• Title/Summary/Keyword: Weld Strength

Search Result 857, Processing Time 0.025 seconds

Study on Friction Welding of Torsion Bar Material(II) - Effect of PWHT on Friction Weld Quality- (토션바재의 마찰용접에 관한 연구(II) -용접 후열처리가 마찰용접 품질에 미치는 영향-)

  • Oh, Sae-Kyoo;Lee, Jong-Du
    • Journal of Ocean Engineering and Technology
    • /
    • v.4 no.2
    • /
    • pp.244-244
    • /
    • 1990
  • This paper deals with investigating experimentally the effects of PWHT on the weld quality such as strength, toughness, hardness and micro-structure of the welded joints in friction welding of torsion bar material SUP9A bar to bar. The results obtained are summarized as follows; 1) It was certified that the condition of the post-weld heat treatment(PWHT) for the friction welded joints was very satisfactory because both strength and toughness of the joints were improved as almost same as those of the base metal or better by the PWHT. 2) The peak of hardness distribution of the friction welded joints can be eliminated by PWHT, resulting in being almost equalized at the weld interface, the HAZ(heat affected zone) and the base metal. 3) The micro-structure of the base meta., HAZ and weld interface(WI) of friction welded joints welded at the optimum welding condition consists of the same sorbite structure obtained by PWHT and fined sorbite at WI, resulting in increasing toughness as well as strength, and no micro structural defect has been found at the friction welded zone.

Mechanical Strength and Ultransonic Testing of End Cap Welds in Pressurized Heavy Water Reactor Fuel (중수로핵연료 봉단마개 용접부의 기계적 특성과 초음파 시험)

  • 이정원;최명선;정성훈;고진현
    • Journal of Welding and Joining
    • /
    • v.9 no.4
    • /
    • pp.60-68
    • /
    • 1991
  • The weld quality of end cap welds in Pressurized Heavy Water Reactor (PHWR) Fuel is extremely important for the fuel performance in the nuclear reactor. The quality of resistance upset welds is currently evaluated mainly by the metallographic examination although it reveals only two weld cross-sections in a circumference welds. This investigation was, firstly, carried out to determine whether the ultrasonic examination would be applied to detect weld defects in the end cap welds and, secondly, to measure the mechanical strength of upset butt welds as a function of phase shift percentage. The major results obtained in this study are as follows: 1. The weld current and amount of upset shrinkage linearly increased with increasing the phase shift percentage. 2. Above the phase shift 55%, the defects in the welds were completely eliminated with increasing the phase of sound weld was over the thickness of cladding tube. 3. The ultrasonic testing well detected such defects in the end cap welds as upset external crack, upset split, corner crack and irregular weld flash comparing with the results of metallography. 4. The micro-fissure in the corner of the end cap welds was reliably detected by ultrasonic testing. 5. The mechanical strength in the welds increased with increasing phase shift percentage but the fracture did't occur in the welds above 55%.

  • PDF

Effect of Heat Input and Interpass Temperature on the Strength and Impact Toughness of Multipass Weld Metal in 570MPa Grade Steel (570MPa급 용접구조용강 다층 용접금속의 강도 및 충격인성에 미치는 입열 및 패스간 온도의 영향)

  • Byun, Ji-Chul;Bang, Kook-Soo;Chang, Woong-Sung;Park, Chul-Gyu;Chung, Woo-Hyun
    • Journal of Welding and Joining
    • /
    • v.24 no.1
    • /
    • pp.64-70
    • /
    • 2006
  • 570MPa grade weldable steels were gas metal arc welded with various heat inputs and interpass temperatures using flux cored wires. Effects of heat input and interpass temperature on the strength and impact toughness of weld metal were investigated in terms of microstructural change, recovery of alloying elements, and the amount of reheated weld metal. Increase of heat input and interpass temperature resulted in decrease of weld metal strength. This is because of the small amount of acicular ferrite, large columnar size and low recovery of alloying elements such as manganese and silicon. In addition to the microstructural change, weld metal toughness was also influenced by the deposition sequence. It increased with an increase of the amount of reheated weld metal.

Study on fatigue experiment for transverse butt welds under 2G and 3G weld positions

  • Kang, Sung-Wook;Park, Yong-Man;Jang, Beom-Seon;Jeon, Yu-Chul;Kim, Seong-Min
    • International Journal of Naval Architecture and Ocean Engineering
    • /
    • v.7 no.5
    • /
    • pp.833-847
    • /
    • 2015
  • Although the transverse butt weld method with ceramic backing strip has been widely used in various industrial fields for its fabricational convenience, it is rarely used in offshore industries since the fatigue strength of the weld joint has not been proved sufficiently. This study conducted fatigue tests for series of butt weld specimens with horizontal (2G) and vertical (3G) welding positions in order to verify the fatigue strength compared to S-N curve by DNV (Det Norske Veritas), IIW (International Institute of Welding) and Eurocode 3. The difference of the 2G specimens and the 3G specimens are investigated in terms of angular distortion and the effect on the fatigue strength are analyzed.

