• Title/Summary/Keyword: auto-hydrolysis

Search Result 7, Processing Time 0.021 seconds

Development of Auto-hydrolysis Method for Preparing Cotton Linter Regenerated Fibers of Textile Fabrics (방직용 재생펄프 제조를 위한 면 린터의 자기가수분해 공정 개발)

  • Sohn, Ha Neul;Park, Hee Jung;Seo, Yung Bum
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.47 no.6
    • /
    • pp.81-88
    • /
    • 2015
  • The molecular weight (MW) and crystallinity of cotton linter need to be controlled to be dissolved well in N-methylmorpholine N-oxide (NMMO) solvent for manufacturing regenerated fibers of clothing fabrics. Electron beam irradiation or sulfuric acid pre-treatment followed by alkaline peroxide bleaching has been used to control MW effectively and to improve brightness of cotton linter. Auto-hydrolysis of cotton linter without electron beam irradiation or chemical pre-treatment was found to be effective as an alternative pre-treatment method. Removal of metal ions, that hampered dissolution of cotton linter by NMMO, was also investigated when the auto-hydrolysis was accompanied with ionic polymers and chelating agent.

Auto-hydrolysis of Lignocellulosics Under Extremely Low Sulphuric Acid and High Temperature Conditions in Batch Reactor

  • Tunde Victio Ojumu;Ba aku Emmanuel AttahDaniel;Eriola Betiku;Bamidele Ogbe Solomon
    • Biotechnology and Bioprocess Engineering:BBE
    • /
    • v.8 no.5
    • /
    • pp.291-293
    • /
    • 2003
  • Batch reactors were employed to investigate the kinetics of cellulose hydrolysis under extremely low acid (ELA) and high temperature condition. The sawdust was pretreated by Auto-hydrolysis prior to the batch reaction. The maximum yield of glucose obtained from the batch reactor experiment was about 70% for the pretreated sawdust, this occurred at 210 and 22$0^{\circ}C$. The maximum glucose yield from the untreated sawdust was much lower at these temperatures, about 55%. The maximum yields of glucose from the lignocellulosics were obtained between 15th and 20th minutes after which gradual decrease was observed.

Kinetics and Mechanism for Alkaline Hydrolysis of C. I. Disperse Blue 79 (C. I. Disperse Blue 79의 알칼리 가수분해 반응속도 및 반응메카니즘)

  • 박건용;박창혁;박병기
    • Textile Coloration and Finishing
    • /
    • v.13 no.5
    • /
    • pp.312-319
    • /
    • 2001
  • Kinetics and mechanism for alkaline hydrolysis of C. I. Disperse Blue 79(B-79) which is 4-N, N- diacetoxyethyl -2- acylamino-5-ethos y -2'-bromo-4',6'-dinitroazobenzene were investigated. The color strength of B-79 in acetone/water solutions of various NaOH concentrations decreased continuously. The hydrolysis rate of B-79 increased with increasing alkali concentration and appeared following first order reaction. The observed rate constants for various concentrations of B-79 showed similar values, and B-79 was hydrolyzed by first order reaction for dye concentration. Therefore, it was confirmed that the overall reaction follow second order kinetics and proceed via $S_N2$ reaction. From the study on kinetics and spectrometric analysis, it was proposed that the rate determining step of the hydrolysis reaction of B-79 is the nucleophilic substitution reaction - that is the reaction of the rapid attack of OH- on the carbon atom, which is in acceptor ring, adjacent to auto group to break the C-N bond. And it was also found that the final hydrolysis products of B-79 include both the acceptor ring in the form of sodium salt and the donor ring possessing 4-N,N-dihydroxyethyl group converted from 4-N, N-diacetoxyethyl group.

  • PDF

Studies on the antitumor components of Korean Basidiomycetes $(IV)^*$ Antitumor Components of Namatoloma Fasciculare (Fr.) Karst.

