A Study on the Fracture Strength of All-Ceramic Crown according to the Zirconia Coping Design using CAD/CAM System L. Bulgan, In-Ho Cho, Soo-Yeon Shin Department of Prosthodontics, Graduate School, Dankook University The fracture strength of prosthesis is important, because it affects the function, and long term success of prosthesis and teeth. The purpose of this study was to compare the fracture strength of zirconia coping designs. Experimental test group were classified into three designs according to coping design, Modified design: Zirconia coping margin was located at 1mm above the axiogingival line angle. Collarless design: The coping margin terminated at the axiogingival line angle Butt design: The coping margin was extended to the finishing line of prepared margin. A $Cercon^{(R)}$(Degussa, Germany) CAD/CAM system was used to make the zirconia coping. Fracture strength was measured using loading machine at a cross head speed of 1mm/min. The results were statistically analyzed using the one-way ANOVA and multiple comparison test. Statistical significance was set in advance at the probability level of less than 0.05. The result : I. Collarless($738N{\pm}155N$) and Modified($755N{\pm}185N$) groups showed significantly a lower fracture strength than Butt($1057N{\pm}262N$) group(p<0.05). II. There were no statistical differences of the fracture strength between Modified($755N{\pm}185N$) and Collarless($738N{\pm}155N$) groups. III. When comparing the fractured surface, all the group showed porcelain fracture, which were fractured at the labial surface of baked porcelain The butt design of the zirconia coping has higher fracture strength than modified and collarless design.
PURPOSE. The aim of the study was to evaluate the effect of abutment shade, ceramic thickness, and coping type on the final shade of zirconia all-ceramic restorations. MATERIALS AND METHODS. Three different types of disk-shaped zirconia coping specimens (Lava, Cercon, Zirkonzahn: ${\phi}10mm{\times}0.4mm$) were fabricated and veneered with IPS e.max Press Ceram (shade A2), for total thicknesses of 1 and 1.5 mm. A total of sixty zirconia restoration specimens were divided into six groups based on their coping types and thicknesses. The abutment specimens (${\phi}10mm{\times}7mm$) were prepared with gold alloy, base metal (nickel-chromium) alloy, and four different shades (A1, A2, A3, A4) of composite resins. The average $L^*$, $a^*$, $b^*$ values of the zirconia specimens on the six abutment specimens were measured with a dental colorimeter, and the statistical significance in the effects of three variables was analyzed by using repeated measures analysis of variance (${\alpha}$=.05).The average shade difference (${\Delta}E$) values of the zirconia specimens between the A2 composite resin abutment and other abutments were also evaluated. RESULTS. The effects of zirconia specimen thickness (P<.001), abutment shade (P<.001), and type of zirconia copings (P<.003) on the final shade of the zirconia restorations were significant. The average ${\Delta}E$ value of Lava specimens (1 mm) between the A2 composite resin and gold alloy abutments was higher (close to the acceptability threshold of 5.5 ${\Delta}E$) than th ose between the A2 composite resin and other abutments. CONCLUSION. This in-vitro study demonstrated that abutment shade, ceramic thickness, and coping type affected the resulting shade of zirconia restorations.
PURPOSE. The purpose of this study was to evaluate the influence of different coping thicknesses and veneer ceramic cooling rates on the failure load of zirconia-ceramic crowns. MATERIALS AND METHODS. Zirconia copings of two different thicknesses (0.5 mm or 1.5 mm; n=20 each) were fabricated from scanning 40 identical abutment models using a dental computer-aided design and computer-aided manufacturing system. Zirconia-ceramic crowns were completed by veneering feldspathic ceramics under different cooling rates (conventional or slow, n=20 each), resulting in 4 different groups (CONV05, SLOW05, CONV15, SLOW15; n=10 per group). Each crown was cemented on the abutment. 300,000 cycles of a 50-N load and thermocycling were applied on the crown, and then, a monotonic load was applied on each crown until failure. The mean failure loads were evaluated with two-way analysis of variance (P=.05). RESULTS. No cohesive or adhesive failure was observed after fatigue loading with thermocycling. Among the 4 groups, SLOW15 group (slow cooling and 1.5 mm chipping thickness) resulted in a significantly greater mean failure load than the other groups (P<.001). Coping fractures were only observed in SLOW15 group. CONCLUSION. The failure load of zirconia-ceramic crowns was significantly influenced by cooling rate as well as coping thickness. Under conventional cooling conditions, the mean failure load was not influenced by the coping thickness; however, under slow cooling conditions, the mean failure load was significantly influenced by the coping thickness.
