• 제목/요약/키워드: adhesive fabrics

검색결과 26건 처리시간 0.026초

신사복의 접착포에 대한 형태 안정성 평가 (Evaluation of Tailorability of Adhesive Fabrics for Men's Suit)

  • 김정숙
    • 한국의류산업학회지
    • /
    • 제8권5호
    • /
    • pp.585-590
    • /
    • 2006
  • In the variation of physical properties of adhesive fabrics, the objective of this study is to analyze fitness of fusible interlining to four sorts of fabrics for men's suit with various structural parameters. Four fusible interlinings are used for adhering to fabrics for men's suit. Mechanical properties of these 16 adhesive fabrics fused with these interlinings are measured by KES-FB system for analysing appearance and wearing properties of garments and for examining the fitness of fusible interlining to the fabrics for men's suit. The variation of bending property for adhesive fabrics are found to be higher in the order of interlining 1(Cotton30/Rayon70, plain), interlining 2(Polyester30/Rayon70, warp knit), interlining 4(Polyester, shingosen fabrics with drawing textured yarn) and interlining 3(Polyester, double dot coating interlining). The variation of adhesive effect shows the same results with bending property and shows negative relation with extensibility in weft direction per extensibility in warp direction(EM2/EM1). The variation of peel strength of adhesive fabrics, woolen fabrics in the case of face fabrics and interlining 3 in the case of interlining shows the largest value respectively.

한지사 혼용 직물의 접착심 접착 후 외관 형성능의 변화 (The Changes of Appearance Formability of Hanji Blended Fabrics after Fusing)

  • 지주원
    • Human Ecology Research
    • /
    • 제59권1호
    • /
    • pp.13-21
    • /
    • 2021
  • In order to examine the changes in the appearance properties and the post-adhesion appearance properties of Hanji yarn blended fabrics : 100% Hanji yarn fabric, two kinds of cotton / Hanji yarn blended fabrics and 100% cotton fabric, were selected and fused with three kinds of interlinings. After fusing, changes of standardized KES values were examined. 1. W/T, B/W of Hanji yarn blended fabrics was higher than that cotton fabric. WC/W, 2HB/W, 2HB/B, and 2HG/G values of Hanji yarn blended fabrics are lower than cotton fabric. This means that the Hanji yarn was mixed, shape retention, wrinkle recovery was improved, and the drape property was lowered. 2. After fusing, W/T, shape retention, wrinkle recovery of Hanji yarn blended fabrics increased, and WC/W values of Hanji yarn blended fabrics decreased. The wrinkle recovery property of Hanji yarn blended fabrics were improved; however, the 2HG/G value of Hanji yarn fabric increased due to fusing, and the wrinkle recovery property of Hanji yarn fabric decreased. 3. In the selection of adhesive core, I1 adhesive core is excellent in terms of shape stability and wrinkle recovery; however, an I3 adhesive core is recommended for drape and silhouette formation. When the fabric of the adhesive core was PET, it was found to penetrate better between the fabrics during adhesion than the case of cotton fabrics.

직물접착심지에 관한 연구(3) (A Study on Fabric Adhesive Interlining(3))

  • 조자
    • 대한가정학회지
    • /
    • 제35권1호
    • /
    • pp.257-262
    • /
    • 1997
  • In this thesis considering the problems shown in the usage of interlining of clothes and in the process of sewing the breaking away strength which is meant by adhesion is analysed by experimennt in which Polyamide content is dealed with at the 5 level to raise the adhesive strength by using the one-sided non woven adhesive interlining made in this country as the samples. After examing the optimum in the process of Cotton and polyester fabrics and adhered fabrics practical for blouse and jacket and analysing the breaking away strength the wanted property of matter and the change with the repeated laundry We reach at the following results. 1. The adhesive strength of the two adhered fabrics were strongly appeared in order of cotton>polyester. 2. The order of the breaking away strength by the interlinings of adhesive fabrics was A5> A4> A3> A2> A1. 3. The breaking away strength of the two adhered fabrics was weakened by the repeated laundry and the breaking away phenomena were fewer under the most suitable conditions than the various conditions.

