STS 304, 316강의 열처리에 따른 산화거동 (An Oxidation Behavior with Heat-treatment in STS 304 and 316)

  • 이경구;윤동주;기회봉;강창석;이도재
    • 열처리공학회지
    • /
    • 제11권3호
    • /
    • pp.186-191
    • /
    • 1998
  • An oxidation behavior of 304 and 316 stainless steels were studied in dry air. After solution treatment, specimens were polished up to $1{\mu}m$ $A1_2O_3$ grade and then subjected to oxidation treatment in dry air at $800^{\circ}C{\sim}1200^{\circ}C$. The oxidation behavior between matrix and oxide scale was analyzed with SEM, EDS and XRD. When oxidation treatment was conducted at $1200^{\circ}C$, large thickness of Fe oxide scale was formed on top of surface and fine $(Cr,Fe)_2O_3$ oxide film was formed below it. Cr rich zone existed at interface between metal and $(Cr,Fe)_2O_3$ oxide layer, and it was believed that this zone acted as obstacle to oxidation. Most of Ni was detected at the interface between metal and $(Cr,Fe)_2O_3$ and also detected at the interface between $Fe_2O_3$ and $(Cr,Fe)_2O_3$.

  • PDF

Study on Oxidation Behavior of (W,Mo)$Si_2$ Powders in Air at 400, 500 and $600^{\circ}C$

  • Peizhong, Feng;Xuanhui, Qu;Xiaohong, Wang;Farid, Akhtar
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1149-1150
    • /
    • 2006
  • The oxidation of (W,Mo)$Si_2$ powders has been investigated at 400, 500 and $600^{\circ}C$ for 12.0 hours in air. It was shown that the low temperature oxidation resistance of (W,Mo)$Si_2$ was worse than that of $MoSi_2$, and they showed great changes in mass, volume and colour. Especialy at $500^{\circ}C$, the amount of volume expansion of (W,Mo)$Si_2$ was as high as about $7\sim8$ times and color changed from black to yellow after 4.0h with $MoO_3$, $WO_3$, (W,Mo)$O_3$ and amorphous $SiO_2$ as main reaction products. The mass gain and oxidation rate were relatively slower at $400^{\circ}C$ and $600^{\circ}C$ than that at $500^{\circ}C$.

  • PDF

촉매 습식산화에 의한 반응성 염료 분해(2) (Decomposition of Reactive Dyes by Catalytic Wet Air Oxidation Process(2))

  • 최장승;우성훈;박승조
    • 대한환경공학회지
    • /
    • 제22권11호
    • /
    • pp.2077-2083
    • /
    • 2000
  • 산업 현장에서 많이 사용되고 있는 반응성 염료인 remazol $black_5$를 연구 대상물로 선택하여 촉매습식 산화공법으로 처리하였다. 이때 반응성 염료성분의 분해효율, 촉매 첨가량 및 반응온도와 상호 관련하여 검토한 결과를 정리하였다. 이산화티탄 담체에 백금을 5.0wt% 담지한 촉매 1.5g/L, 6기압, $200^{\circ}C$ 이상에서 remazol $black_5$는 약 95% 이상 분해되었다. 반응온도 $250^{\circ}C$에서 240분 촉매산화를 하였을 때 uv 흡광 잔존율은 4%이고 반응온도가 $250^{\circ}C$, 120분 경과 후 색도 제거율은 약 95% 이상이었다.

  • PDF

Nitrocarburising 처리된 탄소강의 내식특성에 미치는 Post Oxidation 효과 (The Effect of Post Oxidation on Corrosion Characteristics of Gas Nitrocarburised Carbon Steels)

  • 김영희;정광효
    • 열처리공학회지
    • /
    • 제12권1호
    • /
    • pp.9-20
    • /
    • 1999
  • The effect of post oxidation, water-quenched after holding in air for 5~420 seconds or cooling or furnace cooling, on corrosion resistance and phase formation characteristics of the surface layer of SM20C and SM45C carbon steels after gas nirtrocarbursing in the $NH_3-5%CO_2-N_2$ gas atmosphere at $580^{\circ}C$ for 3hours is studied. The compound layers of two steels consist of ${\varepsilon}-Fe_{2-3}N$, ${\gamma}^{\prime}-Fe_4N$ and $Fe_3O_4$, phases, however, the quantity of ${\gamma}^{\prime}-Fe_4N$ phase increases for the furnace cooled specimen compared to that of air cooling specimen. With increasing $NH_3$ content in the gas mixture and also increasing the keeping time in the air after gas nitrocarburising, the ${\varepsilon}-Fe_{2-3}N$ phase of compound layer increases, while the decreased current density recognizing the improvement of corrosion resistance are shown. the passive current density of SM45C steel is lower than that of SM20C steel at the same nitrocarburising conditions.