PURPOSE. Pre-surface treatments of coping materials have been recommended to enhance the bonding to the veneering ceramic. Little is known on the effect on shear bond strength, particularly with new coping material. The aim of this study was to investigate the shear bond strength of veneering ceramic to three coping materials: i) metal alloy (MA), ii) zirconia oxide (ZO), and iii) lithium disilicate (LD) after various pre-surface treatments. MATERIALS AND METHODS. Thirty-two (n = 32) discs were prepared for each coping material. Four pre-surface treatments were prepared for each sub-group (n = 8); a) no treatment or control (C), b) sandblast (SB), c) acid etch (AE), and d) sandblast and acid etch (SBAE). Veneering ceramics were applied to all discs. Shear bond strength was measured with a universal testing machine. Data were analyzed with two-way ANOVA and Tukey's multiple comparisons tests. RESULTS. Mean shear bond strengths were obtained for MA ($19.00{\pm}6.39MPa$), ZO ($24.45{\pm}5.14MPa$) and LD ($13.62{\pm}5.12MPa$). There were statistically significant differences in types of coping material and various pre-surface treatments (P<.05). There was a significant correlation between coping materials and pre-surface treatment to the shear bond strength (P<.05). CONCLUSION. Shear bond strength of veneering ceramic to zirconia oxide was higher than metal alloy and lithium disilicate. The highest shear bond strengths were obtained in sandblast and acid etch treatment for zirconia oxide and lithium disilicate groups, and in acid etch treatment for metal alloy group.
In this study, We tried to find out the fracture strength of zirconia coping all ceramic crown and collarless porcelain fused gold alloy crown as the compared group. Each of the collarless porcelain fused gold crown and zirconia all ceramic crown has been produced specimen 10 each. And after pasting them on the steel jig, it had load given at porcelain incisal edge by 130$^{\circ}$ and measured fracture strength by Universal Testing Machine and then We have results from that. 1. The average value of fracture strength suggested 950.49 N at collarless porcelain fused gold alloy crown, 656.81 N at zirconia coping all ceramic crown. 2. Fractured pattern showed that the whole of labial part was exposed in collarless porcelain fused gold crown, but porcelain of margin part did not show fracture in advance. In the practice, the concern that collarless might cause fracture strength to be weaken does not matter, we concluded zirconia all ceramic crown made fracture that only a part of labial porcelain was fractured. The combination of zirconia all ceramic crown and turned out to be excellent.
PURPOSE. Fracture of the veneering material of zirconia restorations frequently occurs in clinical situations. The purpose of this in vitro study was to compare the fracture strengths of zirconia crowns veneered with various ceramic materials by various techniques. MATERIALS AND METHODS. A 1.2 mm, $360^{\circ}$ chamfer preparation and occlusal reduction of 2 mm were performed on a first mandibular molar, and 45 model dies were fabricated in a titanium alloy by CAD/CAM system. Forty-five zirconia copings were fabricated and divided into three groups. In the first group (LT) zirconia copings were veneered with feldspathic porcelain by the layering technique. In the second group (HT) the glass ceramic was heat-pressed on the zirconia coping, and for the third group (ST) a CAD/CAM-fabricated high-strength anatomically shaped veneering cap was sintered onto the zirconia coping. All crowns were cemented onto their titanium dies with Rely $X^{TM}$ Unicem (3M ESPE) and loaded with a universal testing machine (Instron 5583) until failure. The mean fracture values were compared by an one-way ANOVA and a multiple comparison post-hoc test (${\alpha}$= 0.05). Scanning electron microscope was used to investigate the fractured interface. RESULTS. Mean fracture load and standard deviation was $4263.8{\pm}1110.8$ N for Group LT, $5070.8{\pm}1016.4$ for Group HT and $6242.0{\pm}1759.5$ N for Group ST. The values of Group ST were significantly higher than those of the other groups. CONCLUSION. Zirconia crowns veneered with CAD/CAM generated glass ceramics by the sintering technique are superior to those veneered with feldspathic porcelain by the layering technique or veneered with glass ceramics by the heat-pressing technique in terms of fracture strength.