  • PDF

부직포 접착심지 부착 전후의 접착포의 열적 쾌적성과 공기투과성에 관한 연구 (A Study on the Thermal Comfort and Air Permeability of Adhesive Fabrics Before and After Adhesion of Nonwoven Adhesive Interlining)

  • 김경희;김승진
    • 한국의류학회지
    • /
    • 제22권7호
    • /
    • pp.807-815
    • /
    • 1998
  • Functions of interlinings to the shell fabric are to improve the garment formability for a beautiful silhouette and elastic potential to the deformed fabric during wearing, and also are to enhance appearance and wearing properties of garment. The objective of this study is to analyse the thermal properties of nonwoven fusible interlining to the thin worsted fabric with various fabric structural parameters. For the purpose fo this study, eight specimens with various weft yarn twists and weft densities of thin worsted fabrics are prepared. Three nonwoven fusible interlinings with different structure which were made by Nylon/Polyester were used for adhering to the thin worsted fabrics. Thermal properties of these 24 adhesive fabrics fused with 3 nonwoven interlinings are measured by KES-F7 System for analysing the thermal suitability of nonwoven fusible interlinings to the thin worsted fabrics with various fabric structural parameters. And air permeability, which was measured by KES-F8-API, of 24 nonwoven adhesive interlining fabrics was also analysed and discussed with the various kinds of nonwoven interlinings and fabric structural parameters.

  • PDF

군용 도포직물의 내후성시험 대체에 대한 연구 (A Study on the Alternative Method for Weathering Test of Military Coated Fabrics)

  • 손찬영
    • 품질경영학회지
    • /
    • 제44권3호
    • /
    • pp.509-526
    • /
    • 2016
  • Purpose: We would like to find the alternative method for the weathering test on rubber coated fabrics and adhesive-coated fabrics for the military products, KS M 0706 (Sunshine carbon arc) to KS M ISO 4892-2 (Xenon arc). Methods: We measured the tensile strength of adhesive-coated fabrics and adhesive products treated with sunshine carbon arc and xenon arc during 100, 150 and 200 hours, respectively. All of the results were treated with statistical test, ANOVA method. We also validate the surface modifications caused by treatment method and time by using FT-IR ATR and, SEM. Results: In case of the thick adhesive-coated fabrics (app. 1 mm), there was no distinctive difference on tensile strength by treatment method and time. In case of the thin mask hood (app. 0.22 mm) and TENT (app. 0.5 mm), there was distinctive difference on tensile strength. Especially, carbon arc showed a huge lowering properties. We could validate the curing from light and moisture, and the functional group change from cross-linking and oxidation using FT-IR ATR. In case of IBS, there was a surface cracks on SEM images. In case of mask hood, there was no distinctive differences, except for a particle falling from decreased affinity between rubber and particles caused by carbon arc. Conclusion: We concluded that there was no problems for changing xenon arc weathering test with same treatment time on IBS, KM7, K21 and adhesive products. In case of TENT and mask hood, there was a difference in tensile strength in accordance with the change of the treated time and method.

접착심지에 관한 연구 (Studies on Adhesive Nonwovenfabrics for Padding Cloths)

  • 성화경
    • 대한가정학회지
    • /
    • 제11권3호
    • /
    • pp.276-284
    • /
    • 1973
  • An experiment, aimed at finding out the adhesive condition when adhesive non-woven fabrics for padding cloths are used for padding cloths of blouse, has been conducted. Materials used were three different kinds-scoured, sanforized, and permanent pressed- of combined fabrics of polyester and cotton. As for padding cloth material, mixed spinning nonwoven fabrics of polyster and viscose rayon have been used. Adhesive conditions were made each at $120^{\circ}C$, $140^{\circ}C$, $160^{\circ}C$ and $180^{\circ}C$, respectively, and adhesive time has been limited to 5, 10, 20, 30, 40 seconds each. External appearance as well as quality have been watched through washing experiment. In case of 12$0^{\circ}C$, all experimental materials were separated at the seventh washing and as for $140^{\circ}C$, all but the material which has been attached on scoured cloth for 40 seconds were separated. In case of 20 seconds only permanent pressed cloth and sanforized cloth were separated. At 30 and 40 seconds, the adhesive conditions have been maintained up to the seventh washing. In case of 5 seconds $180^{\circ}C$it was not turned yellow, but all were separated. In case of 10, 20, 30 and 40 seconds, at above temperature all were turned yellow in the adhesive process. Therefore, the adhesive power could be said strong enough, though it was not very practical. In this experiment, the lower the temperature of iron is, the longer time it has to be touched. At higher temperature however, relatively short time makesn it possible for adhesion and depending upon the finishing methode of cloth, there is slight difference in adhesive power. As a result, the best adhesive condition for all experimental materials is $160^{\circ}C$of iron temperature, and the time of adhesion is between 30 and 40 seconds.

  • PDF

모직물의 접착심지 접착에 의한 물성 변화 (Changes of Mechanical Properties of Wool Fabrics with Fusible Interlinings)

  • 지주완;유효주
    • 한국의류학회지
    • /
    • 제19권4호
    • /
    • pp.671-683
    • /
    • 1995
  • This paper described the changes of mechanical KES values after fusing 4 different (in weave & density) wool face fabrics with 3 different (in weave & extensibility) fusible interlining. The fusing condition was 15$0^{\circ}C$, 4kg.f/cm2 The results of the study were as follows: (1) After fusing, KES mechanical value of B, 2HB, G, 2HGS, WC increased, where as LT, WT werent't changed so much and EM, RT decreased. It means after fusing extensibility and recovery property were decreased and volume and stiffness were increased. (2) Within the limits of this investigation, tensile property seemed to be more influenced by the characteristics of face fabrics, and bending property nil by the effect of adhesive penetration and shear and compression property did by complex of the characteristics of face fabrics and interlining and the effect of adhesive penetration.

