In modern architecture, tiles are used as a decorative material to enhance the appearance of buildings. However, defects occurring during tile installation affect not only the appearance of the building, but also its maintenance. This study aims to investigate stable tile installation by producing tile modules using the floating mortar method and conducting freeze-thaw tests to measure their adhesion strength. Test results showed that the adhesion strength increased as the mesh size decreased, except for S3 mesh. This study highlights the importance of research on tile installation to solve problems related to building appearance and maintenance.
본 연구에서는 고유동성의 VA/VeoVA 개질 시멘트 모르타르의 기초적 성능을 측정한 후 콘크리트의 보수용 재료에 매우 중요한 요구성능인 부착강도에 대한 피착체의 표면에 존재하는 표면수량의 영향을 검토하는 연구가 수행하였다. 시험체의 배합은 VA/VeoVA는 결합재인 시멘트에 대하여 고형분비 (폴리머시멘트비; P/C)에 의하여 10, 20, 30, 50, 75%, 잔골재는 시멘트의 중량에 대하여 각각 1:1, 1:3의 비율을 적용하였다. 고유동성 VA/VeoVA 개질 시멘트 모르타르의 기초적인 성능을 토대로 부착강도, 잔갈림성, 재료분리 저항성이 좋은 시험체를 선택하였다. 시험체는 C:F=1:1인 경우 P/C=20%, 30%의 시험체 2개가 선택되었으며, C:F=1:3인 경우 P/C=50%의 시험체 1개, 총 3개가 선택되었으며 이 3개의 배합에 대하여 피착체의 표면수량에 따른 고유동성 VA/VeoVA 개질 시멘트 모르타르의 특성을 파악하였다. 본 연구를 통해 콘크리트 피착체에 살포된 표면수는 부분적으로 고유동성 VA/VeoVA 개질 시멘트 모르타르의 부착강도를 증진하고, 유동성을 개선하는 효과가 있다는 결론을 얻었다.
이산화탄소 농도가 높은 도심지의 경우 탄산화로 인한 철근부식이 발생하기 쉬우며 이는 콘크리트 구조물의 내구수명을 감소시킨다. 콘크리트 구조물의 경우 다양한 구속조건을 가지며 항상 외부의 재하하중을 받고 있다. 도입된 응력수준은 이산화탄소와 같은 유해인자의 확산을 변화시키며 탄산화 깊이의 변동성을 야기한다. 본 연구에서는 응력재하수준에 따른 탄산화 변동성을 정량화하였으며, 이를 이용하여 탄산화 예측식을 도출하였다. 내구성 설계인자인 피복두께, 이산화탄소 확산계수, 탄산화 반응 수화물, 그리고 외부 이산화탄소 농도를 확률변수로 정의하였으며, MCS을 통하여 영향인자의 변동성에 따른 내구수명을 도출하였다. 또한 응력수준에 따라 변화하는 내구수명을 도출하였으며, 이를 결정론적인 방법의 결과와 비교하였다. 피복두께 및 내부 수화물 생성이 내구수명 변동성에 가장 큰 영향을 미쳤으며, 응력수준을 고려한 내구수명평가는 유지관리 우선순위 설정에 합리적으로 적용할 수 있다.
현대사회에서 건축물은 대다수가 RC구조로 건설되어지고 있다. RC구조의 건축물은 시공상의 하자발생, 설계단계에서의 오차발생 등과 같은 인위적인 요인과 지진, 태풍 등의 자연적인 요인에 의해 구조적 불안정성이 발생하고 이를 해결하기 위해 다수의 보수보강공법이 이루어지고 있다. 보강공법 중 FRP 보강공법에서 사용하는 유기계 에폭시 접착제는 고온에 노출되었을 때 부착파괴가 급격하게 발생하게 되며 이는 보강재의 탈락으로 직결된다. 따라서 본 연구에서는 고온에 노출되었을 때 FRP 보강재에 전달되는 열을 감소시켜주며 일정수준 이상의 부착성능을 가진 무기계 내화 모르타르의 개발을 목적으로 실험을 진행하였다. 실험 결과 EVA수지의 포함으로 상온조건에서 높은 부착강도를 나타내었으며, 가열조건에서도 약 $300^{\circ}C$까지 전혀 성능저하를 나타내지 않았다. 또한, 이면온도는 두께가 증가할수록 낮았으며, 가열 2시간 이후에에서는 약 $780^{\circ}C$의 일정한 온도로 수렴되는 것을 확인하였다.
Recently, the size of tiles used for bathroom walls in apartment houses is gradually increasing in size. The problem is that when these large-sized tiles are attached by the sticking method, due to the nature of the method, there is a concern about the stability of the attachment to the part (pupil) where the tile and the adhesive are not attached. The problem is serious as it leads to lawsuits in the outbreak court. In addition, it is urgent to verify the adhesion stability of the sticking method because secondary damage occurs due to a safety accident caused by the falling of the tile. Ministry of Land, Infrastructure and Transport [Investigation of defects in apartment houses, calculation of repair cost and defect determination criteria] ① The tile adhesion strength is 0.39N/mm2 or more and ② It is specified to fill 80% or more of the base area of the tile backside, but this is currently trendy. It is considered that large-sized tiles need to be verified from multiple angles, and as part of that, we intend to verify the adhesion stability according to the area to be attached to large-sized tiles.