Journal of the Korean Academy of Esthetic Dentistry
/
v.32
no.1
/
pp.4-7
/
2023
Since the end of the 1990s, zirconia, which has been applied to dental prostheses, has been used in the form of coping or framework. The prostheses made in this way have been successfully used in the anterior teeth because they have no metal components as a structure. But in the posterior teeth, its use was limited due to the fracture or chipping of the veneering porcelain during the function. Later, as a solution to this shortcoming, a monolithic zirconia restoration was proposed in which a strong coping material was used in the form of a complete prosthesis. But, this resulted in some unesthetic results due to the characteristics of zirconia, which has excellent resistance to strong forces but is very white and opaque. However, now, due to technological advances in increasing the translucency of zirconia, it is possible to produce strong and esthetic zirconia restorations not only in the posterior region but also in the anterior region. In this article, the structural characteristics of various types of zirconia materials that have been developed so far, were discussed, and where the zirconia products actually in use belong to was explained.
Purpose: The aim of this study was to evaluate the marginal and internal gap of zirconia copings fabricated by CAD/CAM system and to research the effect of cement space on the fit of zirconia prosthesis. Methods: Zirconia copings were designed using 3shape software and then milled from presintered zirconia blocks by Kavo dental milling machine. The cement space was set at $0{\mu}m$ around the margins for all groups, and additional cement space appling 1 mm above the finish lines of tooth. The samples were classified into 4 groups according to the cement space setting(Cs-0, Cs-40, Cs-80, Cs-120). Replica technique used to investigate marginal and internal gap. The silicone film thickness was recorded using a optical microscope with image software analysis system at 75${\times}$magnification. The assessment performed on the six points in bucco-lingual and mesio-distal sections(4 groups, 10 copings per group, 12 measuring points per coping). The data were statistically analyzed with one-way ANOVA followed by pair-wise Tukey's post hoc tests(${\alpha}$<0.05). Results: Better marginal and internal fit values were exhibited by $80{\mu}m$ cement space. The results showed that different cement space values had statistically significant effect on the marginal and internal gap of zirconia copings(p<0.001). The gap of margin and axial wall area was smaller than that the gap of occlusal area in all groups(p<0.001). Conclusion : Effect of different cement spaces on the marginal and internal gap of zirconia copings.
Purpose: To evaluate the accuracy of zirconia copings in terms of clinical verified for the clinical application of CAD/CAM. Methods: Zirconia copings (n=5) were prepared using CAD/CAM system and were sintered using the relevant electrical induction furnace, which uses a 2h sintering program with a maximum temperature of $1500^{\circ}C$. The copings placed at the models and the interval values were measured. Results: The meas interval values between the die and the zirconia copings were $44.14{\mu}m$(A), $44.57{\mu}m$(B), $44.72{\mu}m$(C). 51.05 ${\mu}m$(D). Conclusion: The maximum interval values between the die and the zirconia copings were $51.3{\mu}m$ which is acceptable for clinical use. ${\mu}m$ Proper understanding of the test conditions will help enhancing the accuracy of zirconia coping.
Purpose: The aim of this study was to investigate the shear bond strength between various commercial zirconia coping and veneering ceramic, and to observe the failure mode. Methods: For each zirconia block (iJAM Emerald, LUXEN Smile block, ICE Zirkon transluzent), 10 rectangular specimens were layered with Cercon ceram kiss, IPS e.max ceram, ICE Zirkon ceramic according to recommended by the manufacturer. The shear bond strength tests of the veneering porcelain to zirconia were carried out until fracture by a universal testing machine. After the shear bond tests, failure modes were characterized visually, under a stereomicroscope, such as adhesive, cohesive, or mixed. Data were analyzed with One-way ANOVA followed by Scheffe's tests. Results: The shear bond strength ($mean{\pm}SD$) of zirconia-veneer ceramic were JC group $13.9{\pm}3.6MPa$; JE group $17.7{\pm}2.4MPa$; JI group $15.1{\pm}2.5MPa$; LC group $9.5{\pm}1.5MPa$; LE group $16.2{\pm}2.3MPa$; LI group $12.6{\pm}0.8MPa$; ZC group $16.0{\pm}2.3MPa$; ZE group $18.5{\pm}3.4MPa$; and ZI group $15.3{\pm}3.2MPa$. The One-way ANOVA showed a significant difference between groups (p<0.05). The failure mode in most experimental groups was mixed failure, except for the LC group, which showed adhesive failure, and JE group, LE group and ZE group showed cohesive failure. Conclusion: For IPS e.max ceram, the shear bond strength value was highest for all kinds of zirconia blocks. For ICE Zirkon transluzent, the shear bond strength value was highest for all kinds of veneering ceramics. Most of experimental group interfaces revealed mixed failure mode.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.