Preparation and Characterization of Barium Zirconate Titanate Thin Films

  • Park, Won-Seok;Jang, Bum-Sik;Yonghan Roh;Junsin Yi;Byungyou Hong
    • Journal of the Korean institute of surface engineering
    • /
    • v.34 no.5
    • /
    • pp.481-485
    • /
    • 2001
  • We investigated the structural and electrical properties of the Ba ($Zr_{x}$ $T_{il-x}$ )$O_3$ (BZT thin films with a mole fraction of x=0.2 and thickness 150 nm for the application in MLCC (Multilayer Ceramic Capacitor). BZT films were prepared on $Pt/SiO_2$/Si substrate at various substrate temperatures by the RF-magnetron sputtering system. When the substrate temperature was above $500^{\circ}C$, we could obtain multi-crystalline BZT films oriented at (110), (111), and (200) directions. The crystallization of the film and high dielectric constant were observed with the increase of substrate temperature. Capacitance of the film deposited at high temperature is more sensitive to the applied voltage than that of the film deposited at low temperature. This paper reports surface morphology, dielectric constant, dissipation factor, and C-V characteristics for BZT films deposited at three different temperatures. The BZT film deposited at 40$0^{\circ}C$ shows stable electrical properties but a little small dielectric constant for MLCC application.

  • PDF

Reduce of Etching Damage of PZT Thin Films in $Cl_2/CF_4$ Plasma with addition of Ar and $O_2$ ($Cl_2/CF_4$ 플라즈마 Ar, $O_2$ 첨가에 따른 PZT 막막의 식각 손상 효과)

  • Kang, Myoung-Gu;Kim, Kyoung-Tae;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.21-25
    • /
    • 2001
  • In this study, recovery of plasma etching· damage in PZT thin film with additive gas and re-annealing after etching have been investigated. The PZT thin films were etched as a function of $Cl_2/CF_4$ with addition of Ar and $O_2$ with inductively induced plasma. The etch rates of PZT thin films were 1450 $\AA$/min at 30% additive Ar into $(Cl_2(80%)+CF_4 (20%))$ and 1100 $\AA$/min at 10% additive $O_2$ into $C(Cl_2(80%)+CF_4(20%))$. In order to recovery properties of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures in at $O_2$ atmosphere. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed sample is consistent with the increase of the (100) and (200) PZT peaks revealed by x-ray diffraction (XRD). From x-ray photoelectron spectroscopy (XPS) analysis, intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of $Ti_xO_y$ is recovered by $O_2$ recombination during rapid thermal annealing process.

  • PDF

Reduce of Etching Damage of PZT Thin Firms with Addition of Ar and O2 in Cl2/CF4 Plasma (Cl2/CF4 플라즈마에 Ar, O2 첨가에 따른 PZT 박막의 식각 손상 개선 효과)

  • 강명구;김경태;김창일
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.15 no.4
    • /
    • pp.319-324
    • /
    • 2002
  • In this study, the reduce of plasma etching damage in PZT thin film with addictive gas and re-annealing after etching have been investigated. The PZT thin films were etched as a function of $Cl_2/CF_4$ with addition of Ar and $O_2$ with inductively coupled plasma. The etch rates of PZT thin films were 1450 ${\AA}/min$ at 30% additive Ar and 1100 ${\AA}/min$ at 10% auditive $O_2$ into $Cl_2/CF_4$ gas mixing ratio of 8/2. In order to reduce plasma damage of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures at $O_2$ atmosphere. From the hysteresis curries, the ferroelectric properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed PZT films is consistent wish the increase of the (100) and (200) PZT peaks revealed by x-ray diffraction (XRD). From x ray photoelectron spectroscopy (XPS) analysis, the intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of $Ti_xO_y$ is recovered by $O_2$ recombination during rapid thermal annealing process.

Electrooptic Properties of PLZT Thin Films Prepared by Sol-Gel Method (Sol-Gel법으로 제조한 PLZT 박막의 전기광학특성)

  • Lee, Sung-Gap;Chung, Jang-Ho;Bae, Seon-Gi;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 1996.07c
    • /
    • pp.1505-1507
    • /
    • 1996
  • In this study, $(Pb_{0.88}La_{0.12})(Zr_{0.40}Ti_{0.60})O_{2.97}$ (La/Zr/Ti=12/40/60) ceramic thin films were fabricated from an alkoxide-based by Sol-Gel method. PLZT stock solutions were made and spin-coated on the ITO-glass rubstrate at 4000[rpm] for 30[sec]. Coated specimens were baked to remove the organic materials at $400[^{\circ}C]$ for 10[min]. This procedure was repeated 5 times. The coated films were finally annealed at $450{\sim}700[^{\circ}C]$ for 1[hr]. The ferroelectric perovskite phases precipitated under the sintering of $550{\sim}700[^{\circ}C]$ for 1[hr]. Relative dielectric constant of the PLZT thin were increased with increasing the sintering temperature, the thin file sintered at $650[^{\circ}C]$ showed the highest value of 196. But in the PLZT thin film sintered at $700[^{\circ}C]$, relative dielectric constant was greatly decreased due to reacts between ITO electrode and glass substrate. In all thin films, the transmittance was more than 70[%] (at 632.8[nm]).

