Design and Output Characteristic of AC Pulse Current for MIG Welding of Ai Sheet (박판 Al MIG 용접용 AC펄스 전류 파형의 설계 및 출력특성)

  • 조상명;김태진;이창주;임성룡;공현상;김기정
    • Journal of Welding and Joining
    • /
    • v.21 no.2
    • /
    • pp.57-63
    • /
    • 2003
  • Since new types of vehicles or structures made from thin aluminum alloy are under rapid development and some products are already on the market, welding of aluminium sheet is increasing. MIG(Metal Inert Gas), MIG-Pulse, TIG(Tungsten Inert Gas) welding are the typical Ai welding. MIG welding has the advantage of high speed, but it is difficult to apply to the thin plate, because of bum-through by the high heat input and spatter. MIG-Pulse welding can weld without spatter and burn-through, but when the gap exists at the welding joint, there is quite a possibility of bum-through. TIG welding is difficult to weld at a high speed. AC Pulse welding alternates between DCEP(Direct Current Electrode Positive) and DCEN(Direct Current Electrode Negative). DCEN is higher wire melting rate than DCEP, while lower temperature of droplet than DCEP. In AC Pulse welding, far fixed welding current, wire melting rate increases as the EN ratio increases. For fixed wire feed rate, welding current decreases as the EN ratio increases. Because of these features, the temperature of droplet, the depth of penetration, the width of bead decrease and the reinforcement height increases as EN ratio increases, and these are able to weld at a high speed, lower heat input. It is the purpose of this study that design of AC pulse current waveform for MIG welding of Al sheet and estimation of output characteristic.

Effect of Short Circuit Time Ratio and Current Control Pattern on Spatter Generation in $CO_2$ Welding ($CO_2$용접의 스패터 발생에 미치는 단락시간비 및 단락전류 파형제어의 영향)

  • 조상명
    • Journal of Welding and Joining
    • /
    • v.21 no.1
    • /
    • pp.48-53
    • /
    • 2003
  • The object of this study is to examine the effect of short circuit time ratio (SCTR) and current rise delay time (Td) on the spatter generation at low and medium current range in $CO_2$ welding. The spatter was evaluated by the weight generated in the welding of bead-on-plate for 30 seconds (3 times). Td was varied by order of 0, 0.4, 0.8 and 1.2 msec. At each Td, the short circuit time ratio was varied by the output voltage of the welding power source. In the low current range, it was found that the optimum SCTR was 20~25%, and the minimum spatter generation weight was obtained in the case of Td=0.4msec and SCTR=22% even though the remarkable difference was not showed by the application of Td. In the medium current range, it was confirmed that the arc was stable though the SCTR was increased from 20% to 40% by the control of current wave. Spatter generation weight depended on the variation of Td, and the lowest value of spatter generation weight occurred at Td=0.8~1.2msec.

Study on the Process Parameters for Laser Welding of Coaxial Circular Pipe Inner Flange (동축 파이프 이음부의 레이저용접 공정변수에 관한 연구)

  • Kim, Yong;Park, Ki-Young;Lee, Kyoung-Don
    • Laser Solutions
    • /
    • v.12 no.3
    • /
    • pp.14-17
    • /
    • 2009
  • The laser welding was performed for the flange joint of two overlapped coaxial circular pipes which serve as the inlet and connector pipes of STS 316L. The laser welding test finally resulted in a good penetration depth of 1.8 to 2.0 mm. On the way to get the good welding quality, two important parameters were found to be optimized. One is the focal positioning which is the offset of the laser beam focus to the exact welding seam line, which is more critical in the inner flange laser welding. When the beam spot size was deviated more than $200\;{\mu}m$ from the seam line, welding of two pipes is failed. The other is a gap size since a certain amount of gap is inevitable due to fabrication tolerance, or artificial allowances for smooth insertion of a pipe. However, it is required to restrict the gap allowance within 0.2mm to avoid undesirable undercut on a welding bead.

  • PDF

Dissimilar Metal Welding Characteristics for Medium Carbon Steel and Stainless Steel Using a Nd:YAG Laser (중탄소강과 스테인리스강의 Nd:YAG 레이저 이종용접에서 용접특성)

  • You, Young-Tae;Lee, Hyun-Jung;Kim, Jin-Woo
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.25 no.1
    • /
    • pp.68-74
    • /
    • 2016
  • The Nd:YAG laser welding process is one of the most advanced manufacturing technologies owing to its high speed and penetration, and has increased the automation and flexibility of an entire industry. Laser welding of dissimilar metals has been widely used to improve the wear resistance and corrosion resistance of industrial parts. The objective of this research is to investigate the influence of process parameters on the welding of SM45C and STS304 with CW Nd:YAG lasers. Bead-on-plate welding tests were carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the dissimilar welding, the welding quality of the cut section, strain-stress behavior, and hardness of the welded part were investigated.

The Development of Welding Process to Prevent Porosity in MIG Welding of Al 6082-T6 (Al 6082-T6 MIG 용접에서 기공방지를 위한 용접공정 개발)

  • Baek, Sang-Yeub;Jung, Yon-Ho;Kim, Won-Il;Cho, Sang-Myung
    • Journal of Welding and Joining
    • /
    • v.28 no.6
    • /
    • pp.28-34
    • /
    • 2010
  • This paper was described on investigation to prevent porosity in high speed MIG Welding of Al 6082-T6. Porosity measurement was carried out by using image analysis of micrographs with the help of an analysis software. The main parameter was arc length and torch progressive angle. The porosity ratio was increased as arc length was increased. The arc length was increased depending upon the output voltage. By proper selection of pulse waveform parameter, the stable arc of one pulse one drop was generated. The porosity ratio of optimum condition in one pulse one drop was lower than high voltage condition. When torch progressive angle was an angle of advance $10^{\circ}$, porosity ratio was minium.