  • Lee, Chong-Ock;Choi, Eung-Chil;Kim, Byong-Kak
    • Archives of Pharmacal Research
    • /
    • v.4 no.2
    • /
    • pp.117-122
    • /
    • 1981
  • The carpophores of a mushroom, Naematoloma fasciculare (Fr.) Karst, were extracted with 0.2 N NaOH and the extract was dialyzed through visking tube. It was found to contain an antitumor activity against sarcoma 180 implanted in mice. The components of this aqueous extract were found to be a polysaccharide and a protein by color reactions including Anthrone and Lowery-Folin tests. The hydrolysis of the polysaccharide with 3% HCL-Me-OH and trimethylsily lation of the hydrolysate yielded five monosaccharides, i. e. glucose, frutose, mannose, galactose and xylose, which were detected and analyzed by GLC. After hydrolysis of the protein with 6N HCl, 15 amino acids, including aspartic acid and glutamic acid, were detected and analyzed by an auto amino acid analyzer.

  • PDF

Effect of Delignification Treatment after Autohydrolysis on Yields of Cellulosic Substrates, Lignin Contents, and Enzymatic Hydrolysis (목분(木粉)의 Autohydrolysis후(後) 탈리그닌처리(處理)가 섬유소기질(纖維素基質)의 수율(收率), 리그닌함량(含量)과 효소가수분해(酵素加水分解)에 미치는 영향(影響))

  • Park, Jong-Moon;Ahn, Won-Yung;Shin, Dong-So
    • Journal of the Korean Wood Science and Technology
    • /
    • v.12 no.4
    • /
    • pp.19-30
    • /
    • 1984
  • This experiment was carried out to investigate the effects of autohydrolysis and extraction conditions on the separation of the chemical substances, the extractability of lignin by dioxane, and the yield of reducing sugars from cellulosic substrates by using a commercial cellulase derived from Trichoderma viride. Air-dried wood meals through 0.42mm (40 mesh) screen and retained on 0.25 mm (60 mesh) of Populus alba-glandulosa and Pinus koraiensis were autohydrolyzed with water at $180^{\circ}C$ for 30 and/or 60 minutes in a 6 liter stainless-steel digester with or without 2% 2-naphthol. The hydrothermally-treated wood meals were extracted the lignin with 100%, 90%, 75% and 50% dioxane solutions at $70^{\circ}C$ for 4 hours, respectively. The results obtained were as follows; 1) After autohydrolysis of Populus alba-glandulosa, the yield of wood meals decreased with lengthening the auto hydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. In case of Pinus koraiensis, the yield was not affected by 2%, 2-naphthol addition at the autohydrolysis in the digester. 2) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the yield of wood meals decreased with lengthening the autohydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. Extraction of 50% dioxane solution was the best solvent for the yield among the solutions of 100%, 90%. 75% and 50% dioxane. In case of Pinus koraiensis, the yield was not affected by 2% 2-naphthol addition and the solution of 90% dioxane was the poorest solvent for the yield. 3) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the Klason lignin content in cellulosic substrates for enzymatic hydrolysis decreased with lengthening the autohydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. Klason lignin content was the lowest after extraction by 90% or 75% dioxane solution. The content was also affected by interaction of the three factors-autohydrolysis time, 2% 2-naphthol addition and concentration of dioxane. In case of Pinus koraiensis, the Klason lignin content increased with 2% 2-naphthol addition but was not affected by the concentration of dioxane solution. 4) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the extractable Klason lignin content by extraction increased with lengthening the auto hydrolysis time from 30 minutes to 60 minutes and with 2% 2-naphthol addition. The extractable lignin content was the highest after extraction by 90% or 75% dioxane solution. In case of Pinus koraiensis, the extractable lignin content increased with 2% 2-naphthol addition. Extractions by 100%, 90% and 50% dioxane solutions were more effective for the extraction of Klason lignin than by 75% dioxane solution. 5) After autohydrolysis and lignin extraction of Populus alba-glandulosa, the yield of reducing sugars increased with lengthening the autohydrolysis time from 30 minutes to 60 minutes but was not affected by 2% 2-naphthol addition and the concentration of dioxane. The yield of reducing sugars after enzymatic hydrolysis was slightly higher by extractions with 90%, 75% and 50% dioxane solutions than with 100% dioxane. In case of Pinus koraiensis, the yield of reducing sugars was not affected by 2% 2-naphthol addition but affected by the concentration of dioxane. The yield of reducing sugars was the highest in cellulosic substrates extracted by 100% dioxane solution.