  • PDF

대기 중 휘발성 유기화합물의 광산화 공정 및 광촉매산화 공정의 처리효율 비교 (A Study on the Photolytic and Photocatalytic Oxidation of VOCs in Air)

  • 서정민;정창훈;최금찬
    • 한국대기환경학회지
    • /
    • 제18권2호
    • /
    • pp.139-148
    • /
    • 2002
  • Both UV Photolysis and Phtocatalytic Oxidation Processing are an emerging technology for the abatemant of Volatile Organic Compounds (VOCs) in atmospheric -pressure air streams. However, each process has some drawbacks of their own. The former is little known as an application for air pollution treatment, so it has been a rare choice in the field. Therefore we have to do more experiment and study for its application for treatment of VOCs. Although the latter has been used in the industrial fields, it still has a difficulty in decomposing high concentrations of VOCs. To solute these problems, we have been studying simultaneous application of those two technologies. We have studied the effects of background gas composition and gas temperature on the decomposition chemistry. It has shown that concentration of TCE and B.T.X., diameter of reactor, and wavelength of lamp have effects on decomposition efficiency. When using Photolysis Process only, the rates of fractional conversion of each material are found at TCE 79%, Benzene 65%, Toluene 68%, Xylene 76%. In case of Photocatalytic Oxidation Process only, the rates of fractional conversion decreased drastically above 30 ppm. When there two methods were combined, the rates of fractional conversion of each material are enhanced such as TCE 93%, Benzene 75%, Toluene 81%, Xylene 90%. Therefore, we conclude that the combination of Photolysis-Photocatalytic Oxidation process is more efficient than each individual process.

The High Temperature Oxidation Behavior of l0wt%$Gd_2 O_3$- Doped $UO_2$

  • J.H. Yang;K.W. Kang;Kim, K.S.;K.W. Song;Kim, J.H.
    • Nuclear Engineering and Technology
    • /
    • 제33권3호
    • /
    • pp.307-314
    • /
    • 2001
  • The changes of weight gain, structure, morphology and uranium oxidation states in l0wt% G $d_2$ $O_3$-doped U $O_2$ during the oxidation below 475$^{\circ}C$ and heat treatment at 130$0^{\circ}C$ in air were investigated using TGA, XRD, SEM, EPMA and XPS. The room temperature ( $U_{0.86}$G $d_{0.14}$) $O_2$Cubic Phase Converted to highly distorted ( $U_{0.86}$G $d_{0.14}$)$_3$ $O_{8}$ -type sing1e Phase by oxidation at 475 $^{\circ}C$ in air. This oxidized phase was reduced by annealing at 130$0^{\circ}C$ in air. The room temperature XRD pattern of the 130$0^{\circ}C$ annealed powder revealed that ( $U_{0.86}$G $d_{0.14}$)$_3$ $O_{8}$ -type single phase was separated into Gd-depleted $U_3$ $O_{8}$ and Gd-enriched ( $U_{0.7}$G $d_{0.3}$) $O_2$$_{+x}$ type cubic phase. The reduction and phase separation by the high temperature annealing of kinetically metastable and highly deformed ( $U_{0.86}$G $d_{0.14}$)$_3$ $O_{8}$ -type phase are interpreted in terms of cation size difference between G $d^3$$^{+}$ and U according to the oxidation state of U.U.U.U.U.te of U.U.U.U.U.

  • PDF

한반도 서부유입권역에서 대기 중 에어로졸 성분의 화학적 특성 연구 II. 입자의 산성도 및 산화 특성 (A Study on Chemical Characteristics of Aerosol Composition at West Inflow Regions in the Korean Peninsula II. Characteristics of Inorganic Aerosol Acidity and Organic Aerosol Oxidation)

