Experimental study on vacuum preloading with flocculation for solid-liquid separation in waste slurry

  • Wu, Yajun;Kong, Gangqiang;Lu, Yitian;Sun, De'an
    • Geomechanics and Engineering
    • /
    • v.13 no.2
    • /
    • pp.319-331
    • /
    • 2017
  • This vacuum preloading combined with polyacrylamide (PAM) flocculation was proposed to separating solid-liquid in waste slurry and to improving bearing capacity of soft soil ground. By using waste slurry taken from drilled shaft construction site in Shanghai, China, a series of settling column tests with four typical flocculants and one normal for waste slurry were carried out for comparative analysis. The optimal amounts for each flocculant were obtained from the column tests. Then, model tests on vacuum preloading with anionic polyacrylamide (APAM) flocculation and without flocculants were carried out. The out of water and the settlement of slurry surface ground were monitored during the model tests, and the changes in water content, particle-size and pore-size distributions in different positions after the model tests were measured and discussed. It is found that water content of the waste slurry without APAM flocculation changed from 204 to 195% by 24 hours standing and 15 hours vacuum preloading, while the water content of the waste slurry with APAM flocculation was declined from 163 to 96% by 24 hours standing, and was further reduced into 37% by 136 hours vacuum preloading, which shows that the combined method is feasible and effective.

Effect of Shear Condition on Washless Polyelectrolytes Multilayering Treatment on GCC (전단 조건이 중질탄산칼슘의 무세척 고분자전해질 다층흡착 처리에 미치는 영향)

  • Lee, Jegon;Sim, Kyujeong;Lee, Hak Lae;Youn, Hye Jung
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.46 no.5
    • /
    • pp.51-60
    • /
    • 2014
  • To find a practical application approach of polyelectrolyte multilayering (PEM) on inorganic filler, we introduced PEM process without washing step and investigated the effect of shear condition on the washless PEM treatment of ground calcium carbonate (GCC). Washless multilayering on GCC was conducted under various shear conditions such as stirring, homogenization, and ultrasonication. Highly charged polyelectrolytes combination of polydiallyldimethylammonium chloride (PDADMAC) and poly sodium 4-styrene sulfonate (PSS) and low charged polyelectrolytes combination with cationic starch and anionic polyacrylamide (PAM) were compared. In the case of highly charged polyelectrolytes combination, shear conditions did not affect the zeta potential and the particle size of treated GCC. However, the modified GCC particles with low charged polyelectrolytes were more dispersed under higher shear condition while maintaining the zeta potential. In addition, GCC was successfully modified through laboratory inline washless polyelectrolyte multilayering system which consists of homogenizers and pumps.

Retention Performance of Nanocoated GCC with Positive Charge (양이온성으로 표면 개질된 nanocoated GCC의 보류 성능)

  • Lee, Jegon;Sim, Kyujeong;Lee, Hak Lae;Youn, Hye Jung
    • Journal of Korea Technical Association of The Pulp and Paper Industry
    • /
    • v.45 no.5
    • /
    • pp.14-22
    • /
    • 2013
  • In this study, we investigated retention characteristics of nanocoated GCC that was positively modified by Layer-by-Layer (LbL) multilayering process. Three layers were formed onto GCC particles with poly-DADMAC/PSS/poly-DADMAC (PD3) and C-starch/A-PAM/C-starch (CS3) systems, respectively. Untreated GCC, PD3 GCC (strongly positive charge) and CS3 GCC (weekly positive charge) were retained on pulp fibers under single retention system or microparticle retention system conditions. In single retention system, PD3 particles were not affected by cationic retention aid due to their strong positive charge, whereas CS3 particles reacted with cationic retention aid due to anionic sites on the surface of the weekly positive particles. In a microparticle retention system, positively modified GCC (PD3 and CS3) showed higher retention level than untreated GCC at the same dosage of retention aid. The cationic surface of GCC particles were more reacted with bentonite so the deposition onto pulp fibers was improved. In addition, the retention level of nanocoated GCC was increased with maintaining good formation.

Hydrophilization of hydrophobic membrane surfaces for the enhancement of water flux via adsorption of water-soluble polymers

  • Kim, Ka Young;Rhim, Ji Won
    • Membrane and Water Treatment
    • /
    • v.7 no.2
    • /
    • pp.101-113
    • /
    • 2016
  • In this study, to improve the water flux of porous hydrophobic membranes, various water-soluble polymers including neutral, cationic and anionic polymers were adsorbed using 'salting-out' method. The adsorbed hydrophobic membrane surfaces were characterized mainly via the measurements of contact angles and scanning electron microscopy (SEM) images. To enhance the durability of the modified membranes, the water-soluble polymers such poly(vinyl alcohol) (PVA) were crosslinked with glutaraldehyde (GA) and found to be resistant for more than 2 months in vigorously stirred water. The water flux was much more increased when the ionic polymers used as the coating materials rather than the neutral polymer and in this case, about 70% of $0.31L/m^2{\cdot}h$ (LMH) to 0.50 LMH was increased when 300 mg/L of polyacrylamide (PAAm) was used as the coating agents. Among the cationic coating polymers such as poly(styrene sulfonic acid-co-maleic acid) (PSSA_MA), poly(acrylic acid-comaleic acid) (PAM) and poly(acrylic acid) (PAA), PSSA_MA was found to be the best in terms of contact angle and water flux. In the case of PSSA_MA, the water flux was enhanced about 80%. The low concentration of the coating solution was better to hydrophilize while the high concentration inclined to block the pores on the membrane surfaces. The best coating condition was found: (1) coating concentration 150 to 300 mg/L, (2) ionic strength 0.15, (3) coating time 20 min.