• 제목/요약/키워드: alloy powder

검색결과 1,082건 처리시간 0.021초

Hot Deformation Behavior and Microstructural Evolution of Powder Metallurgy Ti-6Al-4V Alloy (티타늄 합금 분말 소결체의 고온 변형 거동 및 미세조직 연구)

  • Kim, Youngmoo;Song, Young-Beom;Lee, Sung Ho;Kwon, Young-Sam
    • Journal of Powder Materials
    • /
    • 제21권4호
    • /
    • pp.277-285
    • /
    • 2014
  • The effects of processing parameters on the flow behavior and microstructures were investigated in hot compression of powder metallurgy (P/M) Ti-6Al-4V alloy. The alloy was fabricated by a blended elemental (B/E) approach and it exhibited lamellar ${\alpha}+{\beta}$ microstructure. The hot compression tests were performed in the range of temperature $800-1000^{\circ}C$ with $50^{\circ}C$ intervals, strain rate $10^{-4}-10s^{-1}$, and strain up to 0.5. At $800-950^{\circ}C$, continuous flow softening after a peak stress was observed with strain rates lower than $0.1s^{-1}$. At strain rates higher than $1s^{-1}$, rapid drop in flow stress with strain hardening or broad oscillations was recorded. The processing map of P/M Ti-6Al-4V was designed based on the compression test and revealed the peak efficiency at $850^{\circ}C$ and $0.001s^{-1}$. As the processing temperature increased, the volume fraction of ${\beta}$ phase was increased. In addition, below $950^{\circ}C$, the globularization of phase at the slower strain rate and kinking microstructures were found. Based on these data, the preferred working condition of the alloy may be in the range of $850-950^{\circ}C$ and strain rate of $0.001-0.01s^{-1}$.

The Effect of Excess Samarium Oxide on the Preparation of Sm-Fe Alloy Powder by Reduction-diffusion Method (환원-확산법에 의한 Sm-Fe 합금분말 제조시 Sm2O3 첨가량의 영향)

  • Kwak, Hun;Lee, Jung-Goo;Choi, Chul-Jin
    • Journal of Powder Materials
    • /
    • 제16권5호
    • /
    • pp.336-341
    • /
    • 2009
  • To produce alloy powders with only Sm$_2$Fe$_{17}$ single phase by reduction-diffusion (R-D) method, the effect of excess samarium oxide on the preparation of Sm-Fe alloy powder during R-D heat treatment was studied. The quantity of samarium oxide was varied from 5% to 50% whereas iron and calcium were taken 0% and 200% in excess of chemical equivalent, respectively. The pellet type mixture of samarium, iron powders and calcium granulars was subjected to heat treatment at 1100$^{\circ}C$ for 5 hours. The R-D treated pellet was moved into deionized water and agitated to separate Sm-Fe alloy powders. After washing them in deionized water several times, the powders were washed with acetic acid to remove the undesired reaction products such as CaO. By these washing and acid cleaning treatment, only 0.03 wt% calcium remained in Sm-Fe alloy powders. It was also confirmed that the content of unreacted $\alpha$-Fe in Sm$_2$Fe$_{17}$ matrix gradually decreased as the percentage of samarium oxide is increased. However, there was no significant change above 40% excess samarium oxide.

Variation of Lattice Constant in Ni-W and Ni-W-Cu Alloys for YBCO Coated Conductor (YBCO 초전도 박막 선재용 Ni-W 및 Ni-W-Cu 합금의 격자상수 변화)

  • Kim Min-Woo;Jung Kyu-Dong;Jun Byung-Hyuk;Kim Hyoung-Seop;Kim Chan-Joong
    • Progress in Superconductivity
    • /
    • 제7권1호
    • /
    • pp.64-68
    • /
    • 2005
  • We fabricated Ni-based alloy substrates for YBCO coated conductor using powder metallurgy. Tungsten and copper were selected as alloy elements due to their mutual solubility to the base element of nickel. The alloying elements were mixed with nickel using ball milling and dried in air. The powder mixtures were packed in a rubber mold, cold isostatic pressed 200 MPa and made into rods. The compacted rods were sintered at $1150^{\circ}C$ for 6 hours for densification. It was confirmed by neutron diffraction experiment that W and Cu atoms made complete solid solution with Ni. Lattice constant of nickel alloy increased by $0.004{\AA}$ for 1at. $\%$ W in Ni-W alloy, $0.0006{\AA}$ for 1 at. $\%$ Cu in Ni-W-Cu alloy.