Effects of Diffusible Hydrogen Content and Hardness on Cold Cracking in High Strength Weld Metal (고강도강 용접금속 저온균열 발생에 미치는 확산성수소량 및 경도의 영향)

  • Seo, Won-Chan;Bang, Kook-Soo
    • Journal of Ocean Engineering and Technology
    • /
    • v.26 no.2
    • /
    • pp.33-38
    • /
    • 2012
  • The effects of the diffusible hydrogen content and hardness on the cold cracking in high strength weld metal were investigated. The diffusible hydrogen contents were influenced by welding parameters such as the voltage and contact tip-to-work distance (CTWD). The diffusible hydrogen content increased with an increase in voltage. However, it was decreased with an increase in CTWD. CTWD also influenced the weld metal hardness,especially when the wire used had a higher strength than the base metal. This showed that weld metal hardness had a more powerful effect on weld metal cold cracking than the diffusible hydrogen content in this experiment.

A Study on the Weldability and the Fatigue Characteristics in Resistance pot Welding of 5182-O/6061-T6 Dissimilar Aluminum Alloy Sheets (이종 AI합금의 저항점용접부 용접성과 피로특성에 관한 연구)

  • 박진철;정원욱;강성수
    • Journal of Welding and Joining
    • /
    • v.17 no.2
    • /
    • pp.44-52
    • /
    • 1999
  • This study deals with spot weld ability of dissimilar aluminum alloy sheets in order to take advantage of its lightweight and strength. The paper also shows the relationship between weld elements(i.e. current, welding time and tip force) and weld quality on the resistance spot weld part of the same and dissimilar Al alloy. The conclusions are: (1) Because of excessive tip force, deep indentation remained at the Al 5182 side which is lower stiffness at the dissimilar Al alloy. (2) Weld quality (i.e. tensile shear strength) of dissimilar Al alloy is superior to that of the same Al 6061 alloy. (3) As long cycles, fatigue life of spot weld specimen on dissimilar Al alloy sheets was better than that of the same Al alloy.

  • PDF

Effects of Injection Conditions on the Weld Line Creation in Injection Molding (사출성형 시 성형조건이 웰드라인의 생성에 미치는 영향)

  • Kim, Young-Mo;Park, Yeong-Min;Jang, Min-Kyu;Jeong, Yeong-Deug
    • Design & Manufacturing
    • /
    • v.6 no.2
    • /
    • pp.1-5
    • /
    • 2012
  • Weld line in injection molded part is one of the defects in injection molding process. Weld line deteriorates not only appearance quality but mechanical property. In this study, ABS and PP were used as experimental materials. And weld line length, depth and strength have been examined according to the injection molding conditions. As the results of experimental studies, weld line length increased as flow rate increases for all materials. And the flow rate is most influenced to the creation of weld line length. Also weld line strength increased, as flow rate and melt temperature increase for all materials. The whole experiment results was similar to CAE analysis results.

  • PDF

A Study on the Ultrnsonic Distance Amplitude Characteristics Curve for Weld Defects Evaluation of Titanium Weld Zone (티타늄 용접부의 용접결함평가를 위한 초음파거리진폭특성곡선에 관한 연구)

  • Yi, Won;Park, Hee-Dong;Yun, In-Sik
    • Journal of the Korean Society of Safety
    • /
    • v.23 no.4
    • /
    • pp.7-12
    • /
    • 2008
  • This study proposes integrity evaluation method of weld zone in titanium using titanium distance amplitude characteristics curve(TDACC) and ultrasonic signals. For these purposes, the ultrasonic signals for porosity defects of weld zone in titanium are acquired in the type of time series data and echo strength. 4 lines in the DACC indicated damage evaluation standard of weld zone in titanium. The acquired ultrasonic signals agree fairly well with the measured results of reference block and sensitivity block(defect location, bean1 propagation distance, echo strength, etc). The proposed TDACC in this study agree fairy well with the measured results of weld zone in titanium(weld defects as porosity). The proposed TDACC in this study can be used for integrity evaluation of weld zone in titanium.

Construction of Through Transmission Scanning System for Weld Defects Detection of Rail Weld Zone (레일용접부의 용접결함검출을 위한 투과주사시스템의 구축)

  • Yun, In-Sik
    • Journal of the Korean Society of Safety
    • /
    • v.20 no.1 s.69
    • /
    • pp.30-35
    • /
    • 2005
  • This study proposes construction of through transmission for weld defects detection of rail weld zone from ultrasonic signals. For these purposes, the ultrasonic signals for defects(porosity and crack) of weld zone in rails are acquired in the type of time series data and echo strength. 6 lines in the distance amplitude characteristics curve(DACC) indicated damage evaluation standard of weld zone in rails. The acquired ultrasonic signals agree flirty well with the mesured results of reference block and sensitivity block(defect location beam propagation distance, echo strength, etc). The proposed construction of through transmission in this study can be used for weld defects detection of rail weld zone.

Effects of Injection Conditions on the Weld Line Creation in Injection Molding (사출성형시 성형조건이 웰드라인의 생성에 미치는 영향)

  • Kim, Young-Mo;Park, Yeong-Min;Jang, Min-Kyu;Jeong, Yeong-Deug
    • 한국금형공학회:학술대회논문집
    • /
    • 2008.06a
    • /
    • pp.115-119
    • /
    • 2008
  • Weld line in injection molded part is one of the defects in injection molding process. Weld line deteriorates not only appearance quality but mechanical property. In this study, ABS and PP were used as experimental materials. And weld line length, depth and strength have been examined according to the injection molding conditions. As the results of experimental studies, weld line length increased as flow rate increases for all materials. And the flow rate is most influenced to the creation of weld line length. Also weld line strength increased, as flow rate and melt temperature increase for all materials. The whole experiment results was similar to CAE analysis results.

  • PDF