  • PDF

투습방수 직물을 사용한 기능성 아우터의 특성 분석 - 소재, 세탁·취급, 디자인, 패턴, 부자재, 봉제를 중심으로 - (Analysis of Characteristics of Functional Outers with Moisture-permeable Waterproof Fabric - Focus on Fabrics, Washing·Cares, Design, Patterns, Subsidiary Materials, and Sewing -)

  • 노의경;윤미경
    • 한국의류산업학회지
    • /
    • 제23권1호
    • /
    • pp.129-141
    • /
    • 2021
  • This study investigated fabrics, washing and cares, design, pattern, subsidiary materials, and sewing methods with a focus on the functional outers using moisture-permeable waterproof fabric as a shell; in addition, each element was analyzed for differences depending on fabric type. The characteristics of 34 outers were investigated through labels, online product introductions, visual inspection, observations from two experts with more than 30 years experience and wear tests. Moisture-permeable waterproof fabrics used for the outer were classified into two types; in addition, the shell of the high-density fabric and the 2 & 3-layer fabrics had different characteristics. Various fabrics, detailed designs, and three-dimensional patterns suitable for each part of the human body were used to improve functionality. In addition, various subsidiary materials and sewing methods were used to form an organic relationship. The same washing and cares, patterns and subsidiary materials were used regardless of fabric type; however, the fabric type influenced the detailed design and sewing. The outers with high-density fabric had a loose fit, short placket, e-banded cuffs, lock-stitch, and lock-stitch+binding. However, the outer with 2 & 3 layer fabric had a slim fit, hood width adjustment, zippered pockets, cuffs with tab, seamless adhesive sewing such as laminating, lock-stitch+ seam-sealing, and welding.

프라이머 코팅과 열융착 필름 라미네이팅을 통해 제조한 충격 완화용 고강력 에어쿠션 직물에 관한 연구 (Study on the High-Strength Air-Cushion Fabrics for Impact-Relief Application Prepared through Primer Coating and Thermal Film Laminating)

  • 김지연;김훈민;민문홍
    • 한국염색가공학회지
    • /
    • 제33권4호
    • /
    • pp.269-279
    • /
    • 2021
  • In this study, the laminating of TPU film after coating of primer adhesive on the fabrics was applied in order to secure the strength to withstand a fall from a higher altitude by increasing the adhesion between the fabric and the film layer. It seems that the fineness of the yarn and the weave construction have a greater effect than the type of the laminating films. The order of superiority of the laminated fabrics by film type and thickness was the same for 1000 denier and 210 denier fabrics, and the tendency was consistent with the order of superiority in the film properties and peel strength tests. The tear strength of laminating fabrics increased three to four times for 1000 denier fabrics compared to the fabric alone, but it decreased by 2 times for the 210 denier fabrics. Summarizing the above results, it is most appropriate to combine 1000d fabric with three types of laminating films(100~200㎛ thickness) of A(0.2T) or B(0.15T) or D(0.1T) considering the air pressure resistance, the impact resistance during the fall, and the durability against damage during use.

한지사 혼용직물의 접착심 접착 후 역학적 물성 변화 (Changes of Physical Properties of Hanji Yarn Blended Fabrics after Fusing)

  • 지주원
    • 한국의류학회지
    • /
    • 제44권1호
    • /
    • pp.159-174
    • /
    • 2020
  • We selected 100% cotton fabric, 100% Hanji yarn fabric and two kinds of cotton / Hanji yarn blended fabrics and fused them with three kinds of interlinings in order to examine changes to the physical properties and the post-adhesion physical properties of Hanji yarn blended fabrics. Changes in KES values were examined after fusing. First, EM, B, 2HB, MMD values of Hanji yarn blended fabrics were higher than cotton fabric, and LT, RT, G, 2HG, LC, WC values of cotton fabric were higher than Hanji yarn blended fabrics. Tensile recovery was lowered, bending stiffness was increased, and shear stiffness was lowered when Hanji yarn was mixed. Second, the KES value of LT, B, 2HB, G, 2HG, LC, WC increased after fusing, while the EM, MMD values decreased. SMD was shown to decrease or increase depending on the type of fabric. The adhesive effect on bending stiffness and shear stiffness due to the mixing of Hanji shows a different tendency in the comparison of αB and αG.