Effect of Carbon Equivalent and Cooling Rate on Microstructure in A516 Steels for Pressure Vessel (압력용기용 A516 강의 미세조직에 미치는 탄소 당량과 냉각 속도의 영향)

  • Lee, Hyun Wook;Kang, Ui Gu;Kim, Min Soo;Shin, Sang Yong
    • Korean Journal of Materials Research
    • /
    • v.29 no.8
    • /
    • pp.511-518
    • /
    • 2019
  • In this study, the effect of carbon equivalent and cooling rate on microstructure and hardness of A516 steels for pressure vessel is investigated. Six kinds of specimens are fabricated by varying carbon equivalent and cooling rate, and their microstructures and hardness levels are analyzed. Specimens with low carbon equivalent consist of ferrite and pearlite. As the cooling rate increases, the size of pearlite decreases slightly. The specimens with high carbon equivalent and rapid cooling rates of 10 and $20^{\circ}C/s$ consist of not only ferrite and pearlite but also bainite structure, such as granular bainite, acicular ferrite, and bainite ferrite. As the cooling rate increases, the volume fractions of bainite structure increase and the effective grain size decreases. The effective grain sizes of granular bainite, acicular ferrite, and bainitic ferrite are ~20, ~5, and ${\sim}10{{\mu}m$, respectively. In the specimens with bainite structure, the volume fractions of acicular ferrite and bainitic ferrite, with small effective grains, increase as cooling rate increases, and so the hardness increases significantly.

Effects of Composition on Magnetic Hyperfine Field of Acicular Fe-Co Alloy Particles (침상형 Fe-Co 합금입자에서 조성이 초미세자기장에 미치는 효과)

  • 박재윤;박용환
    • Journal of the Korean Magnetics Society
    • /
    • v.8 no.1
    • /
    • pp.1-5
    • /
    • 1998
  • Acicular Fe-Co alloy particles are one of the candidates for high-density magnetic recording media. We examined the effects of Co additions on the magnetic properties of Fe-Co alloy particles by using M$\'{o}$ssbauer spectroscopy, TEM, and X-ray diffraction. Acicular $Fe_n$Co (n=5, 4, 3, 2) alloy particles coated with silica, were prepared by a chemical coprecipitation method and subsequent H $_2$ reduction. The crystal structure was found to be cubic in all n ranges. The lattice constant $a_0$ decreases with increasing Co contents. Analysis of $^{57}Fe$ M\'{o}$ssbauer effect data in terms of the local configurations of Co atoms has permitted the influence of magnetic hyperfine interactions to be monitored.

  • PDF

The Effect of Cooling method on the Surface Reaction Zone of CP Titanium Casting Body (티타늄 주조체 냉각방법이 표면반응층에 미치는 영향)

  • Moom, Soo;Choi, Seog-Soon;Moon, Il
    • Journal of Technologic Dentistry
    • /
    • v.23 no.2
    • /
    • pp.203-210
    • /
    • 2002
  • This test is to conduct applied research the reaction area of the Ti-cast metal body which is made use of Dental Phosphate-silica alumina bonded investment material selling at a market, and the cooling method is how to effect on the acicular. The experimentation is as followings, 1. Experimental specimens After invest with Dental Phosphate-silica alumina bonded investment material, the $10{\times}10{\times}1.0mm^3$ wax pattern was casted by Dental high vacuum argon centrifugal casting machine. 2. Test We can analyze SEM/EDS, XRD utilize the fractography(an optical microscope). 3. Conclusion The pure cast metal body constituted of reaction products layer, stability layer and contamination layer. This pure cast have no connection with the cooling condition. The pure Titanium shows difference in a component distribution according to the cooling condition. Through this experimentation we can establish that acicular in the pure Ti-cast metal is consist of Hexagonal structure a=2.9505$\AA$, c=4.6826$\AA$.

  • PDF

Formation Mechanism of Aragonite by Substitute of Mg2+ Ions

  • Choi, Kyung-Sun;Park, Jin-Koo;Ahn, Ji-Whan;Kim, Hwan
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.12 s.271
    • /
    • pp.889-892
    • /
    • 2004
  • Acicular type aragonite precipitated calcium carbonate was synthesized by carbonation reaction of $Ca(OH)_2$ slurry and $CO_2$ gas. As increasing the initial concentration of $Mg^{2+}$ ion, calcite crystal phase substantially decreased while that of aragonite crystal phase increased. According to XRD and EDS analysis, it was found that the addition of $MgCl_2$ induced the $Mg^{2+}$ ion to substitute in $Ca^{2+}$ ion site of calcite lattice then the unstabled calcite structure be resolved, consequently the growth of calcite structure is interrupted while the growth of aragonite structure is expedited.

