C Repair. The most frequent failure mode of Biodentine was mixed, while that of MTA Repair HP and Bio-C Repair was adhesive.

Push-out bond strength and marginal adaptation of apical plugs with bioactive endodontic cements in simulated immature teeth

  • Maria Aparecida Barbosa de Sa;Eduardo Nunes ;Alberto Nogueira da Gama Antunes ;Manoel Brito Junior ;Martinho Campolina Rebello Horta ;Rodrigo Rodrigues Amaral;Stephen Cohen ;Frank Ferreira Silveira
    • Restorative Dentistry and Endodontics
    • /
    • 제46권4호
    • /
    • pp.53.1-53.11
    • /
    • 2021
  • Objectives: This study evaluates the bond strength and marginal adaptation of mineral trioxide aggregate (MTA) Repair HP and Biodentine used as apical plugs; MTA was used as reference material for comparison. Materials and Methods: A total of 30 single-rooted teeth with standardized, artificially created open apices were randomly divided into 3 groups (n = 10 per group), according to the material used to form 6-mm-thick apical plugs: group 1 (MTA Repair HP); group 2 (Biodentine); and group 3 (white MTA). Subsequently, the specimens were transversely sectioned to obtain 2 (cervical and apical) 2.5-mm-thick slices per root. Epoxy resin replicas were observed under a scanning electron microscope to measure the gap size at the material/dentin interface (the largest and smaller gaps were recorded for each replica). The bond strength of the investigated materials to dentin was determined using the push-out test. The variable bond strengths and gap sizes were evaluated independently at the apical and cervical root dentin slices. Data were analyzed using descriptive and analytic statistics. Results: The comparison between the groups regarding the variables' bond strengths and gap sizes showed no statistical difference (p > 0.05) except for a single difference in the smallest gap at the cervical root dentin slice, which was higher in group 3 than in group 1 (p < 0.05). Conclusions: The bond strength and marginal adaptation to root canal walls of MTA HP and Biodentine cement were comparable to white MTA.

시멘트 모르타르의 황산염침식 저항성에 대한 SO42- 이온 농도의 영향 (Influence of SO42- Ions Concentration on Sulfate Resistance of Cement Mortars)

  • 이승태
    • 대한토목학회논문집
    • /
    • 제28권5A호
    • /
    • pp.757-764
    • /
    • 2008
  • 본 연구는 농도조건을 달리한 시험용액에 침지한 모르타르의 내구성을 평가하기 위하여 수행되었다. 3종류 시멘트 모르타르를 제조한 후, ${SO_4}^{2-}$ 이온의 농도가 4225, 8450, 16900 및 33800 ppm인 4종류 황산나트륨 용액에 540일간 침지하였으며, 침지재령별 압축강도 및 선형팽창을 측정하므로써 모르타르의 황산염침식 저항성을 실험적으로 평가하였다. 실험결과에 의하면, 고농도 황산나트륨 용액에 침지한 모르타르 공시체가 가장 심한 성능저하 현상을 나타내었다. 특히, 고농도 환경에서 모르타르의 팽창 특성은 사용된 시멘트의 $C_3A$량과 직접적인 관련이 있었으며, GGBS를 대체한 SGC 모르타르는 조직구조의 투수성이 상대적으로 낮은 탓으로 인하여 시험용액의 농도조건에 관계없이 우수한 황산염침식 저항성을 나타내었다.

Influence of 10-Methacryloyloxydecyl Dihydrogen Phosphate on Cellular Senescence in Osteoblast-Like Cells

  • Ju Yeon Ban;Sang-Im Lee
    • 치위생과학회지
    • /
    • 제23권4호
    • /
    • pp.264-270
    • /
    • 2023
  • Background: Resin-based dental materials release residual monomers or other substances from incomplete polymerization into the oral cavity, thereby causing adverse biological effects on oral tissue. 10-Methacryloyloxydecyl dihydrogen phosphate (10-MDP), an acidic monomer containing dihydrogen phosphate and methacrylate groups, is the most commonly used component of resin-based dental materials, such as restorative composite resins, dentin adhesives, and resin cements. Although previous studies have reported the cytotoxicity and biocompatibility in various cultured cells, the effects of resin monomers on cellular aging have not been reported to date. Therefore, this study aimed to investigate the effects of the resin monomer 10-MDP on cellular senescence and inflamm-aging in vitro. Methods: After stimulation with 10-MDP, MC3T3-E1 osteoblast-like cells were examined for cell viability by WST-8 assay and reactive oxygen species (ROS) production by flow cytometry. The protein and mRNA levels of molecular markers of aging were determined by western blotting and RT-PCR analysis, respectively. Results: Treatment with 0.05 to 1 mM 10-MDP for 24 hours reduced the survival of MC3T3-E1 cells in a concentration-dependent manner. The intracellular ROS levels in the 10-MDP-treated experimental group were significantly higher than those in the control group. 10-MDP at a concentration of 0.1 mM increased p53, p16, and p21 protein levels. Additionally, an aging pattern was observed with blue staining due to intracellular senescence-associated beta-galactosidase activity. Treatment with 10-MDP increased the levels of tumor necrosis factor-α, interleukin (IL)-1β, IL-6 and IL-8, however their expression was decreased by mitogen-activated-protein-kinase (MAPK) inhibitors. Conclusion: Taken together, these results suggest that the exposure of osteoblast-like cells to the dental resin monomer 10-MDP, increases the level of cellular senescence and the inflammatory response is mediated by the MAPK pathway.

