알루미늄 5083 합금의 플라즈마 미그 하이브리드 용접시 용접부 미세조직과 기계적 성질 변화에 미치는 용접조건의 영향 (Effect of welding condition on microstructures of weld metal and mechanical properties in Plasma-MIG hybrid welding for Al 5083 alloy)

  • 박상현;이희근;김진용;정하택;박영환;강정윤
    • Journal of Welding and Joining
    • /
    • 제33권1호
    • /
    • pp.61-71
    • /
    • 2015
  • The effect of welding condition on microstructure and mechanical property of Plasma-MIG Hybrid Weld between Al 5083 plates(thickness : 10mm) was investigated. 1 pass weld without any defects such as puckering, undercut, and lack of fusion was obtained by 150~200A of plasma current and 5~7mm of welding speed. Gas porosities and shrinkage porosities were existed in the weld near fusion line. As welding speed and plasma current were decreasing, the area fraction of porosity was increasing. The hardness of the weld is increasing as welding speed. On the basis of microstructural analysis, Mg segregated region near dendrite boundaries tends to increase with the welding speed. In the result of hardness test, Distribution of hardness in fusion zone showed little change with the plasma current. However, when the welding speed increased, hardness in weld metal markdly increased. It could be considered that effect of heat input to growth of the dendritic solidification structures. Based on tensile test, tensile properties of weld metal was predominated by area fraction of porosities. Consequently, tensile properties can be controlled by formation site and area fraction of porosity.

PALW을 이용한 소경 스테인리스강 튜브의 용입특성 개선 (Improvement of Penetration Characteristics by Plasma Augmented Laser Welding of Small Diameter Stainless Steel Tubes)

  • 황재련;윤석환;나석주
    • Journal of Welding and Joining
    • /
    • 제22권6호
    • /
    • pp.30-35
    • /
    • 2004
  • Laser welding is obviously an attractive method to join small, thin parts such as small stainless steel tubes, but it is very sensitive to the joint clearance and tolerance, and this makes laser welding difficult to obtain consistent welding qualities over time. Recently, Plasma Augmented Laser Welding(PALW) is being developed to solve these problems. In this study, plasma arc welding(PAW) was introduced to join conventional V-grooved butt joint of thin stainless steel strips using single laser heat source in manufacturing small stainless steel tubes. The effect of the welding speed enhancement is investigated by the experiments. Effects of welding directions, distance between the heat sources and intensity of arc heat source on the optimal welding speed was investigated. Through this research, it was confirmed that PALW process has higher welding speed and robustness than laser welding process.

고주파 전기저항 용접법에서 적정 용접조건의 수학적 모델 (Mathmetical Modeling of Welding Conditions for High Frequency Electric Resistance Welding Process)

  • 강덕일;장영섭;오주섭;공원일;김용석
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 1996년도 특별강연 및 춘계학술발표 개요집
    • /
    • pp.13-14
    • /
    • 1996
  • High Frequency Electric Resistance Welding process has been widely used in manufacturing welded steel pipes because of its high welding speed and quality. This process utilizes the skin effect as well as the proximity effect of the high frequency current in heating the skelp edge. In this study, an analytical solution of the edge temperature was obtained based on several assumptions. The assumptions includes the expontial decay of weldingcurrent from the surface and neglect of the heat loss in the welding direction. This calculation shows a good agreement with the observations made from the high speed camera. Using tile analytical model, tile heat required as a function of the welding speed and the skelp thickness was determined. These results were compared with the experimental results obtained.