A Study on Estimation of Infinite Fatigue Life in Cruciform Fillet Welded Joint (십자형 필릿 용접부에서의 무한 피로수명 평가에 관한 연구)

  • Lee, Yong-Bok
    • Journal of the Korean Institute of Gas
    • /
    • v.17 no.1
    • /
    • pp.19-25
    • /
    • 2013
  • The joining methods of steel structures of gas facilities, bridges, ships etc. by welding are composed mostly of T-type or cruciform fillet welding and full penetration or partial penetration according to the uses and the shape of the structures. In this study, it was examined the characteristics of fatigue crack according to penetration depth in relation to material thickness in the cruciform fillet welded joints. From the results, it was investigated the safe design stresses within the range of infinite life. When the LOP length is long the range of infinite life is small with root failure and when the LOP length is short the range of infinite life is large with teo failure. For the specimen of material thickness, 20mm welded by 3 pass compared with 10mm, 15mm welded by 2 pass, the fatigue strength and the range of infinite life was more improved by increasing of notch toughness from formation of micro-ferrite acicular structure.

A Study on Characteristics of Fatigue Failure and Fatigue Life in Full Penetrated Cruciform Fillet Weld Zone (완전 용입 십자형 필릿용접부에서 피로파괴특성과 피로수명에 관한 연구)

  • Lee, Yong-Bok
    • Journal of the Korean Institute of Gas
    • /
    • v.16 no.4
    • /
    • pp.16-22
    • /
    • 2012
  • The use of welding process has been increased for manufacture of machine, bridges, ships, gas facilities and so on together with development of welding technique. Accordingly, it has been needed to develop the welding methods considering higher productivity and safety design for manufacture of their welding structures. In this study, it was studied basically on characteristics of fatigue strength and fatigue life in full penetrated cruciform fillet weld zone in relation to material thickness, welding passes, loading direction and notch radius of toe zone. Most of fatigue failure occurred in toe zone of cruciform fillet weld joint. Fatigue strength and fatigue life are under the influence of stress concentration due to notch radius and flank angle of toe zone. The metal of toe zone annealed and diffused by multi-layer welding and acicular ferrite structure formed by the result improved fatigue strength and fatigue life.

Preparation of High-Temperature catalytic Support from Gibbsite II. Properties of Amophous Alumina as Precursor of Catalyst Support (깁사이트를 원료로 한 고온촉매용 담체의 제조 II, 비정질 알루미나의 담체 전구체로서의 특성)

  • 김성연;김연식
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.1
    • /
    • pp.92-100
    • /
    • 1996
  • Amorphous alumina(AA) the precursor of ${\gamma}$-alumina for catalyst support was made in the newly designed ball filled heating column. Some properties of AA as precursor were investigated. In observation of microstruc-ture and pore structure of AA and its derivatives scanning electronic microscope(SEM) and transmission electronic microscope(TEM) were used. It was found that the width of one particle in AA was 45~60$\AA$ and the average distance among the particles ranged 9~12 $\AA$ which suggested a micropore structure. When AA was reacted with water the shape of the surface was found to be altered and acicular bioehmite was formed inside AA which contributed inproved formability. Pore distribution was evaluated for the three samples of AA ground and granulated lump and La2O3 coated alumina. Acid sites were quantitatively determined by ammonia TPD method and the effect of impurity of Na on acid sites was discussed. Water adsorption capacity was evaluated in terms of a desiccant.