본 연구는 3종류의 시멘트 혼화용 폴리머 (SBR, PA, St/BA)를 이용하여 폴리머시멘트계 보수재의 개발을 목적으로 공시체의 제작 방법을 6가지 형태로 하여 제작한 폴리머시멘트모르타르 보수재에 대하여, 기중양생, 수중양생, 기중양생 후 동결융해 작용 및 수중양생 후 동결융해 작용을 받는 4가지 양생방법을 적용하였다. 그리고 폴리머의 종류, 양생조건, 폴리머시멘트비에 따른 폴리머시멘트모르타르 보수재의 강도 성상을 파악하고, 휨강도 시험 후의 계면 접착 파괴 유형을 검토하였다. 그 결과, 일부의 모르타르를 제외하면, 폴리머의 종류에 따른 폴리머시멘트모르타르 보수재의 압축강도 및 휨강도는 양생조건에 관계없이 St/BA를 혼입한 폴리머시멘트모르타르 보수재가 SBR 또는 PA를 이용한 것보다 우수한 것으로 나타났다. 폴리머시멘트모르타르 보수재의 휨강도 시험 후 파괴 유형은 공시체의 형상과 폴리머시멘트비에 관계없이 모든 공시체에서 계면 접착 파괴는 발생하지 않았다. 이는 폴리머 혼입에 의한 접착성 개선에 의한 것으로 판단된다. 보통시멘트모르타르에 폴리머시멘트모르타르 보수재를 적용함으로써 기중양생 또는 수중양생 후 동결융해의 반복 작용을 받는 열악한 환경하에서도 보통시멘트모르타르보다 강도 저하가 작게 나타나 폴리머 혼입에 의한 동결융해저항성능을 확인할 수 있었다. 본 연구를 통하여 폴리머시멘트모르타르를 다양한 양생조건과 보수방법에서 사용할 때 나타나는 강도 특성, 내동결융해성능 및 휨 접착 파괴 유형을 알 수 있었다.
본 연구에서는 기존 건설폐기물 파·분쇄 기술의 문제점을 분석하여 저품질 순환골재의 문제점을 진단하고 콘크리트용 순환골재의 고품질화 방안으로 새로운 회전형 마쇄기술을 개발하고자 하였으며, 회전형 마쇄기술의 해석 모델링을 통하여 해당 기술의 현장 적용전 모르타르 박리 유효성을 확인하고, 현장에 적용하여 생산된 순환골재의 품질특성을 확인하여 콘크리트용 순환굵은골재로의 적합성을 확인하는 것을 목적으로 한다. 모르타르 박리기술을 현장에 제작·설치하여 기술 투입전, 투입후 순환골재의 모르타르 부착량, 절대건조밀도 및 흡수율의 상관관계를 분석하였으며, 콘크리트용 순환굵은골재의 핵심 품질특성인 입도, 절대건조밀도 및 흡수율을 시험분석 하였다.
The recycle of domestic waste concrete is, however, still in an early stage, and it has been only partially being used for the road fillers. As a counter-plan of activating recycled concrete, we have confirmed the hydration possibility of the waste concrete powder from the experiment on recycling the aggregate powder since 2000. Though that study, we have known that the strength is increasing when the baking time is longer, and baking temperature maintain in $700^{\circ}C$. Also, the quality is lowered because of the fine aggregate powder which has a bad influence on flowability & compression strength by adhesion of mortar on the aggregate face. Therefore, mortar and interfacial separation of aggregate are large in proper quality for concrete recycling is expected that affect. The purpose of this study is to investigate effective aggregate separation and to determine the most suitable production method controlling the duration of baking time for recycled cement from the compressive strength, X-ray diffraction and ingredient analysis test.
International Journal of Concrete Structures and Materials
/
제8권2호
/
pp.165-172
/
2014
Recycled coarse aggregate (RCA) made from waste concrete is not a suitable structural material as it has high absorption of cement mortar, which adheres on the aggregate surface and on the tiny cracks thereon. Therefore, when using RCA made from waste concrete, much water must be added with the concrete, and slump loss occurs when transporting. Hence, its workability is significantly worse than that of other materials. In this study, surface of RCA was coated with water-soluble polycarboxylate (PC) dispersant so that its characteristics improved. Each possibility was evaluated: whether its slump loss can be controlled, by measuring its workability based on the elapsed time; and whether it can be used as a structural material, by measuring its strength. Moreover, the carbonation due to cement mortar adhesion was measured through a carbonation test. As a result, RCA coated with PC dispersant was found to be better than crushed coarse aggregate and RCA when the physical properties of the fresh concrete and the mechanical, durability of the hardened concrete were tested.
Prepackaged system consists out of a dry mix which contains cement, sand, redispersible polymer powder and admixtures in the right proportions. The purpose of this study is to evaluate the quality of prepackaged-type polymer-modified mortar products using redispersible poly(ethylene-vinyl acetate)(EVA) powder. Polymer-modified mortars using the redispersible polymer powder with powdered with powdered shrinkage-reducing agent were prepared with cellulose fiber contents of 0, 0.5, 1.0% and shrinkage-reducing agent contents of 0, 4%, and tested for drying shrinkage, strength, adhesion in tension, water absorption. From the test results, the prepackaged-type polymer-modified mortar products with 4% of shrinkage-reducing agent content give good properties. and that their properties largely depends on the shrinkage-reducing agent content rather than the cellulose fiber contents.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.