• Title/Summary/Keyword: Zn-Ni

Search Result 1,579, Processing Time 0.024 seconds

Power Loss and Electro-Magnetic Characteristics of Ni-Cu-Zn Ferrites (Ni-Cu-Zn페라이트의 손실과 자성 특성)

  • Otsuki E.;Kim Jeong-Su
    • Proceedings of the Korean Institute of Resources Recycling Conference
    • /
    • 2004.12a
    • /
    • pp.3-11
    • /
    • 2004
  • The power loss analysis was carried out for Ni-Cu-Zn ferrite samples with different content of NiO and ZnO. The power loss, Pcv decreases monotonically wi increasing temperature and attains to a certain value at around $100\~120$ degrees Celsius. The frequency dependence of Pcv can be explained by $Pcv\~f^n$', and n is independent of the frequency, f up to 1MHz. The Pcv decreases with an increase in ZnO/NiO. The Pcv was separated to hysteresis loss, Ph and residual loss, (Pcv-Ph). The temperature characteristics and compositional dependence of Pcv can be attributed to the Ph, while (Pcv-Ph) is not affected by both temperature and ZnO/NiO. By analyzing temperature and composition dependence of Ph and initial permeability, ${\mu}^i$ following equations could be formularized. $${\mu}_i{\mu}o=I_x\;^2/(K_1+bs_ol_s)\;\;\;\;(1)$$ $Wh=13.5(I_s\;^2/{\mu}_i{\mu}_o)\;\;\;\;(2)$$ Were ${\mu}_o$ is permeability of vacuum, $I_s$ saturation magnetization, $K_1$ anisotropy constant, $S_o$ internal heterogeneous stress, $I_s$, magnetostriction constant, b unknown constant. Wh hysteresis loss per one cycle of excitation (Ph: Wh*f). Steinmetz constant of Ni-Cu-Zn ferrites, $m=1.64\~2.2$ is smaller than the one of Mn-Zn ferrites, which suggests the difference of loss mechanism between these materials.

  • PDF

Effect of annealing on the magnetic behavior and microstructures of spherical NiZn ferrite particle prepared by ultrasonic spray pyrolysis

  • Nam, Joong-Hee
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.1
    • /
    • pp.11-17
    • /
    • 2007
  • The spherical NiZn ferrite particles were prepared by ultrasonic spray pyrolysis with mixed solution of aqueous metal nitrates. The NiZn ferrite particle was observed with nano-sized primary particles of about 10 nm or less before annealing which represented as paramagnetic behavior measured at 77 K and room temperature. The typical abnormal growth of primary particles like polyhedral primary particles was observed by annealing at 1273 K with Zn-concentration dependency. The XRD patterns showed good crystallinity of NiZn ferrite powder after annealing. In annealing process, the intra-particle sintering phenomenon was observed and the spherical particle morphology was collapsed at 1673 K. The saturation magnetization of NiZn ferrite powder for each annealing temperature was decreased with measuring temperature of $77{\sim}$300K.

A Study on the Electromagnetic Wave Absorption Properties by the Composition Ratio and Sintering Condition of NiCuZn Ferrite (NiCuZn 페라이트의 조성 및 소결조건에 따른 전자파흡수 특성에 관한 연구)

  • 이영구;박찬규;이문수
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.5 no.5
    • /
    • pp.994-1000
    • /
    • 2001
  • With the development of electromagnetic communication technology and increased use of electromagnetic wave, the countermeasure of EMI(Electromagnetic Interference) becomes more important socially, and interest for the electromagnetic wave absorber has also increased. In this paper, we have studied characteristics of frequency dependency on complex permittivity and complex permeability according to the changes of composition rate and sintering temperature of NiCuZn ferrite also known as electromagnetic wave absorber and further looked into effect of electromagnetic wave absorption properties. From the measurement where the composition of $Fe_2O_3$ and ZnO of NiCuZn ferrite was fixed at 49 and 34 mol% respectively while composition of NiO and CuO has been varied at each test, we found out that Initial permeability and permittivity were high and the absorbing ability of electromagnetic wave recorded best with $loss tangent(=\mur"/\mur')$ displays more than 1 within the frequency band of 2MHz~9.5MHz when the composition ratio of NiO was ranged around 8.5~9.5 mol% and the sintering temperature was $1080^{\circ}C$.TEX>.

