• 제목/요약/키워드: Weld Length

검색결과 187건 처리시간 0.019초

AZ61 필러 와이어를 첨가한 AZ31B-H24 마그네슘 합금의 레이저 용접 (Laser Welding of AZ31B-H24 Mg Alloy with AZ61 Filler Wire)

  • 류충선;방국수;이목영;장웅성
    • Journal of Welding and Joining
    • /
    • 제26권6호
    • /
    • pp.54-58
    • /
    • 2008
  • Laser welding with AZ61 filler wire was carried out to improve formability though reduction of porosity and formation of under fill bead. Optimum welding condition and mechanical properties of butt joint for $400{\times}500{\times}1.3mm$ magnesium sheets were studied. Optimal welding conditions of laser power, welding speed, and defocusing length are 1000W, 3m/min, and 2mm, respectively. Results of tensile test indicated that both tensile strength and elongation of specimens welded with filler wire were improved at room temperature because of reduction of porosity and under-filled bead formation in addition to the precipitation hardening and microstructure refinement by Al-Mn and Mg-Al-Zn precipitates. At elevated temperature of $200{\sim}350^{\circ}C$, fracture location of tensile specimen was shifted from weld metal to base metal, indicating less softening of weld metal than base metal.

다균열 간섭, 합체, 성장이론을 고려한 십자형 필렛용접 이음부의 피로균열진전수명 평가 (Fatigue Life Estimation of Cruciform Welded Joint Considering Interaction, Coalescence and Growth of Multi-crack)

  • 한정우;한승호;신병천;임전;김재훈
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2004년도 춘계학술대회
    • /
    • pp.120-125
    • /
    • 2004
  • Fatigue life of welded joints are governed by the propagation of multiple collinear surface cracks distributed randomly along weld bead. These cracks propagate in mutual interaction and coalescence of them. To estimate the fatigue life, the influences of above two mechanisms on the fatigue life should be taken into account. These two mechanisms appear through the stress intensity factors disturbed mutually. However, it is difficult to calculate the stress intensity factors of multiple surface cracks located in vicinity of weld toe. The stress intensity factors are calculated normally by using the Mk-factors, but such Mk-factors are very rare in literature. In this study, the Mk-factors were obtained from a parametric study on crack length and depth, in which a finite element method is used. A fatigue test for a cruciform welded joint was conducted. The fatigue life of the tested specimen was estimated through present method with the informations obtained from the test, e.g. the number, size and locations of the cracks. The estimated and measured fatigue life showed a good agreement.

  • PDF

경량화 피스톤 로드에 사용되는 SM45C/SM45C-Pipe의 마찰용접시 업셋압력이 미치는 영향 (Effect of Upset pressure on weldability in the Friction Welding of SM45C-Solid and SM45C-Pipe which is used in the Piston-Rod)

  • 민병훈;최원용;민택기
    • 한국공작기계학회논문집
    • /
    • 제17권5호
    • /
    • pp.36-43
    • /
    • 2008
  • This research is tendencious to manufacture solid piston-rod of shock absorber as hollow piston-rod using friction welding. The SM45C has been welded to the SM45C-pipe in order to investigate the effect of upset pressure on friction weldability. The friction time and upset pressure was variable conditions under the conditions of spindle revolution of 2,000rpm, friction pressure of 55MPa, and upset time of 2.0seconds. Under these conditions, the microstructure of weld interface, tensile fracture surface and mechanical tests were studied of friction weld, and so the results were as follows. When the upset pressure is sufficient, gets the high tensile strength. The optimal welding conditions were n=2,000rpm, $P_1$=55MPa, $P_2$=95MPa, $t_1$=1.5sec, $t_2$=2.0sec when the total upset length is 4.5mm.

