• 제목/요약/키워드: amorphous alloys

검색결과 256건 처리시간 0.028초

압출공정을 이용한 Cu 계 비정질 합금의 미세조직제어 (Microstructure Control of Cu base amorphous Alloys by Extrusion)

  • 김택수;이진규
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.236-240
    • /
    • 2007
  • In order to control the microstructure of amorphous/crystalline composites, gas atomized $Cu_{54}Ni_{6}Zr_{22}Ti_{18}$ metallic glass powders wrapped in a crystalline brass were extruded repeatedly. The size of microstructure in the resultant composites was varied depending on the pass of extrusion as well as on the area reduction ratio. The microstructure could be estimated using an equation of $r_n=r_{n-1}/R^{1/2}$, where R is reduction ratio and $r_n$ is the resultant radius of the extruded bar after n pass. Theory of microstructural refinement as well as the relationship between the resultant microstructures and mechanical properties was discussed.

  • PDF

인체에 유해하지 않은 원소를 사용한 Ti 계 벌크 비정질 합금 개발 (Development of Ti-based Bulk Metallic Glasses with Non-toxic Elements)

  • 이철규;이승훈
    • 한국주조공학회지
    • /
    • 제32권4호
    • /
    • pp.177-180
    • /
    • 2012
  • Ti-based bulk metallic glasses with high glass forming ability were developed through a systematic alloy design technique. The main alloy design strategy was the selection of alloying elements that may not be toxic in the human body. The $Ti_{45.0}Cu_{40.1}Zr_{12.7}Si_{2.2}$ alloy could be cast into an amorphous rod with the diameter of 3 mm by a suction casting technique using Cu mold. The compressive strength of the amorphous rod was measured as 1826 MPa. Since the Ti-based amorphous alloys consist of non-toxic elements, they can be widely used as bio-materials and eco-materials with unique and beneficial properties.

철계비정질합금의 고주파 자기특성 연구 (A Study on the Magnetic Properties of Fe-base Amorphous Alloys in High Frequency)

  • 송재성;김기욱;정순종
    • 대한전기학회논문지
    • /
    • 제41권4호
    • /
    • pp.379-384
    • /
    • 1992
  • The Fe-base amorphous ribbons with 15mm width and about 20x10S0-6Tm thickness, (FeS179-xTCrS1xT)BS116TSiS15T and (FeS181-xTMnS1xT) BS112TSiS17T (x:0-6), were prepared melt spinner. The thickness of the ribbons followed by PFC (Planar Flow Casting). The initial permeability and total core losses were measured as a function of additive elements (Cr, Mn) and annealing conditions in high frequency for the purpose of using these materials as a core of magnetic amplifier and switched mode power supplies. The initial permeabilities were enhanced and core losses were decreased by non-magnetic field annealing in proper conditions. The lowest core loss in 0.2T/10kHz was measured at 3% Cr addition amorphous ribbon, and the loss was 5.6W/kg. The permeability of the ribbon at 10kHz was about 9000.

$Fe_{80}B_{12}Si_8$ 비정질 합금의 자구 및 자왜와 자기적 성질에 미치는 Mo 첨가와 자장 열처리 효과 (The effect of Mo addion and Magnetic field annealing on the magnetic properties, Magnetostriction and Domain structures of $Fe_{80}B_{12}Si_8$ amorphous alloy.)

  • 고창진;강계명;송진태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1989년도 춘계학술대회 논문집
    • /
    • pp.49-51
    • /
    • 1989
  • The effect of Mo elenent and annealing condition on the magnetic properties were investigated in Fe$_{80}$B$_{12}$Si$_{8}$ amorphous alloy. With increasing Mo contents, soft magnetic properties were improved by decreasing coercive force and increasing maximum permeability. These improvements were attributed to the decreasing of magnetostriction by Mo addition. The annealing treatment also improved the soft magnetic properties of (Fe$_{1-x}$ Mo$_{x}$)$_{80}$ B$_{12}$ Si$_{8}$ amorphous alloys. It could be thought that these improvements were ascribed to the relaxation of internal stress.nal stress.ess.