  • PDF

Synthesis and Properties of Ni-Zn Ferrite by Wet-Direct Process (습식 직접 합성법에 의한 Ni-Zn Ferrite의 합성 및 물성 연구)

  • 이경희;이병하;이융걸;황우연
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.3
    • /
    • pp.225-233
    • /
    • 1991
  • In this study, we tried to find out the appropriate synthetic condition and magnetic properties of Ni-Zn ferrite {(NixZn1-x)Fe2O4} powders (where X=0, 0.1, 0.2, 0.3, ……0.9, 1). Ferrite powders were prepared by wet-direct method at 86℃ for 6hrs from FeCl36H2O, NiCl26H2O, and ZnCl2. The powders of (NixZn1-x)Fe2O4 (where X=0.4, 0.5, 0.6) have a good crystallinity, but the other ferrite powders consist of crystal and precursor ferrite. The ferrite powder's lattice constant is increased when ratio of ZnO contant is increased in the ferrite composition. And initial permeability was measured after sintering, result indicated regular pattern except (Ni0.4Zn0.6)Fe2O4 when the frequency were changed 10KHz to 10MHz.

  • PDF

ZnNiO thin films deposited by r.f. magnetron sputtering method (RF Magnetron Sputtering법으로 증착된 ZnNiO박막의 특성)

  • 오형택;이태경;김동우;박용주;박일우;김은규
    • Journal of the Korean Vacuum Society
    • /
    • v.12 no.4
    • /
    • pp.269-274
    • /
    • 2003
  • The electrical, optical and structural properties of ZnNiO thin _ films deposited on Si substrates using rf-magnetron sputtering method have been investigated before and after the thermal annealing processes. The crystallinity of the ZnNiO thin film become degraded with increasing the Ni contents. This is mainly because the lattice of the thin film was expanded due to the oxygen-deficient conditions. Concerning the electrical properties of the thin film, the carrier concentration increases ($6.81\times10^{14}\textrm{cm}^{-2}$) and Hall mobility decreases (36.3 $\textrm{cm}^2$/Vㆍs) with higher doping concentration of Ni. However, the carrier concentration and Hall mobility became low ($1.10\times10^{14}\textrm{cm}^2$ and high (209.6 $\textrm{cm}^2$/Vㆍs), respectively, after the thermal annealing process at $1000 ^{\circ}C$. We also observed a strong luminescene center peaking at 546 nm in photoluminescence spectra, which was caused by a deep level center in the ZnO band gap with oxygen deficient ZnNiO structure.

Bioassessment of Nanoparticle Toxicity based on Seed Germination and Germination Index of Various Seeds (다양한 씨앗의 발아 및 발아지수에 근거한 나노입자 생물학적 독성평가)

  • Gu, Bon Woo;Lee, Min Kyeung;Shi, Yu Tao;Kong, In Chul
    • Clean Technology
    • /
    • v.21 no.1
    • /
    • pp.39-44
    • /
    • 2015
  • This study investigated the effects of six metal oxide nanoparticles (NPs: CuO, NiO, TiO2, Fe2O3, Co3O4, ZnO) on seed germination and germination index (G.I) for five types of seeds: Brassica napus L., Malva verticillata L., Brassica olercea L., Brassica campestris L., Daucus carota L. NPs of CuO, ZnO, NiO show significant toxicity impacts on seed activities [CuO (6-27 mg/L), ZnO (16-86 mg/L), NiO (48-112 mg/L)], while no significant effects were observed at > 1000 mg/L of TiO2, Fe2O3, Co3O4. Tested five types of seed showed different sensitivities on seed germination and root activity, especially on NPs of CuO, ZnO, NiO. Malva verticillata L. seed was highly sensitive to toxic metal oxide NPs and showed following EC50s : CuO 5.5 mg/L, ZnO 16.4 mg/L, NiO 53.4 mg/L. Mostly following order of toxicity was observed, CuO > ZnO > NiO > Fe2O3 ≈ Co3O4 ≈ TiO2, where slightly different toxicity order was observed for carrot, showing CuO > NiO ≈ ZnO > Fe2O3 ≈ Co3O4 ≈ TiO2.

