  • This research was conducted to examine the feasibility of developing fire retardant particleboard and complyboard. Particleboard were manufactured using meranti particle(Shorea spp.)made with Pallmann chipper, and complyboard meranti particle and apitong veneer (Dipterocarpus spp.). Particles were passed through 4mm (6 mesh) and retained on 1mm (25 mesh). Urea formaldehyde resin was added 10 percent on ovendry weight of particle. Face veneer for complyboard was 0.9, 1.6 and 2.3mm in thickness and spread with 36 g/(30.48 cm)$^2$ glue on one side. Veneers were soaked with 10 percent solution of five fire retardant chemicals (diammonium phosphate, ammonium sulfate, monoammonium phosphate, Pyresote and Minalith), and particles with 5, 10, 15 and 20 percent solution of five chemicals. Particleboard and complyboard were evaluated on physical and mechanical properties, and fire retardancy. The results obtained were summarized as follows. 1. Among five fire retardant chemicals treated to particleboard and complyboard, the retention of ammonium sulfate in 5 percent solution showed the lowest as 1.39 kg/(30.48 cm)$^3$ exceeding the minimum retention of 1.125 kg/(30.48 cm)$^3$ recommended by Forest Products Laboratory and Koch. 2. Particleboard and complyboard treated with diammonium phosphate showed higher modulus of rupture (MOR), modulus of elasticity (MOE), internal bond strength and screw holding power than those with the other chemicals. 3. MOR and MOE of complyboard treated with fire retardant chemicals were greater than those of fire retardant particleboard. 4. Thickness swelling of fire retardant complyboard was lower than that of fire retardant particleboard. 5. The moisture content of the boards treated with Pyresote and Minalith increased and with monoammonium phosphate reduced. 6. Fire retardant particleboard showed no ignition, and fire retardant complyboard started ignition, but time required to ignite was prolonged comparing the controlboard. Complyboard with only shell veneer treated showed ignition and lingering flame, but lingering flame time was shorter than controlboard. Complyboard with treated both core and veneer showed ignition but not lingering flame. 7. Flame length, carbonized area and weight loss were smaller than controlboard but had no significant difference among chemicals treated. 8. Temperature of unexposed surface of fire retardant particleboard was lowered with the increasing concentration of five chemicals. 9. Temperature of unexposed surface of fire retardant particleboard was lowered with the highest in Pyresote and the lowest in Minalith. 10. Temperature of unexposed surface of fire retardant complyboard was lower than that of controlboard.

  • PDF

Studies on Fire-Retardant-Treatment and Press Drying of Plywood (합판(合板)의 내화처리(耐火處理)와 열판건조(熱板乾燥)에 관(關)한 연구(硏究))

  • Lee, Phil-Woo;Kim, Jong-Man
    • Journal of the Korean Wood Science and Technology
    • /
    • v.10 no.1
    • /
    • pp.5-37
    • /
    • 1982
  • Plywood used for construction as a decorative inner material is inflammable to bring large fire accidents and burn out human life and their properties. To diminish the fire disaster, fire retardant plywood has been required indeed. In the methods of manufacturing the fire retardant plywood the soaking method is occasionally used. However after soaking plywood into fire retardant chemical solutions, redrying of soaked plywood is the most important. In this study, 3.5mm thin and 5.0mm thick plywoods were selected for fire retardant treatment. Treating solutions were prepared for 20% dilute solutions of ammonium sulfate, monoammonium phosphate, diammonium phosphate, borax-boric acid and minalith, and water solution. 1-, 3-, 6-, and 9 hour-soaking treatments were applied and after treatments hot plate drying was applied to those treated plywoods at $90^{\circ}C$, $120^{\circ}C$ and $150^{\circ}C$, of press temperature. Drying rates, drying curves, water absorption rates of fire retardant chemicals, weight per volume and fire retardant degree of plywood were investigated. The results may be summarized as follows: 1. The plywoods treated with ammonium sulfate, monoammonium phosphate and diammonium phosphate and diammonium phosphate showed increase of chemical absorption rate with proportion to increase of treating time, but not in case of the plywood treated with borax-boric acid and minalith. 2. In the treatment of definite time, the absorption rate per unit of volume of plywood showed higher in thin plywood (thickness of 3.5mm) than in thick plywood (thickness of 5.0mm). In both thin and thick plywoods, the highest absorption rate was observed in 9 hour-treatment of ammonium sulfate. The value was 1.353kg/$(30cm)^3$ in thin plywood and 1.356kg/$(30cm)^3$ in thick plywood. 3. The volume per weight of plywood after chemical treatment increased remarkably and. after hot plate drying, the values were to a little extent higher than before chemical treatment. 4. The swelling rates of thickness in chemical-treated plywoods increased similarly with that of water-treated plywood in 1- and 3 hour-treatment of both thin and thick plywoods. But in 6- and 9 hour-treatment, the greater increased value showed in water-treated ply wood than any other chemical, especially in thick plywood. 5. The shrinkage rates after hot plate drying showed the same tendency as the swelling rate, and the rate showed the increasing tendency with proportion to increase of treating time in thick plywood of both chemical and water treatments. 6. Among drying curves, the curves of water-treated plywood placed more highly than chemical-treated plywood without-relation to thickness in 6- and 9 hour-treatment except in 1- and 3 hour-treatment. 7. The drying rate related to thickness of treated plywood, was twice above in thin plywood compared with thick plywood. 8. The drying rate remarkably increased with proportion to increase of the plate temperature and, the values were respectively 1.226%/min., 6.540%/min., 25.752%/min. in hot plate temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in thin plywood and 0.550%/min., 2.490%/min, 8.187%/min, in hot plate temperature of $90^{\circ}C$, $120^{\circ}C$, $150^{\circ}C$ in thick plywood. 9. In the treatment at $120^{\circ}C$ of hot plate temperature, the drying rates of chemical-treated plywood showed the highest value in monoammonium phosphate of thin plywood and in diammonium phosphate of thick plywood. But the drying rate of water-treated plywood was highest in 6- and 9 hour-treatment. 10. The fire retardant degree of chemical-treated plywood was higher than that of the untreated plywood as shown in loss of weight, burning time, flame-exhausted time and carbonized area. 11. The fire-retardant effect among fire retardant chemicals were the greatest in diammonium phosphate, the next were in monoammonium phosphate and ammonium sulfate, and the weakest were in borax-boric and minalith.