  • 최진수;김정호;이태형;최용주;박태현;안준영;박진수;김현재;구윤서;김신도;홍유덕;홍지형
    • 한국대기환경학회지
    • /
    • 제32권5호
    • /
    • pp.485-500
    • /
    • 2016
  • We examined acidity state of inorganic aerosol and oxidation state of organic aerosol by High Resolution Time of Flight Aerosol Mass Spectrometer (HR-ToF-AMS) at Baengnyeong Super site from Jan 2012 to Dec 2013. Additionally, we carried out the analysis for the aerosol component group of organic matter ($C_xH_y$, $C_xH_yO_1$, $C_xH_yO_z$, $C_xH_yO_zN_p$) and elemental composition to calculate H/C, O/C, N/C, OM/OC and identify the oxidation state. The aerosol chemical composition in this study is dominated by sulfate ($SO_4{^{2-}}$), nitrate ($NO_3{^-}$) plays a smaller role in aerosol acidity. Ammonium ($NH_4{^+}$) was found in a formation of $(NH_4)_3H(SO_4)_2$. However, the binding formations of $NH_4NO_3$ and $NH_4Cl$ increase in the winter. $C_xH_yO_1$ indicating the oxidized state of $PM_{1.0}$ has the highest ratio of 41% while $C_xH_y$ indicating the non-oxidized state has a lower ratio of 36%, meaning that the oxidation level of $PM_{1.0}$ in Baengnyeong Island is high. The ratio between H/C and O/C was 1.33 and 0.78 respectively, showing the characteristic of LV-OOA (Low volatility-Oxygenated Organic Aerosol). Acidic and oxidized aerosols sampled during this field study were largely anthropogenic in origin from Chinese continent and photochemically aged.

니켈기 합금 Alloy 617의 950℃ 대기/헬륨 분위기에서 산화거동 고찰 (Investigation of Oxidation Behavior of Alloy 617 under Air/Helium Environments at 950℃)

  • 정수진;이경근;김동진
    • Corrosion Science and Technology
    • /
    • 제17권5호
    • /
    • pp.218-224
    • /
    • 2018
  • Alloy 617 is a candidate Ni-based superalloy for intermediate heat exchanger (IHX) of a high-temperature gas reactor (VHTR), because of its good creep strength and corrosion resistance at high temperature. Small amount of impurities such as $H_2O$, $H_2$, CO and $CH_4$ are introduced inevitably in helium, as a coolant during operation of a VHTR. Reactions of material and impurities are accelerated with increase of temperature to $950^{\circ}C$ of operating temperature of a VHTR, leading to material corrosion aggravation. In this circumstance, high-temperature corrosion tests were performed at $950^{\circ}C$ in air and impure helium environments, up to 250 hours in this study. Oxidation rate of $950^{\circ}C$ in an air environment was higher than that of impure helium, explained by difference in outer oxide morphology and microstructure as a function of oxygen partial pressure. An equiaxed Cr-rich surface oxide layer was formed in an air environment, and a columnar Cr-rich oxide was formed in an impure helium environment.

Ti-Al-N코팅층의 내산화 특성에 관한 연구 (Study on the Oxidation Resistance of Ti-Al-N Coating Layer)

  • 김충완;김광호
    • 한국세라믹학회지
    • /
    • 제34권5호
    • /
    • pp.512-518
    • /
    • 1997
  • The high temperature oxidation behaviors of titanium nitride films prepared by PACVD technique were studied in the temperature range of from 50$0^{\circ}C$ to 80$0^{\circ}C$ under air atmosphere. Ti0.88Al0.12N film, which showed the excellent microhardness from the previous work, was investigated on its oxidation resistance compared with pure TiN film. Ti-Al-N film showed superior oxidation resistance up to $700^{\circ}C$, whereas TiN film was fast oxidized into rutile TiO2 crystallites from at 50$0^{\circ}C$. It was found that an amorphous layer having AlxTiyOz formula was formed on the surface region due to outward diffusion of Al ions at the initial stage of oxidation. The amorphous oxide layer played a role as a barrier against oxygen diffusion, protected the remained nitride layer from further oxidation, and thus, resulted in the high oxidation resistive characteristics of Ti-Al-N film.

  • PDF

Ti-33.8wt% Al 금속간 화합물의 고온 산화거동 (High temperature oxidation behavior of Ti-33.8wt% Al intermetallic compounds)

  • 최송천;조현준;이동복
    • 한국표면공학회지
    • /
    • 제26권5호
    • /
    • pp.235-244
    • /
    • 1993
  • The oxidation behavior of a two-phase(Ti3Al+TiAl) intermetallic compound, Ti-33.8wt%Al, has been in-vestigated in air at 800, 900 and $^1000{\circ}C$. Though the isothermal oxidation behavior followed a parabolic law up to 100$0^{\circ}C$ indicating that protective oxide scales were formed, the cyclic oxidation behavior followed a lin-ear law in the entire temperature range tested because flaky or stratified scales were usually spalled from the surface during cooling. During oxidation at 80$0^{\circ}C$, the alloy showed excellent oxidation resistance because continuous protective Al2O3 films were formed on the outermost surface of the alloy. However, above $900^{\circ}C$, the oxidation resistance of the alloy was decreased gradually because relatively non-protective TiO2 scales as well as some of Al2O3 scales were formed on the outer oxide scale. The oxidation mechanism of the alloy at different temperature was proposed.

  • PDF