A New Proposal for the Allowable Local Thickness of Straight Pipes in ASME Code Case N-597-2 (ASME 코드 케이스 N-597-2의 직관 국부허용두께의 새로운 제안)

  • Park, Jai-Hak;Shin, Kyu-In;Park, Chi-Yong;Lee, Sung-Ho
    • Journal of the Korean Society of Safety
    • /
    • v.22 no.1 s.79
    • /
    • pp.13-18
    • /
    • 2007
  • Structural integrity assessment of thin-walled pipes and pipe items has become one of the major issues in the nuclear power plant. ASME Section XI Code Case N-597-2 provides a criterion for acceptance of the pipes. But the code case has several limitations for application and sometimes gives too conservative or non-conservative results. So it is necessary to understand fully the technical bases of the code case. In the code case N-597, the allowable local thicknesses of thinned straight pipes are given for three different cases. Because of the different technical base, each case gives different thickness values and sometimes gives contradictory values. In this paper attempts were made in order to propose a unified rule for the allowable local thickness and in order to remove or relax the restrictions on the application of the code case. For this purpose elastic stress analyses were made using the finite element method and the stress results were examined. Based on the obtained bending stress results, a very simple procedure was proposed to obtain the consistent allowable local thickness for the thinned straight pipes.

Evaluation of Local Allowable Wall Thickness of Thinned Pipe Subjected to Internal Pressure and Bending Moment (내압과 굽힘하중하에서 감육배관의 국부허용두께 평가)

  • Kim, Jin-Won;Park, Chi-Yong;Kim, Beom-Nyeon
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.25 no.1
    • /
    • pp.81-88
    • /
    • 2001
  • This study proposed an analytical method to evaluate a local allowable wall thickness (LAWT) for locally thinned pipe subjected to internal pressure and bending moment. In this method, the stresses in the thinned region were calculated by finite element analysis and plastic collapse was applied as a failure criterion of thinned pipe. Using this method, LAWT for a simplified thinned pipe was evaluated with variation in axial extent of thinned area, and it was compared with allowable wall thickness provided by previous pipe wall thickness criteria. The results showed that the LAWT was lower, about 50%, than that calculated by construction code or ASME Code N-597, and it was higher, about 2 times, than that estimated by evaluation model based on pipe experiments. In addition, LAWT was decreased with increasing axial extent of thinned area and saturated with further increase in axial extent. And, the variation in LAWT with axial extent of thinned area depended on type of load, especially a magnitude of bending moment, considering in the evaluation.

A Study on the Structural Behavior and the Strength of Circular Hollow Steel(CHS) Section Columns (원형강관 기둥의 구조적인 거동 및 강도에 관한 연구)

  • Kang, Doo Won;Kwon, Young Bong
    • Journal of Korean Society of Steel Construction
    • /
    • v.21 no.5
    • /
    • pp.505-514
    • /
    • 2009
  • This paper describes the structural behavior and the ultimate strengths of circular hollow steel (CHS) sections based on a series of compression tests. The ultimate strengths of CHS section columns are mainly dependent on both diameter-thickness ratio and column slenderness ratio. For the CHS sections with a high diameter-thickness ratio, an elastic or an inelastic local buckling may occur prior to the overall buckling, and it may decrease the column strength. Test sections were fabricated from SM400 steel plate of 2.8 mm and 3.2 mm in thickness and were tested to failure. The diameter-thickness ratios of the test sections ranged from 45 to 170 to investigate the effect of local buckling on the column strength. The compression tests indicated that the CHS sections of lower diameter-thickness ratio than the yield limit in the current design specifications showed an inelastic local buckling and a significant post-buckling strength in the local mode. Their ultimate stresses were larger than the nominal yield stress. It was known that the allowable stresses of the sections predicted by the Korean Highway Bridge Design Specifications (2005) were too conservative in comparison with test results. The Direct Strength Method which was newly developed was calibrated for application to the CHS sections by the experimental and numerical results. The Direct Strength Method proposed can predict properly the ultimate strength of CHS section columns whether a local buckling and an overall buckling occur nearly simultaneously or not.

