X20CrMoV 12 1 강의 용접부에서의 균열진전 특성연구 (Time-dependent Crack Growth in X20CrMoV 12 1 Steel Weld joint)

  • 이남우;김광수;정용근;박종근
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.322-327
    • /
    • 2000
  • This paper investigates the time-dependent crack growth in X20CrMoV 12 1 steel weld joints. Crack growth test are carried out $545^{\circ}C$ on side-grooved 1/2T CT specimens under static loads. A simulated material is produced for the intercritical HAZ, where fracture normally occurs. Constitutive properties are obtained for the simulated HAZ material as well as for the base metal and weld metal. Finite element analyses of crack growth are performed on the models with and without a HAZ layer, using the experimental crack length-time history. The inclusion of HAZ layer increase the load line velocities significantly. The crack growth rates are correlated reasonably well with $C^*$. The smallest crack size for the validity of $C^*$ is found much smaller than the ASTM crack initiation size for 1T CT specimen of creep ductile materials.

  • PDF

차체구조용 SCPI 강도부재의 점용접간격이 압궤특성에 미치는 영향 (Influence of Spot Weld Pitches on Collapse Characteristics of SCPI Vehicle Members)

  • 차천석;박제웅;양인영
    • Journal of Welding and Joining
    • /
    • 제20권6호
    • /
    • pp.78-78
    • /
    • 2002
  • Front-side members are structures with the greatest energy absorbing capability in a front-end collision of vehicles. This paper was performed to analyze initial collapse characteristics of spot welded hat and double hat-shaped section members, which are basic shape of side members, on the shift of flange weld pitches. The impact collapse tests were carried out by using home-made vertical air compression impact testing machine, and impact velocity of hat-shaped section members is 4.17m/sec and that of double hat-shaped section members is 6.54m/sec. In impact collapse tests, the collapsed length of hat-shaped section members was about 45mm and that of double hat-shaped section members was about 50mm. In consideration of these condition, axial static collapse tests(0.00017m/sec) of hat and double hat-shaped section members were carried out by using UTM which was limited displacement, about 50mm. As the experimental results, to obtain the best initial collapse characteristics, it is important that stiffness of vehicle members increases as section shapes change and the progressively folding mode induces by flange welding pitch.

차체구조용 SCP1 강도부재의 점용접간격이 압궤특성에 미치는 영향 (Influence of Spot Weld Pitches on Collapse Characteristics for SCP1 Vehicle Members)

  • 차천석;박제웅;양인영
    • Journal of Welding and Joining
    • /
    • 제20권6호
    • /
    • pp.802-808
    • /
    • 2002
  • Front-side members are structures with the greatest energy absorbing capability in a front-end collision of vehicles. This paper was performed to analyze initial collapse characteristics of spot welded hat and double hat-shaped section members, which are basic shape of side members, on the shift of flange weld pitches. The impact collapse tests were carried out by using home-made vertical air compression impact testing machine, and impact velocity of hat-shaped section members is 4.17m/sec and that of double hat-shaped section members is 6.54m/sec. In impact collapse tests, the collapsed length of hat-shaped section members was about 45mm and that of double hat-shaped section members was about 50mm. In consideration of these condition, axial static collapse tests(0.00017m/sec) of hat and double hat-shaped section members were carried out by using UTM which was limited displacement, about 50mm. As the experimental results, to obtain the best initial collapse characteristics, it is important that stiffness of vehicle members increases as section shapes change and the progressively folding mode induces by flange welding pitch.

사출성형 해석을 이용한 게이트 위치 최적화 (Optimization of Gate Location Using Computer-Aided Injection Molding Analysis)

  • 문종신
    • 한국산학기술학회논문지
    • /
    • 제15권10호
    • /
    • pp.5968-5973
    • /
    • 2014
  • 게이트 위치는 제품 품질 및 생산성 등에 큰 영향을 미치기 때문에 사출성형에 있어서 게이트 위치를 결정하는 것은 대단히 중요하며 이를 위하여 사출성형 CAE가 적용되고 있다. 사출성형 해석의 증가와 3차원 유한요소의 사용은 더 많은 계산 시간을 필요로 하게 되면서, 컴퓨터 자원을 적게 사용하면서도 빠른 시간 내에 게이트 위치 최적화를 수행하는 것은 중요한 이슈가 되었다. 본 논문에서는 유동 균형과 웰드라인을 고려하기 위하여 유동 거리에 기반한 최적화 기법을 제시하였다. 그리고 원판 형상의 모델에 적용하여 웰드라인이 응력집중이 예상되는 슬릿홀을 피하면서도 유동 균형을 유지하는 결과를 도출하였다.

반복 인장 하중을 받는 YP47 극후판 Butt 용접부의 잔류응력 재분포에 관한 연구 (A Study on Evaluation of Residual Stress Redistribution for FCA Butt Weldment of Ultra-Thick YP47 Steel Plate under Tensile Cyclic Load)

  • 강봉국;이동주;신상범
    • Journal of Welding and Joining
    • /
    • 제34권4호
    • /
    • pp.28-33
    • /
    • 2016
  • The purpose of this study is to evaluate the redistribution of transverse residual stress in the multi-pass FCA butt weld of YP47 in the hatch coaming top plate of ultra large size containership under the tensile cyclic load. In order to do it, the configuration of modified H type specimen including restraint length was first designed to simulate the restraint condition of the butt weld in hatch coaming top plate. FE analysis procedure for evaluating the transverse residual stress was verified by comparing the calculated mean and surface residual stresses with the measured results in the test specimen. After that, the effect of the cyclic load on the redistribution of transverse residual stress was evaluated by comprehensive FEA. From the results, it was found that although the maximum transverse residual stress decreased with an increase in the applied maximum load, the effect of the cyclic load on the mean residual stress is small enough to be negligible. It is because the maximum stress of the ship corresponding to the probability of 10E-8 is less than 70% of yield stress of the weld.