  • PDF

박판 강재의 고속 심 용접성에 미치는 Sn 도금의 영향 (Effect of Tin Coating on the High Speed Seam Weldability of Thn Gage Sheet Steels)

  • 김기철;이목영
    • Journal of Welding and Joining
    • /
    • 제16권5호
    • /
    • pp.86-92
    • /
    • 1998
  • High speed wire seam weldability of tin coated thin gage sheet steels was investigated. Thickness and coating weight ranges of the test materials were 0.21~0.35mm and 1.1/1.1~2.8/11.2g/$m^2$, respectively. Test results indicated that the surface roughness value, Rz decreased as increasing the coating weight. The Rz was thought to be one of the important factors to influence the optimum welding condition range, $\triangle$Q. The $\triangle$Q showed close relationship with welding conditions such as welding pressure and travel speed. Higher welding pressure widened the $\triangle$Q while higher travel speed reduced the $\triangle$Q value. Results also demonstrated that tin coating weight should be optimized based on the weldability or the serviceability after welding. At th HAZ of sheet materials with thinner coating layer, tin depleted zone was produced since molten film of the coating material on the base metal agglomerated by the surface tension, which could result in reducing the corrosion resistance of the HAZ in the service environment.

  • PDF

용접 조건이 소형 용기용 Sn 도금 강재의 와이어 심 용접성에 미치는 영향 (Effect of Welding Parameters on Wire Seam Weldability of Tin Coated Steels for Small Containers)

  • 김기철;이기호;이목영
    • Journal of Welding and Joining
    • /
    • 제15권5호
    • /
    • pp.74-83
    • /
    • 1997
  • Effect of welding parameters such as current, speed and electrode pressure on the weld quality of tin coated steels for small containers was discussed in this paper. Welding was performed with low frequency wire seam welding system which was loaded with 1.5mm in diameter copper wire electrode. The welding parameters were monitored at the position close to the welding spot so as to minimize the instrumentation error, and the signals were stored into a digital data acquisition system before analysis. Results showed that critical current for sufficient nugget size increased as the base material thickness increased, while the width of the optimum welding range was reduced. The acceptable welding condition derived from this study was found to be effective within the thickness range of $\pm$10% of the nominal (0.25mm) thickness. Tin coating layer was proved not to affect seriously on the weld quality, i.e. strength and formability, since consumable wire electrode was used in this process. Test results also demonstrated that the welding current was thought to be the most effective parameter to form an acceptable weld, while welding speed or electrode pressure exerted less effect on the nugget formation. However, these two parameters played an important role because the former was related to the nugget overlap interval, and the latter, to the formation of expulsion during welding.

  • PDF

오스테나이트계 304 스테인리스강의 Nd:YAG 레이저 맞대기 용접특성 (Butt Welding Characteristics of Austenitic 304 Stainless Steel Using a Continuous Wave Nd:YAG Laser Beam)

  • 유영태;오용석;신호준;임기건
    • 대한기계학회논문집A
    • /
    • 제28권2호
    • /
    • pp.165-173
    • /
    • 2004
  • Laser beam welding is increasingly being used in welding of structural steels. The laser welding process is one of the most advanced manufacturing technologies owing to its high speed and deep penetration. The thermal cycles associated with laser welding are generally much faster than those involved in conventional arc welding processes, leading to a rather small weld zone. Experiments are performed for 304 stainless steel plates changing several process parameters such as laser power, welding speed, shielding gas flow rate, presence of surface pollution, with fixed or variable gap and misalignment between the similar and dissimilar plates, etc. The following conclusions can be drawn that laser power and welding speed have a pronounced effect on size and shape of the fusion zone. Increase in welding speed resulted in an increase in weld depth/ aspect ratio and hence a decrease in the fusion zone size. The penetration depth increased with the increase in laser power.

마찰 표면개질 시스템 개발 및 공정인자의 영향 평가 (Development of Friction Surface Modification System and Evaluation to the Effect of Process Parameter)

  • 천창근;장웅성;노중석;정태휘;조중선
    • Journal of Welding and Joining
    • /
    • 제24권1호
    • /
    • pp.43-49
    • /
    • 2006
  • This paper describes the friction surface modification which has been successfully developed with the friction stir welding recently There are several problems including just position control and backlash in conventional friction surface modification system. Therefore it has been developed the friction surface modification system which has been controlled precisely both position and force by driving hydraulic cylinder in this paper. The mechtrode rotation speed(N) and feeding speed(Vz), travel speed(Vx,y) are of critical importance for the width and thickness of the coating in friction surfacing process. But there is no theoretical method of determining interrelations between process parameters affect the coating width and thickness. As a result of DOE(design of experiment) with developed system, the coating thickness and width seemed to decrease according to increase the mechtrode rotation speed(N) and traveling speed(Vx,y), to decrease feeding speed(Vz) apparently. However as the result of regression analysis the main effect was only the mechtrode rotation speed in the coating thickness.