The Characteristics of Magnetic of Ni-Zn Ferrite dependent on pH (pH에 따른 Ni-Zn 페라이트의 자기적 특성)

  • 김한근;사공건
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1993.11a
    • /
    • pp.124-127
    • /
    • 1993
  • In this paper, the magnetic properties of Ni-Zn ferrite powders dependent on pH have been studied. Ni-Zn ferrite powders were synthesized by coprecipitation method(pH were 7. 9. 11 and 13. respetively) using FeCl$_3$$.$ 6H$_2$O, NiCl$_2$$.$6H$_2$O and ZnCl$_2$as starting materials and its powders were calcined at 1,000($^{\circ}C$). The saturated magnetizations of the Ni-Zn ferrite powders dependent on various pH. such as 7, 9, 11 and 13 were 11.44, 29.77, 69.62 and 66.75(emu/g), respetively.

  • PDF

The Characteristics of Hetero Junction Using NiCuZn Ferrite and Dielectric for LTCC (LTCC를 위한 NiCuZn 페라이트계와 유전체의 이종접합의 특성)

  • Kim, Nam Hyun;Park, Hyun;Kim, Kyung Nam
    • Journal of Surface Science and Engineering
    • /
    • v.45 no.5
    • /
    • pp.188-192
    • /
    • 2012
  • The hetero junction on dielectrics and ferrite for LTCC was prepared by using NiCuZn ferrite. The shrinkage behaviour of ferrite tapes in combination with a dielectric tape was investigated. The characteristics of NiCuZn ferrite were investigated using XRD (X-ray diffractometer), Dilatometer, FE-SEM (Field emission scanning electron microscope), EDS (Energy dispersive spectrometer). NiCuZn ferrite calcined at $700^{\circ}C$ had a good apparent density and initial permeability of magnetic properties. The shrinkage rate of the NCZF700 ferrite and dielectric material was similar. The multilayer revealed dense, uniform morphologies with excellent interface quality. Diffusion of hetero junction such as dielectric and ferrite was not occuring at $900^{\circ}C$.

Influence of Toxic Heavy Metals on Germination of Rice Seeds and Growth of Rice Seedling (수도생육(水稻生育)에 대한 유해(有害) 중금속(重金屬)의 영향(影響) - 발아 및 묘대기(苗垈期) 생육(生育)에 대하여 -)