  • PDF

Effect of Process-Control Agents on Characteristics of Amorphous Al-Y-Ni-Co Alloy Powder Produced by Mechanical Alloying

  • Nguyen, H.V.;Kim, J.C.;Kim, J.S.;Kwon, Y.J.;Kwon, Y.S.
    • Journal of Powder Materials
    • /
    • 제17권1호
    • /
    • pp.7-12
    • /
    • 2010
  • In this work, effect of various process-control agents (PCAs) on the mechanical alloying of amorphous alloy of $Al_{85}Y_8Ni_5Co_2$ has been investigated. The dependence of the particle shape, size and crystallization behavior of the amorphous alloy powders on the type of PCAs and their concentrations was investigated by using X-ray diffraction, field-emission scanning electron microscopy and differential scanning calorimetry. It was found that the additive of toluene could affect positively the amorphization and thermally induced crystallization processes, as well as the size refinement, morphology and particle-size distribution of as-milled powders in comparison with alloy obtained without PCA.

The Effects of the Amount of $\textrm{SiO}_2$ Dopant on the Melt Oxidation Behavior of the Al-Alloy (Al-합금의 용융산화거동에 미치는 $\textrm{SiO}_2$도판트 량의 영향)

  • Gang, Jeong-Yun;Kim, Il-Su
    • Korean Journal of Materials Research
    • /
    • 제9권6호
    • /
    • pp.609-614
    • /
    • 1999
  • The effect of the amount of $SiO_2$dopant on the behavior of $AlO_2$$O_3$-composite formation by melt oxdation of Al-alloy was examined in this paper. The $SiO_2$powder was spread on the top surface of the Al-1Mg-3-Si-5Zn-1Cu alloy in th alumina crucible. The selected amount of each powder was 0.03, 0.10, 0.16g/$\textrm{cm}^2$. The oxidation behavior was determined by observing the weight gain after the heat treatment for 10 hours at 1373K. The macroscopic structure of formed oxide layer was examined by an optical microscope. The top surface and the cross-section of the grown oxide layer were investigated by SEM and analysed by EDX. The $SiO_2$ powder was determined to enhance oxidation by thermit reaction with Al which reduced the growth incubation period of the oxidation layer. As the amount of the $SiO_2$dopant increased, the growth rate decreased due to the precipitated Si which blocked the Al-alloy channel in the composite materials. However, more uniform layer was obtained due to the occurrance of the enhanced oxidation reaction in the whole alloy surface compared to the case of addition of less amount of dopant.

  • PDF

Fabrication and Tensile Properties of Alloy 617 base ODS Alloy (Alloy 617계 산화물 분산강화(ODS) 합금의 제조와 인장특성)

  • Min, Hyoung-Kee;Kang, Suk-Hoon;Kim, Tae-Kyu;Han, Chang-Hee;Kim, Do-Hyang;Jang, Jin-Sung
    • Journal of Powder Materials
    • /
    • 제18권6호
    • /
    • pp.482-487
    • /
    • 2011
  • Alloy 617, Ni-22Cr-12Co-9Mo base oxide dispersion strengthened alloy was fabricated by using mechanical alloying, hot isostatic pressing and hot rolling. Uniaxial tensile tests were performed at room temperature and at $700^{\circ}C$. Compared with the conventional Alloy 617, ODS alloy showed much higher yield strength and tensile strength, but lower elongation. Fracture surfaces of the tensile tested specimens were investigated in order to find out the mechanism of fracture mode at each test temperature. Grain adjustment during tensile deformation was analyzed by electron backscattered diffraction mapping, inverse pole figures and TEM observation.

Development of Tungsten Heavy Alloy with Hybrid Structure for Kinetic Energy Penetrator

  • Baek, Woon-Hyung;Kim, Eun-Pyo;Song, Heung-Sub;Hong, Moon-Hee;Lee, Seong;Kim, Young-Moo;Lee, Sung-Ho;Noh, Joon-Woong;Ryu, Joo-Ha
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.944-945
    • /
    • 2006
  • A new tungsten heavy alloy with hybrid structure was manufactured for the kinetic energy penetrator. The tungsten heavy alloy is composed of two parts: core region is molybdenum added heavy alloy to promote the self-sharpening; outer part encompassing the core is conventional heavy alloy to sustain severe load in a muzzle during firing. From ballistic test, it was found that the penetration performance of the hybrid structure tungsten heavy alloy is higher than that of conventional heavy alloy. This heavy alloy is thought to be very useful for the penetrator in the near future.