  • PDF

The Effects of Mn and Cr Additions on the Microstructure of A356 Alloys Containing Impure Fe (불순 Fe를 함유한 A356 주조합금에서 미세조직 형성에 관한 Mn과 Cr의 효과)

  • Han, Sang-Won
    • Journal of Korea Foundry Society
    • /
    • v.25 no.3
    • /
    • pp.128-133
    • /
    • 2005
  • The effects of Mn and Cr on the crystallization behaviors of Fe-bearing intennetallics in A356 alloy were studied. Coarse and acicular ${\beta}-Al_{5}$FeSi phase in A356-0.20wt.%Fe alloy was modified into small ${\alpha}$-Al(Fe,Mn)Si and ${\alpha}$-Al(Fe,Cr)Si phases in response to Mn and Cr addition, respectively. Increasing of Mn addition amount elevates the crystallizing temperature of ${\alpha}$-Al(Fe,Mn)Si and the Mn/Fe ratio in the ${\alpha}$-Al(Fe,Mn)Si. Cr is more effective to modify ${\beta}-Al_{5}$FeSi in comparison with Mn. ${\alpha}$-Al(Fe,Mn)Si phase had BCC/SC dual structure.

Corrosion behaviors of Cp-Ti and Ti-6Al-4V alloys by TiN coating (TiN 코팅된 Ti 및 Ti-6Al-4V합금의 부식거동)

  • Lee, Soon-Hyun;Jung, Yoong-Hun;Choi, Han-Chul;Ko, Yeong-Mu
    • Journal of Technologic Dentistry
    • /
    • v.30 no.1
    • /
    • pp.25-31
    • /
    • 2008
  • Cp-Ti and Ti-6Al-4V alloys commonly used dental implant materials, particularly for orthopaedic and osteosynthesis because of its suitable mechanical properties and excellent biocompatibility. This alloys have excellent corrosion behavior in the clinical environment. The first factor to decide the success of dental implantation is sufficient osseointegration and high corrosion resistance between on implant fixture and its surrounding bone tissue. In this study, in order to increase corrosion resistance and biocompatibility of Cp-Ti and Ti-6Al-4V alloy that surface of manufactured alloy was coated with TiN by RF-magnetron sputtering method. The electrochemical behavior of TiN coated Cp-Ti and Ti-6Al-4V alloy were investigated using potentiodynamic (EG&G Co, PARSTAT 2273. USA) and potentiostatic test (250mV) in 0.9% NaCl solution at 36.5 $\pm$ 1$^{\circ}C$. These results are as follows : 1. From the microstructure analysis, Cp-Ti showed the acicular structure of $\alpha$-phase and Ti-6Al-4V showed the micro-acicular structure of ${\alpha}+{\beta}$ phase. 2. From the potentiodynamic test, Ecorr value of Cp-Ti and Ti-6Al-4V alloys showed -702.48mV and -319.87mV, respectively. Ti-6Al-4V alloy value was higher than Cp-Ti alloy. 3. From the analysis of TiN and coated layer, TIN coated surface showed columnar structure with 800 nm thickness. 4. The corrosion resistance of TiN coated Cp-Ti and Ti-6Al-4V alloys were higher than those of the non-coated Ti alloys in 0.9% NaCl solution from potentiodynamic test, indicating better protective effect. 5. The passivation current density of TiN coated Cp-Ti and Ti-6Al-4V alloys were smaller than that of the noncoated implant fixture in 0.9% NaCl solution, indicating the good protective effect resulting from more compact and homogeneous layer formation.

  • PDF

Effects of Hydrothermal Conditions on the Morphology of Hematite Particles (Hematite 입자형상에 미치는 수열반응조건의 영향)

  • 변태봉;손진군
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.2
    • /
    • pp.117-128
    • /
    • 1994
  • Hematite particles were obtained by hydrothermal reaction of ferric hydroxide in the presence of small amount of citric acid which is acted as crystal growth controller. The effects of hydrothermal reaction condition son the morphology and crystal structure of powder were investigated using X-ray, TEM and FT-IR. Ellipsoidal or rectangular hematite particles were formed in the range of pH 10.75~11.75 as initial basicity of reactants and 3$\times$10-5 ~9$\times$10-5 mol as citric acid content. Crystallization of hematite was inhibited in the range of pH9. 0~10.5 and above citric acid content of $1.5\times$10-4 mol. Hematite particle length and aspect ratio were decreased gradually with increasing of citric acid content. Hematite particles formed at 14$0^{\circ}C$ exhibited particle properties with the length of 0.7 ${\mu}{\textrm}{m}$ and aspect ratio of 8. Hematite particles having a good acicular-type were not obtained above 22$0^{\circ}C$.