  • PDF

Recovery of Etching Damage of the etched PZT Thin Films With $O_{2}$ Re-Annealing. ($O_{2}$ re-annealing에 의한 식각된 PZT 박막의 식각 damage 개선)

  • Kang, Myoung-Gu;Kim, Kyoung-Tae;Kim, Chang-Il;Chang, Eui-Goo;Lee, Byeong-Ki
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.05b
    • /
    • pp.8-11
    • /
    • 2001
  • In this study. the recovery of plasma induced damage in the etched PZT thin film with $O_2$ re-annealing have been investigated. The PZT thin films were etched as a function of $Cl_2/Ar$ and additive $CF_4$ into $Cl_{2}(80%)/Ar(20)%$. The etch rates of PZT thin films were $1600\dot{A}/min$ at $Cl_{2}(80%)/Ar(20)%$ gas mixing ratio and $1970\dot{A}/min$ at 30 % additive $CF_4$ into $Cl_{2}(80%)/Ar(20)%$. The etched profile of PZT films was obtained above 70 by SEM. In order to recovery properties of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures in $O_2$ atmosphere. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed sample is consistent with the increase of the (100) and (200) PZT phase revealed by x-ray diffraction (XRD). From XPS analysis, intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of TixOy is recovered by $O_2$ recombination during rapid thermal annealing process. From AFM images, it shows that the surface roughness of re-annealed sample after etching is improved.

  • PDF

$Ba(Zr_{0.85}Y_{0.15})O_{3-\delta}$-NI Composite Membrane for Hydrogen Separation by Aerosol Deposition Method (에어로졸 증착법(Aerosol Depostion method)에 의한 $Ba(Zr_{0.85}Y_{0.15})O_{3-\delta}$-NI 수소분리막 제조)

  • Park, Young-Soo;Choi, Jin-Sub;Byoun, Myoung-Sub;Kim, Jin-Ho;Hwang, Kwang-Taek
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.21 no.4
    • /
    • pp.271-277
    • /
    • 2010
  • $(Ba(Zr_{0.85}Y_{0.15})O_{3-\delta})$ oxide, showing high protonic conductivity at high temperatures and good chemical stability with $CO_2$ are referred to as hydrogen separation membrane. For high efficiency of hydrogen separation ($H_2$ flux and selectivity) and low fabrication cost, ultimate thin and dense BZY-Ni layer has to be coated on a porous substrate such as $ZrO_2$. Aerosol depostion (AD) process is a novel technique to grow ceramic film with high density and nano-crystal structure at room-temperature, and may be applicable to the fabrication process of AD integration ceramic layer effectively. XRD, SEM, X-ray mapping measurements were conducted in order to analyze the characteristics of BZY-Ni membrane fabricated by AD process. it is observed that it is homogeneous distribution for BZY-Ni. The result of $H_2$ permeation rate suggests that BZY-Ni composite is higher than BZY.

Reduce of Etching Damage of PZT Thiin Films in $Cl_{2}/CF_{4}$ Plasma with addition of Ar and $O_2$ ($Cl_{2}/CF_{4}$ 플라즈마에 Ar,$O_2$첨가에 따른 PZT 박막의 식각 손상 효과)

  • 강명구;김경태;김창일
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.21-25
    • /
    • 2001
  • In this study, recovery of plasma etching damage in PZT thin film with additive gas and re-annealing after etching have been investigated. The PZT thin films were etched as a function of Cl$_2$/CF$_4$ with addition of Ar and $O_2$ with inductively induced plasma. The etch rates of PZT thin films were 1450$\AA$/min at 30% additive Ar into (Cl$_2$(80%)+CF$_4$ (20%)) and 1100$\AA$/min at 10% additive $O_2$ into C(Cl$_2$(80%)+CF$_4$ (20%)). In order to recovery properties of PZT thin films after etching, the etched PZT thin films were re-annealed at various temperatures in at $O_2$ atmosphere. From the hysteresis curves, ferroelectrical properties are improved by $O_2$ re-annealing process. The improvement of ferroelectric behavior at annealed sample is consistent with the increase of the (100) and (200) PZT peaks revealed by x-ray diffraction (XRD). From x-ray photoelectron spectroscopy (XPS) analysis, intensity of Pb-O, Zr-O and Ti-O peak are increased and the chemical residue peak is reduced by $O_2$ re-annealing. The ferroelectric behavior consistent with the dielectric nature of Ti$_{x}$O$_{y}$ is recovered by $O_2$ recombination during rapid thermal annealing process.s.s.