레이저 용접 판재의 U-벤딩시 스프링백 특성에 관한 연구 (Springback Characteristics of Tailor-Welded Strips in U-bending)

  • 장성호;신장모;서대교
    • 소성∙가공
    • /
    • 제12권5호
    • /
    • pp.440-448
    • /
    • 2003
  • Sheet or plate bending is one of the most important industrial metal forming processes. Considerable attention has been focused on gaining a better understanding of bending characteristics. One of defaults in bending process is the springback. In this study, the springback characteristics of tailor-welded strips in U-bending process was investigated. Furthermore, effect of the process variables such as the geometry of the tools, thickness combination of workpiece, and welding prcoessing on springback were experimentally clarified. First, tailor-welded strips are joined by the laser welding process and consisted of two types of thickness combinations of the SCPl sheet, $0.8t{\times}1.2t$ and $0.8t{\times}1.6t$ to investigate the effect of different thickness combination on the springback. Secondly, two different directionly welded strips, one was welded along the centerline of the strip-width and the other was along the centerline of strip-length, were adopted to compare the effects of the location of weld line on the springback. Some cases of the experimental results were compared to the results simulated by using a commercial FEM code, PAM-STAMP and the theoretical results using the springback formula as well.

테일러드블랭크 용접을 위한 전단 공정 연구 (A Study on Mechanical Shearing Process for Tailored Blank Welding)

  • 유병길;이경돈
    • Journal of Welding and Joining
    • /
    • 제17권2호
    • /
    • pp.66-75
    • /
    • 1999
  • Weld bead quality in tailored blank(TB) is critically affected by edge preparation of sheets. The edge quality of prepared sheets for TB can be classified into straightness and the cross section quality of sheared plane such as a ratio of shear face, shear plane angle, etc. In order to have a good edg quality for butt-welding sheets, precision shearing will be recommended. In this paper, the feasibility of a conventional mechanical shearing as the edge preparation for tailored blanks is studyied. It reveals that fine shearing may not be the unique solution as it is generally accepted. To obtain the good shearing condition with a conventional mechanical shearing, experiments were carried out using Tahuchi method. The major parameters affecting a sheared contour are the clearance between upper blade and lower blade, and shear angle. The optimal shearing condition yields a very good straightness along the entire length of the cut, which gives a butt joint gap less than 10% of the base material thickness. The good cross section of sheared plane is also achieved in the optimal shearing condition such as a ratio of the shear face above 65%, a cross section's shear plane angle above 85%, little burr, which is providing finally good weld beads.

  • PDF

60kgf/$\textrm{mm}^2$급 자동차 범퍼빔용 레이저 용접 튜브 제조기술 및 장치연구 (Production of Laser Welded Tube for Automobile Bumper Beam from 60kgf/$\textrm{mm}^2$Grade Steel Sheet)

  • 서정;이제훈;김종수;김정오;강희신;이문용;정병훈
    • 한국정밀공학회지
    • /
    • 제21권7호
    • /
    • pp.136-144
    • /
    • 2004
  • Optimal process and system to produce the laser welded tube for one body formed bumper beam are studied. The calculated size of tube is a thickness of 1.4mm, diameter of 105.4mm and length of 2000mm. The tube is shaped from a cold rolled high strength steel sheet(tensile strength: 60kgf/$\textrm{mm}^2$ grade). Two roll bending method is the optimal tube shaping process compared to UO-bending, bending on press brake, multi-step continuous roll forming and 3 roll bending methods. Weld quality monitoring and seam tracking along the butt-joint lengthwise to the tube axis are also studied. The longitudinal butt-joint is welded by the $CO_2$ laser welding system equipped with a seam tracker and plasma sensor. The constructed $CO_2$laser tube welding system can be used for the precision seam tracking and the real-time monitoring of weld quality. Finally, the obtained laser welded tube can be used for one-body formed automobile bumper beam.

MIAB용접에서 코일에 의한 자속밀도 분포의 수치적 해석에 관한 연구 (A Study on the Numerical Analysis of Magnetic Flux Density by a Solenoid for MIAB Welding)

  • 최동혁;김재웅
    • 한국정밀공학회지
    • /
    • 제18권12호
    • /
    • pp.73-81
    • /
    • 2001
  • The MIAB welding uses a rotating arc as its heat source and is known as an efficient method fur pipe butt welding. The arc is rotated around the weld line by the electro-magnetic force resulting from the interaction of arc current and magnetic field. The electro-magnetic force is affected by magnetic flux density, arc current, and arc length. Especially, the magnetic flux density is an important factor on arc rotation and weld quality. This paper presents a 2D finite element model for the analysis of magnetic flux density in the actual welding conditions. The magnetic flux density is mainly dependent on gap between two pipes, the position of coil from gap center, exciting current, and relative permeability. Thus, the relations between magnetic flux density and main factors were investigated through experiment and analysis. Experiments were performed for the steel pipes(48.1mm O.D and 2.0mm thickness). The analysis results of magnetic flux density reveal that it increases with increasing exciting current, increasing relative permeability, decreasing distance from gap center to coil, and decreasing gap size. It is considered that the results of this study can be used as important data on the design of coil system and MIAB welding system.