  • PDF

Effect of Deodorizing Temperature on Physicochemical Characteristics in Corn Oil IV. Effect of Deodorizing Temperature on Volatile Flavor Component Composition in Corn Oil (탈취온도가 옥수수기름의 이화학적 특성에 미치는 영향 제4보, 탈취온도가 옥수수기름의 휘발성 냄새성분 변화에 미치는 영향)

  • 이근보;한명규;이미숙
    • The Korean Journal of Food And Nutrition
    • /
    • v.11 no.3
    • /
    • pp.272-277
    • /
    • 1998
  • We carried out separation and guantitation of flavor components by GC about essential oils extracted from deodorized corn oil at the different deodorizing temperature. Flavor components were detected total 16 kinds included aldehydes of 8 kinds, major components were propane, pentane, hexanal etc. These major components content was about 70~75% of the total flavor components. According to rise of deodorizing temperature, both ethane and aldehydes of 8 kinds content were in proportion to increase, but propane, pentane, hexane, octan, pentyl furan content were decreased by contraries, respectively. On the other hand, total flavor component content was appeared the lowest level at 245$^{\circ}C$ treating group, aldehydes content was in proportion to increase according to rise of deodorizing temperature. These phenomenons consider that the undesirable reactions such as partial auto-oxidation, degradation, polymerization and hydrolysis etc. by effecting factors of stripping steam and vacuum degree. Conclusively, deodorizing temperature under high temperature was undesirable for the minimization of off-flavor materials.

  • PDF

AN IN-VITRO WEAR STUDY OF INDIRECT COMPOSITE RESINS AGAINST HUMAN ENAMEL (법랑질에 의한 수종의 간접복합레진의 마모에 관한 연구)

  • Yi, Hyun-Jeong;Jeon, Young-Chan;Jeong, Chang-Mo;Jeong, Hee-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.5
    • /
    • pp.611-620
    • /
    • 2007
  • Statement of problem: Second-generation indirect composite resins have been improved flexural strength, compressive strength, hydrolytic degradation resistance, wear resistance compared to first-generation indirect composite resins, but there are still some problems as hydrolysis and low wear resistance. Some manufacturers claim that wear resistance of their materials has been improved, but little independent study has been published on wear properties of these materials and the properties specified in the advertising materials are largely derived from in-house or contracted testing. Purpose: This study was to evaluate the wear of indirect composite resins (SR Adore, Sinfony, Tescera ATL) and gold alloy against the human enamel. Material and method: Extracted human incisors and premolars were sectioned to $2{\times}2{\times}2mm$ cube and embedded in the clear resin and formed conical shaped antagonist to fit the jig of pin-on-disk tribometer. Total 20 antagonists were stored in distilled water. Five disk samples, 24mm in diameter and 1.5mm thick, were made for each of three groups of indirect composite resins and gold alloy group, and polished to #2,000 SiC paper on auto-polishing machine. Disk specimens were tested for wear against enamel antagonists. Wear test were conducted in distilled water using a pin-on-disk tribometer under condition (sliding speed 200rpm contact load 24N, sliding distance 160m). The wear of the enamel was determined by weighing the enamel antagonist before and after test, and the weight was converted to volumes by average density. The wear tracks were analyzed by scanning electron microscopy and surface profilometer to elucidate the wear mechanisms. Statistical analysis of the enamel wear volume, wear track depth and wear tract width of disk specimens were accomplished with one-way ANOVA and the means were compared for significant differences with Scheffe's test. Results: 1. The enamel wear was most in gold alloy, but there were no statistically significant differences among all the groups (P>.05). 2. In indirect composite resin groups, the group to make the most shallow depth of wear tract was Sinfony, followed by Tescera ATL, SR Adoro (P<.05). Gold alloy was shallower than Sinfony, but there was no statistically significant difference between Sinfony and gold alloy (P>.05). 3. The width of wear tract of SR Adore was larger than the other groups (P<.05), and there were no statistically significant differences among the other groups (P>.05). 4. SEM analysis revealed that Sinfony and gold alloy showed less wear scars after test, Tescera ATL showed more wear scars and SR Adore showed the most. Conclusion: Within the limits of this study, Sinfony and gold alloy showed the least wear rates and showed similar wear patterns.