Influence of geometry and safety factor on fatigue damage predictions of a cantilever beam

  • Pecnik, Matija;Nagode, Marko;Seruga, Domen
    • Structural Engineering and Mechanics
    • /
    • 제70권1호
    • /
    • pp.33-41
    • /
    • 2019
  • The influence of two parameters on fatigue damage predictions of a variably loaded cantilever beam has been examined. The first parameter is the geometry of the cantilever beam and the weld connecting it to a rear panel. Variables of the geometry examined here include the cantilever length, the weld width on the critical cross-section and the angle of the critical cross-section. The second parameter is the safety factor, as set out by the Eurocode 3 standard. An analytical approach has been used to calculate the stresses at the critical cross-section and standard rainflow counting has been used for the extraction of the load cycles from the load history. The results here suggest that a change in the width and angle of the critical cross-section has a non-linear impact on the fatigue damage. The results also show that the angle of the critical cross-section has the biggest influence on the fatigue damage and can cause the weld to withstand fatigue better. The second parameter, the safety factor, is shown to have a significant effect on the fatigue damage calculation, whereby a slight increase in the endurance safety factor can cause the calculated fatigue damage to increase considerably.

금형온도가 사출성형품의 웰드라인과 치수안정성에 미치는 영향에 관한 연구 (Effects of Mold Temperature on the Weldline and Dimensional Stability of Injection-molded Parts)

  • 김동학;이재원;김태완
    • 한국산학기술학회논문지
    • /
    • 제4권3호
    • /
    • pp.172-176
    • /
    • 2003
  • 본 논문은 금형의 온도 변화가 사출성형품의 미시구조에 미치는 영향에 관해 연구했다. 웰드라인의 폭과 길이는 금형온도가 증가함에 따라 모두 감소되었다 그리고 금형의 온도에 따른 결정성수지인 PP(Polypropylene)와 비결정성수지인 PS(Polystyrene)의 치수안정성에 관해 연구했다. PS성형품은 금형온도가 높을수록 수축률이 줄어들고, 두께 편차가 적어졌고, PP성형품의 경우에는 결정의 생성으로 인해 상반된 경향이 나타났다. 캐비티의 충전성과 전사성은 금형온도가 높을수록 향상되었다.

  • PDF

신소재 금형펀치의 이종재 마찰용접 개발과 AE품질평가를 위한 연구 (Friction Welding of Dissimilar Press Punch Materials and Its Evaluation by AE)

  • 오세규;박일동;이원석
    • Journal of Welding and Joining
    • /
    • 제15권2호
    • /
    • pp.43-53
    • /
    • 1997
  • The complete joining method for dissimilar press punch materials and its real-time evaluation method is not available at present. Brazing method has been used for joining them, but it is known that the welded joint by the brazing has the lower bonding efficiency and reliability than the diffusion welding. The friction welding with a diffusion mechanism in bonding was applied in this study. This work was carried out to determine the proper friction welding conditions and to analyze mechanical properties of friction welded joints of sintered carbide tool materials (SKNM50 for the blade part of press punch) to alloy steel (SCM440 for the shank part of press punch) using aluminum (A6061 for the interlayer material) as an insert material between the sintered carbide tool materials and the alloy steel. In addition, acoustic emission test was carried out during friction welding to evaluate the weld quality.

  • PDF

박판 단속 Fillet 용접부의 변형 특성에 관한 연구 (A Study on the Welding Distortion at the FCA Intermittent Fillet Weldment of Thin plate)

  • 신대희;신상범;이주성
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2006년 추계학술발표대회 개요집
    • /
    • pp.51-53
    • /
    • 2006
  • The purpose of this study is to establish the predictive equation of angular distortion and longitudinal shrinkage force at the intermittent fillet weldment using FEA and experiment. The angular distortion and shrinkage force of the intermittent fillet weldment linearly increases with an increase in the ratio of weld length(Lw) to weld span(Ls). Based on the results, The predictive equation of distortion at the intermittent fillet weldment was defined as a linear function of Lw/Ls and the predictive equation of the distortion for continuous fillet weldment.

  • PDF

사각통 드로잉시 테일러드 블랭크의 용접선이동 및 성형성에 관한 연구 (A Study on the Weldline Movement and Formability of Tailored Blanks in Square Cup Drawing)

  • 박석완
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 1997년도 춘계학술대회논문집
    • /
    • pp.42-45
    • /
    • 1997
  • Weldline movement of tailored blanks originates from two sources, primary and secondary. Primary movement occurs by geometrical reason, that is, just scratched lines on the no-weld blanks move during drawing to be fitted to geometrical change. Secondary movement is induced by the characteristics of tailored blanks itself. The primary movement was mainly dependent on the weldline location and not affected by the type of material. The secondary movement caused by laser welding and/or small strength difference in this study was not dominant compared with primary movement. The formability of tailored blanks always inferior to those of original blanks. This is due to the existence of hardened weld bead. The closer a weldline is to punch corner where drawing is most active, the worse its formability becomes. This is because the weldline prohibits the drawing process. It was confirmed by measuring diagonal length at the blank corner. The mode of fracture was changed form wall break to draw break when the weldling was close to the punch corner.

  • PDF