  • PDF

고강도 Fe계 합금의 고온 변형 특성 (High Temperature Deformation Behavior of Fe-base High Strength Alloys)

  • 권운현;최일동
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제32권6호
    • /
    • pp.938-946
    • /
    • 2008
  • Fe-base amorphous alloy and two crystalline phases composite were fabricated. The effect of temperature and strain rate on mechanical properties was evaluated utilizing compression test. Mixture of non-crystalline and crystalline phases were found using X-ray diffraction (XRD) and differential thermal analysis (DTA) tests. Based on glass transition temperature and crystallization temperature. compression tests were performed in the temperature ranging from $560^{\circ}C$ to $700^{\circ}C$ with $20^{\circ}C$ interval. Relationship between microstructure, including fracture surface morphology, and mechanical behavior was studied. The peak stress of Fe-base amorphous alloy was over 2GPa and expected to have a good wear resistance, but it is expected hard to deform because of low ductility. The peak stress and elongation of two crystalline phases composite was over 1GPa and about 20%, therefore it is possible to deform high strength wear resistant materials such as engine valve.

Fe-계 비정질 합금의 절연 코팅이 자기적 성질에 미치는 영향 (Influence of Insulated Coatings on The Magnetic Properties of Fe-Based Amorphous Alloy)

  • 김현식;오영우;김병걸;전순종;김기욱;민복기;송재성
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1994년도 하계학술대회 논문집 C
    • /
    • pp.1311-1313
    • /
    • 1994
  • The development of an insulated coating which can be used for amorphous alloys is extremely important from the practical point of view. This importance may be enhanced by the influence of the coating on the magnetic properties. The aim of the study is to show how some coating influence the magnetic properties of $Fe_{87}Zr_7B_5Ag_1(at%)$ amorphous alloy.

  • PDF

다른 하중속도 조건에서 압입에 의한 벌크 금속유리의 변형거동 (Deformation Behavior of Zr-based Bulk Metallic Glass by Indentation under Different Loading Rate Conditions)

  • 신형섭;장순남
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.42-47
    • /
    • 2004
  • Metallic glasses are amorphous meta-stable solids and are now being processed in bulk form suitable for structural applications including impact. Bulk metallic glasses have many unique mechanical properties such as high yield strength and fracture toughness, good corrosion and wear resistance that distinguish them from crystalline metals and alloys. However, only a few studies could be found mentioning the dynamic response and damage of metallic glasses under impact or shock loading. In this study, we employed a small explosive detonator for the dynamic indentation on a Zr-based bulk amorphous metal in order to evaluate the damage behavior of bulk amorphous metal under impact loading. These results were compared with those of spherical indentation under quasi-static and impact loading. The interface bonded specimens were adopted to observe the appearances of subsurface damage induced during indentation under different loading conditions.

  • PDF

비정질 Fe-Co-Re-B(RE=Nd, Sm, Gd, Tb) 합금의 자기적 성질 (A Study on the Magnetic Properties of Amorphous Fe-Co-RE-B (RE=Nd, Sm, Gd, Tb) Alloys)

  • 김경섭;유성초;김창식;김종오
    • 한국자기학회지
    • /
    • 제1권2호
    • /
    • pp.55-59
    • /
    • 1991
  • 희토류-3d 천이원소인 비정질${[{(Fe_{80}CO_{20})}_{0.98}RE_{0.02}]}_{80}B_{20}(RE=Nd,\;Sm,\;Gd,\;Tb)$ 합금 리본시료에 대한 자기적 성질을 조사하기 위하여 시료진동형 자력계(vibrating sample magnetometor)를 이용하여 77 K부터 900 K까지의 온도 영역에서 포화자화 값을 온도의 함수로 측정 한후, Curie 온도 ($T_{c}$)와 Bloch 상수등을 추정하였다. 이들로 부터 spin wave stiffness 상수, 교환상호작용(exchange interaction)의 범위와 평균자승거리($$)등을 계산하였으며 각 희토류 원소에 대한 치환효과를 비교 분석하였다.

  • PDF