The microstructural evolution during mechanical alloying of elemental Fe and Si powders, average composition $Fe_{30}Si_{70}$ and $Fe_{50}Si_{50}$, has been investigated by X-ray diffraction (XRD), Scanning electron microscopy (SEM) and Differential scanning calorimetry (DSC). Mechanical alloying was performed by using a SPEX 8000 Mixer/Mill under argon atmosphere with/without hexane as a process control agent (PCA). In the presence of PCA, the milling process was dominated by fracture resulting in the decrease in particle size to about $1{\mu}m$. The structural development with milling time depended on the average composition of starting powders. The mixture of $Fe_{50}Si_{50}$ and $Fe_{30}Si_{70}$ resulted in the formation of FeSi(${\varepsilon}$ - phase) and $FeSi_2$(${\beta}$ - phase), respectively. In the case of $Fe_{33.3}Si_{66.7}$, a mixture and $FeSi_2({\beta})$ was formed. These results were discussed by considering the thermodynamics and kinetics concerning the milling process.
In order to investigate the formation of AlN, mechanical alloying was carried out in $N_2$ and $NH_3$ atmosphere. Differential thermal analysis (DTA), x-ray diffraction (XRD) and chemical analysis were carried out to examine the formation behavior of aluminum nitrides. No diffraction pattern of AlN was observed in XRD analysis of the as-milled powders in $NH_3\;or\;N_2$ atmosphere. However, DTA and chemical analysis indicated that the precursors for AlN were formed in the Al powders milled in $NH_3$ atmosphere. The AlN precursors transformed to AlN after heat treatment at and above $600^{\circ}C$. It was considered that the reaction between Al and $NH_3$ was possible by the formation of fresh Al surface during mechanical alloying of Al powders.
Ferritic stainless steel is currently increasingly used for automotive exhaust material. The material for exhaust manifold is used in the temperature range of 500∼$850^{\circ}C$. Therefore, high temperature characteristic is an important one that affects it's life span. It has been investigated the effect of alloying elements of Cr, Mo, Nb, Ti in the ferritic stainless steel for exhaust manifold on the high temperature tensile strength. There was a few difference in the tensile strength at $600^{\circ}C$ with the exception of low Cr steel, but the steels containing higher Cr, Mo or Nb elements showed significantly higher tensile strength at the temperature of $800^{\circ}C$. The precipitates of the specimens after heat treating at the test temperature were electrolytic extracted, and quantitatively analysed using by SEM-EDS and TEM. The alloying elements of Cr and Mo increased the tensile strength as a solid solution strengthener, and on the other hand Nb element enhanced the strength by forming the fine intermetallic compounds such as NbC or $Fe_2Nb$.
Surface alloying of Ti alloy by $CO_2$ laser is able to produce few hundred micrometers thick TiN or TiC surface-alloyed layer with high hardness on the substrate by injecting reaction gas($N_2$ or $CH_4$). Laser surface alloying by means of process control is in many applications essential in order to obtain predictable hardening layer. This research has been investigated the effect of such parameters on TiN and TiC gas alloying of Ti-6Al-4V alloy by $CO_2$ laser. The maximum surface hardness of TiN layer was obtained 1750Hv on the conditions of 0.8kW laser power, 0.8m/min scanning speed and 100% $N_2$ atmosphere. However, the maximum hardness of TiC formation layer after laser treatment was about 630Hv. As scanning speed was increased, the hardness and depth of these layers were decreased at constant laser power.
Intermetallic compound NbAl₃and amorphous phases were synthesized by mechanical alloying of elemental powder mixtures of niobium and aluminum. The composition of the powder mixtures was Nb-45wt%Al(75at%Al). The mechanical alloying was performed with a high energy SPEX 8000 mixer/mill up to 72 hrs. The resulting powders were analyzed by XRD, DTA, SEM and TEM. The mechanically alloyed powders exhibited lamellar structures in the early stage. And the elements of Nb and Al were homogeneously distributed over the Powder when a steady state was reached. An intermetallic compound, NbAl₃, was formed by mechanical alloying for 4 hrs. The mechanically alloyed powders exhibited a large exotherm around 600℃, corresponding to formation of stable NbAl₃and stress relief.