A Study on the Characteristics of SM570TMC Plates in Compression Members (SM570TMC 강재의 압축재 특성에 관한 연구)

  • Im, Sung Woo;Kim, Yo Suk;Chang, In Hwa
    • Journal of Korean Society of Steel Construction
    • /
    • v.17 no.3 s.76
    • /
    • pp.357-363
    • /
    • 2005
  • There is a great need for high-strength steel especially for the high-rise steel building structure. High-strength steels, however, may have mechanical properties that are significantly different from those of the conventional steels. The application of high-strength steels to building structures should be reviewed as to whether the inelastic behavior equivalent to that of conventional steels can be attained or not. In this study, SM570TMC steel was tested to evaluate buckling strength under axial compressive force. The comparison tests for local buckling strength evaluation of box-type and H-shaped welded columns were performed with variable width-thickness ratios. As for the experimental check, the maximum strength of stub column was determined by local buckling as far as the limit of width-to-thickness ratio was satisfied with current design codes. Also, the strength of the stub column did not decrease suddenly by local buckling before maximum strength even when the ratio is not satisfied. The buckling strength of SM570TMC steel was higher than both ASD (Allowable Stress Design) and LRFD (Load and Resistance Factor Design) specifications.

An Experimental Study on Failure Behavior of TP316 Stainless Steel Pipe with Local Wall Thinning and Cracking (국부 감육과 균열이 발생한 TP316 스테인리스강 배관의 파괴거동에 관한 실험적 연구)

  • Cheung, Jin Hwan;Kim, In Tae;Choi, Seock Jin;Choi, Hyung Suk;Kim, Hee Sung
    • Journal of Korean Society of Steel Construction
    • /
    • v.24 no.6
    • /
    • pp.647-657
    • /
    • 2012
  • Although nuclear power plant piping system is designed conforming to design specifications, the piping systems are deteriorated with increase in service life. In this study, monotonic and cyclic loading tests were carried out on TP316 stainless steel pipe specimens, and the effect of local wall thinning and cracking on failure behavior was investigated. In the tests, 0%, 35% and 75% wall thinning and cracking of initial thickness were artificially introduced to inside elbow and straight pipe specimens, and internal pressures of 20MPa were applied to simulate real operation condition. From the test results, the effect of local wall thinning and cracking on failure mode, ultimate load, number of cycle and strain energy was presented, and maximum bending moment was compared with allowable bending moment calculated by ASME code.

Technical Application and Analysis for Reduction of Water Loss in Water Distribution Systems (상수도 관망의 유수율 제고 기술의 적용 및 분석)

  • Kim, Ju-Hwan;Lee, Doo-Jin;Bae, Cheol-Ho;Woo, Hyung-Min
    • Proceedings of the Korea Water Resources Association Conference
    • /
    • 2009.05a
    • /
    • pp.260-266
    • /
    • 2009
  • Non-revenue water reduction(NRW) technologies are implemented to evaluate and manage leakages scientifically in water distribution systems under local governments. A development of quantitative leakage indicator by measuring minimum night flow, pressure control policy by installation of PRV(pressure reducing valve) and the establishment of leakage prevention schemes by residual life modeling of deteriorated water pipes are reviewed and studied. Estimation models of allowable leakage are developed by measuring and analyzing minimum night flow at residential and commercial area in Nonsan city, which is suggested from UK water industry and can improve an existing leakage indicator for the evaluation of non-revenue water. Also, pressure control method is applied and analyzed to Uti distribution area in Sacheon city in the operation aspect. As results, $466\;m^3/day$ of leakage can be reduced and it is expected that 113million won of annual cost can be saved. In the part of corrosion velocity and residual life assessment, non-linear prediction models of residual thickness are proposed by assessment of corrosion velocity based on exposure years, soil and water quality etc., since the deteriorated water pipe play a major role to increase leakage. It is expected that collection data and analyzing results can be applied effectively and positively to reduce non-revenue water by accumulating surveying data and verifying the results in the business field of water distribution systems under local governments.