  • Kim, B.J.;Ha, Y.L.;Kim, J.O.;Han, K.H.
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.11 no.2
    • /
    • pp.119-126
    • /
    • 1979
  • Rice seeds, suweon 264, were germinated under 5 levels of toxic heavy metals, Cd(0, 0.05, 0.5, 5, 20ppm), Cu(0, 0.05, 0.5, 5, 20, ppm), Cr(0, 0.5, 1, 5, 10ppm), Ni(0, 0.5, 1, 5, 10ppm), Co(0, 0.5, 1, 5, 10ppm), Zn(0, 0.5, 5, 20, 40, ppm), Pb(0, 0.5, 5, 20, 40ppm) and Mn(0, 1, 10, 25, 50, ppm) in culture solution, and then grown with supplying culture solution contained respective concentrations. Germination and growth response to the toxic heavy metals were studied. Results obtained are as follows : 1) The germination injury of rice seeds by excess concentration of toxic heave metal in culture solution occured in Cd and Cu; below 0.05 ppm, Ni; below 0.5 ppm, Mn; below 1.0 ppm, Co and Cr; 0.5-1.0 ppm, and 0.5-5 ppm, Zn and Pb. Thereby, in the order of degrees of the elements toxicity to germination, they were arranged as follows : Cd>Cu>Ni>Co>Cr>Mn>Zn$$\geq_-$$Pb. 2) Toxic heavy metal concentrations in culture solution, which result in decreasing dry weight due to the injury of excess concentration of treated elements, were Cd: below 0.05 ppm, Ni, Cr and Co; below 0.5 ppm, Cu and Zn; 0.5-5 ppm, Pb; 5-20 ppm and Mn; 10-25 ppm. The order was Ni>Cd>Cr>Co>Cu$$\geq_-$$Zn>Pb>Mn. 3) The critical contents of Cd, Ni, Pb, Cu, Zn, Mn, and Co in dry matter, Which result in decreasing dry weight, were considered to be 0.05-15.5, 1.50-25.0, 24.0-28.0, 26.5-62.5, 470-645.0, 231.0-500.0 and below 15.0 ppm, respectively. 4) The contents of Cr, Co, Cd, Pb, Ni, Cu and Zn in dry matter by 0.5 ppm treatment concentration of each heavy metals was trace, 15.0, 17.5, 24.0, 25.0, 84.5 and 470.0 ppm, respectively. Thereby, in the order of each element to uptaked by rice seedlings, they were arranged as follow; Zn>Cu>Ni>Pb>Cd>Co>Cr. 5) The hazardous concentrations of root activity by toxic heavy metals in culture solution were Cd; below 0.05, Cu; 0.05-0.5, Cr; below 0.5, Ni; 0.5-1.0, Co; 0.5-1.0, Zn; above 0.5, Pb; 0.5-5.0 and Mn; 1.0-10.0 ppm. The hazardous degree of root activity by toxic heave metals was in the order of Cd>Cu>Cr>Zn>Ni>Co>Pb>Mn.

  • PDF

Sequential Extraction of Heavy Metals in the Vicinity of the Oksung Cu-Zn Mine (옥성(玉城) 동(銅)-아연(亞鉛) 광산(鑛山) 주변(周邊) 토양중(土壤中) 중금속(重金屬)의 형태별(形態別) 함량(含量))

  • Cho, Jae-Young;Kim, Euen-Hyuk;Han, Kang-Wan
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.33 no.6
    • /
    • pp.446-452
    • /
    • 2000
  • This study was carried out to investigate the effect of mine activity on paddy fields, agricultural water, and plants in the ruined Oksung Cu-Zn mine area. Soil samples collected from paddy fields adjacent to the Cu-Zn mine sites were sequentially extracted and determined the contents of heavy metals such as Cd, Zn, Cu, Pb, Cr and Ni. Distribution of exchangeable heavy metals in soils was 30.2% of Cd, 11.3% of Zn, 2.2% of Cu, 4.6% of Cr, 0.6% of Pb and 3.9% of Ni. Water soluble heavy metals were only detected with Zn. The contents of heavy metals in water collected from the mine were 0.01 of Cd, 27.35 of Zn, 4.86 of Cu, 1.04 of Pb, 0.03 of Cr and $0.08mg\;L^{-1}$ of Ni. while the contents in waler collected out of the mine were 16.67 of Zn, 0.59 of Cu, 0.49 of Pb, 0.05 of Cr and $0.06mg\;L^{-1}$ of Ni. On the other hand, agricultural water near mine area were 1.26 of Zn, 0.05 of Cu, 0.05 of Pb and $0.02mg\;L^{-1}$ of Ni. Both Cd and Cr were not detected in the agricultural water.

  • PDF