하이드로포밍용 열연 강재의 레이저 용접성 및 성형 특성 (Laser Weldability and Formability of Hot Rolled Steels for Hydroforming Applications)

  • 이원범;이종봉
    • Journal of Welding and Joining
    • /
    • 제22권6호
    • /
    • pp.19-24
    • /
    • 2004
  • The laser welding and its analysis of thin-sheet carbon steels were carried out with high power $CO_{2}$ laser. The main factor of weld quality of laser welding is gap and edge quality. This work was preformed to focus on the gap tolerance problem during laser welding. First, bead on plate welding of thin sheet was examined to investigate the effect of laser welding variables, and to obtain optimum welding condition. Butt welding was also carried out to show the effect of gap on the laser weldability of thin sheet. In order to investigate the effect of gap on formability of welded thin sheet, LDH test was caried out. At high welding speed, the partial penetration was obtained by low heat input. Otherwise, porosity was formed in the bead at low weld speed because of too much heat input. The optimum welding condition of welding was derived from bead width, penetration and hardness property. The maximum gap tolerance on laser welding was observed to be about 0.2mm. This gap size has good relationship with beam size of laser spot(about 0.3mm). The formability of welded sheet was about $80{\%}$ value of base metal and the gap size has not affected on the formability, although weld quality is dependent on the gap size.

용접 조건이 Al-7075-T651의 마찰교반용접부의 인장 특성에 미치는 영향 (Effect of Welding Condition on Tensile Properties of Friction Stir Welded Joints of Al-7075-T651 Plate)

  • 김치옥;김선진
    • 동력기계공학회지
    • /
    • 제15권2호
    • /
    • pp.61-68
    • /
    • 2011
  • This paper investigates the tensile properties of the friction stir welded joints of Al 7075-T651 aluminum plate according to the welding conditions. A 7075-T651 aluminum alloy plate with a thickness of 6.0 mm was used in this investigation. For the friction stir welding (FSW) process, a tool with shoulder diameter of 20 mm and probe diameter of 9 mm was used. The rotation speed and traverse speed conditions were changed in this study, the other welding conditions are constant. The welding direction was aligned with the material rolling direction, and dimension of the FSW plate were $250{\times}100{\times}6\;mm$. As far as this work is concerned, the optimal FSW conditions are determined as the rotation speed, 600 rpm and traverse speed 0.8 mm/sec or the rotation speed, 800 rpm and traverse speed 0.5 mm/sec.

테일러드 블랭크용 박판 강재의 레이저 용접성 (1) (Laser Weldability of Sheet steels for Tailored Blank Manufacturing(1))

  • 김기철
    • Journal of Welding and Joining
    • /
    • 제16권1호
    • /
    • pp.77-87
    • /
    • 1998
  • This paper deals with the effect of laser welding parameters on the weld formation. Thin steels for automotive application were prepared so as to be welded with high power carbon dioxide laser system. Major process parameters were position of focus and travel speed. The effect of shielding gas was also discussed by employing the high speed photometry. Test results showed that the optimal position of focus varied in accordance with the joint configuration; bead-on-plate, butt or lap welding. It was recommended that the position of focus for the lap welding be located at slightly inner part of the material to be welded. In this case, however, it was noticeable that the weld penetration ratio, d/t$_{0}$ dropped drastically at the critical region. Results also demonstrated that both the bead width and penetration reduced as the travel speed increased. The penetration ratio showed two distinct regions; stabilized zone at the lower range of the travel spped and sudden drop zone at the higher range of travel speed. Lower limit of the penetration for acceptable weld was proved to be about 90% of the parent metal thickness based on the physical properties of the weld. Mixed gas application for both the shielding of molten metal and laser induced plasma control was recommended as far as the penetration was concerned.d.