Austempered Ductile Iron (ADI) castings having various chemical composition and heat treatment conditions were investigated. Especially, this study was investigated the influence of various parameters on austempering temperature and alloying elements. The addition of Mo, Cu, and Ni individually or combined in these alloys also investigated. The alloying elements influence the austempering reaction, the microstructures, mechanical properties and amount of retained austenite. In this study, the mechanical properties (ultimate tensile strength(UTS), hardness, elongation) are analysed to show the relationship between alloying elements, austempering temperatures and amount of retained austenite. The amount of retained austenite was the range of 15 - 40%. In case of the alloy to witch Mo, Cu, and Ni was added, the amount of retained austenite was the largest at a constant austempering temperature.
Mechanical alloying under various gas atmospheres such as Ar, an Ar-$H_2$ mixture, and He gases were carried out, and its effects on the powder properties, microstructure and mechanical properties of ODS ferritic steels were investigated. Hot isostatic pressing and hot rolling processes were employed to consolidate the ODS steel plates. While the mechanical alloyed powder in He had a high oxygen concentration, a milling in Ar showed fine particle diameters with comparably low oxygen concentration. The microstructural observation revealed that low oxygen concentration contributed to the formation of fine grains and homogeneous oxide particle distribution by the Y-Ti-O complex oxides. A milling in Ar was sufficient to lower the oxygen concentration, and this led a high tensile strength and fracture elongation at a high temperature. It is concluded that the mechanical alloying atmosphere affects oxygen concentration as well as powder particle properties. This leads to a homogeneous grain and oxide particle distribution with excellent creep strength at high temperature.
We investigated the effects of the chemical composition and the relative density on the plastic deformation behavior of sintered Fe-based alloys by means of compressive tests. Overall compressive stresses increased as the amount of alloying elements and the relative density were respectively increased. Addition of alloying elements except for Mo increased the yield stress regardless of the relative density. The relationship between the effects of the chemical composition and the relative density and the mean rate of the stress increase was analyzed. A constitutive equation based on the Ludwik equation with the regressed parameters was proposed to predict the compressive true stress-true strain curves of the sintered Fe-based alloys. The K and n values used in the proposed equation were regressed as a function of the alloying elements and the relative density based on the individual K and n values. The plastic deformation behavior predicted using the proposed constitutive equation showed reliable accuracy compared with experimental data.
Recently, it has been found that mechanical alloying (MA) facilitates the nanocomposites formation of metal-metal oxide systems through solid-state reduction during ball milling. In this work, we studied the MA effect of Fe$_{3}$O$_{4}$-M (M = Al, Ti) systems, where pure metals are used as reducing agents. It is found that composite powders in which $Al_{2}$O$_{3}$ and TiO$_{2}$ are dispersed in $\alpha$-Fe matrix with nano-sized grains are obtained by mechanical alloying of Fe$_{3}$O$_{4}$ with Al and Ti for 25 and 75 hours, respectively. It is suggested that the large negative heat associated with the chemical reduction of magnetite by aluminum is responsible for the shorter MA time for composite powder formation in Fe$_{3}$O$_{4}$-Al system. X-ray diffraction results show that the reduction of magnetite by Al and Ti if a relatively simple reaction, involving one intermediate phase of FeAl$_{2}$O$_{4}$ or Fe$_{3}$Ti$_{3}$O$_{10}$. The average grain size of $\alpha$-Fe in Fe-TiO$_{2}$ composite powders is in the range of 30 nm. From magnetic measurement, we can also obtain indirect information about the details of the solid-state reduction process during MA.
Kim, Sug-Won;Kim, Dong-Keon;Lee, Eui-Kwoon;Jang, Ho-Yeal
Journal of Korea Foundry Society
/
v.12
no.6
/
pp.450-457
/
1992
The study aims to investigate the influence of alloying elements(V,Ti) and heat treatment on the mechanical properties in hypo-eutectic chromium cast iron. Before heat treatment, all of the specimen were fully annealed(950$^{\circ}C{\times}5Hr$) to homogenize their structures. The influence of heat treatment and alloying elements(V,Ti) on hardness, retained austenite volume, and charpy impact energy as well as tensile strength of the specimen was tested systematically. Retained austenite decreased with the increase of V and Ti, but incresed with the increase of number of cycles. The impact energy decreased, and hardness and tensile strength increased with the increase of alloying elements (V,Ti) and the decrease of the number of cycles. The hardness and tensile strength increased, but impact energy decreased with the increase of V and Ti elements and the temperature of destabillization heat treatment. After the destabillization heat treatment at the same temperature, the impact energy is increased, while hardness and tensile strength decreased as the increase of tempering temperature. Retained austenite increased with increase of destabilizatoin heat treatment temperature, while decrease with the increase of tempering temperature.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.