  • PDF

HVOF Spray Coating of Co-alloy(T800) for the Improvement of durability of High Speed Spindle (초고속 회전체의 내구성향상을 위한 Co-alloy(T800)의 초고속 용사코팅)

  • Cho, Tong-Yul;Yoon, Jae-Hong;Kim, Kil-Su;Youn, Suk-Jo;Back, Nam-Ki;Park, Byung-Chul;Chun, Hui-Gon
    • Transactions of the Korean Society of Machine Tool Engineers
    • /
    • 제15권6호
    • /
    • pp.32-37
    • /
    • 2006
  • Micron size Co-alloy(T800) powder was coated on Inconel 718 by HVOF thermal spraying for the studies of the improvement of durability of high speed spindle by using Taguchi program for the parameters of spray distance, flow rates of hydrogen and oxygen and powder feed rate. The optimal coating process was determined by the studies of coating properties such as micro-structure, porosity, surface roughness and micro hardness. Friction and wear behaviors of coatings were investigated by sliding wear test at room temperature and $1000^{\circ}F(538^{\circ}C)$. At both room temperature and $538^{\circ}C$ the sliding wear debris and friction coefficients of the coating were drastically reduced compared with the surface of non-coated parent material. This shows that Co-alloy powder coating is highly recommendable for the durability improvement surface coating of high speed air-bearing spindle. At high temperature wear traces and friction coefficients of both coating and non-coating were drastically reduced compared with those of room temperature since the brittle oxides were formed easily on the surface, and the brittle oxide phases were attrited by the reciprocating sliding wear according to the complicated mixed wear mechanisms These oxide particles, partially melts and the melts play role as lubricant and reduce the wear and friction coefficient. This also shows that Co-alloy powder coating is highly recommendable far the durability improvement surface coating on the surface vulnerable to frictional heat such as high speed spindles.

The Effect of Mn Addition on Nitrogenation Behavior and Magnetic Properties of Sm-Fe Alloy Powder Produced by Reduction-diffusion Method (환원-확산법에 의해 제조된 Sm-Fe 합금분말의 질화거동 및 자기특성에 미치는 Mn첨가 효과)

  • Seo, Young-Taek;Baek, Youn-Kyoung;Lee, Jung-Goo;Choi, Chul-Jin
    • Journal of Powder Materials
    • /
    • 제20권1호
    • /
    • pp.13-18
    • /
    • 2013
  • In the present study, we systematically investigated the effect of Mn addition on nitrogenation behavior and magnetic properties of Sm-Fe powders produced by reduction-diffusion process. Alloy powders with only $Sm_2(Fe,Mn)_{17}$ single phase were successfully produced by the reduction-diffusion process. The coercivity of $Sm_2(Fe,Mn)_{17}$ powder rapidly increased during nitrogenation and reached the maximum of 637 Oe after 16 hours. After further nitrogenation, it decreased. In contrast, the coercivity of $Sm_2Fe_{17}$ powder gradually increased during nitrogenation for 24 hours. The coercivity of $Sm_2(Fe,Mn)_{17}$ powder was higher than that of $Sm_2Fe_{17}$ powder at the same condition of nitrogenation. It was considered that the Mn addition facilitates the nitrogenation of $Sm_2Fe_{17}$ powder and enhances the coercivity.

Microstructure and Mechanical Properties of Rapidly Solidified Powder Metallurgy Al-Fe-V-Si-X Alloys

  • Genkawa, Takuya;Yamasaki, Michiaki;Kawamura, Yoshihito
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1041-1042
    • /
    • 2006
  • High heat-resistant Al-Fe-V-Si and Al-Fe-V-Si-X rapidly solidified powder metallurgy (RS P/M) alloys have been developed under well-controlled high purity argon gas atmosphere. The $Al_{90.49}Fe_{6.45}V_{0.68}Si_{2.38}$ (at. %) RS P/M alloy exhibited high elevated-temperature strength exceeding 300 MPa and good ductility with elongation of 6 % at 573 K. Reduction of $H_2O$ partical pressure in P/M processing atmosphere led to improvement in mechanical properties of the powder-consolidated alloys under elevated-temperature service conditions. Ti addition to the Al-Fe-V-Si conduced to enhancement of the strength at room temperature. The tensile yeild strength and ultimate strenght were 545 MPa and 722 MPa, respectively.

  • PDF