  • PDF

Microstructure and Electrical Properties of the Pt/Pb1.1Zr0.53Ti0.47O3/PbO/Si (MFIS) Using the PbO Buffer Layer (PbO 완충층을 이용한 Pt/Pb1.1Zr0.53Ti0.47O3/PbO/Si (MFIS)의 미세구조와 전기적 특성)

  • Park, Chul-Ho;Song, Kyoung-Hwan;Son, Young-Guk
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.2 s.273
    • /
    • pp.104-109
    • /
    • 2005
  • To study the role of PbO as the buffer layer, Pt/PZT/PbO/Si with the MFIS structure was deposited on the p-type (100) Si substrate by the r.f. magnetron sputtering with $Pb_{1.1}Zr_{0.53}Ti_{0.47}O_3$ and PbO targets. When PbO buffer layer was inserted between the PZT thin film and the Si substrate, the crystallization of the PZT thin films was considerably improved and the processing temperature was lowered. From the result of an X-ray Photoelectron Spectroscopy (XPS) depth profile result, we could confirm that the substrate temperature for the layer of PbO affects the chemical states of the interface between the PbO buffer layer and the Si substrate, which results in the inter-diffusion of Pb. The MFIS with the PbO buffer layer show the improved electric properties including the high memory window and low leakage current density. In particular, the maximum value of the memory window is 2.0V under the applied voltage of 9V for the Pt/PZT(200 nm, $400^{\circ}C)/PbO(80 nm)/Si$ structures with the PbO buffer layer deposited at the substrate temperature of $300^{\circ}C$.

Etching Property of the TaN Thin Film using an Inductively Coupled Plasma (유도결합플라즈마를 이용한 TaN 박막의 식각 특성)

  • Um, Doo-Seung;Woo, Jong-Chang;Kim, Dong-Pyo;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.06a
    • /
    • pp.104-104
    • /
    • 2009
  • Critical dimensions has rapidly shrunk to increase the degree of integration and to reduce the power consumption. However, it is accompanied with several problems like direct tunneling through the gate insulator layer and the low conductivity characteristic of poly-silicon. To cover these faults, the study of new materials is urgently needed. Recently, high dielectric materials like $Al_2O_3$, $ZrO_2$ and $HfO_2$ are being studied for equivalent oxide thickness (EOT). However, poly-silicon gate is not compatible with high-k materials for gate-insulator. To integrate high-k gate dielectric materials in nano-scale devices, metal gate electrodes are expected to be used in the future. Currently, metal gate electrode materials like TiN, TaN, and WN are being widely studied for next-generation nano-scale devices. The TaN gate electrode for metal/high-k gate stack is compatible with high-k materials. According to this trend, the study about dry etching technology of the TaN film is needed. In this study, we investigated the etch mechanism of the TaN thin film in an inductively coupled plasma (ICP) system with $O_2/BCl_3/Ar$ gas chemistry. The etch rates and selectivities of TaN thin films were investigated in terms of the gas mixing ratio, the RF power, the DC-bias voltage, and the process pressure. The characteristics of the plasma were estimated using optical emission spectroscopy (OES). The surface reactions after etching were investigated using X-ray photoelectron spectroscopy (XPS) and auger electron spectroscopy (AES).

  • PDF

Substrate Effects on the Response of PZT Infrared Detectors (상이한 기판조건에 따른 PZT 적외선 감지소자의 성능 변화)

  • Go, Jong-Su;Gwak, Byeong-Man;Liu, Weiguo;Zhu, Weiguang
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.3
    • /
    • pp.428-435
    • /
    • 2002
  • Pyroelectric $Pb(Zr_{0.3}Ti_{0.7})O_3$ (PZT30/70) thin film IR detectors has been fabricated and characterised. The PZT30/70 thin film was deposited onto $Pt/Ti/Si_3N_4/SiO_2/Si$ substrate by the sol-gel process. Four different substrate conditions were studied for their effects on the pyroelectric responses of the IR detectors. The substrate conditions were the combinations of the Si etching and the Pt/Ti patterning. In the Si etched substrate, the $Si_3N_4/SiO_2$ composite layer was used as silicon etch-stop, and was used as the membrane to support the PZT pyroelectric film element as well. The measured pyroelectric current and voltage responses of detectors fabricated on the micro-machined thin $Si_3N_4/SiO_2$ membrane were two orders higher than those of the detectors on the bulk-silicon. For detectors on the membrane substrate, the Pt/Ti patterned detectors showed a 2-times higher pyroelectric response than that of not-patterned detectors. On the other hand, the pyroelectric response of the detectors on the not-etched Si substrate was almost the same, regardless of the Pt/Ti patterning. It was also found that the rise time strongly depended on the substrate thickness: the thicker the substrate was, the longer the rise-time.