A Study on the Metal Transfer and Spatter Generation in High Current $CO_2$ Welding (고전류 $CO_2$용접에서의 금속이행 및 스패터 발생 현상에 관한 연구)

  • 김남훈;유회수;김희진;고진현
    • Journal of Welding and Joining
    • /
    • v.21 no.3
    • /
    • pp.51-57
    • /
    • 2003
  • The metal transfer in $CO_2$ welding shows the transition of transfer mode from short-circuiting to repelled transfer will the increase of welding current. While the short-circuiting mode in $CO_2$ welding has been studied very extensively relating with droplet formation and spatter generation, the repelled transfer has little been understood. In this study, high current $CO_2$ welding has been performed with bead-on-plate welds along with the waveform analyzer and high speed camera. The image of high speed camera was synchronized with its waveform so that the moment of spatter generation could be realized during drop detachment. As a results of this study, it was found that welding arc changes its location either once or three times and thus single or double pulse signals were developed in the voltage waveform. Whenever the arc moved its location, new arc was developed in a explosive way and thus it caused spatter generation. Specially severe spattering took place when the waveform showed a double-peak pattern. As a consequence of these results, new waveform control techniques could be suggested for suppressing the spatter generation in the high-current $CO_2$ welding.

Welding Characteristics of Cold Rolled Carbon Steel utilize CW Nd:YAG Laser (CW Nd:YAG 레이저를 이용한 냉연강판의 용접특성)

  • Shin B.H.;Yoo Y.T.;Shin H.J.;Ahn D.G.
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2006.05a
    • /
    • pp.17-18
    • /
    • 2006
  • Laser welding of metals has been widely used to improve a wear resistance and a corrosion resistance of the industrial parts. The objective of this research works is to investigate the influence of the process parameters, such as the welding for metals with CW Nd:YAG lasers. The bead-on-plate welding tests are carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the butt welding, the welding quality of the cut section, stain-stress behavior and the hardness of the welded part are investigated. From the results of the investigation, it has been shown that the optimal welding condition without defects in the vicinity of the welded area and with a good welding quality is 1400W of the laser power, 0.8m/min, 0.9m/min of welding speed and $4{\ell}$ in of pressure for shielding gas.

  • PDF

Dissimilar Metal Welding of Medium Carbon Steel and Austenitic Stainless Steel utilize CW Nd:YAG Laser (CW Nd:YAG 레이저를 이용한 중탄소강과 오스테나이트계 스테인레스강의 이종금속 용접)

  • Shin Ho-Jun;Ahn Dong-Gu;Im Kie-Gon;Shin Byung-Heon;Yoo Young-Tae
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.23 no.3 s.180
    • /
    • pp.47-55
    • /
    • 2006
  • Laser welding of dissimilar metals has been widely used to improve a wear resistance and a corrosion resistance of the industrial parts. The objective of this research is to investigate the influence of the process parameters, such as the welding for SM45C and STS304 with CW Nd:YAG lasers. The bead-on-plate welding tests are carried out for several combinations of the experimental conditions. In order to quantitatively examine the characteristics of the dissimilar welding, the welding quality of the cut section, stress-strain behavior and the hardness of the welded metal are investigated. From the results of the investigation, it has been shown that the optimal voiding condition without defects in the vicinity of the welded area and with a good welding quality is 1600W of the laser power, 0.85m/min of welding speed and $4{\ell}/min$ of pressure for shielding gas.

A Study on the Distortion Control Characteristics of the STS 304 Multi-pass Butt Weldment by Tensioning Method (인장하중법에 따른 STS 304 다층 맞대기 용접부의 변형 제어 특성에 관한 연구)

  • Kim, Ha-Geun;Lee, Dong-Ju;Shin, Sang-Beom
    • Journal of Welding and Joining
    • /
    • v.28 no.3
    • /
    • pp.73-78
    • /
    • 2010
  • The purpose of this study is to develop the control technology of the welding distortion caused by Auto NG-GTA(Narrow Gap-GTA) welding process at the STS 304 multi-pass butt weldment. Heat input model for Auto NG-GTA welding process was established and verified by measuring temperature change and molten pool shape at the bead-on-plate weldment. With the heat input model developed, the effect of tension load on the welding distortion at the STS 304 multi-pass butt weldment was evaluated using the thermo-elasto-plastic FE analysis. In accordance with FEA results, the angular distortion and transverse shrinkage sharply decreased with an increase in tension load. This result indicated that tensioning method was an effective countermeasure against the welding distortion of the STS 304 multi-pass butt weldment.

A Study on a Development of the Grinding Robot to Remove Welding-bid of Working Pieces (취부용 피스(piece)제거 및 사상 작업 자동화장비 개발에 관한 연구)

  • Noh, Hyo-Won;Kim, Ki-Jung;Leem, Rae-Soo;Kim, Ho-Kyoung
    • Special Issue of the Society of Naval Architects of Korea
    • /
    • 2008.09a
    • /
    • pp.136-143
    • /
    • 2008
  • This paper presents the application of a robot which aims at grinding automatically welding-bead remained in the removal job of working pieces for shipbuilding. In specific, the investigation on this application is composed of two parts; one topic is on the development of a robot platform vertically movable on a steel plate of hull, while the other topic is of the development of a grinding tool mechanism in order to remove welding-beads by using a diamond wheel installed on a servo cylinder (which can result in high working pressure on the grinding wheel). Besides, the development of a vision system for tracking welding-beads as well as recognizing welding surfaces is added for the convenience of this robot application to the removal of welding-beads remained in the working pieces for shipbuilding.

  • PDF