  • PDF

GTA-GMA 하이브리드공정에 따른 자동차용 아연도금강판의 용접부 기공감소 (II) - 하이브리드공정 적용 결과 (Porosity Reduction during Gas Tungsten Arc-Gas Metal Arc Hybrid Welding of Zinc Coated Steel Sheets (II) - Hybrid Welding Results)

  • 안영남;김철희
    • Journal of Welding and Joining
    • /
    • 제34권4호
    • /
    • pp.48-54
    • /
    • 2016
  • The use of Zn coated steel has increased in the automotive industry due to its excellent corrosion resistance. Conventionally the BIW(body-in-white) structure and the hang-on parts have been made of Zn coated steel and more recently Zn coated steel began to be applied in the chassis parts. During gas metal arc (GMA) welding of the chassis part, lap fillet joint used to be adopted but spatter generation and porosities are most important concerns. In the industrial applications, an intentional joint gap was made to avoid the weld defects but it is not easy to control the size of joint gap. In this research, gas tungsten arc (GTA) is combined with GMA welding where GTA precedes GMA. As pulsed arc was adopted as GMA, GTA was oscillated along the longitudinal direction by pulsing GMA, but the arc oscillation did not disturb the molten droplet transfer of GMA welding. By increasing the distance between GTA and GMA, the length of weld pool increased and porosity could be reduced. Moreover porosity in the welds was fully removed when the distance between two arcs was 15 mm.

FCAW에서 용접금속 확산성수소량에 미치는 용접변수 영향의 정량적 해석 (Quantitative Analysis on the Effects of Welding Parameters on Diffusible Hydrogen Contents in Weld Metal Produced by FCAW Process)

  • 한동우;방국수;정홍철;이종봉
    • Journal of Welding and Joining
    • /
    • 제28권2호
    • /
    • pp.54-59
    • /
    • 2010
  • The effects of welding parameters such as contact tip-to-work distance (CTWD), voltage, and current on the weld metal diffusible hydrogen contents (HD) were investigated and rationalized by the calculation of heating time and amount of heat generated in the extension length of flux cored wire. As CTWD increased from 15 to 25mm, HD decreased from 8.46 to 5.45mL/100g deposited metal. Calculations showed that, with an increase of CTWD, the amount of heat generated increased from 46 to 92J in addition to an increase of heating time. Increase of current from 250 to 320A, however, gave little variation of HD. It showed that no significant change in the amount of heat generated was found, and heating time was decreased with an increase of current. It also showed that CTWD is more influential than voltage in relatively lower heat input ranges, while voltage is more in higher input ranges

탄소강 용접접합부의 모재블록전단내력에 관한 실험적 연구 (An Experimental Study on Block Shear Strength of Carbon Steel Fillet Welded Connection with Base Metal Fracture)

  • 이화영;황보경;이후창;김태수
    • 대한건축학회논문집:구조계
    • /
    • 제34권1호
    • /
    • pp.11-18
    • /
    • 2018
  • An experimental study on the ultimate behaviors of the mild carbon steel (SPHC) fillet-welded connection is presented in this paper. Seven specimens were fabricated by the shielded metal arc welding (SMAW). All specimens failed by typical block shear fracture in the base metal of welded connections not weld metal. Block shear fracture observed in the base metal of welded connection is a combination of single tensile fracture transverse to the loading direction and two shear fractures longitudinal to the loading direction. Test strengths were compared with strength predictions by the current design equations and suggested equations by previous researchers. It is known that current design specifications (AISC2010 and KBC2016) and Oosterhof & Driver's equation underestimated overly the ultimate strength of the welded connection by on average 44%, 31%, respectively and prediction by Topkaya's equation was the closest to the test results. Consequently, modified equation is required to be proposed considering the stress triaxiality effect and material property difference on the block shear strength for base metal fracture in welded connections fabricated with mild carbon steel.