Effect of irrigation protocols on smear layer removal, bond strength and nanoleakage of fiber posts using a self-adhesive resin cement

  • Rodrigo Stadler Alessi;Renata Terumi Jitumori ;Bruna Fortes Bittencourt;Giovana Mongruel Gomes ;Joao Carlos Gomes
    • Restorative Dentistry and Endodontics
    • /
    • 제48권3호
    • /
    • pp.28.1-28.13
    • /
    • 2023
  • Objectives: This study aimed to investigate the effect of the application method of 2% chlorhexidine (CHX) and its influence on the adhesion of fiberglass posts cemented with a self-adhesive resin cement. Materials and Methods: Sixty human mandibular premolars were endodontically treated and divided into 5 groups (n = 12), according to the canal irrigant and its application method: 2 groups with conventional syringe irrigation (CSI)-2.5% sodium hypochlorite (NaOCl) (control) and 2% CHX- and 3 groups with 2% CHX irrigation/activation-by passive ultrasonic irrigation (PUI), Easy Clean file, and XP-Endo Finisher file. Two roots per group were evaluated for smear layer (SL) removal by scanning electron microscopy. For other roots, fiber posts were luted using a self-adhesive resin cement. The roots were sectioned into 6 slices for push-out bond strength (BS) (7/group) and nanoleakage (NL) (3/group). Data from SL removal were submitted to Kruskal-Wallis and Student-Newman-Keuls tests (α = 0.05). Data from BS and NL were evaluated by 2-way analysis of variance and Tukey's test (α = 0.05). Results: For SL removal and BS, the CHX irrigation/activation promoted better values than CSI with CHX (p < 0.05), but it was not significantly different from CSI with NaOCl (p > 0.05). For NL, the lowest values were obtained by the chlorhexidine irrigation/activation groups (p < 0.05). Conclusions: Active 2% CHX irrigation can be used to improve the post space cleaning and adhesion before fiber post cementation with self-adhesive resin cements.

반복 하중이 Full veneer crown의 유지력에 미치는 영향에 관한 연구 (THE EFFECT OF CYCLIC LOADING ON THE RETENTIVE STRENGTH OF FULL VENEER CROWNS)

  • 김기연;이선형;정헌영;양재호;허성주
    • 대한치과보철학회지
    • /
    • 제38권5호
    • /
    • pp.583-594
    • /
    • 2000
  • Dislodgement of a crown or extension bridge and the loosening of a retainer of a bridge is a serious clinical problem in fixed restoration. Generally these problems are considered to be associated with deformation of the restoration. During biting, the restoration is subjected to complex forces and deforms considerably within the limit of its elasticity. Deformation of the restoration under the occlusal force induces excessive stress in the cement film, which then leads to the cement fracture. Such a fracture may eventually cause loss of the restoration. Because most of the past retention tests for full veneer crown were done without fatigue loading, they were not exactly simulating intraoral environment. And the purpose of this study was to evaluate the effect of cyclic cantilever loading on the retentive strength of full veneer crowns depending on different type of cements and taper of prepared abutment. Steel dies with $8^{\circ}\;or\;16^{\circ}$ convergence angle were fabricated through milling and crowns with the same method. These dies and crowns were divided into 8 groups. Group 1 : $16^{\circ}$ taper die, cementation with zinc phosphate cement, without loading Group 2 : $16^{\circ}$ taper die, cementation with zinc phosphate cement, with loading Group 3 : $8^{\circ}$ taper die, cementation with zinc phosphate cement, without loading Group 4 : $8^{\circ}$ taper die, cementation with zinc phosphate cement, with loading Group 5 : $16^{\circ}$ taper die, cementation with Panavia 21, without loading Group 6 : $16^{\circ}$ taper die, cementation with Panavia 21, with loading Group 7 : $8^{\circ}$ taper die, cementation with Panavia 21 without loading Group 8 : $8^{\circ}$ taper die, cementation with Panavia 21, with loading After checking the fit of die and crown, the luting surface of dies and inner surface of crowns were air-abraded for 10 seconds. The crowns were cemented to the dies, with cements mixed according to the manufacturer's recommendations. A static load of 5kg was then applied for 10 minutes with static loading device. Twenty-four hours later, group 1, 3, 5, 7 were only thermocycled, group 2, 4, 6, 8 were subjected to cyclic loading after thermocycling. Retentive tests were performed on the Instron machine. From the finding of this study, the following conclusions were obtained 1. Panavia 21 showed significantly higher retentive strength than zinc phosphate cement for all groups (p<0.05). 2. There was a significant difference in the retentive strength between $8^{\circ}\;and\;16^{\circ}$ taper for zinc phosphate cement(p<0.05), but no significant difference for Panavia 21 (p>0.05). 3. Cyclic loading significantly decreased the retentive strength for all groups(p<0.05). 4. For zinc phosphate cement, there was 35% reduction of the retentive strength after loading in the $16^{\circ}$ taper die, 25% in the $8^{\circ}$ taper die, and for Panavia 21, 21% in the $16^{\circ}$ taper die, 18% in the $8^{\circ}$ taper die.

  • PDF